Search NASA⌕ Search

SEARCH · Search NASA

Results for “Lithium plating”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Electrochemically induced amorphous-to-rock-salt phase transformation in niobium oxide electrode for Li-ion batteries

Intercalation-type metal oxides are promising negative electrode materials for safe rechargeable lithium-ion batteries due to the reduced risk of Li plating at low voltages. Nevertheless, their lower energy and power density along with cycling instability remain bottlenecks for their implementation, especially for fast-charging applications. Here, we report a nanostructured rock-salt Nb 2 O 5 electrode formed through an amorphous-to-crystalline transformation during repeated electrochemical cycling with Li + . This electrode can reversibly cycle three lithiums per Nb 2 O 5 , corresponding to a capacity of 269 mAh g –1 at 20 mA g –1 , and retains a capacity of 191 mAh g –1 at a high rate of 1 A g –1 . Further, it exhibits superb cycling stability with a capacity of 225 mAh g –1 at 200 mA g –1 for 400 cycles, and a Coulombic efficiency of 99.93%. We attribute the enhanced performance to the cubic rock-salt framework, which promotes low-energy migration paths. Our work suggests that inducing crystallization of amorphous nanomaterials through electrochemical cycling is a promising avenue for creating unconventional high-performance metal oxide electrode materials.

25 ENERGY STORAGE↗

Final Design for Thermal/Epithermal eXperiments (TEX) with Lithium Absorbers to Provide Validation Benchmarks for Y-12 Electrorefining Facility

One of the main goals of the Thermal/Epithermal eXperiments (TEX) project is to use existing Nuclear Criticality Safety Program (NCSP) assets to create critical experiment plutonium and uranium test beds for materials important to criticality safety that have insufficient benchmark evaluations. The plutonium test bed experiments were completed in 2018 and are published in the 2020 edition of the International Criticality Safety Benchmark Evaluation Project (ICSBEP) Handbook. The uranium test bed assemblies were completed in 2023 and accepted in the 2024 edition of the ICSBEP Handbook. The Nuclear Criticality Safety (NCS) group at Y-12 National Security Complex has identified programmatic need for validation cases for uranium electrorefining operations at Y-12. The electrorefining operation credits lithium enriched in 6 Li in addition to 35 Cl as absorbers in the design criticality safety evaluation for precluding criticality under upset conditions in the large and geometrically unfavorable electro-refiner. There is, however, inadequate experimental validation for the 6 Li absorbers. As an extension of the TEX uranium test bed, TEX-Cl critical experiments were performed with sodium chloride salt to address the 35 Cl thermal absorption as well as other validation needs at Los Alamos National Laboratory (LANL). These experiments were completed in 2024 and accepted into the 2025 ICSBEP Handbook. To continue the methodology used in TEX-Cl, TEX-Li aims to accomplish the same. The overall design of both experiments was to use commercially available, high purity, salts with polyethylene moderator and HEU plates to configure a critical assembly. Three experiments are planned for TEX-Li using encapsulated lithium carbonate (Li 2 CO 3 ), with natural 6 Li abundance. For all experiments, the highly enriched uranium (HEU) Jemima plates will be used as fissile material. Multiple layers will be stacked together with encapsulated Li 2 CO 3 alternated with polyethylene in standard configurations. Standard stacking was found to be optimal in matching the different sensitivity profiles provided by the Y-12 models. Three configurations are proposed with varying polyethylene moderation and a constant 1/4” absorber thickness. The first uses 11 layers of 5/4” polyethylene, the second uses 9 layers of 3/4” polyethylene, and the third uses 10 layers of 1/2” polyethylene. Calculations showed that some alternative forms of lithium-based materials provided slightly less-optimal sensitivity profiles when compared to lithium carbonate but come with other drawbacks. These alternatives included lithium aluminate (LiAlO 2 ), Aluminum-2050 alloy, Aluminum-8090, Aluminum-2095, lithium hydride (LiH), and lithium fluoride (LiF). Lithium aluminate and aluminum-2050 provided comparable sensitivity profiles when compared to lithium carbonate and can be used instead if lithium carbonate cannot be readily procured. After a broad material study, lithium carbonate outperformed any alternative material with a balance in affordability and workability. The assessment of experimental uncertainties of the non-absorber and absorber components was predicted to be 0.00089 and 0.00093 Δk eff , respectively. The largest uncertainties may be reduced with precision dimensional inspection of the components. Many of the parts and equipment for IER 575 have already been fabricated or procured for previous projects and therefore do not contribute significantly to the overall cost of this experiment. This includes the Jemima plates and Comet critical assembly machine, which are existing NCSP assets, as well as the aluminum platen and polyethylene reflector rings, which were fabricated and authorized for the TEX experiment involving HEU with polyethylene. Lithium carbonate containers will be procured by LANL and will be filled by LLNL. The total material costs for TEX-Li experiments are estimated to be on the order of $\$$47,400. Precision inspection, including dimensional, mass, density, and impurity, is recommended for all components for an estimated cost of $\$$12,000.

