Search NASA⌕ Search

SEARCH · Search NASA

Results for “Electrochemical interfaces”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Design principles for heterointerfacial alloying kinetics at metallic anodes in rechargeable batteries

How surface chemistry influences reactions occurring thereupon has been a long-standing question of broad scientific and technological interest. Here, we consider the relation between the surface chemistry at interfaces and the reversibility of electrochemical transformations at rechargeable battery electrodes. Using Zn as a model system, we report that a moderate strength of chemical interaction between the deposit and the substrate—neither too weak nor too strong—enables highest reversibility and stability of the plating/stripping redox processes. Focused ion beam and electron microscopy were used to directly probe the morphology, chemistry, and crystallography of heterointerfaces of distinct natures. Analogous to the empirical Sabatier principle for chemical heterogeneous catalysis, our findings arise from competing interfacial processes. Using full batteries with stringent negative electrode–to–positive electrode capacity (N:P) ratios, we show that such knowledge provides a powerful tool for designing key materials in highly reversible battery systems based on Earth-abundant, low-cost metals such as Zn and Na.

25 ENERGY STORAGE↗

Simulating microgalvanic corrosion in alloys using the PRISMS phase-field framework

In this prospective paper, we first review the existing simulation tools to simulate microgalvanic corrosion during free immersion. Then, we describe a recently developed application that employs PRISMS-PF, an open-source, high-performance phase-field modeling framework. The model employed in the application accounts for the electrochemical reaction at the metal/electrolyte interface and ionic migration in the electrolyte to determine the evolution of the corrosion front. We present the implementation details for the application and discuss its features such as super-linear parallel scaling performance for a sufficiently large system. Finally, we demonstrate the capability of the application by simulating corrosion of the matrix phase of an alloy near a secondary phase particle in two and three dimensions.

36 MATERIALS SCIENCE↗

Revitalizing interface in protonic ceramic cells by acid etch

Protonic ceramic electrochemical cells hold the promise to be operated at intermediate temperatures below 600 °C. Although the high proton conductivity of the bulk electrolyte has been demonstrated, it cannot be fully utilized in electrochemical full cells due to unknown causes. A practical solution is thus urgently needed. Here we showed that it comes from poor contacts between the low-temperature processed oxygen electrode-electrolyte interface. We demonstrated that a simple acid treatment can effectively rejuvenate the high-temperature annealed electrolyte surface, resulting in reactive bonding between the oxygen electrode and the electrolyte and improved electrochemical performance and stability. This enables exceptional protonic ceramic fuel-cell performance down to 350 °C, with peak power densities of 1.6 W cm -2 at 600 °C, 650 mW cm -2 at 450 °C, and 300 mW cm -2 at 350 °C, as well as stable electrolysis operations at large current densities above 3.9 A cm -2 under 1.4 V applied voltage at 600 °C. Furthermore, our work highlights the critical role of interfacial engineering in ceramic electrochemical devices and offers new understanding and practices towards sustainable energy infrastructure.

08 HYDROGEN↗

Remote Floating-Gate Field-Effect Transistor with 2-Dimensional Reduced Graphene Oxide Sensing Layer for Reliable Detection of SARS-CoV-2 Spike Proteins

Despite intensive research of nanomaterials-based field-effect transistors (FETs) as a rapid diagnostic tool, it remains to be seen for FET sensors to be used for clinical applications due to a lack of stability, reliability, reproducibility, and scalability for mass production. In this work, we propose a remote floating-gate (RFG) FET configuration to eliminate device-to-device variations of two-dimensional reduced graphene oxide (rGO) sensing surfaces and most of the instability at the solution interface. Also, critical mechanistic factors behind the electrochemical instability of rGO such as severe drift and hysteresis were identified through extensive studies on rGO–solution interfaces varied by rGO thickness, coverage, and reduction temperature. rGO surfaces in our RFGFET structure displayed a Nernstian response of 54 mV/pH (from pH 2 to 11) with a 90% yield (9 samples out of total 10), coefficient of variation (CV) < 3%, and a low drift rate of 2%, all of which were calculated from the absolute measurement values. As proof-of-concept, we demonstrated highly reliable, reproducible, and label-free detection of spike proteins of severe acute respiratory syndrome coronavirus 2 (SARS-CoV-2) in a saliva-relevant media with concentrations ranging from 500 fg/mL to 5 μg/mL, with an R 2 value of 0.984 and CV < 3%, and a guaranteed limit of detection at a few pg/mL. Taken together, this new platform may have an immense effect on positioning FET bioelectronics in a clinical setting for detecting SARS-CoV-2.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Modeling the electrochemical behavior and interfacial junction profiles of bipolar membranes at solar flux relevant operating current densities

