Search NASA⌕ Search

SEARCH · Search NASA

Results for “ELECTRON BEAM WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Welding in Space: Lessons Learned for Future In Space Repair Development

Welds have been made in the harsh environment of space only twice in the history of manned space flight. The United States conducted the M5 12 experiment on Skylab and the former Soviet Union conducted an Extravehicular Activity. Both experiments demonstrated electron beam welding. A third attempt to demonstrate and advance space welding was made by the Marshall Space Flight Center in the 90's but the experiment was demanifested as a Space Shuttle payload. This presentation summarizes the lessons learned from these three historical experiences in the areas of safety, design, operations and implementation so that welding in space can become an option for in space repair applications.

Russell, C. K.↗

Green strength of zirconium sponge and uranium dioxide powder compacts

Zirconium metal sponge is compacted into rectangular or cylindrical shapes using hydraulic presses. These shapes are stacked and electron beam welded to form a long electrode suitable for vacuum arc melting and casting into solid ingots. The compact electrodes should be sufficiently strong to prevent breakage in handling as well as during vacuum arc melting. Usually, the welds are strong and the electrode strength is limited by the green strength of the compacts, which constitute the electrode. Green strength is also required in uranium dioxide (UO{sub 2}) powder compacts, to withstand stresses during de-tensioning after compaction as well as during ejection from the die and for subsequent handling by man and machine. The strengths of zirconium sponge and UO{sub 2} powder compacts have been determined by bending and crushing respectively, and Weibul moduli evaluated. The green density of coarse sponge compact was found to be larger than that from finer sponge. The green density of compacts from lightly attrited UO{sub 2} powder was higher than that from unattrited category, accompanied by an improvement in UO{sub 2} green crushing strength. The factors governing green strength have been examined in the light of published literature and experimental evidence. The methodology and results provide a basis for quality control in metal sponge and ceramic powder compaction in the manufacture of nuclear fuel.

36 MATERIALS SCIENCE↗

Research study on materials processing in space experiment number M512

Conclusions of the team of specialists can be generalized as: (1) Brazing and welding of metal structures in an orbital near zero gravity condition are quite feasible. (2) Design of joints for fabrication in zero gravity will place less emphasis on the tolerances and proximity of the adjacent structures than on the quantity of liquid metal available. (3) Brazing of metallic joints has many advantages over electron beam welding for practical reasons: simplicity, launch weight, development costs, joint design tolerances, remotization, etc. (4) No evidence of different physical or mechanical properties of liquid metals in zero gravity was observed. However, many differences in liquid behavior were observed. Many of these effects have been called adhesion-cohesion phenomena.

Tobin, J. M.↗

M551 metals melting experiment

Electron beam welding studies were conducted in the Skylab M551 metals melting experiment, on three different materials; namely 2219-T87 aluminum alloy, 304L stainless steel, and commercially pure tantalum (0.5 wt % columbium). Welds were made in both one gravity and zero gravity (Skylab) environments. Segments from each of the welds were investigated by microhardness, optical microscopy, scanning microscopy, and electron probe techniques. In the 2219-T87 aluminum alloy samples, macroscopic banding and the presence of an eutectic phase in the grain boundaries of the heat affected zone were observed. The stainless steel samples exhibited a sharp weld interface and macroscopic bands. The primary microstructural features found in the tantalum were the presence of either columnar grains (ground base) or equiaxed grains (Skylab). The factors contributing to these effects are discussed and the role of reduced gravity in welding is considered.

Busch, G.↗

Interdiffusion behavior of tungsten or rhenium and group 5 and 6 elements and alloys of the periodic table, part 1

Arc cast W, CVD W, CVD Re, and powder metallurgy Re materials were hot isostatically pressure welded to ten different refractory metals and alloys (Cb, Cb-1Zr, Ta, Ta-10W, T-111, ASTAR-811C, W-25Re, Mo-50Re, W-30Re-20Mo, ect.) and thermally aged at 10 to the minus 8th power torr at 1200, 1500, 1630, 1800, and 2000 C for 100 to 2000 hours. Electron beam microprobe analysis was used to characterize the interdiffusion zone width of each couple system as a function of age time and temperature. Extrapolations of interdiffusion zone thickness to 10,000 hours were made. Classic interdiffusion analysis was performed for several of the systems by Boltzmann-Matano analysis. A method of inhibiting Kirkendall voids from forming during thermal ageing of dissimilar metal junctions was devised and experimentally demonstrated. An electron beam weld study of Cb-1Zr to Re and W-25Re demonstrated the limited acceptability of these welds.