35Cl↗

Increasing the Pressure‐Free Stripping Capacity of the Lithium Metal Anode in Solid‐State‐Batteries by Carbon Nanotubes

Abstract Lithium metal is the key anode material for solid‐state‐batteries as its successful implementation will drastically increase their energy and power densities. However, anode contact loss during stripping leads to dendrites upon plating and subsequent cell failure. Design strategies to mitigate these issues are crucial to enable the use of lithium metal anodes. This paper reports the dissolution kinetics of composite anodes made of lithium metal and carbon nanotubes (CNTs) with a garnet‐type solid electrolyte (SE). In addition to an enhancement of the effective diffusion within the anode, its dissolution is fundamentally changed from being 2D to 3D. By maintaining contact with the SE, the CNTs facilitate lithium transport to the interface, which yields more than 20 mAh cm −2 discharge capacity at 100 µ A cm −2 without the application of external stack pressure ( > 1 MPa). Conclusions drawn from electrochemical data on the anode microstructure are validated using cryo‐focused‐ion‐beam scanning electron microscopy and correlated with the mechanical properties. Micro‐indentation, acoustic analysis, and stress–strain testing show that mechanical properties of the anode, like yield strength and hardness, are adjustable. Overall, it is shown that the mechanical and electrochemical properties of Li–CNT composite electrodes can be tailored to suit the requirements of a practical cell.

Fuchs, Till↗

Toward Lithium Recovery Using Modular (and Membraneless) Phase Separation and Extraction (MPSE) Technology with Ionic Liquid (IL) Solvents: Effect of Coatings

In this work, a single-channel slope-plate Modular and Membrane-less Phase Separation and Extraction (MPSE) device was fabricated using 3D printing. The slope-plate was designed with an insertable glass slide to enable surface modification with coatings. Self-assembled monolayers (SAMs) and perfluoropolyether (Zdol) coatings were applied to tailor surface wettability and enhance phase separation. Using a model biphasic system of water and hexadecane, both coatings significantly improved the separation efficiency compared to the uncoated device by promoting selective wetting. Building on these results, lithium extraction from a simulated saline solution was investigated using 1-ethyl-3-methylimidazolium bis(trifluoromethylsulfonyl)imide ([EMIM][NTf₂]) as the ionic liquid (IL) extractant. The IL effectively extracted Li⁺ from the aqueous phase in bulk extraction, demonstrating its potential for lithium recovery. However, the low interfacial tension between the IL and aqueous phases posed challenges for phase separation. The application of SAM and Zdol coatings effectively mitigated this issue. Overall, integrating tailored surface chemistry with the slope-plate MPSE design shows great promise as an efficient and scalable platform for studying liquid–liquid separation and optimizing ionic liquid–based extraction processes for lithium recovery from saline sources.

3D printing↗

Electrochemical Formation of Li-M-(M')-Si Phases Using Multivalent Electrolyte Salt Additives

Lithium-rich silicides (Li 15 Si 4 ), formed during the electrochemical lithiation of silicon, show high reactivity with electrolyte components that contribute to capacity decay, formal lithium loss, and low coulombic efficiency. Recently, the reactivity of lithium silicides was found to be suppressed by substituting a multivalent cation (i.e. Mg, Ca) for lithium that results in the room temperature formation of a ternary Li-M-Si phase. In this study, we explored a range of multivalent electrolyte salt additives (M = Ni, Cu, La, Ce, Sr, Ba, and Ca-Mg mixed salt) in a lithium-ion cell configuration and identified a room temperature electrochemical route to the formation of new ternary and quaternary lithium silicides. Using this method, both nickel and copper salts were found to plate onto the silicon electrode surface upon lithiation. Further, based on refined synchrotron XRD data, multivalent cations with an ionic radius similar to Na (~1.03 Å) or smaller can be inserted electrochemically into a formally cation-deficient Li 15 Si 4 host lattice to form new ternary (or quartenary) phases. The electrochemical synthesis of a new quaternary Li-M-M’-Si phase represents a facile route to preparing and scaling materials isostructural to the Heusler phase and electron-precise Li 14 MgSi 4 phase that results in enhanced cycling and calendar life performance.

