Search NASA⌕ Search

SEARCH · Search NASA

Results for “STEELS, STAINLESS - REZISTAL”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Dynamic Data-Driven Multiscale Modeling for Predicting Microstructure and Mechanical Properties of 316L Stainless Steel

We have developed a long short-term memory stacked ensemble (LSTM-SE) surrogate modeling approach that can provide rapid predictions of microstructural evolution and the resultant mechanical properties of American Iron and Steel Institute (AISI) 316L series stainless steel (316LSS) fuel cladding under conditions of varying temperature and radiation dose rate. To acquire training data, we developed and implemented a kinetic Monte Carlo (KMC) model to simulate precipitation kinetics of M 23 C 6 , γ', and G phases within SS316L cladding. Experimentally reported precipitation kinetics of SS316L in literature were linked to the kinetic parameters of the simulated precipitation in our KMC model. The model was then used to simulate microstructure evolution under synthetically generated treatments of varying temperature and radiation dose rate, for periods of up to 3000 hours. Changes in volume fraction, number density, and particle size of precipitates were recorded, and particle area fractions were correlated using statistical methods to develop the surrogate model. Simultaneously, the mechanical properties of the simulated microstructures were evaluated using microstructure-based finite element method (FEM) analysis to determine the elastic modulus, yield stress, ultimate tensile strength, and elongation to failure of the aged microstructures. Using this approach, our surrogate model can predict precipitation behavior within 0.25% volume fraction and mechanical properties within 6% relative error from the values predicted by the KMC and FEM models using 50 training simulations as input. The trained recurrent neural network-based model can return estimations of precipitation kinetics and mechanical properties ~1000 times faster than the physics-based codes. This work demonstrates, as a proof of concept, that reactor material service lifetimes under variable service conditions can be predicted for a statistics-based model from a practicably obtainable dataset.

36 MATERIALS SCIENCE↗

Demystify radiation-enhanced hydrogen isotope diffusion in Fe-Ni-Cr austenitic stainless steels

Understanding and containing hydrogen isotope diffusion is crucial for many nuclear applications. In situ experiments have consistently shown that radiation significantly enhances isotope diffusion in austenitic stainless steels. Despite extensive research, the mechanism behind this phenomenon remains elusive, as most radiation-induced defects (e.g., vacancies, dislocations, and grain boundaries) typically trap hydrogen, thereby slowing diffusion. While grain boundaries may increase in-plane diffusivity and interstitials may enhance diffusion due to material swelling, these effects are relatively minor. Utilizing an Fe-Ni-Cr-H interatomic potential for stainless steels, we conducted extensive molecular dynamics simulations to investigate the origins of radiation-enhanced diffusion. Here, our findings reveal that when a system is resolidified, mimicking defects created by radiation displacements, the resulting structure contains a mixture of phases, boundaries, and dislocation networks. This defective structure significantly increases hydrogen diffusivity, enhancing it by approximately 1.7 times at 900 K. These results suggest that the complex defect structures formed during radiation displacements are the primary drivers of the observed diffusion enhancement, providing valuable insights into the mechanisms underlying radiation-enhanced diffusion in nuclear materials.

36 MATERIALS SCIENCE↗

Characterization of Electron Beam Free-Form Fabricated 2219 Aluminum and 316 Stainless Steel

Researchers at NASA Langley Research Center have developed an additive manufacturing technology for ground and future space based applications. The electron beam free form fabrication (EBF3) is a rapid metal fabrication process that utilizes an electron beam gun in a vacuum environment to replicate a CAD drawing of a part. The electron beam gun creates a molten pool on a metal substrate, and translates with respect to the substrate to deposit metal in designated regions through a layer additive process. Prior to demonstration and certification of a final EBF3 part for space flight, it is imperative to conduct a series of materials validation and verification tests on the ground in order to evaluate mechanical and microstructural properties of the EBF3 manufactured parts. Part geometries of EBF3 2219 aluminum and 316 stainless steel specimens were metallographically inspected, and tested for strength, fatigue crack growth, and fracture toughness. Upon comparing the results to conventionally welded material, 2219 aluminum in the as fabricated condition demonstrated a 30% and 16% decrease in fracture toughness and ductility, respectively. The strength properties of the 316 stainless steel material in the as deposited condition were comparable to annealed stainless steel alloys. Future fatigue crack growth tests will integrate various stress ranges and maximum to minimum stress ratios needed to fully characterize EBF3 manufactured specimens.

