Effect of prior creep at 1365 K on the room temperature tensile properties of several oxide dispersion strengthened alloys

An experimental study was conducted to determine whether oxide dispersion-strengthened (ODS) Ni-base alloys in wrought bar form are subject to creep degradation effects similar to those found in thin-gage sheet. The bar products evaluated included ODS-Ni, ODS-NiCr, and advanced ODS-NiCrAl types; the alloys included microstructures ranging from an essentially perfect single crystal to a structure consisting of very small elongated grains. Tensile test specimens were exposed to creep at various stress levels at 1365 K and then tensile tested at room temperature. Low residual tensile properties, change in fracture mode, appearance of dispersoid free bands, grain boundary cavitation, and/or internal oxidation are interpreted as creep degradation effects. The amount of degradation depends on creep strain, and degradation appears to be due to diffusional creep which produces dispersoid free bands around grain boundaries acting as vacancy sources.

Whittenberger, J. D.↗

Requirements for high-efficiency solar cells

Minimum recombination and low injection level are essential for high efficiency. Twenty percent AM1 efficiency requires a dark recombination current density of 2 x 10 to the minus 13th power A/sq cm and a recombination center density of less than 10 to the 10th power /cu cm. Recombination mechanisms at thirteen locations in a conventional single crystalline silicon cell design are reviewed. Three additional recombination locations are described at grain boundaries in polycrystalline cells. Material perfection and fabrication process optimization requirements for high efficiency are outlined. Innovative device designs to reduce recombination in the bulk and interfaces of single crystalline cells and in the grain boundary of polycrystalline cells are reviewed.

Sah, C. T.↗

Multiscale Modeling of Ultra High Temperature Ceramics (UHTC) ZrB2 and HfB2: Application to Lattice Thermal Conductivity

We are developing a multiscale framework in computational modeling for the ultra high temperature ceramics (UHTC) ZrB2 and HfB2. These materials are characterized by high melting point, good strength, and reasonable oxidation resistance. They are candidate materials for a number of applications in extreme environments including sharp leading edges of hypersonic aircraft. In particular, we used a combination of ab initio methods, atomistic simulations and continuum computations to obtain insights into fundamental properties of these materials. Ab initio methods were used to compute basic structural, mechanical and thermal properties. From these results, a database was constructed to fit a Tersoff style interatomic potential suitable for atomistic simulations. These potentials were used to evaluate the lattice thermal conductivity of single crystals and the thermal resistance of simple grain boundaries. Finite element method (FEM) computations using atomistic results as inputs were performed with meshes constructed on SEM images thereby modeling the realistic microstructure. These continuum computations showed the reduction in thermal conductivity due to the grain boundary network.

Lawson, John W.↗

Multiscale Modeling of UHTC: Thermal Conductivity

We are developing a multiscale framework in computational modeling for the ultra high temperature ceramics (UHTC) ZrB2 and HfB2. These materials are characterized by high melting point, good strength, and reasonable oxidation resistance. They are candidate materials for a number of applications in extreme environments including sharp leading edges of hypersonic aircraft. In particular, we used a combination of ab initio methods, atomistic simulations and continuum computations to obtain insights into fundamental properties of these materials. Ab initio methods were used to compute basic structural, mechanical and thermal properties. From these results, a database was constructed to fit a Tersoff style interatomic potential suitable for atomistic simulations. These potentials were used to evaluate the lattice thermal conductivity of single crystals and the thermal resistance of simple grain boundaries. Finite element method (FEM) computations using atomistic results as inputs were performed with meshes constructed on SEM images thereby modeling the realistic microstructure. These continuum computations showed the reduction in thermal conductivity due to the grain boundary network.

Lawson, John W.↗

Structural development in the Santa Catharina meteorite

A metallographic study was undertaken to seek support for the idea that Santa Catharina is really massive cloudy taenite. Available metal-rich nuggets of Santa Catharina appear to have been single crystals of taenite in the few centimeter size range, separated from each other by grain boundaries occupied by troilite and schreibersite. Metallographic and electron microprobe data allow one to postulate the following cooling and structural development history: (1) single crystal taenite formed at high temperature; (2) phosphate formed within the taenite and grain boundary schreibersite formed at interfaces with troilite or with other taenite crystals; (3) schreibersite began to precipitate within taenite at about 650 C; (4) at about 450 C the meteorite entered the three phase field at which point kamacite precipitated and started growing; and (5) kamacite/schreibersite interface measurements indicate that cooling continued down to about 350 C, with large Ni diffusion gradients developing within schreibersites.