25 ENERGY STORAGE↗

Fundamental Studies of Tritium Formation and Diffusivity in Pure and Defective Zircaloy-4 Getters

Zirconium (Zr) and its alloys are used as fuel cladding in nuclear reactors. These materials have their low absorption cross-section for thermal neutrons and have good mechanical and thermal properties. In addition, they are used as tritium getters in tritium-producing burnable absorber rods (TPBARs), in the form of nickel-plated Zircaloy-4 tubes. To produce 3 H, the breading blankets such as lithium aluminate are irradiated in pressurized water. 3 H produced in this process is captured by the getter and 3 H reacts chemically with Zr to form metal hydride (ZrTx). The precipitation of metal hydride results in not only the volume increase and hydrogen embrittlement of zircaloy but also changes in getter’s chemical properties. This degrades the getter’s performance. Therefore, understanding the behavior of 3 H (such as diffusion and solubility) in zircaloy is important to understand getter performance.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

In Situ Li Seed Formation Enables Uniform Plating in Anode-Free Solid-State Batteries

Anode-free solid-state batteries (AFSSBs) are a promising route toward achieving high energy density. In these cells, the anode contains no pre-stored lithium (Li). Instead, all Li inventory originates from the cathode and is freshly deposited onto a bare current collector during charging. However, achieving uniform and defect-free Li plating on this bare current collector remains a major challenging, often resulting in low Li plating/stripping efficiency and rapid capacity decay. Here, for the first time, operando neutron imaging is employed to visualize Li plating/stripping behavior in an anode-free full cell with LiNi 0.82 Mn 0.07 Co 0.11 O 2 (NMC) as the cathode. Operando measurements reveal that complete stripping of Li leaves isolated Li residues on the current collector, which degrades interfacial contact between the current collector and solid-state electrolyte. To mitigate this interfacial issue and promote more uniform Li deposition, we implement a discharge cutoff voltage strategy that intentionally retains a thin residual Li layer after stripping. This thin Li layer, serving as an in situ–formed seed layer, not only enables more homogeneous subsequent Li plating but also improves interfacial contact. As a result, the anode-free cell with a controlled discharge voltage of 3.5 V exhibits excellent long-term cycling stability, maintaining a discharge capacity of 116 mAh g -1 with a retention rate of 83.4% and an average Coulombic efficiency of approximately 99.9% after 430 cycles at 0.25 C. In contrast, the cell with a conventional discharge cutoff voltage of 2.8 V exhibits rapid capacity decay, retaining only 59.7 mAh g -1 after 50 cycles with a capacity retention of 40.7%. This work offers a practical strategy to unlock the long-term viability of anode-free solid-state batteries.

25 ENERGY STORAGE↗

Resolving Current-Dependent Regimes of Electroplating Mechanisms for Fast Charging Lithium Metal Anodes

Poor fast-charge capabilities limit the usage of rechargeable Li metal anodes. Understanding the connection between charging rate, electroplating mechanism, and Li morphology could enable fast-charging solutions. In this report we develop a combined electroanalytical and nanoscale characterization approach to resolve the current-dependent regimes of Li plating mechanisms and morphology. Measurement of Li + transport through the solid electrolyte interphase (SEI) shows that low currents induce plating at buried Li||SEI interfaces, but high currents initiate SEI-breakdown and plating at fresh Li||electrolyte interfaces. The latter pathway can induce uniform growth of {110}-faceted Li at extremely high currents, suggesting ion-transport limitations alone are insufficient to predict Li morphology. At battery relevant fast-charging rates, SEI-breakdown above a critical current density produces detrimental morphology and poor cyclability. Thus, prevention of both SEI-breakdown and slow ion-transport in the electrolyte is essential. This mechanistic insight can inform further electrolyte engineering and customization of fast-charging protocols for Li metal batteries.

