Search NASA⌕ Search

SEARCH · Search NASA

Results for “SILICONES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Influence of hydrogen effusion from hydrogenated silicon nitride layers on the regeneration of boron-oxygen related defects in crystalline silicon

The degradation effect boron doped and oxygen-rich crystalline silicon materials suffer from under illumination can be neutralized in hydrogenated silicon by the application of a regeneration process consisting of a combination of slightly elevated temperature and carrier injection. In this paper, the influence of variations in short high temperature steps on the kinetics of the regeneration process is investigated. It is found that hotter and longer firing steps allowing an effective hydrogenation from a hydrogen-rich silicon nitride passivation layer result in an acceleration of the regeneration process. Additionally, a fast cool down from high temperature to around 550 °C seems to be crucial for a fast regeneration process. It is suggested that high cooling rates suppress hydrogen effusion from the silicon bulk in a temperature range where the hydrogenated passivation layer cannot release hydrogen in considerable amounts. Thus, the hydrogen content of the silicon bulk after the complete high temperature step can be increased resulting in a faster regeneration process. Hence, the data presented here back up the theory that the regeneration process might be a hydrogen passivation of boron-oxygen related defects.

36 MATERIALS SCIENCE↗

Thin silicon foils produced by epoxy-induced spalling of silicon for high efficiency solar cells

We report on the drastic improvement of the quality of thin silicon foils produced by epoxy-induced spalling. In the past, researchers have proposed to fabricate silicon foils by spalling silicon substrates with different stress-inducing materials to manufacture thin silicon solar cells. However, the reported values of effective minority carrier lifetime of the fabricated foils remained always limited to ∼100 μs or below. In this work, we investigate epoxy-induced exfoliated foils by electron spin resonance to analyze the limiting factors of the minority carrier lifetime. These measurements highlight the presence of disordered dangling bonds and dislocation-like defects generated by the exfoliation process. A solution to remove these defects compatible with the process flow to fabricate solar cells is proposed. After etching off less than 1 μm of material, the lifetime of the foil increases by more than a factor of 4.5, reaching a value of 461 μs. This corresponds to a lower limit of the diffusion length of more than 7 times the foil thickness. Regions with different lifetime correlate well with the roughness of the crack surface which suggests that the lifetime is now limited by the quality of the passivation of rough surfaces. The reported values of the minority carrier lifetime show a potential for high efficiency (>22%) thin silicon solar cells.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Radiation Effects of n-type, Low Resistivity, Spiral Silicon Drift Detector Hybrid Systems

We have developed a new thin-window, n-type, low-resistivity, spiral silicon drift detector (SDD) array - to be used as an extraterrestrial X-ray spectrometer (in varying environments) for NASA. To achieve low-energy response, a thin SDD entrance window was produced using a previously developed method. These thin-window devices were also produced on lower resistivity, thinner, n-type, silicon material, effectively ensuring their radiation hardness in anticipation of operation in potentially harsh radiation environments (such as found around the Jupiter system). Using the Indiana University Cyclotron Facility beam line RERS1, we irradiated a set of suitable diodes up to 5 Mrad and the latest iteration of our ASICs up to 12 Mrad. Then we irradiated two hybrid detectors consisting of newly, such-produced in-house (BNL) SDD chips bonded with ASICs with doses of 0.25 Mrad and 1 Mrad. Also we irradiated another hybrid detector consisting of previously produced (by KETEK) on n-type, high-resistivity SDD chip bonded with BNL's ASICs with a dose of 1 Mrad. The measurement results of radiated diodes (up to 5 Mrad), ASICs (up to 12 Mrad) and hybrid detectors (up to 1 Mrad) are presented here.

43 PARTICLE ACCELERATORS↗

Temperature-Dependent Photoluminescence Imaging and Characterization of a Multi-Crystalline Silicon Solar Cell Defect Area: Preprint

Photoluminescence (PL) imaging is used to detect areas in multi-crystalline silicon that appear dark in band-to-band imaging due to high recombination. Steady-state PL intensity can be correlated to effective minority-carrier lifetime, and its temperature dependence can provide additional lifetime-limiting defect information. An area of high defect density has been laser cut from amulti-crystalline silicon solar cell. Both band-to-band and defect-band PL imaging have been collected as a function of temperature from~85 to 350 K. Band-to-band luminescence is collected by an InGaAs camera using a 1200-nm short-pass filter, while defect band luminescence is collected using a 1350-nm long pass filter. The defect band luminescence is characterized by cathodo-luminescence.Small pieces from adjacent areas within the same wafer are measured by deep-level transient spectroscopy (DLTS). DLTS detects a minority-carrier electron trap level with an activation energy of 0.45 eV on the sample that contained defects as seen by imaging.