A 1-dimensional, multi-physics model that accounts for the migration and diffusion of solution species, electrostatics, and chemical reactions, in particular water dissociation (WD), at bipolar membrane (BPM) interfaces was developed to study the electrochemical behavior of bipolar membranes (BPMs) at solar flux relevant operating current densities (tens of mA cm -2 ). Significant partial current densities for WD were observed at BPM voltages much less than the equilibrium voltage, e.g., 59 mV × ΔpH from both experiments and modeling. The co-ion leakage across the BPM at pH differentials accounted for the early presence of the partial current density for WD. Two distinctive electric field dependent WD pathways, the un-catalyzed pathway and the catalyzed pathway, were quantitatively and parametrically studied to improve the turn-on potential of the BPM. The catalyzed pathway accounted for the majority of the partial current density for WD at low voltages, while the un-catalyzed pathway dominated the WD at relatively high voltages. Significant WD was observed only within the interfacial CL (<5 nm), in which a large electric field was present. To improve the electrochemical behavior and the turn-on potential of BPMs, the impacts of the pKa of the immobilized WD catalysts, the electric-field dependent rate constant, the thickness of the catalyst layer and fixed charge density in BPMs on the partial current densities for WD were studied systematically. In addition, the electrochemical behavior and concentration profiles of BPMs in a buffered electrolyte were studied and contrasted with those in an un-buffered electrolyte from both modeling and experiments.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Atomic dynamics of electrified solid–liquid interfaces in liquid-cell TEM

Electrified solid–liquid interfaces (ESLIs) play a key role in various electrochemical processes relevant to energy, biology and geochemistry. The electron and mass transport at the electrified interfaces may result in structural modifications that markedly influence the reaction pathways. For example, electrocatalyst surface restructuring during reactions can substantially affect the catalysis mechanisms and reaction products. Despite its importance, direct probing the atomic dynamics of solid–liquid interfaces under electric biasing is challenging owing to the nature of being buried in liquid electrolytes and the limited spatial resolution of current techniques for in situ imaging through liquids. Here, with our development of advanced polymer electrochemical liquid cells for transmission electron microscopy (TEM), we are able to directly monitor the atomic dynamics of ESLIs during copper (Cu)-catalysed CO 2 electroreduction reactions (CO 2 ERs). Our observation reveals a fluctuating liquid-like amorphous interphase. It undergoes reversible crystalline–amorphous structural transformations and flows along the electrified Cu surface, thus mediating the crystalline Cu surface restructuring and mass loss through the interphase layer. Furthermore, the combination of real-time observation and theoretical calculations unveils an amorphization-mediated restructuring mechanism resulting from charge-activated surface reactions with the electrolyte. Our results open many opportunities to explore the atomic dynamics and its impact in broad systems involving ESLIs by taking advantage of the in situ imaging capability.

36 MATERIALS SCIENCE↗

Electrochemical mechanisms of leakage‐current in photovoltaic modules

Abstract This paper analyzes the mechanisms and pathways for leakage current flow observed in Si photovoltaic modules subjected to high temperature and humidity and a large voltage bias with respect to ground. The current inside of the frame is in the form of electron motion, but in the glass and polymer, it is in at least a large part attributable to the movement of ions. When the mode of current flow changes from electronic to ionic conduction, electrochemical reactions will take place at the interface. This can include reactions that produce volatile chemical species like H 2 , CO x , and O 2 , along with ionic species such as OH − and H 3 O + . Here, we see evidence of the importance of different charge carriers with different diffusion rates and the influence of electrochemical processes involved. The application of negative voltage to the cell circuit affects the resistivity of glass producing surfaces with poor conductivity but with some increases in the electrochemical potential producing complicated interactions that are important when the voltage is changed. In the polymer, there is the development of a space charge region and a chemical gradient providing two oppositional forces to current flow, which when released create a complicated discharge process. Here, we give a basic understanding of the charge/discharge of PV cells highlighting how the specific mechanisms are important in understanding some of the degradation processes in PV modules. We find that there is evidence of multiple significant charge carrier species with different diffusion time scales. The glass/polymer interface forms a depleted region of higher resistance after prolonged exposure to current. Charge also builds up at the polymer to cell antireflective coating interface and mostly flows to the gridlines to experience electrochemical reactions. These complexities result in non‐linear behavior where the apparent resistivities of the different layers change during charge/discharging processes, making the modeling of the current flow extremely difficult.