25 ENERGY STORAGE↗

Low-temperature and high-rate-charging lithium metal batteries enabled by an electrochemically active monolayer-regulated interface

Stable operation of rechargeable lithium (Li)-based batteries at low temperatures is vital for cold-climate applications but is plagued with dendritic Li plating and unstable solid-electrolyte interphase (SEI). Here we report high-performance Li-metal batteries under low-temperature and high-rate-charging conditions. This is realized by utilizing a self-assembled monolayer of electrochemically active molecules on current collectors that regulates the nanostructure and composition of SEI and deposition morphology of Li metal anodes. A multilayer SEI containing a LiF-rich inner phase and amorphous outer layer effectively seals the Li surface in contrast to the conventional impassive SEI at low temperatures. As a result, galvanic Li corrosion and self-discharge were suppressed; stable Li deposition was realized from -60º to 45ºC; and a Li|LiCoO 2 cell with a capacity of 2.0 mAh cm -2 displayed a 200-cycle life at -15ºC with a recharge time of 45 minutes.

25 ENERGY STORAGE↗

The Impact of Lithium Anode Interface on Capacity Fade in Polymer Electrolyte-Based Solid-State Batteries

This study investigates the Li stripping-plating morphology and failure mechanisms in full cells consisting of a solid polymer electrolyte (SPE) with two commercial Li anodes: Li chip and Li foil. The primary identified failure mechanism of the SPE cell is capacity fade, regardless of the Li manufacturer. While the cathode’s role in capacity fade is evident, the Li anode significantly influences cycling performance, with Li foil cells cycling 50% longer than Li chip cells, a statistical difference. Further, post-mortem scanning electron microscopy and X-ray photoelectron spectroscopy results attribute the Li chip’s faster capacity fade to a loss of contact and continuous growth of the solid electrolyte interphase (SEI). Conversely, Li foil maintains consistent contact with the solid polymer, displaying a thin and stable SEI. Additionally, failure mechanisms between a gel electrolyte in previous work and the dry SPE are compared.

25 ENERGY STORAGE↗

Modeling the influence of the solid electrolyte interphase on the sand’s time and dendrite formation on lithium metal electrodes

Lithium metal is a sought after battery material for its high energy density due to the low electrochemical potential and density. However, lithium metal is also highly reactive, which results in a strong propensity for dendrite formation. The Sand’s time has previously been used to predict the time of dendrite initiation on metals that do not form a solid-electrolyte interphase (SEI), but it has been shown that the Sand’s time is not accurate for lithium electrodes when using transport parameters associated with the electrolyte. Thus, we built a numerical model to simulate lithium ion transport through a growing SEI to predict the Sand’s time. The numerical model is shown to be more accurate than previous analytical solutions, especially for low current densities. We then analyze the sensitivity of the Sand’s time to different SEI properties and the chemical potential gradients present in the SEI, driving lithium transport. The results showed that high lithium concentration has a greater impact at high current density, while fast diffusivity is more important at low current density. Lastly, we modeled the influence of surface roughness on the plating evolution and chemical potential gradients when an SEI is present in comparison to the electrolyte. As a result, we demonstrate that the SEI plays a critical role in lithium electrode stability, and that improved characterization techniques are needed to better understand transport through the SEI and increase lithium metal utilization in energy storage devices.

Chemistry↗

The Critical Stack Pressure to Alter Void Generation at Li/Solid-Electrolyte Interfaces during Stripping

The lithium stripping process generates vacancies, which may accumulate as voids and lead to uneven current distribution and dendrite growth in the following plating cycles. A stack pressure is typically required during stripping, but how to optimize the stack pressure is not clear. In this work, extremely lithiophilic Li/Li 2 O and lithiophobic Li/LiF interfaces were used to reveal the combining effect of interface interaction and stack pressure induced lithium creep on the stripping critical current density (CCD). A multiscale simulation scheme with Density Functional Theory (DFT), kinetic Monte Carlo (KMC) simulations, and an analytical model was developed. The analytical model predicted lithiophobic interfaces require a higher stack pressure than lithiophilic interfaces to reach the same CCD. The KMC simulations also showed higher stack pressure is needed at lithiophobic interfaces to accelerate Li vacancy diffusion into the bulk and maintain a flat surface. This stack pressure needs to be high enough to alter the Li forward-and-backward hopping barriers at the interface. This multiscale simulation scheme illustrates the importance to include the chemical-mechanical effects during Li stripping morphology evolution. It can be used to design ideal interlayer coating materials to maintain a flat Li surface during cycling.