Clarke, R. S., Jr.↗

Development of a Power Metallurgy Superalloy for Use at 1800-2000 F (980-1090 C)

A program was conducted to develop a powder metallurgy nickel-base superalloy for 1800-2000 F (980-1090 C) temperature applications. The feasibility of a unique concept for alloying carbon into a superalloy powder matrix and achieving both grain growth and a discrete particle grain boundary carbide precipitation was demonstrated. The process consisted of blending metastable carbides with a carbon free base alloy and consolidating this blend by hot extrusion. This was followed by heat treatment to grow a desired ASTM No. 2-3 grain size and to solution the metastable carbides to allow precipitation of discrete particle grain boundary carbides during subsequent aging heat treatments. The best alloy developed during this program was hydrogen-atomized, thermal-mechanically processed, modified MAR-M246 base alloy plus VC (0.28 w/o C). Although below those for cast MAR-M246, the mechanical properties exhibited by this alloy represent the best combination offered by conventional powder metallurgy processing to date.

Kortovich, C. S.↗

Role of Hf and Zr in the hydrogen embrittlement of Ta and Cb alloys

Investigation of the hydrogen embrittlement of aged Ta alloy T-111 (Ta-8W-2Hf) and similar Ta and Cb alloys. It is found that aging ternary Ta alloys such as T-111 near 1040 C for 1000 hr or longer increases their sensitivity to low-temperature hydrogen embrittlement. Segregation of Hf to grain boundaries during aging causes embrittlement upon testing at -196 C and is responsible for the observed hydrogen embrittlement. Binary Ta and Cb alloys, Ta-2Hf and Cb-1Zr, are not susceptible to hydrogen embrittlement under the conditions of this study and did not exhibit grain boundary segregation of Hf or Zr. Ternary alloys Ta-8W-.5Hf, Ta-8W-1Hf, and Ta-4W-2Hf are superior to T-111 for containment of alkali metals in that they do not exhibit aging embrittlement. However, these alloys in the aged condition are susceptible to hydrogen embrittlement.

Stephens, J. R.↗

Chemical Reactions in the Processing of Mosi2 + Carbon Compacts

Hot-pressing of MoSi2 powders with carbon at high temperatures reduces the siliceous grain boundary phase in the resultant compact. The chemical reactions in this process were examined using the Knudsen cell technique. A 2.3 wt pct oxygen MoSi2 powder and a 0.59 wt pct oxygen MoSi2 powder, both with additions of 2 wt pct carbon, were examined. The reduction of the siliceous grain boundary phase was examined at 1350 K and the resultant P(SiO)/P(CO) ratios interpreted in terms of the SiO(g) and CO(g) isobars on the Si-C-O predominance diagram. The MoSi2 + carbon mixtures were then heated at the hot-pressing temperature of 2100 K. Large weight losses were observed and could be correlated with the formation of a low-melting eutectic and the formation and vaporization of SiC.

Jacobson, Nathan S.↗

Room temperature tensile ductility in powder processed B2 FeAl alloys

It has been shown that it is possible to obtain significant room temperature tensile ductility in FeAl alloys using iron-rich deviations from stoichiometry. A comparison of the room temperature tensile and compressive behaviors of Fe-50 at. pct Al and Fe-40 at. pct Al shows that FeAl is brittle at higher Al contents because it fractures along grain boundaries before general yielding. Lower aluminum contents reduce the yield stress substantially and hence some ductility is observed before fracture. Addition of boron results in measurable improvements in ductility of Fe-40 at. pct Al and is accompanied by an increase in transgranular tearing on the fracture surface, suggesting a grain boundary strengthening mechanism. Increasing the cooling rate following annealing at 1273 K results in a large increase in the yield strength and a corresponding decrease in ductility.

