Use of LEED, Auger emission spectroscopy and field ion microscopy in microstructural studies.

The studies reported were conducted to gain a fundamental understanding of adhesion and dynamic friction on an atomic or microscopic level. Fundamental aspects of low energy electron diffraction (LEED), Auger emission spectroscopy (AES), and field ion microscopy (FIM) are discussed. Typical results of studies conducted are considered, giving attention to LEED-AES experiments, pin and disk experiments, and field ion microscope investigations.

Ferrante, J.↗

Auger electron spectroscopy study of initial stages of oxidation in a copper - 19.6-atomic-percent-aluminum alloy

Auger electron spectroscopy was used to examine the initial stages of oxidation of a polycrystalline copper - 19.6 a/o-aluminum alloy. The growth of the 55-eV aluminum oxide peak and the decay of the 59-, 62-, and 937-eV copper peaks were examined as functions of temperature, exposure, and pressure. Pressures ranged from 1x10 to the minus 7th power to 0.0005 torr of O2. Temperatures ranged from room temperature to 700 C. A completely aluminum oxide surface layer was obtained in all cases. Complete disappearance of the underlying 937-eV copper peak was obtained by heating at 700 C in O2 at 0.0005 torr for 1 hr. Temperature studies indicated that thermally activated diffusion was important to the oxidation studies. The initial stages of oxidation followed a logarithmic growth curve.

Ferrante, J.↗

Sliding of poly(vinyl chloride) on metals studied by Auger electron spectroscopy

The sliding of polyvinyl chloride on nickel, iron and S-Monel has been studied by Auger electron spectroscopy. Polymer was not transferred to the metals, rather shear appeared to take place at the interface. The metal was progressively chlorinated as the polymer made multiple passes on the surface. The thickness of this chlorine film was the order of one atomic layer. Electron-induced desorption studies indicate that the chlorine is chemisorbed to the metal. These results are interpreted as evidence for mechanically induced and/or thermal degradation of the polymer during sliding. Degradation products of HCl and Cl2 which chemisorb to the metal are evolved near the interface.

Pepper, S. V.↗

Auger measurements on T-027 samples exposed during the Skylab 2 mission

Auger electron spectroscopy measurements performed on Skylab 2 indicate a low rate of deposition of permanent, continuous film contamination on nickel and gold surfaces positioned on the antisolar side of the spacecraft. These measurements and supportive evidence indicate that for the particular locations and orientations of these samples permanent films of less than 3 nm (30 A) thickness were deposited during an exposure of 40 hours at a temperature of approximately -32 C.

Peters, P. N.↗

Adhesion, friction and Auger spectroscopy analysis of a commercial cobalt base aircraft turbine shroud alloy

A commercially used cast cobalt base alloy was investigated as a turbine shroud material which revealed a surface enriched with tungsten and carbon suggesting a surface layer of tungsten carbide. Adhesion and friction of this segregated surface layer are higher than for the bulk cobalt base alloy composition. Auger spectroscopy analysis of the segregation of tungsten in the alloy indicates that it occurs between 850 and 1000 C.

Buckley, D. H.↗

Auger electron spectroscopy and depth profile study of oxidation of modified 440C steel

Auger electron spectroscopy (AES) and sputtering were used to study selective oxidation of modified 440C steel. The sample was polycrystalline. Oxidation was performed on initially clean surfaces for pressures ranging from 1 x 10 to the minus 7th power to 1 x 10 to the minus 5th power torr and temperatures ranging from room temperature to 800 C. AES traces were taken during oxidation. In situ sputtering depth profiles are also obtained. A transition temperature is observed in the range 600 to 700 C for which the composition of the outer surface oxide changed from iron oxide to chromium oxide. Heating in vacuum about 5 x 10 to the minus 10 power torr to 700 C causes conversion of the iron oxide surface to chromium oxide.

Ferrante, J.↗

Surface segregation in titanium as monitored by Auger electron spectroscopy

Investigation of the surface diffusion and segregation of bulk impurities in titanium single crystals under well-defined and controlled experimental conditions. It is shown that an atomically clean titanium single-crystal surface can be obtained by argon ion bombardment within the temperature range from 700 to 800 C. It is demonstrated by Auger electron spectroscopy that, if such clean surfaces are subjected to thermal treatment, bulk impurities, especially sulfur, diffuse out to the crystal surface, and that the rate of surface segregation increases with increasing temperature.

Khan, I. H.↗

Auger spectroscopy of fracture surfaces of ceramics

Results of Auger electron spectroscopy (AES) studies of fracture surfaces in a series of ceramic materials, including Al2O3, MgO, and Si3N4, which were formed using different processing techniques. AES on the fractured surface of a lunar sample is also discussed. Scanning electron micrograph fractography is used to relate the surface chemistry to the failure mode. Combined argon ion sputtering and AES studies demonstrate the local variations in chemistry near the fracture surface. The problems associated with doing AES in insulators are also discussed, and the experimental techniques directed toward solving them are described.

Marcus, H. L.↗

Reaction of sulfur dioxide with modified 440C, studied by Auger electron spectroscopy and depth profiling

Auger electron spectroscopy and sputtering were used to study the interaction of SO2 with modified 440C, which is a nominally 77-wt%-Fe, 14-wt%-Cr, and 4-wt%-Mo bearing steel with C, S, Si, Ni, V, P, and Mn making up the balance. The sample was polycrystalline. Three temperatures were used: room temperature, 500 C, and 600 C. The reaction time was varied from 30 minutes to 2 hours. A surface cleaned of oxides was the starting point for each reaction. For reactions at 500 C, the major constituents Cr, O, Fe, and S were present in the surface film. At 600 C, the principal constituents of the film were Cr, O, and S with no Fe present. Therefore, a transition in film composition occurred between 500 and 600 C. Oxides were the primary constituents of the films at both temperatures. Room-temperature reactions indicated that SO2 adsorbed dissociatively, with approximately equal quantities of S and O on the surface. For the same reaction time (1 hr) and pressure, a strong temperature dependence of film thickness was observed. The film formed at 600 C was approximately seven times thicker than that formed at 500 C.