25 ENERGY STORAGE↗

Dual Passivation of Cathode and Anode through Electrode–Electrolyte Interface Engineering Enables Long-Lifespan Li Metal–SPAN Batteries

The reliability and durability of lithium metal (Li 0 )–sulfur batteries are largely limited by the undesired Li 0 plating-stripping irreversibility and the detrimental polysulfide dissolution, yet approaches that can simultaneously address the above anodic and cathodic problems are scarce. In this study, we report the stable operation of a Li 0 -SPAN (sulfurized polyacrylonitrile) battery via an anode–cathode dual-passivation approach. By combination of a fluorinated localized high concentration electrolyte (LHCE) and a Li 3 N-forming additive (TMS-N 3 ), robust and highly conductive electrode passivation layers are formed in situ on the surface of both the Li 0 anode and the SPAN cathode. The resulting highly reversible, dendrite-free, and high-density Li 0 plating morphology enables a high Coulombic efficiency of 99.4%. Advanced tender energy X-ray spectroscopy also reveals the eliminated Li 2 S formation and minimized polysulfide dissolution in SPAN cathodes, leading to a high capacity of 580 mAh/g SPAN and stable cycling with negligible capacity decay (0.7%) for 800 cycles. This electrode–electrolyte interphase engineering strategy has tackled the major limitations of Li–S batteries in both ether- and carbonate-based electrolyte systems and under a wide temperature range from –10 to +50 °C, thus providing insightful guidelines for the rational design of highly durable and high-energy-density Li 0 -S batteries.

25 ENERGY STORAGE↗

The passivity of lithium electrodes in liquid electrolytes for secondary batteries

Rechargeable Li metal batteries are currently limited by electrolyte decomposition and rapid Li consumption. Li plating and stripping greatly depend on the solid electrolyte interphase formed at the Li metal-liquid electrolyte interface. This Review discusses the reactions occurring at this interface from a corrosion science perspective, highlighting the requirements for an ideal passivation layer. Rechargeable Li metal batteries are currently limited by safety concerns, continuous electrolyte decomposition and rapid consumption of Li. These issues are mainly related to reactions occurring at the Li metal-liquid electrolyte interface. Additionally, the formation of a passivation film (that is, a solid electrolyte interphase) determines ionic diffusion and the structural and morphological evolution of the Li metal electrode upon cycling. In this Review, we discuss spontaneous and operation-induced reactions at the Li metal-electrolyte interface from a corrosion science perspective. We highlight that the instantaneous formation of a thin protective film of corrosion products at the Li surface, which acts as a barrier to further chemical reactions with the electrolyte, precedes film reformation, which occurs during subsequent electrochemical stripping and plating of Li during battery operation. Finally, we discuss solutions to overcoming remaining challenges of Li metal batteries related to Li surface science, electrolyte chemistry, cell engineering and the intrinsic instability of the Li metal-electrolyte interface.

25 ENERGY STORAGE↗

Recent advances in plasma control and physics research in the Large Helical Device

The Large Helical Device (LHD), the largest superconducting helical system in the world, is equipped with advanced heating and diagnostic tools, facilitating plasma control and physics research. Data assimilation was employed for electron temperature control using a real-time Thomson scattering system and real time prediction code. A virtual LHD environment enabled visualization of escaping high-energy tritium ions and demonstrated that these ions impact the rear side of the divertor plate. Pioneering results crucial to plasma control have also been achieved. Real-time wall conditioning using Lithium granule dropping improved bulk ion energy and particle transport while simultaneously enhancing the heavy impurity transport. Progress has also been made in the investigation of turbulence-driven transport. At the confinement bifurcation, ion-scale turbulence decreased, while electron-scale turbulence increased. A change in the anisotropy of turbulent eddies was also observed at the confinement bifurcation. Coexistence of local and non-local turbulence was identified in electron-scale turbulence. Non-local turbulence exhibited the rapid spatial propagation of perturbations throughout the plasma, while local turbulence followed the temperature gradient. A transition between drift-wave turbulence and magnetohydrodynamics (MHD) turbulence was observed with the turbulence minimized at the transition condition. Machine learning analysis was employed to evaluate the temperate and density conditions of this turbulence transition. Then, real-time control of fueling and heating was applied to maintain the turbulence transition condition, improving the energy confinement enhancement factor by 20%. In addition, evidence was obtained for collisionless ion heating by energetic-ion-driven geodesic acoustic modes and MHD bursts. These achievements represent unique contributions to the development of fusion reactors.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