Crimp, M. A.↗

Large-area silicon sheet task

A set of computer models was used to define a growth system configuration that was then built and used to grow web with lower thermally generated stress. Aspects of research in the edge-defined film-fed growth (EFG) method of making Si ribbon are reported. A technique was developed to determine base resistivity and carrier lifetime in semicrystalline wafers. Automated growth of 150 kg of 15 cm-dia ingot material per crucible is reviewed. Scanning transmisson electron microscopy (STEM) and microprobe investigations of processed EFG ribbon are reported. The chemical composition of the large precipitates was studied. The structural arrangement and the electrical activity of distentions or close to the central twin plane in processed material were studied. The electrical and structural properties of grain boundaries in silicon are discussed. Temperature-dependence measurements of zero-bias conductance, a photoconductivity technique, and deep-level transient spectroscopy (DLTS) were developed. A grooving and staining technique, secondary ion mass spectroscopy, and EBIC measurements in scanning electron microscopy were used to study enhanced diffusion of phosphorus at grain boundaries in polycrystaline silicon. The fundamental mechanisms of abrasion and wear and the deformation of Si by a diamond in various fluid environments are described. The efficiency of solar cells made from EFG ribbon and Semix Inc. material is reported.

Morrison, A. D.↗

Strength and microstructure of Si3N4 sintered with ZrO2 additions

Densities greater than 99 percent of theoretical were obtained with stabilized ZrO2 additions to Si3N4. Material sintered at 2140 C under 2.5 MPa nitrogen overpressure with 3.8, 9.9, and 13.4 wt pct ZrO2 had a predominantaly equiaxed grain size ranging from 0.2 to 7.0 microns. At 1370 C, the latter composition exhibited a flexural strength of about 487 MPa, equal to that of a finer-grain-size, hot-pressed Si3N4 + ZrO2 material having excellent high-temperature static fatigue properties. Transmission electron microscopy of the sintered Si3N4 revealed a glassy grain-boundary phase at all three ZrO2 levels and partially crystalline triple points for the 9.9 and 13.4 wt pct ZrO2-containing materials. Slow crack growth was observed for 1370 C flexure tests and correlated with nonlinear load deflection traces for stresses greater than 503 MPa. The crystallization of the grain-boundary glass is insterpreted as beneficial to the attainment of high (1370 C) flexural strength.

Sanders, W. A.↗

The impact of defects on the photovoltaic potential of RTR silicon ribbon

Silicon ribbon grown at a high rate by the ribbon-to-ribbon (RTR) method contains a variety of defects and can exhibit an unusual dendritic morphology. This paper is a study of the effect of the defect structure and dendritic morphology on the photovoltaic potential of RTR ribbon. Defects found in RTR ribbon include grain boundaries, twin planes, stacking faults and dislocations. The electrical activity of these defects is investigated by measuring the diffusion length in the ribbon; by fabricating small area diodes on the ribbon and evaluating their photoresponse; and by using a scanning electron microscope in the electron beam induced current mode. It is concluded that although grain boundaries serve very effectively as recombination centers, they do not occur frequently enough in RTR ribbons to significantly affect the generation current. Dislocation densities up to 1,000,000/sq cm can be tolerated without strongly reducing the photoresponse. Similarly, linear boundaries such as twin planes or stacking faults do not affect the cell performance up to densities of 1000/sq cm.

Baghdadi, A.↗

Ultrahigh Temperature Ceramics for Thermal Protection of Next Generation Space Vehicles

Materials with improved properties are needed for thermal protection of next generation space vehicles. Sharp leading edges on these vehicles will have to withstand exposure to high temperatures (> 2200 C or 4000 F) and severe thermal cycling in both neutral and oxidizing environments. These extreme conditions will require materials that possess superior oxidation resistance, low creep, and excellent thermal shock properties. This presentation will first discuss the system requirements for thermal protection of advanced space vehicles and then show how they are driving development of new materials systems. The presentation will focus on ultrahigh temperature ceramics (UHTCs) that are promising candidates for such applications. ZrB2 and HfB2 and composites of those ceramics with SiC are two particular families of UHTCs that are currently under development for sharp leading edges. These ceramics are appealing because their melting temperatures are 3245 C (5873 F) for ZrB2 and 3380 C (6116 F) for HfB2 and because they may form protective, oxidation resistant coatings in use. The mechanical properties of the UHTCs are strongly dependent on phase purity and the processing route used to make them, both of which factors are being actively investigated. For example, oxide impurities could form glassy grain boundary phases that soften at high temperatures and make the ceramic susceptible to creep deformation. Results from scanning and transmission electron microscopic studies of the UHTCs have shown how their processing can be improved to give better properties. This presentation will discuss the UHTC characterization results in some detail, focusing particularly on the structure and composition of the ceramic grain boundaries. The presentation will conclude with some remarks on how the properties of these promising UHTCs can be further improved and how they might be made more economically.