Ekrami, Yasamin↗

Porous Interlayers that Getter Surface-Segregating Species for Improved Silver Wetting, Adhesion, and Electrical Contact on Stainless Steel SOFC Components

Here, porous nickel interlayers or porous platinum interlayers were shown to promote the wetting, spreading, and adhesion of silver on alumina-forming ferritic stainless steel (AFFSS) and chromia-forming ferritic stainless steel (CFFSS). These interlayers resulted in dense, crack-free AFFSS|Ag-Ni|CFFSS and AFFSS|Ag-Pt|CFFSS braze joints that, after 300 h in 650 °C air, displayed shear strengths up to 70 MPa similar to, or larger than, those of AFFSS|Ag-CuO|CFFSS or AFFSS|Ag|CFFSS joints subjected to identical treatment. Similarly, after exposure to 25 cycles of (50 switches between) 12 h of 650 °C air and 12 h of 650 °C 4%H 2 –96%N 2 , AFFSS|Ag-Ni|CFFSS and AFFSS|Ag-Pt|CFFSS braze joints displayed shear strengths significantly larger than those of AFFSS|Ag-CuO|CFFSS or AFFSS|Ag|CFFSS joints subjected to identical treatment. In addition, nickel and platinum were found to chemically getter surface-segregating steel constituents, particularly Al from the AFFSS. As a result, Ag-Ni and Ag-Pt electrical contact resistances on AFFSS and CFFSS substrates were several orders of magnitude lower than those of conventional Ag-CuO reactive air brazes or Heraeus C8710 Ag contact pastes. Together, these results suggest that Ag-Pt and especially Ag-Ni may be useful for the fabrication of durable joints, seals, and/or electrical contacts in electrical/electrochemical devices exposed to high temperatures and/or variable oxygen partial pressure environments.

36 MATERIALS SCIENCE↗

Influence of Spatter on Porosity, Microstructure, and Corrosion of Additively Manufactured Stainless Steel Printed Using Different Island Size

Specimens of 316 L stainless steel were printed using laser powder bed fusion (LPBF), a popular metal additive manufacturing (AM) technique, with varying island sizes. Not many researchers have considered the impact of spatter while optimizing LPBF printing parameters. In this research, the influence of spatter was considered while also investigating the effect of varied island size on the microstructure, surface roughness, microhardness, and corrosion resistance of LPBF-316 L. No correlation was observed between surface roughness or microhardness and minor variations in island size. However, a correlation was drawn between varied island sizes and porosity in LPBF-316 L. The specimens associated with larger island sizes showed significantly enhanced corrosion resistance due to fewer manufacturing defects and reduced porosity, attributed to the minimal influence of the spatter. Based on analysis, the LPBF parameters were revised, which lead to superior corrosion resistance of LPBF-316 L, attributed to high density and reduced porosity.

36 MATERIALS SCIENCE↗

Leak-tight crack repair for 304L stainless steel using friction surfacing

Here, friction surfacing (FS) was investigated as a method for sealing 50 μm wide thru-cracks in 3-mm-thick 304L stainless steel (304L) plate. Friction surfacing was performed using two sizes of 304L consumable rod, with diameters of 9.52 mm and 12.7 mm, on two substrate conditions (clean and oxidized). Friction surfacing was able to deposit a 600 μm thick coating and repair cracks to a depth of 100 μm - 200 μm below the original surface, when using the 12.7-mm-diameter consumable rod for both substrate conditions. Helium leak rates of 10 -10 atm-cc/s were achieved on crack repairs, designating them as leak-tight by the ANSI N14.5 standard. Optical and scanning electron microscopy were used to investigate the coating microstructure and bond interfaces. In this study, the 12.7-mm-diameter rod performed better with disruption of the oxide layer on the oxidized substrate and providing a more homogenous coating. Mechanical properties of the coated samples were evaluated by performing micro-indentation, tensile, bending, and adhesion testing. Higher hardness in the coatings was observed due to the fine equiaxed grains resulting from dynamic recrystallization. Complete consolidation of plastically deformed material on the substrate and a strong diffusion bond across the interface was observed. This was reflected in tensile and bending properties of the FS coatings being comparable to those of uncoated specimen. No delamination of the FS coating was observed during adhesion testing. The results demonstrate that friction surfacing is a viable option to seal cracks in stainless steels.