14 SOLAR ENERGY↗

Black Silicon Enhanced Thin Film Silicon Photovoltaic Devices

SiOnyx has developed an enhanced thin film silicon photovoltaic device with improved efficiency. Thin film silicon solar cells suffer from low material absorption characteristics resulting in poor cell efficiencies. SiOnyx’s approach leverages Black Silicon, an advanced material fabricated using ultrafast lasers. The laser treated films show dramatic enhancement in optical absorption with measured values in excess of 90% in the visible spectrum and well over 50% in the near infrared spectrum. Thin film Black Silicon solar cells demonstrate 25% higher current generation with almost no impact on open circuit voltage as compared with representative control samples. The initial prototypes demonstrated an improvement of nearly 2 percentage points in the suns Voc efficiency measurement. In addition we validated the capability to scale this processing technology to the throughputs (< 5 min/m2) required for volume production using state of the art commercially available high power industrial lasers. With these results we clearly demonstrate feasibility for the enhancement of thin film solar cells with this laser processing technique.

14 SOLAR ENERGY↗

Pre-strain effect on frequency-based impact energy dissipation through a silicone foam pad for shock mitigation [Pre-strain effect on the frequency response of shock mitigation through a silicone foam pad]

Silicone foams have been used in a variety of applications from gaskets to cushioning pads over a wide range of environments. Particularly, silicone foams are used as a shock mitigation material for shock and vibration applications. Understanding the shock mitigation response, particularly in the frequency domain, is critical for optimal designs to protect internal devices and components more effectively and efficiently. The silicone foams may be subjected to pre-strains during the assembly process which may consequently influence the frequency response with respect to shock mitigation performance. A Kolsky compression bar was modified with pre-compression capabilities to characterize the shock mitigation response of silicone foam in the frequency domain to determine the effect of pre-strain. Lastly, a silicone sample was also intentionally subjected to repeated pre-strain and dynamic loadings to explore the effect of repeated loading on the frequency response of shock mitigation.

36 MATERIALS SCIENCE↗

In Situ Transmission Electron Microscopy of Oxide Shell-Induced Pore Formation in (De)lithiated Silicon Nanowires

Silicon (Si) nanowires with a silicon oxide (SiOx) shell were observed in situ during lithiation and delithiation using transmission electron microscopy (TEM). The oxide shell constrains the volume expansion, which prevents full lithiation of the nanowire and retention of a crystalline Si core. Pores form in the amorphized silicon upon the first delithiation. We propose that this is caused by a high barrier to vacancy migration in the SiOx shell, which prevents vacancies formed during delithiation from transporting through the shell to the nanowire surface. These in situ studies demonstrate the importance of the direct observation of structural changes that occur in a material during cycling upon the addition of a coating.

Adkins, Emily R.↗

Phase transformation as the single-mode mechanical deformation of silicon

The mixture of the metastable body-centered cubic (bc8) and rhombohedral (r8) phases of silicon that is formed via nanoindentation of diamond cubic (dc) silicon exhibits properties that are of scientifc and technological interest. This letter demonstrates that large regions of this mixed phase can be formed in crystalline Si via nanoindentation without signifcant damage to the surrounding crystal. Cross-sectional transmission electron microscopy is used to show that volumes 6 μm wide and up to 650 nm deep can be generated in this way using a spherical tip of ~21.5 μm diameter. The phase transformed region is characterised using both Raman microspectroscopy and transmission electron microscopy. It is found that uniform loading using large spherical indenters can favor phase transformation as the sole deformation mechanism as long as the maximum load is below a critical level. We suggest that the sluggish nature of the transformation from the dc-Si phase to the metallic (b-Sn) phase normally results in competing deformation mechanisms such as slip and cracking but these can be suppressed by controlled loading conditions.

