The effect of sulfur content on weld penetration in austenitic stainless steel orbital tube welds
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Provide material solutions to enabling design, construction, licensing and operation of advanced reactors Including Fast Reactors, Gas-cooled Reactors and Molten Salt Reactors (solid or liquid fuel) Could be of modular or micro designs, and from hundreds of MWe to kWe Provide technical bases needed for design and licensing of advanced reactor components Develop & validate improved high temperature design methodology Provide qualification data (to NQA-1 or equivalent) on structural materials Utilize consensus standards when appropriate (e.g., ASME, ASTM, etc.) Target resolution of issues needed for near to mid-term deployment of advanced reactors
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Understanding the progression of irradiation-induced defects in real materials and alloys requires insight into the interaction between point defects, defect clusters, and the existing microstructure. This is particularly true when it comes to additively manufactured (AM) materials with complicated microstructures and residual stresses. In this work, we employ molecular dynamics (MD) to simulate the creation of point defects via primary radiation damage modeling and point defect interactions with extended defects such as voids and dislocations using simplified but representative alloy compositions. We analyze the effect of alloying elements on the formation energies of the defect clusters and measure interactions such as sink strengths and binding energies. This study provides insight into the unique behaviors of irradiation damage in AM materials and information necessary to bridge the gap in length and time scales to connect the atomistic behavior of defects to longer length scale simulations such as cluster dynamics.
Explore the source record for details and available documents.
The carburizing supercritical CO 2 (sCO 2 ) environment limits the use of lower cost steels in the lower temperature (450–650°C) portions of the sCO 2 Brayton cycle because of concerns about internal carburization and embrittlement. Results on a ferritic–martensitic steel and conventional and advanced austenitic steels at 450–650°C in 30 MPa sCO 2 with and without 1% O 2 and 0.1% H 2 O additions have indicated that sCO 2 environments will have lower maximum operating temperatures compared to steam plants. Pack Al and Cr coatings were evaluated at 650°C on T91 and 316H substrates and showed some benefit for up to 2000 h at 650°C, especially without impurities. However, characterization indicated Al 2 O 3 was not formed and Cr-rich carbides formed in the Cr coatings. With the addition of impurities in the sCO 2 , the coatings were less protective at 650°C. Subsequent exposures at 600°C in sCO 2 showed similar behavior. Postexposure evaluations included measuring the bulk C content and room temperature tensile properties. Finally, improvements were indicated but the tensile results were complicated by the high temperature pack coating process affecting the substrate properties.
Supercritical CO2 (sCO2) power cycles, particularly direct-fired cycles, have the possibility of revolutionizing clean fossil energy. However, in the lower temperature sections of the cycle, lower cost steels are needed in order to lower the cost of the sCO2 technology. Representative 9 and 12%Cr steels and conventional and advanced austenitic steels are being evaluated at 450-650°C using mass change, bulk carbon (C) content and room temperature tensile properties to determine the maximum use temperatures for both direct- and indirect-fired sCO2 cycles. After 1000 h exposures in research grade (RG) sCO2 at 300 bar and RG sCO2 with 1% O2 and 0.1% H2O additions, the results suggest that increasing the Cr content from 9 to 12% yielded no signficant benefit under these conditions but the higher Cr and Ni contents in S31025 provided better compatibility in RG sCO2 at 650°C but limited benefit at 550°C with impurities. For S31609, the formation of Fe-rich oxide after exposure to RG sCO2 at 650°C resulted in both an increase in the bulk C content and a large drop in room temperature ductility. The evidence suggests thin, protective oxides prevented C ingress in these conditions.