14 SOLAR ENERGY↗

Structure of the Electrical Double Layer at the Interface between an Ionic Liquid and Tungsten Oxide in Ion-Gated Transistors

The structure of electrical double layers at electrified interfaces is of utmost importance for electrochemical energy storage as well as printable, flexible, and bioelectronic devices, such as ion-gated transistors (IGTs). Here we report a study based on atomic force microscopy force–distance profiling on electrical double layers forming at the interface between the ionic liquid 1-ethyl-3-methylimidazolium bis(trifluoromethylsulfonyl)imide and sol–gel films of mesoporous tungsten oxide. Here, we successfully followed, under in operando conditions, the evolution of the arrangement of the ions at the interface with the tungsten oxide films used as channel materials in IGTs. Our work sheds light on the mechanism of operation of IGTs, thus offering the possibility of optimizing their performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Enhanced Carbon‐Carbon Coupling at Interfaces with Abrupt Coordination Number Changes

Abstract Cu‐catalyzed electrochemical CO 2 reduction reaction (CO 2 RR) produces multi‐carbon (C 2+ ) chemicals with considerable selectivities and activities, yet required high overpotentials impede its practical application. Here, we design interfaces with abrupt coordination number (CN) changes that greatly reduce the applied potential for achieving high C 2+ Faradaic efficiency (FE). Encouraged by the mechanistic finding that the coupling between *CO and *CO(H) is the most probable C−C bond formation path, we use Cu 2 O‐ and Cu‐phthalocyanine‐derived Cu (OD−Cu and PD−Cu) to build the interface. Using operando X‐ray absorption spectroscopy (XAS), we find that the Cu CN of OD−Cu is ~11, favoring CO* adsorption, while the PD−Cu has a COH*‐favorable CN of ~4. Operando Raman spectroscopy revealed that the interfaces with abrupt CN changes promote *OCCOH formation. As a result, the designed catalyst achieves a C 2+ FE of 85±2 % at 220 mA cm −2 in a zero‐gap CO 2 electrolyzer. An improvement of C 2+ FE by 3 times is confirmed at the low potential regime where the current density is 60–140 mA cm −2 , compared to bare OD−Cu. We report a 45‐h stable CO 2 RR operation at 220 mA cm −2 , producing a C 2+ product FE of ~80 %.

Chemistry↗

Mechanical Milling – Induced Microstructure Changes in Argyrodite LPSCl Solid-State Electrolyte Critically Affect Electrochemical Stability

Microstructure of argyrodite solid-state electrolyte (SSE) critically affects lithium metal electrodeposition/dissolution. While the stability of unmodified SSE is mediocre, once optimized state-of-the-art electrochemical performance is achieved (symmetric cells, full cells with NMC811) without secondary interlayers or functionalized current collectors. Planetary mechanical milling in wet media (m-xylene) is employed to alter commercial Li 6 PS 5 Cl (LPSCl) powder. Quantitative stereology demonstrates how milling progressively refines grain and pore size/distribution in the SSE compact, increases its density, and geometrically smoothens the SSE-Li interface. Mechanical indentation demonstrates that these changes lead to reduced site-to-site variation in the compact's hardness. Milled microstructures promote uniform early-stage electrodeposition on foil collectors and stabilize solid electrolyte interphase (SEI) reactivity. Analysis of half-cells with bilayer electrolytes demonstrates the importance of microstructure directly contacting current collector, with interface roughness due to pore and grain size distribution being key. For the first time, short-circuiting Li metal dendrite is directly identified, employing 1.5 mm diameter “mini” symmetrical cell and cryogenic focused ion beam (cryo-FIB) electron microscopy. The branching sheet-like dendrite traverses intergranularly, filling the interparticle voids and forming an SEI around it. Importantly, mesoscale modeling reveals the relationship between Li-SSE interface morphology and the onset of electrochemical instability, based on underlying reaction current distribution.