36 MATERIALS SCIENCE↗

Light-trapping optimization in wet-etched silicon photonic crystal solar cells

We demonstrate, by numerical solution of Maxwell's equations, near-perfect solar light-trapping and absorption over the 300–1100 nm wavelength band in silicon photonic crystal (PhC) architectures, amenable to fabrication by wet-etching and requiring less than 10 μm (equivalent bulk thickness) of crystalline silicon. These PhC's consist of square lattices of inverted pyramids with sides comprised of various (111) silicon facets and pyramid center-to-center spacing in the range of 1.3–2.5 μm. For a wet-etched slab with overall height H = 10 μm and lattice constant a = 2.5 μm, we find a maximum achievable photo-current density (MAPD) of 42.5 mA/cm{sup 2}, falling not far from 43.5 mA/cm{sup 2}, corresponding to 100% solar absorption in the range of 300–1100 nm. We also demonstrate a MAPD of 37.8 mA/cm{sup 2} for a thinner silicon PhC slab of overall height H = 5 μm and lattice constant a = 1.9 μm. When H is further reduced to 3 μm, the optimal lattice constant for inverted pyramids reduces to a = 1.3 μm and provides the MAPD of 35.5 mA/cm{sup 2}. These wet-etched structures require more than double the volume of silicon, in comparison to the overall mathematically optimum PhC structure (consisting of slanted conical pores), to achieve the same degree of solar absorption. It is suggested these 3–10 μm thick structures are valuable alternatives to currently utilized 300 μm-thick textured solar cells and are suitable for large-scale fabrication by wet-etching.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Plasma-initiated rehydrogenation of amorphous silicon to increase the temperature processing window of silicon heterojunction solar cells

The dehydrogenation of intrinsic hydrogenated amorphous silicon (a-Si:H) at temperatures above approximately 300°C degrades its ability to passivate silicon wafer surfaces. This limits the temperature of post-passivation processing steps during the fabrication of advanced silicon heterojunction or silicon-based tandem solar cells. We demonstrate that a hydrogen plasma can rehydrogenate intrinsic a-Si:H passivation layers that have been dehydrogenated by annealing. The hydrogen plasma treatment fully restores the effective carrier lifetime to several milliseconds in textured crystalline siliconwafers coated with 8-nm-thick intrinsic a-Si:H layers after annealing at temperatures of up to 450°C. Plasma-initiated rehydrogenation also translates to complete solar cells: A silicon heterojunction solar cell subjected to annealing at 450°C (following intrinsic a-Si:H deposition) had an open-circuit voltage of less than 600 mV, but an identical cell that received hydrogen plasma treatment reached a voltage of over 710 mV and an efficiency of over 19%.

14 SOLAR ENERGY↗

Recent Advances in Hot-Wire CVD R&D at NREL: From 18% Silicon Heterojunction Cells to Silicon Epitaxy at Glass-Compatible Temperatures

Our research aiming to improve silicon photovoltaic materials and devices extensively utilizes hot-wire chemical vapor deposition (HWCVD). We have recently achieved 18.2% heterojunction silicon solar cells by applying HWCVD a-Si:H front and back contacts to textured p-type silicon wafers. This is the best reported p-wafer heterojunction solar cell by any technique. We have also dramatically improved the quality of HWCVD silicon epitaxy and recently achieved 11 {micro}m of epitaxial growth at a rate of 110 nm/min.

14 SOLAR ENERGY↗

Epitaxial Crystal Silicon Absorber Layers and Solar Cells Grown at 1.8 Microns per Minute: Preprint

We have grown device-quality epitaxial silicon thin films at growth rates up to 1.8 ..mu..m/min, using hot-wire chemical vapor deposition from silane at substrate temperatures below 750 degrees C. At these rates, which are more than 30 times faster than those used by the amorphous and nanocrystalline Si industry, capital costs for large-scale solar cell production would be dramatically reduced,even for cell absorber layers up to 10 ?m thick. We achieved high growth rates by optimizing the three key parameters: silane flow, depletion, and filament geometry, based on our model developed earlier. Hydrogen coverage of the filament surface likely limits silane decomposition and growth rate at high system pressures. No considerable deterioration in PV device performance is observed whengrown at high rate, provided that the epitaxial growth is initiated at low rate. A simple mesa device structure (wafer/epi Si/a-Si(i)/a-Si:H(p)/ITO) with a 2.3 um epitaxial silicon absorber layer was grown at 700 nm/min. The finished device had an open-circuit voltage of 0.424 V without hydrogenation treatment.