Loehman, R. E.↗

Alloy NASA-HR-1

NASA-HR-1 is a high-strength Fe-Ni-base superalloy that resists high-pressure hydrogen environment embrittlement (HEE), oxidation, and corrosion. Originally derived from JBK-75, NASA-HR-1 has exceptional HEE resistance that can be attributed to its gamma-matrix and eta-free (Ni3Ti) grain boundaries. The chemistry was formulated using a design approach capable of accounting for the simultaneous effects of several alloy additions. This approach included: (1) Systematically modifying gamma-matrix compositions based on JBK-75; (2) Increasing gamma (Ni3(Al,Ti)) volume fraction and adding gamma-matrix strengthening elements to obtain higher strength; and (3) Obtaining precipitate-free grain boundaries. The most outstanding attribute of NASA-HR-1 is its ability to resist HEE while showing much improved strength. NASA-HR-1 has approximately 25% higher yield strength than JXK-75 and exhibits tensile elongation of more than 20% with no ductility loss in a hydrogen environment at 5 ksi, an achievement unparalleled by any other commercially available alloy. Its Cr and Ni contents provide exceptional resistance to environments that promote oxidation and corrosion. Microstructural stability was maintained by improved solid solubility of the gamma-matrix, along with the addition of alloying elements to retard eta (Ni3Ti) precipitation. NASA-HR-1 represents a new system that greatly extends the compositional ranges of existing HEE-resistant Fe-Ni-base superalloys.

Chen, Po-Shou↗

High temperature low cycle fatigue mechanisms for nickel base and a copper base alloy

Damage mechanisms were studied in Rene' 95 and NARloy Z, using optical, scanning and transmission in microscopy. In necklace Rene' 95, crack initiation was mainly associated with cracking of surface MC carbides, except for hold time tests at higher strain ranges where initiation was associated more with a grain boundary mechanism. A mixed mode of propagation with a faceted fracture morphology was typical for all cycle characters. The dependence of life on maximum tensile stress can be demonstrated by the data falling onto three lines corresponding to the three tensile hold times, in the life against maximum tensile stress plot. In NARloy Z, crack initiation was always at the grain boundaries. The mode of crack propagation depended on the cycle character. The life decreased with decreasing strain rate and with tensile holds. In terms of damage mode, different life prediction laws may be applicable to different cycle characters.

Shih, C. I.↗

Mineralogy and Petrology of Amoeboid Olivine Inclusions in CO3 Chondrites: Relationship to Parent-Body Aqueous Alteration

Petrographic and mineralogic studies of amoeboid olivine inclusions (AOIs) in CO3 carbonaceous chondrites reveal that they are sensitive indicators of parent-body aqueous and thermal alteration. As the petrologic subtype increases from 3.0 to 3.8, forsteritic olivine (Fa(sub 0-1)) is systematically converted into ferroan olivine (Fa(sub 60-75)). We infer that the Fe, Si and O entered the assemblage along grain boundaries, forming ferroan olivine that filled fractures and voids. As temperatures increased, Fe(+2) from the new olivine exchanged with Mg(+2) from the original AOI to form diffusive haloes around low-FeO cores. Cations of Mn(+2), Ca(+2) and Cr(+3) were also mobilized. The systematic changes in AOI textures and olivine compositional distributions can be used to refine the classification of CO3 chondrites into subtypes. In subtype 3.0, olivine occurs as small forsterite grains (Fa(sub 0-1)), free of ferroan olivine. In petrologic subtype 3.2, narrow veins of FeO-rich olivine have formed at forsterite grain boundaries. With increasing alteration, these veins thicken to form zones of ferroan olivine at the outside AOI margin and within the AOI interior. By subtype 3.7, there is a fairly broad olivine compositional distribution in the range Fa(sub 63-70), and by subtype 3.8, no forsterite remains and the high-Fa peak has narrowed, Fa(sub 64-67). Even at this stage, there is incomplete equilibration in the chondrite as a whole (e.g., data for coarse olivine grains in Isna (CO3.8) chondrules and lithic clasts show a peak at Fa(sub39)). We infer that the mineral changes in A01 identified in the low petrologic types required aqueous or hydrothermal fluids whereas those in subtypes greater than or equal to 3.3 largely reflect diffusive exchange within and between mineral grains without the aid of fluids.

