Search NASA⌕ Search

SEARCH · Search NASA

Results for “CORROSION RESISTANCE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Localized corrosion of high performance metal alloys in an acid/salt environment

Various vacuum jacketed cryogenic supply lines at the Space Shuttle launch site at Kennedy Space Center use convoluted flexible expansion joints. The atmosphere at the launch site has a very high salt content, and during a launch, fuel combustion products include hydrochloric acid. This extremely corrosive environment has caused pitting corrosion failure in the thin walled 304L stainless steel flex hoses. A search was done to find a more corrosion resistant replacement material. The study focussed on 19 metal alloys. Tests which were performed include electrochemical corrosion testing, accelerated corrosion testing in a salt fog chamber, and long term exposure at a beach corrosion testing site. Based on the results of these tests, several nickel based alloys were found to have very high resistance to this corrosive environment. Also, there was excellent agreement between the electrochemical tests and the actual beach exposure tests. This suggests that electrochemical testing may be useful for narrowing the field of potential candidate alloys before subjecting samples to long term beach exposure.

Macdowell, L. G.↗

Alumina-Forming MAX Phases in Turbine Material Systems

Coatings for high temperature turbine components are based on low conductivity YSZ thermal barriers and protective NiAl, NiCoCrAlY bond coats. Good oxidation hot corrosion resistance, intermediate CTE, and strain tolerance of Ti2AlC and Cr2AlC MAX phases are thus of special interest. Their alumina scale growth follows a cubic law in accord with FeCrAlY alloys, with oxygen grain boundary diffusivity: Dgb 1.8 x 10-10 exp(-375 kJmole) m3s. Protective cubic kinetics are also found in high pressure burner rig (6 atm., 25 ms) and TGA tests of MAXthal 211Ti2AlC. The initial portion (0.1 hr) is dominated by fast TiO2 growth (with little evidence of scale volatility in high pressure water vapor, as found for SiO2 scales). Bulk Ti2AlC and Cr2AlC substrates show promise as potential bond coats for YSZ TBCs in 1000-1200 C furnace life (500 h) tests. Cr2AlC is proving to be very resistant to 700-900 C Na2SO4 hot corrosion and is of interest for disk alloys. Preliminary diffusion bonded Cr2AlC-superalloy hybrid couples have survived 1000 hr interrupted furnace tests at 800C with no indication of cracking or debonding. Diffusion zones of -NiAl+Cr7C3 were produced in these above 1000 C, but did not grow to any great extent after 1000 hr at 800 C. Processing as coatings presents challenges, however the basic properties of MAX phases provide novel opportunities for high temperature turbine components.

MAX phase↗

Characterization of Al-Cu-Li Alloy 2090 Near Net Shape Extrusion

Aluminum-lithium (Al-Li) alloys near net shape extrusions are being evaluated for potential application in launch vehicle structures. The objective of this study was to determine tensile and fracture properties, corrosion resistance, and weldability of integrally stiffened panels of Al-Cu-Li alloy 2090 in the T8 temper. The microstructure was pre-dominantly unrecrystallized. Texture analyses revealed the presence of fiber components in the stiffeners and a combination of fiber and rolling components in the skin. Variations in grain morphology and texture through the extruded cross section were correlated with the tensile, fracture, and corrosion behavior. Tensile strengths at room and cryogenic temperatures of the 2090 extrusions were similar to other 2090 product forms and were higher than 2219-T87, the primary structural material in the Space Shuttle external tank; however, ductilities were lower. The fracture resistance of the 2090 extrusion was lower than 2219-T87 plate at room temperature. At cryogenic temperatures, tensile ductility and fracture behavior of the 2090 extrusion were similar to other 2090 product forms but were lower than 2219-T87 plate. The exfoliation and stress corrosion resistance of the 2090 extrusion compared favorably with the characteristics of other 2090 product forms. The weldability and weldment properties of the extrusions were similar to 2090 and 2219 plates.

Birt, M. J.↗

Corrosion Behavior of Hydrophobic Coatings in Aqueous CO2 Environments

Internal corrosion is caused by gas impurities such as CO2, moisture, and H2S, leading to material degradation. To combat this, the National Energy Technology Laboratory (NETL) developed a novel hydrophobic coating to reduce surface hydrophobicity and enhance the corrosion resistance of steel. NETL’s approach uses multi-layer hydrophobic coatings, a novel and promising coating that could potentially revolutionize the industry's approach to internal corrosion mitigation. This work aims to investigate the corrosion performance of the hydrophobic coating and determine the water uptake. Electrochemical corrosion experiments were carried out on bare X65 carbon steel without and with coating in 3.5 wt.% NaCl saturated with CO2 at 20 °C to follow the water uptake as a function of exposure time. Linear polarization resistance (LPR) was used to determine the corrosion rate for carbon steel immersed in a NaCl electrolyte saturated with CO2. Electrochemical impedance spectroscopy (EIS) of uncoated and coated bare carbon steel was investigated. The analyses of impedance models and water uptake behaviors of hydrophobic coatings were studied for 200 hours during the corrosion process. The water uptake was estimated using the Brasher and Kingsbury relation. The results showed that the superhydrophobic coating that was developed used innovative nano-based materials to act as protection layers on the surface of metallic parts against mechanical aggressors, corrosion, and fouling agents.