Arcella, F. G.↗

Weldability, strength, and high temperature stability of chemically vapor deposited tungsten

Three types of CVD tungsten (fluoride-produced, chloride-produced and the combination of the two which is termed duplex) were evaluated to determine their weldability, high temperature strength and structural stability during 5000 hour exposure to temperatures of 1540 C and 1700 C. Each type of CVD tungsten could be successfully electron beam welded but the results for the chloride product were not as satisfactory as those of the other two materials. The high temperature strength behavior of the three materials did not differ greatly. However a large difference was noted for the grain growth behavior of the two basic CVD tungsten materials. Fluoride tungsten was found to be relatively stable while for the most part the grain size of chloride tungsten increased appreciably. The examination of freshly fractured surfaces with a scanning electron microscope revealed numerous bubbles in the fluoride material following its exposure to 1700 C for 5000 hours. Less severe thermal treatments produced relatively few bubbles in this material. Only at certain locations within the chloride material associated with the interruption of tungsten were bubbles noted.

Bryant, W. A.↗

Gigacycle Fatigue Strength Evaluation of Welded 316L Stainless Steels for Mercury Target Vessel

At the Materials and Life Science Experimental Facility (MLF) in J-PARC, liquid mercury target for the pulsed spallation neutron source is in operation. An enclosure vessel for the liquid mercury target made of type 316L stainless steel (SS316L) suffers two kinds of cyclic stress during operation. One is the thermal stress due to the internal heating and swings by proton beam trip. The other is the impulsive stress by the pressure waves generated by the proton beam injection. The total number of loading cycles for the former is ∼104, and the latter is ∼4 × 108 for a year operation in the J-PARC mercury target vessel. The target vessel is assembled by an electron beam welding (EBW) and a gas tungsten arc welding (GTAW). However, fatigue data of welded SS316L up to gigacycle is limited. Ultrasonic fatigue testing, applying load cycles by utilizing ultrasonic resonance, for the welded SS316L was performed to investigate the effect of welding on fatigue behavior up to a gigacycle. The result showed that the fatigue strength degradation by EBW and EBW with GTAW were not recognized up to 109 cycles. Crack initiation in welded specimens nucliated at off-center areas of the specimen whereas the cracks in base metal specimen originated at the specimen center.

Naoe, Takashi [Japan Atomic Energy Agency (JAEA)]↗

Feasibility of EB Welded Hastelloy X and Combination of Refractory Metals

As NASA continues to expand its horizon, exploration and discovery creates the need of advancement in technology. The Jupiter Icy Moon Orbiter's (JIMO) mission to explore and document the outer surfaces, rate the possibility of holding potential life forms, etc. within the three moons (Callisto, Ganymede, and Europa) proves to be challenging. The orbiter itself consists of many sections including: the nuclear reactor and the power conversion system, the radiator panels, and the thrusters and antenna. The nuclear reactor serves as a power source, and if successfully developed, can operate for extended periods. During the duration of my tenure at NASA Glenn Research Center's (NASA GRC) Advanced Metallics Branch, I was assigned to assist Frank J. Ritzert on analyzing the feasibility of the Electron Beam Welded Hastelloy X (HX), a nickel-based superalloy, to Niobium- 1 %Zirconium (Nb-1 Zr) and other refractory metals/alloys including Tantalum, Molybdenum, Tungsten, and Rhenium alloys. This welding technique is going to be used for the nuclear reactor within JIMO.