Direct-fired supercritical CO2 (sCO2) power cycles are being commercialized to revolutionize fossil energy as a low-emission power source. However, the cycle will increase O2 and H2O in the sCO2 and the implications of these additions have not been fully studied, particularly for lower cost steels that are needed in the lower temperature segments of the plant. Representative 9 and 12%Cr ferritic-martensitic (FM) steels and conventional and advanced austenitic steels were evaluated at 450-650°C to determine the maximum use temperatures in sCO2 with 1%O2 and 0.1%H2O at 300 bar. Compared to research grade (low impurity) sCO2 in indirect-fired cycles, the mass gains and scale thickness were not significantly changed for FM steels: both formed thick duplex Fe-rich scales. For stainless steels, higher mass gains were observed in all cases with increased Fe-rich oxide nodule formation. After 1000h at 650°C, the measured bulk C content was high for all of the steels with the addition of impurities suggesting a lower maximum operating temperature for steels. The post-exposure impact of the environment on room temperature tensile properties also will be discussed.
We measured the austenitic FeCr18Ni12.5 stainless steel Hugoniot as a function of crystallographic direction to approximately 60 GPa. We shock-compressed FeCr18Ni12.5 samples oriented along $\langle$100$\rangle$, $\langle$110$\rangle$, and $\langle$111$\rangle$ to mean stresses ranging 30.5–58.1 GPa via Ta plate impact in a large-bore powder gun and measured the free-surface velocities with laser interferometry. We unambiguously observed the largest post-shock free-surface velocity along $\langle$100$\rangle$ in each experiment, which consequently produced the lowest shock velocity along that orientation. However, the propagation of experimental uncertainties through the impedance matching scheme used to compute the shock velocity produced sufficient uncertainty overlap to preclude definitive conclusion of Hugoniot anisotropy.
In recent years, interest in increasing the efficiency of power plants based on steam generation has led to the need to develop and qualify materials capable of operating at steam temperatures and pressures significantly higher than those employed in current power plants. The overall focus of this international program is on using ferritic-martensitic steels to the maximum possible temperature, before switching to austenitic steels and/or Ni-based alloys. The relatively low Cr content of these alloys raises concerns regarding their resistance to steam oxidation at these higher temperatures. Earlier work in this collaboration addressed the reliability of data from atmospheric pressure, laboratory-based steam oxidation tests. This raised issues regarding how representative the laboratory-grown oxides were compared to those formed on service-exposed material and how the tests could be made more reliable by introducing added complexity. In general laboratory-scale exposures are conducted under isothermal conditions at ambient or slightly elevated pressure, using a relatively low flow rate of steam. The coupons used in these tests are normally flat cuboids which have been ground to homogenise the surface and remove any pre-existing features. However, there is a concern that these samples and exposures are not representative of service conditions, and so it is necessary to quantify the influence of transient conditions, such as heat flux, pressure and sample geometry/surface conditions. To address such concerns a new collaborative program of work was initiated to determine the influence of these added features on oxidation kinetics and oxide scale morphology. The overall aim was to improve the understanding of alloy performance in ultrasupercritical (USC) steam conditions and qualify suitable test procedures.