corrosion behavior↗

Unlocking the Future of Aircraft Manufacturing: The Environmental Benefits of Laser Patterning for Surface Enhancement of Aircraft-Certified Alloys

Surface protection and functional modification of aircraft-certified aluminum alloys are essential for corrosion resistance, durability, and long-term airworthiness. At the same time, increasingly restrictive environmental regulations motivate the development of alternatives to legacy wet-chemical surface treatments. This study presents an integrated assessment of ultrafast femtosecond laser surface texturing as a surface functionalization approach for Aluminum 6061 alloys within an aerospace manufacturing and sustainability context. Ultrashort-pulse laser processing enables controlled micro- and nano-scale surface topographical modification with limited thermal impact, allowing adjustment of wettability and surface functionality while preserving bulk material integrity. As a dry and contactless process, femtosecond laser treatment eliminates the use of hazardous chemicals, reduces consumable inputs, and generates minimal secondary waste. A streamlined cradle-to-gate life cycle assessment conducted in accordance with ISO 14040/14044 indicates a lower global-warming potential per functional unit compared with conventional surface treatments, including anodization, plasma-assisted coatings, and organic coating systems. Complementary qualitative analyses addressing environmental health and safety, supply-chain risk, and ESG alignment indicate potential advantages related to occupational safety, regulatory compliance, waste management, and end-of-life recyclability. The investigation is performed on planar Aluminum 6061 reference surfaces with a treated area of 25 mm 2 , providing a controlled laboratory-scale basis for analyzing process behavior, functional surface modification, and associated environmental metrics. Within this defined scope, the results support further evaluation of femtosecond laser surface texturing as a surface engineering option for future aerospace manufacturing.

corrosion resistance↗

Incorporating corrosion design constraints in desalination process optimization: A case study in mechanical vapor compression

Corrosion is an expensive and complex challenge for desalination, yet current design approaches do not explicitly account for corrosion mechanisms in process modeling and technoeconomic analysis. Here, to address this gap, we present a workflow for incorporating corrosion design constraints directly into desalination process optimization models. We develop surrogate models for general and localized corrosion metrics as functions of temperature, pH, salinity, dissolved oxygen, and material using data from OLI Systems’ Corrosion Analyzer. We then integrate these surrogates as corrosion design constraints in a cost-optimization MVC model that minimizes the levelized cost of water (LCOW). For a case study of mechanical vapor compression (MVC) treating seawater across a range of recoveries, we find dissolved oxygen (DO) is the dominant driver of localized corrosion, and thus of cost-optimal material choice and operating conditions. Reducing the DO from 8 mg/L to 0.5 mg/L reduces the LCOW by 15-35%, informing the breakeven costs for implementing DO removal or selecting highly corrosion-resistant alloys. This framework is broadly applicable across corrosion types, materials, and components and enables desalination process design that minimizes capital costs.

36 MATERIALS SCIENCE↗

Technology development for phosphoric acid fuel cell powerplant, phase 2

Component development has resulted in routine molding of 12 in. by 17 in. bipolar plates with 80 percent acceptance. A 5 C per hour post-cure heating cycle for these plates was found to give blister free materials. Lowering the resin in a bipolar plate content from 32 percent to 22 percent decreases the resistivity more than 50 percent. Evaluation of the corrosion resistance of Novolak and Resol resins at 185 C in phosphoric acid indicates a slow etch. aerosol modified phenolics, however, decompose rapidly. Estimates of acid loss by the use of analytical expressions known as Margule, van Laar, and Wilson equations were not satisfactory. Experimental evaluation of the P4O10 vapor concentration of 103 wt percent acid at 191 C provided a value of 2 ppm. This value is based on a single experiment.