Martinez, Diana A.↗

Production of Seamless Superconducting Radio Frequency Cavities from Ultra-fine Grained Niobium, Phase II Final Report

The positron and electron linacs of the International Linear Collider (ILC) will require over 14,000, nine-cell, one meter length, superconducting radio frequency (SRF) cavities [ILC Reference Design Report, 2007]. Manufacturing on this scale will benefit from more efficient fabrication methods. The current methods of fabricating SRF cavities involve deep drawing of the halves of each of the elliptical cells and joining them by high-vacuum, electron beam welding, with at least 19 circumferential welds per cavity. The welding is costly and has undesirable effects on the cavity surfaces, including grain-scale surface roughening at the weld seams. Hydroforming of seamless tubes avoids welding, but hydroforming of coarse-grained seamless tubes results in strain-induced surface roughening. Surface roughness limits accelerating fields, because asperities prematurely exceed the critical magnetic field and become normal conducting. This project explored the technical and economic feasibility of an improved processing method for seamless tubes for hydroforming. Severe deformation of bulk material was first used to produce a fine structure, followed by extrusion and flow-forming methods of tube making. Extrusion of the randomly oriented, fine-grained bulk material proceeded under largely steady-state conditions, and resulted in a uniform structure, which was found to be finer and more crystallographically random than standard (high purity) RRR niobium sheet metal. A 165 mm diameter billet of RRR grade niobium was processed into five, 150 mm I.D. tubes, each over 1.8 m in length, to meet the dimensions used by the DESY ILC hydroforming machine. Mechanical properties met specifications. Costs of prototype tube production were approximately twice the price of RRR niobium sheet, and are expected to be comparable with economies of scale. Hydroforming and superconducting testing will be pursued in subsequent collaborations with DESY and Fermilab. SRF Cavities are used to construct particle accelerators for high-energy physics research, as well as for lower energy particle accelerators, and Free Electron Lasers. These machines have applications in the fields of basic science, industrial processing, medical diagnostics, pharmaceutical research and weapons systems. The scientific community and the general public will benefit from the implementation of this technology since lower production costs will increase the availability of SRF particle accelerators.

36 MATERIALS SCIENCE↗

Thermal conductance characterization of a pressed copper rope strap between 0.13 K and 10 K

Mechanically pressing the ends of a copper braid in solid copper is an effective way of constructing solderless conductive straps for cryogenic applications. In this paper we present thermal conductance data of such a copper strap measured using the two-heater one-thermometer method. The measurements span a wide temperature range of 0.13–10 K applicable to a variety of cryogenic systems employing liquid helium, pulse tube coolers, adiabatic demagnetization refrigerators, and others. Above ≈1.5 K, the braid thermal conductivity dominates the strap conductance resulting in a near-linear dependence with temperature. The variation with temperature below ≈1.5 K is near-quadratic indicating dominance of the pressed contact conductance at the strap ends. In conclusion, electron-beam welding the braid to the strap ends is shown to be a promising solution for improving sub-Kelvin thermal conductance of the strap.

43 PARTICLE ACCELERATORS↗

Design of Silicide-Strengthened Nb–Si–Cr–(Mo) alloys for additive manufacturing

Three high–intermetallic volume Nb–Si–Cr–(Mo) alloys were designed using CALPHAD modeling with the goal of identifying high–specific strength, oxidation-resistant alloys that can be additively manufactured using powder bed fusion. The silicides Nb 5 Si 3 and Nb 9 Si 2 Cr3 were targeted as the primary strengthening phases, and the addition of Cr promoted the NbCr 2 phase. These alloys were cast and surface-processed with electron beam welding at different speeds to simulate additive manufacturing, and the phases and microstructures of both cast and welded regions were characterized. The weld processing was found to produce fine-grained microstructures in each alloy with fine-scale intermetallics uniformly distributed among a body-centered cubic Nb matrix. Microstructural refinement and hardness were found to increase with weld velocity; one alloy reached its highest hardness of approximately 16 GPa before the brittleness at higher velocities became detrimental. One alloy was found to be qualitatively the least brittle while also attaining a hardness of 13 GPa and was therefore identified as a good candidate for additive manufacturing.

36 MATERIALS SCIENCE↗

A cryogenic high pressure cell for inelastic neutron scattering measurements of quantum fluids and solids

We present our new development of a high pressure cell for inelastic neutron scattering measurements of helium at ultra-low temperatures. The cell has a large sample volume of ~140 cm3, and a working pressure of ~70 bar, with a relatively thin wall-thickness (1.1 mm) - thanks to the high yield strength aluminum used in the design. Two variants of this cell have been developed; one with permanently joined components using electron-beam welding and explosion welding, methods that have little or no impact on the global heat treatment of the cell, and another with modular and interchangeable components, which include a capacitance pressure gauge, that can be sealed using traditional indium wire technique. The performance of the cell has been tested in recent measurements on superfluid liquid helium near the solidification line.