The use of transition metal carbides is reported for use as a hydrogen trapping mechanism for ferritic and austenitic steel materials. The program combined computational modeling and simulations to guide experiments towards candidate metal carbide traps, both for interfacial and interior trapping. It was found that interfacial trapping is less effective than interior trapping, with the group IVB transition metal carbides being the most effect internal traps with a loss of carbon. The sub-stoichiometric rocksalt structure accommodate the hydrogen atoms in its octahedral interstices. Using percolation theory, carbon loss of approximately 25% or more was sufficient to ensure an interconnected network of vacancies for such trapping from the surface to the internal sites within the carbide. Using this as a guide, the program developed a means to provide a uniform dispersion of ZrC nanoparticles with either Fe or 304L micron-scale powders which was then consolidated by direct current sintering. Electrolytic hydrogen diffusivity studies confirmed the reduction of hydrogen diffusion in the matrix with increasing ZrC content, which was a linear response over the sample range studied (0.01 to 1.0 wt.%). The consolidated material was micro-tensile tested in either a non-hydrogen or hydrogen charge condition and compared to a control with no carbides. Additions up to 0.05 wt.% ZrC increased the yield strength with no loss in ductility in either the non-hydrogen or hydrogen tested condition. ZrC concentrations above this amount further increased the yield strength at the expense of ductility. While these samples had a lower absolute ductility value prior to failure, the relative change in ductility between the non-hydrogen and hydrogen charge states was less for the carbides than that of the control. Metal-rich ZrC nanoparticles were fabricated through a conformal coating process yielding ZrC0.66 particles that were then incorporated into a metal matrix. Notch fatigue testing in a hydrogen environment was conducted where the number of cycles to failure was found to be less in the control than that of the carbide addition. However, the spread in experimental data and the number of samples tested limits a conclusive outcome based on defects noticed in the gauge section of all the powder processed samples. The collective outcomes of this report provide further insight into the mechanisms by which carbides act as hydrogen traps; a means to process such carbides through powder metallurgy; and their associated mechanical performance in either a non-hydrogen or hydrogen-charged condition.
A modified cage plasma nitriding technique is used to coat a Ni film onto a 316L substrate as a protective layer for austenitic steels in molten fluoride salts. The coating is achieved by deposition of Ni atoms sputtered from a Ni cage with a 316L substrate floated at the same potential as the cage to reduce plasma sputtering on the substrate. The Ni coating is porosity-free and precipitation-free and forms a γ-(Fe, Ni) phase due to interdiffusion from the substrate. Beneath the interdiffusion layer exists a thick γ-phase layer mainly affected by long-range nitrogen diffusion along the grain boundary. This layer develops grain boundary Cr nitride precipitates. Ion irradiation on the polished cross-section of the plasma-treated sample shows no void swelling in the surface-deposited Ni layer, very limited void formation in N diffusion layer, and significant void swelling in bulk unaffected by nitrogen. The studies demonstrate the feasibility of the technique for Ni coating and show good swelling resistance of the coating layer and N diffusion-affected layer. Mechanisms are discussed in this paper.
In searching for new working fluids for power generation, supercritical CO 2 (sCO 2 ) offers some attractive features for efficient cycles. However, compatibility with structural alloys is a concern. NiCr-based alloys have excellent compatibility at 600°-800°C at 20-30 MPa sCO 2 . However, conventional steels have restrictions in temperature because of carburization and accelerated oxidation in sCO 2 , similar to observations in CO 2 . To assess the impact of carburization on steel mechanical properties, small (25mm long) dogbone tensile bars are being exposed and tested after exposure at 450°-650°C. Only highly alloyed advanced austenitic steels are resistant to carburization at 650°-750°C, suggesting that Crrich oxide scales are good barriers to C ingress. Above 800°C, it is only possible to conduct subcritical evaluations at this time, but initial results suggest most conventional high-temperature Fe- and Ni-based alloys are more rapidly degraded by CO 2 at higher temperatures. Coatings are a potential solution that require more study.
Supercritical CO2 (sCO2) power cycles, particularly direct-fired cycles, have the possibility of revolutionizing clean fossil energy with peak temperatures above 700 °C and wrought precipitation strengthened alloys like Haynes 282™ for structural components. At temperatures <650 °C, it would be desirable to use less expensive alloys, however, steels are known to be susceptible to carburization. Laboratory 300 bar sCO2 autoclave results were collected on a range of alloys including less expensive Ni-based alloys like 825 compared to advanced austenitic steels like alloy 709 at 600 °C. Both alloys 825 and 709 formed thin, protective Cr-rich oxides after 1,000 h. Alloy 825 also was exposed for 1,000 h in sCO2 at 800 °C and compared to a range of Ni-based alloys. Comparing alloys 625, 825, and 282, the mass gain increased with increasing alloy Ti content under these conditions. High Al superalloys did not perform significantly better under these conditions at 800 °C.