25 ENERGY STORAGE↗

Thermally Driven Interfacial Degradation between Li 7 La 3 Zr 2 O 12 Electrolyte and LiNi 0.6 Mn 0.2 Co 0.2 O 2 Cathode

Solid-state batteries offer higher energy density and enhanced safety compared to the present lithium-ion batteries using liquid electrolytes. A challenge to implement them is the high resistances, especially at the solid electrolyte interface with the cathode. Sintering at elevated temperature is needed in order to get good contact between the ceramic solid electrolyte and oxide cathodes and thus to reduce contact resistances. Many solid electrolyte and cathode materials react to form secondary phases. It is necessary to find out which phases arise as a result of interface sintering and evaluate their effect on electrochemical properties. Herein, we assessed the interfacial reactions between LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) and Li 7 La 3 Zr 2 O 12 (LLZO) as a function of temperature in air. We prepared model systems by depositing thin-film NMC622 cathode layers on LLZO pellets. The thin-film cathode approach enabled us to use interface-sensitive techniques such as X-ray absorption spectroscopy in the near-edge as well as the extended regimes and identify the onset of detrimental reactions. We found that the Ni and Co chemical environments change already at moderate temperatures, on-setting from 500 °C and becoming especially prominent at 700 °C. By analyzing spectroscopy results along with X-ray diffraction, we identified Li 2 CO 3 , La 2 Zr 2 O 7 , and La(Ni,Co)O 3 as the secondary phases that formed at 700 °C. The interfacial resistance for Li transfer, measured by electrochemical impedance spectroscopy, increases significantly upon the onset and evolution of the detected interface chemistry. Our findings suggest that limiting the bonding temperature and avoiding CO 2 in the sintering environment can help to remedy the interfacial degradation.

36 MATERIALS SCIENCE↗

Oxide‐Based Solid‐State Batteries: A Perspective on Composite Cathode Architecture

Abstract The garnet‐type phase Li 7 La 3 Zr 2 O 12 (LLZO) attracts significant attention as an oxide solid electrolyte to enable safe and robust solid‐state batteries (SSBs) with potentially high energy density. However, while significant progress has been made in demonstrating compatibility with Li metal, integrating LLZO into composite cathodes remains a challenge. The current perspective focuses on the critical issues that need to be addressed to achieve the ultimate goal of an all‐solid‐state LLZO‐based battery that delivers safety, durability, and pack‐level performance characteristics that are unobtainable with state‐of‐the‐art Li‐ion batteries. This perspective complements existing reviews of solid/solid interfaces with more emphasis on understanding numerous homo‐ and heteroionic interfaces in a pure oxide‐based SSB and the various phenomena that accompany the evolution of the chemical, electrochemical, structural, morphological, and mechanical properties of those interfaces during processing and operation. Finally, the insights gained from a comprehensive literature survey of LLZO–cathode interfaces are used to guide efforts for the development of LLZO‐based SSBs.

25 ENERGY STORAGE↗

Digitalization of an experimental electrochemical reactor via the smart manufacturing innovation platform

The exponential increase in data produced over the last two decades has revolutionized the way we collect, store, process, analyze, model, and interpret information to improve profitability. Manufacturing is no exception. How- ever, Smart Manufacturing, the digital practice, organization, workforce, and infrastructure transformation for collection and deployment of data and models at scale and at all levels of manufacturing, is a complex, costly, and labor-intensive journey that is still seeing slow adoption. The Clean Energy Smart Manufacturing Innovation Institute (CESMII), a national Manufacturing USA public-private partnership sponsored by the Department of Energy, is addressing this scaled use of data and modeling in manufacturing. CESMII has focused on how to col- lect and use operating data for numerous applications that improve productivity, precision, and performance of manufacturing operations from factory floor to supply chain using process simulation, predictive analytics, mon- itoring and control, and real-time optimization. Because contextualized data are key, CESMII has developed the Smart Manufacturing Innovation Platform (SMIP) to lower the barriers to the data that are needed to accelerate data-based model building, improve data visualization, and more quickly gain insights. Reusable, standards-based ways of doing data collection, ingestion, and contextualization are particularly important for scaling access and use of data. The SMIP uses a standards-based definition and construct for reusable information models called an SM Profile. When an SM Profile is used in conjunction with the SMIP, the SMIP ensures the availability of contextualized, operational data for model building. The present work demonstrates Smart Manufacturing and the application of the SMIP for building several data-centered models for the operation and control of an ex- perimental electrochemical reactor that reduces carbon dioxide (CO 2 ) gas to valuable liquid and gas chemicals, such as alcohols, olefins, and syngas. We describe how the SMIP plays a central role in more effective model building and we demonstrate how the electochemical reactor can be controlled and optimized for the desired products. Use of the SMIP involves the transmission of real-time sensor measurements to a cloud resource so that the operating data are available to all model building experts. The data collection and transmission process is fully automated to greatly reduce the need for manual manipulation of the data. Data-driven machine learning models are used for advanced real-time state estimation, real-time optimization, and model-based feedback control for the reactor. The application models are implemented as a system to monitor the data flow and control the electrochemical reactor with a single visualization interface. SM Profiles are used to demonstrate reusability of the information models for the reactor and the instrumentation. The application packages, algorithms, and user interfaces developed are cast as Docker images in a library to facilitate reusability of the application models.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

pH-Driven Restructuring of Hydration Layers and Cation Adsorption at the Alumina–Water Interface

