Synergistic role of carbonaceous reinforcements on multi length scale tribology of electrophoretically deposited nickel-boron nitride coatings
Highlights: • Electrophoretic deposition of Ni-BN coating. • Reinforcement of Ni-BN with carbon allotropes (diamond, carbon nanotubes and graphene). • Enhanced hardness and elastic modulus in Ni-BN-D than Ni-BN-CNT and Ni-BN-Gr. • High wear resistance (0.45 × 10{sup −8} m{sup 3}) from fretting and micro-scratch testing of Ni-BN-D. • High compressive stress (−601 MPa) exist in Ni-BN-D coating which restricts wear. - Abstract: Electrophoretically deposited Ni-BN composite coating was strengthened with graphene (Ni-BN-Gr), carbon nanotubes (Ni-BN-CNT) and diamond (Ni-BN-D) carbonaceous reinforcements. Highest hardness (2.0 GPa) and elastic modulus (133.5 GPa) of Ni-BN-D coating than Ni-BN-CNT (1.96 GPa and 102.1 GPa, respectively), Ni-BN-Gr (1.94 GPa and 92.0 GPa respectively) and also from Ni-BN (1.89 GPa and 91.5 GPa, respectively) coatings was linked through high compressive stress (−601 MPa), dislocation density (8.9 × 10{sup 15} m{sup −2}) and yield strength (4.4 GPa). The micro-scratching damage was contributed by ploughing and adhesion components, which were compared with that of experimental frictional values. Addition of graphene, CNT and diamond in Ni-BN composite showed a decrease in wear volume (from 1.66 × 10{sup −8} m{sup 3} to 0.45 × 10{sup −8} m{sup 3}) due to the synergetic lubricating effect of BN and carbonaceous reinforcements. Thus, Ni-BN-D restrict inception of multiscale wear and can be a potential three phase metal-ceramic coating for engineering and industrial applications.