Christner, L.↗

Long term exposure of metals to hydrazine nitrate blend

A long term testing program is being conducted to determine the effects of materials in contact with a hydrazine nitrate blend for the purpose of designing chemical propulsion systems which can be used for current as well as future planetary spacecraft. Analysis of this data indicates that some aluminum alloys are acceptable for use with the particular blend of fuel used. Titanium alloy was identified as being acceptable for 10-year applications. Corrosion resistant steels, however, were found to have excessive corrosion rates and are therefore considered unacceptable for long-term use. There is also some evidence that the propellant decomposed at a rate far in excess of the acceptable rate of 0.1 percent per year when in contact with stainless steel.

Moran, Clifford M.↗

Non-Magnetic, Tough, Corrosion- and Wear-Resistant Knives From Bulk Metallic Glasses and Composites

Quality knives are typically fabricated from high-strength steel alloys. Depending on the application, there are different requirements for mechanical and physical properties that cause problems for steel alloys. For example, diver's knives are generally used in salt water, which causes rust in steel knives. Titanium diver's knives are a popular alternative due to their salt water corrosion resistance, but are too soft to maintain a sharp cutting edge. Steel knives are also magnetic, which is undesirable for military applications where the knives are used as a tactical tool for diffusing magnetic mines. Steel is also significantly denser than titanium (8 g/cu cm vs. 4.5 g/cu cm), which results in heavier knives for the same size. Steel is hard and wear-resistant, compared with titanium, and can keep a sharp edge during service. A major drawback of both steel and titanium knives is that they must be ground or machined into the final knife shape from a billet. Since most knives have a mirrored surface and a complex shape, manufacturing them is complex. It would be more desirable if the knife could be cast into a net or near-net shape in a single step. The solution to the deficiencies of titanium, steel, and ceramic knives is to fabricate them using bulk metallic glasses (or composites). These alloys can be cast into net or near-net shaped knives with a combination of properties that exceed both titanium and steel. A commercially viable BMG (bulk metallic glass) or composite knife is one that exhibits one or all of the following properties: It is based on titanium, has a self-sharpening edge, can retain an edge during service, is hard, is non-magnetic, is corrosion-resistant against a variety of corrosive environments, is tough (to allow for prying), can be cast into a net-shape with a mirror finish and a complex shape, has excellent wear resistance, and is low-density. These properties can be achieved in BMG and composites through alloy chemistry and processing. For each desired property for knife fabrication and performance, there is an alloy development strategy that optimizes behavior. Although BMG knives have been demonstrated as far back as 1995, they never found commercial success because they had to be ground (which presented problems because the alloys contained beryllium), they weren't low cost (because they weren't cast to a net-shape), they were brittle (because they were made with a low-quality commercial material), and they had extremely poor corrosion resistance (because corrosion was not well-understood in these materials). Ultimately, these shortcomings prevented the widespread commercialization. In the current work, the inventors have applied more than a decade of research on BMGs from Caltech and JPL to develop a better understanding of how to make BMG knives that exhibit an optimal combination of properties, processing and cost. Alloys have been developed based in titanium (and other metals), that exhibit high toughness, high hardness, excellent corrosion resistance, no ferromagnetism, edge-retaining selfsharpening, and the ability to be cast like a plastic using commercially available casting techniques (currently used by commercial companies such as Liquidmetal Technologies and Visser Precision Casting). The inventors argue that depending on the application (diving, military, tactical, utility, etc.) there is an optimal combination of design and alloy composition. Moreover, with new casting technologies not available at the inception of these materials, net-shaped knives can be cast into complex shapes that require no aftermarket forming, except for sharpening using water-cooled polishing wheel. These combinations of discoveries seek to make low-cost BMG knives commercially viable products that have no equal among metal or ceramic knives. Current work at JPL focuses on net-shape casting of these alloys and testing their mechanical properties versus commercially available knives to demonstrate their benefits.

Hoffman, Douglas C.↗

Adhesive and Protective Characteristics of Ceramic Coating A-417 and Its Effect on Engine Life of Forged Refractaloy-26 (AMS 5760) and Cast Stellite 21 (AMS 5385) Turbine Blades

The adhesive and protective characteristics of National Bureau of Standards Coating A-417 were investigated, as well as the effect of the coating on the life of forged Refractaloy 26 and cast Stellite 21 turbine blades. Coated and uncoated blades were run in a full-scale J33-9 engine and were subjected to simulated service operations consisting of consecutive 20-minute cycles (15 min at rated speed and approximately 5 min at idle). The ceramic coating adhered well to Refractaloy 26 and Stellite 21 turbine blades operated at 1500 degrees F. The coating also prevented corrosion of the Refractaloy 26, a corrosion-sensitive nickel-base alloy, and of the Stellite 21, a relatively corrosion-resistant cobalt-base alloy. Although the coating prevented corrosion of both alloys, it had no apparent effect on blade life.

ALLOYS, HEAT-RESISTING↗