14 SOLAR ENERGY↗

Photoluminescence of amorphous and crystalline silicon nanoclusters in silicon nitride and oxide superlattices

The photoluminescence properties of silicon nitride and oxide superlattices fabricated by plasmaenhanced chemical vapor deposition are studied. In the structures annealed at a temperature of 1150°C, photoluminescence peaks at about 1.45 eV are recorded. The peaks are defined by exciton recombination in silicon nanocrystals formed upon annealing. Along with the 1.45-eV peaks, a number of peaks defined by recombination at defects at the interface between the nanocrystals and silicon-nitride matrix are detected. The structures annealed at 900°C exhibit a number of photoluminescence peaks in the range 1.3–2.0 eV. These peaks are defined by both the recombination at defects and exciton recombination in amorphous silicon nanoclusters formed at an annealing temperature of 900°C. The observed features of all of the photoluminescence spectra are confirmed by the nature of the photoluminescence kinetics.

36 MATERIALS SCIENCE↗

Silicon-based anodes for lithium-ion batteries: Effectiveness of materials synthesis and electrode preparation

Lithium-ion batteries are widely used throughout the world for portable electronic devices and mobile phones and show great potential for more demanding applications like electric vehicles. Unfortunately, lithium-ion batteries still lack the required level of energy storage to completely meet the demands of such applications as electric vehicles. Among advanced materials being studied, silicon nanoparticles have demonstrated great potential as an anode material to replace the commonly used graphite. Silicon has been shown to have a high theoretical gravimetric capacity, approximately 4200 mA h/g, compared to only 372 mA h/g for graphite. Though silicon nanoparticles have remarkably high capacity, they suffer from rapid degradation with each cycle due to electrode volume expansion of approximately 400% during lithiation, placing a large strain on the material. With each cycle that strain creates cracks in the electrode particles and causes them to break down into smaller particles, which create void spaces between the particles and lead to poor contact as reflected in poor conductivity. In this review, we discuss exciting new research on silicon-based anodes conducted during the past couple of years. Besides stressing the importance of well-designed nanostructures of Si, we focus on optimization of the Si electrode and resulting performance enhancement by properly selecting binders and synergistically integrating them with various carbon materials during electrode design and fabrication. Importantly, although each improvement strategy has its own advantage, appropriate combination of them will yield much higher anode performance. We summarize the core issues in developing the silicon anode and effective strategies in yielding more promising results. (C) 2016 Elsevier Ltd. All rights reserved.

Casimir, Anix↗

Strength and thermal shock resistance of porous reaction-bonded silicon nitride by direct nitriding of binder jet additively manufactured silicon

The direct nitridation of binder jet additively manufactured silicon to produce porous silicon nitride was explored. The Taguchi Design of Experiments method was used to systematically study the effect of time, temperature, and nitrogen flow rate on the direct nitriding of binder jet additively manufactured silicon to produce porous reaction-bonded silicon nitride (RBSN). Highly porous (61%) samples with high conversion (99%) to silicon nitride were achieved using a thermal profile that utilized two isothermal holds. Further, it was shown that these samples exhibited thermal shock resistance and a low coefficient of thermal expansion. These results indicate that RBSN is readily achievable through additive manufacturing.

Ceramics↗

Porous reaction-bonded silicon nitride: Size effects for pressureless nitriding of binder jet additively manufactured silicon

The direct nitridation of binder jet additively manufactured silicon to produce porous reaction-bonded silicon nitride was explored to determine the maximum thickness of the sample that could be converted to >99% silicon nitride. The maximum thickness that could be nitrided was investigated by nitriding cubes of increasing physical size on the millimeter scale. Highly porous samples with high conversion ( > 99%) to silicon nitride were achieved in cubes with 35 mm edge length. It was shown that the silicon nitride phase content changes with increasing sample size.

Aguirre, Trevor [ORNL] (ORCID:0000000281469630)↗