Cryogenics↗

Innovative compact braze-free accelerating cavity

We report that high energy physics experiments using particle accelerators as well as industrial and medical applications are continuously seeking more compact, robust and cheaper accelerating structures. As of today, stable operating gradients, exceeding 100 MV/m, have been demonstrated by the SLAC group in the X-Band (11.424 GHz). These experiments show that hard structures, fabricated without high-temperature processes, achieve a better high gradient performance in terms of accelerating gradients. Therefore, we present an innovative and compact type of accelerating cavity that avoids any high-temperature processes like brazing or diffusion bonding. All cells are joined together by means of specifically designed and proprietary screws which ensure good vacuum and RF contacts. Two three-cell standing-wave accelerating structures, designed to operate in the pi-mode at 11.424 GHz, have been successfully built and cold tested. In order to guarantee a vacuum envelope and mechanically robust assembly, we used the Electron Beam Welding (EBW) and the Tungsten Inert Gas (TIG) processes. Lastly, this work has been carried out in the framework of a funded project by the Vth Committee of the INFN for the Laboratori Nazionali di Frascati (LNF), within a large international collaboration between LNF, SLAC and KEK for the development of X-Band accelerating cavities using "hard structure" technology.

43 PARTICLE ACCELERATORS↗

Hydroforming SRF Three-cell Cavity from Seamless Niobium Tube

We are developing the manufacturing method for superconducting radio frequency (SRF) cavities by using a hydroforming instead of using conventional electron beam welding. We expect higher reliability and reduced cost with hydroforming. For successful hydroforming, high-purity seamless niobium tubes with good formability as well as advancing the hydroforming technique are necessary. Using a seamless niobium tube from ATI Wah Chang, we were able to successfully hydroform a 1.3 GHz three-cell TESLA-like cavity and obtained an Eacc of 32 MV/m. A barrel polishing process was omitted after the hydroforming. The vertical test was carried out with very rough inside surface. We got amazing and interesting result.

43 PARTICLE ACCELERATORS↗

Test Result of 650 MHz, Beta 0.61 Single Cell Niobium Cavity

VECC has been involved in the design, analysis and development of 650 MHz, beta 0.61 (LB650), elliptical Superconducting RF linac cavity, as part of research and development activities on SRF cavities and associated technologies under Indian Institutions Fermilab Collaboration (IIFC). A single-cell niobium cavity has been indigenously designed and developed at VECC, with the help of Electron Beam Welding (EBW) facility at IUAC, New Delhi. Various measurements, processing and testing at 2K in Vertical Test Stand (VTS) of the single-cell cavity was carried out at ANL and Fermilab, USA, with active participation of VECC engineers. It achieved a maximum accelerating gradient(Eacc) of 34.5 MV/m with Quality Factor of 2·10⁹ and 30 MV/m with Quality Factor of 1.5·10¹⁰. This is probably the highest accelerating gradient achieved so far in the world for LB650 cavities. This paper describes the design, fabrication and measurement of the single cell niobium cavity. Cavity processing and test results of Vertical Test of the single-cell niobium cavity are also presented.

43 PARTICLE ACCELERATORS↗

Unveiling the Interplay: Cold Work, Recrystallization, and Flux Expulsion in SRF Cavities

The fabrication of SRF cavities from sheet materials includes deep-drawing, electron beam welding, chemical and mechanical polishing, high-temperature heat treatment, and material diffusion. The performance of these cavities is frequently limited by magnetic flux trapping giving rise to additional rf loss. In this presentation, we thoroughly examine how recrystallization influences flux expulsion in SRF cavities, using cold-worked niobium sheets from various suppliers. Our findings reveal that cold-worked sheets enhance flux expulsion, especially at lower heat treatment temperatures, by promoting improved recrystallization. In particular, a traditionally fabricated Nb cavity half-cell from an annealed poly-crystalline Nb sheet after an 800 C heat treatment leads to a bi-modal microstructure that ties in with flux trapping and inefficient flux expulsion. This non-uniform microstructure is related to varying strain profiles along the cavity shape. A novel approach to prevent this non-uniform microstructure is presented by fabricating a 1.3 GHz single cell Nb cavities with a cold-worked sheet and subsequent heat treatment leading to better flux expulsion after 800 C/3h