Oxide−water interfaces underpin ion separations, catalysis, and electrochemical energy technologies, where the electrical double layer (EDL) controls adsorption, transport, and reactivity. However, the molecular-scale links between pHdependent surface protonation, hydration-layer structure, and counterion adsorption remain poorly defined. Here, we combine in situ crystal truncation rod (CTR) and resonant anomalous X-ray reflectivity (RAXR) with streaming potential measurements and ab initio molecular dynamics (AIMD) simulations to resolve the chemical and structural evolution of the EDL at the single-crystal alumina (012)−water interface in 10 mM Rb + over pH 3−12. CTR measurements reveal two distinct adsorbed water layers at ∼2.2 and ∼3.5 Å above the surface. Each water layer shifts toward the substrate at transition pHs near 6.5 and 10.6, respectively, reflecting changes in primary hydration layer structure in response to the deprotonation of bridging and terminal aluminol groups. RAXR shows a 10-fold increase in Rb + coverage and a decrease in mean adsorption height from ∼3.5 to ∼2.7 Å with increasing pH, indicating enhanced counterion binding accompanied by Stern layer contraction. Streaming potential measurements demonstrate that the zeta potential, i.e., the potential at the hydrodynamic shear plane, is positive at pH 3 and becomes negative at pH ≥ 3.5. The negative charge magnitude increases with increasing pH, consistent with progressive surface deprotonation at higher pH. AIMD identifies inner- and outer-sphere Rb+ complexes whose adsorption heights and coordination geometries depend sensitively on the protonation state of surface oxygens, providing atomistic support for the experimentally inferred trends. These measurements establish two discrete, site-specific pH transitions in hydration-layer structure that track aluminol (de)protonation and quantitatively link them to a pH-driven contraction of the Stern layer (increasing Rb + coverage and decreasing adsorption height). This provides a direct structural basis for connecting surface acid−base chemistry to ion binding distances at an oxide−water interface.

Adsorption↗

pH-Driven Restructuring of Hydration Layers and Cation Ad-sorption at the Alumina-Water Interface

Oxide-water interfaces underpin ion separation, catalysis, and electrochemical energy technologies, where the electrical double layer (EDL) controls adsorption, transport, and reactivity. Yet, the molecular-scale link between pH-dependent surface protonation, hydration-layer structure, and counter-ion adsorption remains poorly defined. Here, we combine in situ crystal truncation rod (CTR) and resonant anomalous X-ray reflectivity (RAXR) with streaming potential measurements and ab initio molecular dynamics (AIMD) simulations to resolve the chemical and structural evolution of the EDL at the single-crystal alumina (012)-water interface in 10 mM Rb+ over pH 3-12. CTR measurements reveal two distinct adsorbed water layers at ~2.2 and ~3.5 Å above the surface that each shift toward the substrate at transition pHs near 6.5 and 10.6, respectively, directly reflecting changes in primary hydration layer structure in response to the deprotonation of bridging and terminal aluminol groups. RAXR shows a 10-fold increase in Rb+ coverage and a decrease in mean adsorption height from ~3.5 to ~2.7 Å with increasing pH, indicating enhanced counter-ion binding accompanied by Stern layer contraction. Streaming potential measurements demonstrate that the zeta potential, i.e., potential at the hydrodynamic shear plane, is positive at pH 3 and becomes negative at pH ≥3.5. This negative charge magnitude increases with increasing pH, consistent with progressive surface deprotonation at higher pH. AIMD identifies inner- and outer-sphere Rb+ complexes whose adsorption heights and coordination geometries depend sensitively on the protonation state of surface oxygens, providing atomistic support for the experimentally inferred trends. These measurements establish two discrete, site-specific pH transitions in hydration-layer structure that track aluminol (de)protonation and quantitatively link them to a pH-driven contraction of the Stern layer (increasing Rb+ coverage and decreasing adsorption height). This provides a direct structural basis for connecting surface acid-base chemistry to ion binding distances at an oxide-water interface.

Electrical double layer (EDL), Surface protonation↗