Ferrante, J.↗

Auger spectroscopy of HCl interaction with Al at low pressures

The purpose of the present study was to determine some adsorption characteristics of HCl with partially clean polycrystalline Al by Auger electron spectroscopy. The adsorption was found to exhibit a Freundlich-type behavior pattern in which the number of molecules adsorbed varied with HCl pressure linearly on a log-log plot. Assuming that the adsorption behaves according to the Clausius-Clapeyron equation, the isosteric heat of adsorption increases with coverage at low pressures, appearing to approach a constant value of 4-5 kcal/mole.

Lassiter, W. S.↗

Mechanical test in-situ fracture device for Auger electron spectroscopy

An in-situ fracture device for Auger spectroscopy was described. The device is designed to handle small tensile specimens or small double cantilever beam specimens and is fully instrumented with load and displacement transducers so that quantitative stress-strain measurements can be made directly. Some initial test results for specimens made from 4130 and 1020 steel were presented.

Moorhead, R. D.↗

Oxidation of metals and alloys in controlled atmospheres using in situ transmission electron microscopy and Auger spectrography

Single-crystalline thin films of copper were oxidized at an isothermal temperature of 425 C and at an oxygen partial pressure of .005 Torr in situ in a high-resolution electron microscope. The specimens were prepared by epitaxial vapor deposition onto polished 100 and 110 faces of rocksalt and mounted in a hot stage inside an ultra-high-vacuum specimen chamber of the microscope. Large amounts of sulfur, carbon, and oxygen were detected by Auger electron spectroscopy on the surface of the as-received films and were removed in situ by ion-sputter etching immediately prior to the oxidation. The nucleation and growth characteristics of Cu2O on Cu were studied. Results show that neither stacking faults nor dislocations are associated with the Cu2O nucleation sites. The growth of Cu2O nuclei is linear with time. The experimental findings, including results from oxygen dissolution experiments and from repetitive oxidation-reduction-oxidation sequences, fit well into the framework of an oxidation process involving (a) the formation of a surface-charge layer, (b) oxygen saturation in the metal and (c) nucleation, followed by surface diffusion of oxygen and bulk diffusion of copper for lateral and vertical oxide growth, respectively.

Rao, D. B.↗

Mechanical testing - In situ fracture device for Auger electron spectroscopy

An in situ fracture device for Auger spectroscopy is described. The device is designed to handle small tensile specimens or small double-cantilever beam specimens and is fully instrumented with load and displacement transducers so that quantitative stress-strain measurements can be made directly. Some initial test results for specimens made from 4130 and 1020 steel are presented. Results indicate that impurity segregation at interfaces other than grain boundary may play a significant role in the mechanism of ductile fracture.

Moorhead, R. D.↗

Angular distribution of Auger electrons due to 3d-shell ionization of krypton

Cross sections for electron impact ionization of krypton due to ejection of a 3rd shell electron have been calculated using screened hydrogenic and Hartree-Slater wave functions for target atom. While the total ionization cross sections in the two approximations are within 10% of each other, the Auger electron angular distribution, related to cross sections for specific magnetic quantum numbers of the 3rd electrons, is widely different in the two approximations. The angular distribution due to Hartree-Slater approximation is in excellent agreement with measurement. The physical reason for the discrepancies in the two approximations is explained.

Omidvar, K.↗

Use of Auger spectroscopy in the evaluation of thermionic cathodes

Auger spectroscopy has been used to evaluate the properties of 'good' and 'poor' impregnated tungsten cathodes used in high-power microwave wave tubes. The results were interpreted to analyze failure modes in cathodes removed from TWT's because of poor emission characteristics. Most of the poor cathodes evaluated in this program were obtained from fabricated electron guns that had been employed and discarded from the 200-W TWT tubes developed for the Communication Technology Satellite program. The results of these measurements have shown there are at least two types of failure modes that one observes with poor cathodes. They are (1) chemical contamination of the cathode surface and (2) low partial layer barium coverage of the cathode surface.

Forman, R.↗

Electrode surface studies by LEED-Auger

The role the electronic and geometric structures of the metal surface play in electrochemical surface reactions remains as yet an unknown factor. In order to investigate these surface contributions to electrochemical reactions, a low-energy-electron diffraction (LEED) and an Auger electron spectrometer (AES) have been combined with an electrochemical thin-layer cell. The surface to be studied electrochemically is first characterized by LEED-AES and then transferred into a second chamber where it becomes part of the electrochemical thin-layer cell. Electrochemical reactions are then run on this surface. The sample may then be transferred back to the LEED-AES chamber for further characterization. Data on Pt (111) will be presented.

Ogrady, W. E.↗

Angular distribution of Auger electrons due to 3d-shell impact ionization of krypton

Cross sections for electron impact ionization of krypton due to ejection of a 3d-shell electron have been calculated using screened hydrogenic and Hartree-Slater wavefunctions for the target atom. While the total ionization cross sections in the two approximations are within 10% of each other, the Auger electron angular distribution, related to cross sections for specific magnetic quantum numbers of the 3d electrons, are widely different in the two approximations. The angular distribution due to the Hartree-Slater approximation is in excellent agreement with measurement. The physical reason for the discrepancies in the two approximations is explained.

Omidvar, K.↗