Dhakal, P. [Old Dominion Univ., Norfolk, VA (Unite↗

Geometric Optimization of the 56MHz SRF Cavity and its Frequency Table

It is essential to know the frequency of a Superconducting Radio Frequency (SRF) cavity at its “just being fabricated” stage because frequency is the key parameter in constructing the cavity. In this paper, we report our work on assessing it. We can estimate the frequency change from stage to stage theoretically and/or by simulation. At the operating stage, the frequency can be calculated accurately, and, from this value, we obtain the frequencies at other stages. They are listed in a table that serves to check the processes from stage to stage. Equally important is optimizing the geometric shape of the SRF cavity so that the peak electric-field and peak magnetic-field are as low as possible. It is particularly desirable in the 56MHz SRF cavity of RHIC to maximize the frequency sensitivity of the slow tuner. After undertaking such optimization, our resultant peak electric-field is only 35.3MV/m, and the peak magnetic-field is 840G at 2MV of voltage across the cavity gap. To quench superconductivity in an SRF cavity, it is reported that the limit of the peak magnetic-field is 1800G [1], and that of the peak electric-field is more than 100MV/m for a SRF cavity [2]. Naturally, for the complex geometry of this cavity (including numerous electron beam welds) and 4.2K operations we do not expect record field performance, but a useful 2 MV gap voltage is reasonable to expect. Our simulations employed the codes Superfish and Microwave Studio.

43 PARTICLE ACCELERATORS↗

Final Report on MEGAPIE Target Irradiation and Post-Irradiation Examination

Megawatt pilot experiment (MEGAPIE) was successfully performed in 2006. One of the important goals of MEGAPIE is to understand the behaviour of structural materials of the target components exposed to high fluxes of high-energy protons and spallation neutrons in flowing LBE (liquid lead-bismuth eutectic) environment by conducting post-irradiation examination (PIE). The PIE includes four major parts: non-destructive test, radiochemical analysis of production and distribution of radionuclides produced by spallation reaction in LBE, analysis of LBE corrosion effects on structural materials, T91 and SS 316L steels, and mechanical testing of the T91 and SS 316L steels irradiated in the lower part of the target. The non-destructive test (NDT) including visual inspection and ultrasonic measurement was performed in the proton beam window area of the T91 calotte of the LBE container, the most intensively irradiated part of the MEGAPIE target. The visual inspection showed no visible failure and the ultrasonic measurement demonstrated no detectable change in thickness in the beam window area. Gamma mapping was also performed in the proton beam window area of the AlMg 3 safety-container. The gamma mapping results were used to evaluate the accumulated proton fluence distribution profile, the input data for determining irradiation parameters. Radiochemical analysis of radionuclides produced by spallation reaction in LBE is to improve the understanding of the production and distribution of radionuclides in the target. The results demonstrate that the radionuclides of noble metals, 207 Bi, 194 Hg/Au are rather homogeneously distributed within the target, while radionuclides of electropositive elements are found to be deposited on the steel-LBE interface. The corrosion effect of LBE on the structural components under intensive irradiation was investigated by metallography. The results show that no evident corrosion damages. However, unexpected deep cracks were found in the EBW (electron beam weld) of the LBE container in the intensive irradiation zone of the target, which should be formed during irradiation. In the SS 316L steel of the flow guide tube, inclusions or precipitates enriched with O, Si, S, Ca, Ti and Mn were observed. Many of them are very long, up to a few mm, and located on grain boundaries along the extrusion direction of the tube. The degradation of the mechanical properties of the T91 and SS 316L steels has been investigated by conducting tensile tests on the specimens extracted from the T91 and SS 316L components in the intensive irradiation region. The results obtained from the proton beam window of the T91 calotte exhibit a good ductility of T91 steel after irradiation at 6-7 dpa (displacement per atom) in contact with flowing LBE.

36 MATERIALS SCIENCE↗