36 MATERIALS SCIENCE↗

Corrosion of 316H stainless steel in flowing FLiNaK salt

In this report type 316H stainless steel samples were exposed to flowing FLiNaK salt for 1000 h in a monometallic thermal convection loop (TCL) with a maximum temperature of 650 °C and a minimum of 540 °C. Samples in the hottest part of the TCL lost mass, with a maximum mass loss of 1.4 mg/cm 2 , while samples in the coldest parts of the TCL gained mass, with a maximum mass gain of 1.0 mg/cm 2 . Analysis of the samples that gained mass showed an Fe-rich layer on the sample surfaces, indicating that Fe, not Cr, was the primary deposition product in the TCL. Cr loss was apparent to a depth of ~5 µm in the hot leg. Post-exposure analysis of the salt showed major increases in the Cr, Fe, and Mn contents. The TCL was modeled using the TRANSFORM code. Modeled values matched the experimental temperature measurements showing that TRANSFORM is capable of accurately simulating the TCL conditions.

36 MATERIALS SCIENCE↗

Effect of Microstructural Bands on the Localized Corrosion of Laser Surface-melted 316L Stainless Steel

The localized corrosion of laser surface melted (LSM) 316L stainless steel is investigated by a combination of potentiodynamic anodic polarization in 0.1M HCl and microscopic investigation of the initiation and propagation of localized corrosion. The pitting potential of LSM 316L is significantly lower than the pitting potential of wrought 316L. The LSM microstructure is highly banded as a consequence of the high laser power density and high linear energy density. The bands are composed of zones of changing modes of solidification, cycling between very narrow regions of primary austenite solidification and very wide regions of primary ferrite solidification. Pits initiate in the outer edge of each band where the mode of solidification is primary austenite plane front solidification and primary austenite cellular solidification. The primary austenite regions have low chromium concentration (and possibly low molybdenum concentration), which explains their susceptibility to pitting corrosion. The ferrite is enriched in chromium, which explains the absence of pitting in the primary ferrite regions. The presence of the low chromium regions of primary austenite solidification explains the lower pitting resistance of LSM 316L relative to wrought 316L. The influence of banding on localized corrosion is applicable to other rapidly solidified processes such as additive manufacturing.

36 MATERIALS SCIENCE↗

Effects of low-temperature neutron irradiation on the microstructure and tensile properties of duplex 2304 stainless steel and its electron-beam welds

A lean duplex stainless steel material (2304-grade) in its base metal and electron beam (e-beam) welded conditions were studied microstructurally and mechanically as a function of irradiation conditions to evaluate its use as a structural material at low temperatures (60–100 °C). Neutron irradiation up to a fluence of 1.40 × 10 19 n/cm 2 (E > 0.1 MeV) or ~0.011 dpa decreased the total elongation of both base metal and e-beam welded samples. Overall, radiation hardening was observed in all the samples. The transversely cut irradiated samples showed some nonuniform quasi-cleavage and shearing in their fracture surfaces, indicating the variance of ductile nature of the two-phased (deformable austenite and harder ferrite) duplex structure. The e-beam welded samples also showed quasi-cleavage fracture, which is a characteristic of radiation-induced embrittlement. Furthermore, these observations of the e-beam welded samples were attributed to the formation of coarse ferrites, grain boundary and intragranular phases such as γ 2 and γ 3 , and minor impurity phases such as CrN and Cr 2 N in the weld pool and/or heat-affected zone of the samples. Radiation-induced elemental segregation was also identified in the post-irradiated base metal.

36 MATERIALS SCIENCE↗

Proton irradiation and characterization of additively manufactured 304L stainless steels

Irradiations were performed with 1.5 MeV protons to 0.6 dpa at 40–150 °C on additively manufactured (AM) 304L stainless steel and the changes in microstructure and mechanical behavior after irradiation were compared to wrought 304L stainless steel. Interestingly, all microstructural and hardness results after irradiation suggest the samples evolve toward a similar state, despite significant differences in the unirradiated microstructures and hardness values. A TEM and nanoindentation-based investigation of before and after proton irradiation at 40–150 °C is presented. Results are interpreted in terms of initial dislocation content, dislocation structures, and microstructural and chemical homogeneity.

36 MATERIALS SCIENCE↗

Application of the Chloride Susceptibility Index to Study the Effects of Ni, Cr, Mn and Mo on the Repassivation of Stainless Steels

The effects of Ni, Cr, Mn and Mo on the very earliest stages of repassivation of stainless steels are quantified using the Chloride Susceptibility Index (CSI), which is an ab initio-based index for the evaluation of repassivation tendency. The quinary system of Fe-Ni-Cr-Mn-Mo is studied with density functional theory analysis and an electrochemisorption model developed previously by the authors, which are required to determine the CSI. The adsorption energies of O and Cl to different surface configurations are calculated, and then surface coverage maps of different species on the surface are obtained from the adsorption energies based on the Langmuir isotherm. Finally, CSI is calculated for different compositions of stainless steels. It is found that the effect of alloying elements on promoting repassivation of Fe alloys is in the order of Mn > ≈Ni > Cr > Mo when solute composition is less than 28 wt.%. A strong synergy is found between Cr and Mo such that a combination of these two elements at a certain ratio can give an optimal (low) CSI. Here, the usage of CSI for evaluating repassivation tendency of CRAs is validated by experimental measured repassivation potential, which shows a strong monotonic negative relation with CSI.