Chizmadia, Lysa J.↗

Flow and fracture behavior of NiAl in relation to the brittle-to-ductile transition temperature

NiAl has only three independent slip systems operating at low and intermediate temperatures whereas five independent deformation mechanisms are required to satisfy the von Mises criterion for general plasticity in polycrystalline materials. Yet, it is generally recognized that polycrystalline NiAl can be deformed extensively in compression at room temperature and that limited tensile ductility can be obtained in extruded materials. In order to determine whether these results are in conflict with the von Mises criterion, tension and compression tests were conducted on powder-extruded, binary NiAl between 300 and 1300 K. The results indicate that below the brittle-to-ductile transition temperature (BDTT) the failure mechanism in NiAl involves the initiation and propagation of cracks at the grain boundaries which is consistent with the von Mises analysis. Furthermore, evaluation of the flow behavior of NiAl indicates that the transition from brittle to ductile behavior with increasing temperature coincides with the onset of recovery mechanisms such as dislocation climb. The increase in ductility above the BDTT is therefore attributed to the climb of the 001 line type dislocations which in combination with dislocation glide enable grain boundary compatibility to be maintained at the higher temperatures.

Noebe, R. D.↗

Formation of Oxides in the Interior of Friction Stir Welds

In friction stir welding (FSWing) the actual solid state joining takes place between the faying surfaces which form the weld seam. Thus the seam trace is often investigated for clues when the strength of the weld is reduced. Aluminum and its alloys are known to form a native, protective oxide on the surface. If these native surface oxides are not sufficiently broken up during the FSW process, they are reported to remain in the FSW interior and weaken the bond strength. This type of weld defect has been referred to as a lazy "S", lazy "Z", joint line defect, kissing bond, or residual oxide defect. Usually these defects are mitigated by modification of the process parameters, such as increased tool rotation rate, which causes a finer breakup of the native oxide particles. This study proposes that there may be an alternative mechanism for formation of oxides found within the weld nugget. As the oxidation rate increases at elevated temperatures above 400ºC, it may be possible for enhanced oxidation to occur on the interior surfaces during the FSW process from entrained air entering the seam gap. Normally, FSWs of aluminum alloys are made without a purge gas and it is unknown how process parameters and initial fit up could affect a potential air path into the interior during the processing. In addition, variations in FSW parameters, such as the tool rotation, are known to have a strong influence on the FSW temperature which may affect the oxidation rate if internal surfaces are exposed to entrained air. A series of FSWs were made in 3 different thickness panels of AA2219 (0.95, 1.27 and 1.56 cm) at 2 different weld pitches. As the thickness of the panels increased, there was an increased tendency for a gap to form in advance of the weld tool. If sufficient air is able to enter the workpiece gap prior to consolidation, the weld temperature can increase the oxidation rate on the interior surfaces. These oxidation rates would also be accelerated in areas of localized liquation. Metallographs from the weld panels showed indications of liquation at the grain boundaries. In FSWs of thicker panels, these regions of liquation were found to be heavily oxidized. The quality of the FSWs was evaluated from tensile testing at room temperature. As the panel thickness increased, a slight decrease in tensile strength was observed which was attributed to the presence of oxides. No oxide formation was observed in the thinner workpieces, although there were indications of localized liquation at the grain boundaries. Results from this study will assist in a better understand of the mechanisms of oxide formation in FSW interiors and provide methodology for minimizing their occurrence.

Schneider, Judy↗