On the crystallography and reversibility of lithium electrodeposits at ultrahigh capacity

Abstract Lithium metal is a promising anode for energy-dense batteries but is hindered by poor reversibility caused by continuous chemical and electrochemical degradation. Here we find that by increasing the Li plating capacity to high values ( e.g ., 10–50 mAh cm −2 ), Li deposits undergo a morphological transition to produce dense structures, composed of large grains with dominantly (110) Li crystallographic facets. The resultant Li metal electrodes manifest fast kinetics for lithium stripping/plating processes with higher exchange current density, but simultaneously exhibit elevated electrochemical stability towards the electrolyte. Detailed analysis of these findings reveal that parasitic electrochemical reactions are the major reason for poor Li reversibility, and that the degradation rate from parasitic electroreduction of electrolyte components is about an order of magnitude faster than from chemical reactions. The high-capacity Li electrodes provide a straightforward strategy for interrogating the solid electrolyte interphase (SEI) on Li —with unprecedented, high signal to noise. We find that an inorganic rich SEI is formed and is primarily concentrated around the edges of lithium particles. Our findings provide straightforward, but powerful approaches for enhancing the reversibility of Li and for fundamental studies of the interphases formed in liquid and solid-state electrolytes using readily accessible analytical tools.

59 BASIC BIOLOGICAL SCIENCES↗

CRADA Final Report: Ultralong Cycle Life and Ultrafast Charging Batteries to Electrify High Duty-Cycle, Mobile Platforms

As part of the Cyclotron Road program, Tyfast Energy Corp. aimed to investigate the Li 3 V 2 O 5 (LVO) anode material for next generation lithium batteries. State of the art and fast charging lithium-ion batteries are based on the lithium titanate or Li 4 Ti 5 O 12 (LTO) anode chemistry. LTO cells demonstrate fast charging times (<6 mins), long cycle life (>20,000 cycles), but at the expense of very low energy density (<200Wh/L, <80Wh/kg). Silicon anodes have the promise of achieving fast charging times, however, issues with cycling stability in combination with fast charging is unknown. LVO has unique properties that enable new performance window for lithium batteries. First, LVO operates at an average potential of 0.6V vs. Li/Li + , well above the Li-metal plating region allowing ultrafast charge capability without sacrificing safety. Second, the LVO has a high specific capacity of 250 mAh/g making battery pack energy density equivalent with current high-energy Li-ion chemistries.

25 ENERGY STORAGE↗

A Self-Healable Sulfide/Polymer Composite Electrolyte for Long-Life, Low-Lithium-Excess Lithium-Metal Batteries

Solid electrolyte-protected lithium-metal anodes promise energy-dense, safe cells. While sulfide solid electrolytes enable facile processability and fast ion transport, they suffer from complex chemo-mechanical issues, including Li plating-induced fracture and Li stripping-induced contact loss. To address these issues, a grafting approach is implemented to functionalize the sulfide solid electrolyte (Li 3,85 Sn 0.85 Sb 0.15 S 4 ) with a self-healing unit. This leads to a dynamic bonding between the solid electrolyte network and a mechanically robust polymer scaffold, which reversibly accommodates the volume changes of the lithium-metal anode. Thus, the approach improves the interfacial contact between the lithium-metal anode and the composite electrolyte, enabling stable cycling at a mild stack pressure (160 kPa). With a negative to positive capacity ratio equals to 1, pouch full cells with a high-nickel cathode (nickel content > 90%) and lithium-metal anode display 92% capacity retention for 140 cycles. Engineering the interface between solid electrolyte and the polymeric binder offers a promising pathway to address the chemo-mechanical issues.