36 MATERIALS SCIENCE↗

The Effects of Acid Passivation, Tricresyl Phosphate Presoak, and UV/Ozone Treatment on the Tribology of Perfluoropolyether-Lubricated 440C Stainless Steel Couples

The boundary-lubrication performance of two perfluoropolyether (PFPE) thin films in the presence of passivated 440C stainless steel is presented. The study used a standard ball on disk (BoD) tribometer in dry nitrogen and a vacuum spiral orbit tribometer (SOT). Stainless steel surfaces were passivated with one of four techniques: high and low temperature chromic acid bath, a tricresyl phosphate (TCP) soak, or UV/Ozone treated for 15 min. After passivation, each BoD disk had a 400A film of Krytox 16256 (PFPE) applied to it. The lifetimes of these films were quantified by measuring the number of sliding cycles before an increase in friction occurred. The lubricated lifetime of the 440C couple was not altered as a result of the various passivation techniques. The resulting surface chemistry of each passivation technique was examined using X-ray photoelectron spectroscopy (XPS). The SOT was used to examine the effects of the TCP treatment on the lubricated lifetime of another PFPE, Brayco 815Z, under rolling conditions. None of the passivation techniques were found to dramatically increase the oxide film thickness or lubricated lifetimes.

Shogrin, Bradley A.↗

Corrosion study of bare and coated stainless steel

A program was conducted at Kennedy Space Center from February 1968 to February 1971 to evaluate the performance of austenitic stainless steel alloys used in fluid systems lines. For several years, there had been numerous failures of stainless steel hardware caused by pitting and stress corrosion cracking. Several alloys were evaluated for effectiveness of certain sacrificial-type protective coverings in preventing corrosion failures. Samples were tested in specially designed racks placed 91 meters (100 yards) above high-tide line at Cape Kennedy. It is concluded that: (1) unprotected tubing samples showed evidence of pitting initiation after 2 weeks; (2) although some alloys develop larger pits than others, it is probable that the actual pitting rate is independent of alloy type; (3) the deepest pitting occurred in the sheltered part of the samples; and (4) zinc-rich coatings and an aluminum-filled coating have afforded sacrificial protection against pitting for at least 28 months. It is believed that a much longer effective coating life can be expected.

Morrison, J. D.↗

Mechanical properties and oxidation and corrosion resistance of reduced-chromium 304 stainless steel alloys

An experimental program was undertaken to identify effective substitutes for part of the Cr in 304 stainless steel as a method of conserving the strategic element Cr. Although special emphasis was placed on tensile properties, oxidation and corrosion resistance were also examined. Results indicate that over the temperature range of -196 C to 540 C the yield stress of experimental austenitic alloys with only 12 percent Cr compare favorably with the 18 percent Cr in 304 stainless steel. Oxidation resistance and in most cases corrosion resistance for the experimental alloys were comparable to the commercial alloy. Effective substitutes for Cr included Al, Mo, Si, Ti, and V, while Ni and Mn contents were increased to maintain an austenitic structure.

Stephens, J. R.↗

Influence of Microstructure on the Absorption of Tritium into Gold-Plated 316 Stainless Steel

The interaction of tritium with metal surfaces is the initial step in the overall absorption of tritium by the substrate metal. As a result, limiting the adsorption of tritium to the surface may effectively reduce the quantity of tritium absorbed by a metal when it is in contact with tritium gas. To limit tritium adsorption, many tritium users electroplate gold onto the substrate metal. The gold layer is expected to reduce tritium adsorption, and subsequently absorption, by reducing water adsorption. The present work shows a comparison between tritium inventories in nonplated 316 stainless steel to the inventories in 316 stainless-steel samples electroplated with gold by various commercial vendors and laboratories. Of the various gold-plated samples, only one type of plating shows ~25% reduction in tritium inventory, relative to non-plated steel samples. The degree of tritium absorption appears to be significantly influenced by the porosity, texture, and completeness of the gold layer. Incomplete and/or porous layers lead to increased absorption, while gold layers with smaller surface features lead to similar tritium inventories as non-plated samples. Furthermore, reduced tritium absorption was observed only for complete gold layers with small surface features.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