Deconstructing poplar lignin from ionic liquid pretreatment for biological conversion through sulfonation and Fenton chemistry
We present a method for depolymerization of poplar lignin for microbial conversion via sulfonation and Fenton chemistry.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
We present a method for depolymerization of poplar lignin for microbial conversion via sulfonation and Fenton chemistry.
Gold microstructures are produced with a femtosecond laser in thin films of a polystyrene sulfonate matrix containing gold ions. Two-photon induced metal reduction is obtained by addition of 0.1 wt % of ruthenium(II)tris(bipyridine) in the formulation. Laser power is reduced to 5 mW, thereby limiting thermal effects. Lines of typically 150 nm heights and 1 {mu}m widths are fabricated as well as freestanding bidimensional structures. An additional electroless plating step produces gold structures with conductivities only ten times smaller than the bulk metal.
The new type of electrolyte membrane materials has been prepared by blend sulfonated polystyrene (SPS), lignosulfonate (LS), and alumina (SPS-LS-Al{sub 2}O{sub 3}) by casting polymer solution. The resulting polymer electrolyte membranes were then characterized by functional groups analysis, mechanical properties, water uptake, ion exchange capacity, and proton conductivity. SPS-LS-Al{sub 2}O{sub 3} membranes with alumina composition various have been proven qualitatively by analysis of functional groups. Increasing the Al{sub 2}O{sub 3} ratio resulted in higher ion exchange capacity (IEC), mechanical strength and proton conductivity, but water uptake decreased. The SPS-LS-Al{sub 2}O{sub 3} blend showed higher proton conductivity than Nafion 117.
The structural dynamics of a series of 1-alkyl-3-methylimidazolium bis(trifluoromethylsulfonyl)imide (C n mimNTf 2 , n = 2, 4, 6, 10: ethyl—Emim; butyl—Bmim; hexyl—Hmim; decyl—Dmim) room temperature ionic liquids confined in the pores of polyether sulfone (PES 200) membranes with an average pore size of ~350 nm and in the bulk liquids were studied. Time correlated single photon counting measurements of the fluorescence of the fluorophore coumarin 153 (C153) were used to observe the time-dependent Stokes shift (solvation dynamics). The solvation dynamics of C153 in the ionic liquids are multiexponential decays. The multiexponential functional form of the decays was confirmed as the slowest decay component of each bulk liquid matches the slowest component of the liquid dynamics measured by optical heterodyne-detected optical Kerr effect (OHD-OKE) experiments, which is single exponential. The fact that the slowest component of the Stokes shift matches the OHD-OKE data in all four liquids identifies this component of the solvation dynamics as arising from the complete structural randomization of the liquids. Although the pores in the PES membranes are large, confinement on the mesoscopic length scale results in substantial slowing of the dynamics, a factor of ~4, for EmimNTf2, with the effect decreasing as the chain length increases. By DmimNTf 2 , the dynamics are virtually indistinguishable from those in the bulk liquid. The rotation relaxation of C153 in the four bulk liquids was also measured and showed strong coupling between the C153 probe and its environment.
Reaching exceptionally long times up to 500 ns in equilibrium and nonequilibrium molecular dynamics simulations studies, we have attained a fundamental molecular understanding of the correlation of ionomer clusters structure and multiscale dynamics, providing new insight into one critical, long-standing challenge in ionic polymer physics. The cluster structure in melts of sulfonated polystyrene with Na + and Mg 2+ counterions are resolved and correlated with the dynamics on multiple length and time scales extracted from measurements of the dynamic structure factor and shear rheology. We find that as the morphology of the ionic clusters changes from ladderlike for Na + to disordered structures for Mg 2+ , the dynamic structure factor is affected on the length scale corresponding to the ionic clusters. Lastly, rheology studies show that the viscosity for Mg 2+ melts is higher than for Na + ones for all shear rates, which is well correlated with the larger ionic clusters’ size for the Mg 2+ melts.
In this article, strongly charged polyelectrolytes (PEs) demonstrate complex solution behavior as a function of chain length, concentrations, and ionic strength. The viscosity behavior is important to understand and is a core quantity for many applications, but aspects remain a challenge. Molecular dynamics simulations using implicit solvent coarse-grained (CG) models successfully reproduce structure, but are often inappropriate for calculating viscosities. To address the need for CG models which reproduce viscoelastic properties of one of the most studied PEs, sodium polystyrene sulfonate (NaPSS), we report our recent efforts in using Bayesian optimization to develop CG models of NaPSS which capture both polymer structure and dynamics in aqueous solutions with explicit solvent. We demonstrate that our explicit solvent CG NaPSS model with the ML-BOP water model [Chan et al. Nat Commun 10, 379 (2019)] quantitatively reproduces NaPSS chain statistics and solution structure. The new explicit solvent CG model is benchmarked against diffusivities from atomistic simulations and experimental specific viscosities for short chains. We also show that our Bayesian-optimized CG model is transferable to larger chain lengths across a range of concentrations. Overall, this work provides a machine-learned model to probe the structural, dynamic, and rheological properties of polyelectrolytes such as NaPSS and aids in the design of novel, strongly charged polymers with tunable structural and viscoelastic properties
Here, sulfonated Diels-Alder poly(phenylene) (SDAPP) membranes were synthesized and characterized as potential electrolyte separators for vanadium redox flow batteries. The SDAPP membranes studied had ion exchange capacities of 1.4, 1.8 and 2.3 meq/g. Transmission electron microscopy imaging shows that the ionic domains in SDAPP are roughly 0.5 nm in dimension, while Nafion has a hydrophilic phase width of around 5 nm. The sulfuric acid uptake by SDAPP was higher than that for Nafion, but the materials had similar water uptake from solutions of various sulfuric acid concentrations. In equilibration with sulfuric acid concentrations ranging from 0–17.4 mol·kg -1 , SDAPP with a IEC of 2.3 meq/g had the highest conductivity, ranging from 0.21 to 0.05 S·cm -1 , while SDAPP with a IEC of 1.8 had conductivity close to Nafion 117, ranging from 0.11 to 0.02 S·cm -1 . With varying sulfuric acid concentration and temperature, vanadium permeability in SDAPP is positively correlated to the membrane's IEC. The vanadium permeability of SDAPP 2.3 is similar to that of Nafion, but permeability values for SDAPP 1.8 and SDAPP 1.4 are substantially lower. The vanadium permeation decreases with increasing electrolyte sulfuric acid concentration. Lastly, vanadium diffusion activation energy is about 20 kJ·mol -1 in both SDAPP and Nafion.
The phase-out of long-chain PFAS has led to the proliferation of highly recalcitrant short-chain analogs, and mineralization technologies for these short-chain PFAS are needed to mitigate their deleterious effects on environmental and human health. In this study, we utilize a statistical design of experiments, specifically, response surface methodology, to rapidly evaluate the electrochemical degradation of the short-chain PFAS, perfluorobutane sulfonate (PFBS). We evaluate the impacts of the three primary electrochemical parameters (concentration of PFBS, concentration of supporting electrolyte, and applied current) over multiple orders of magnitude on the three primary reaction outcomes of electrochemical PFBS degradation (incomplete PFBS decomposition, complete PFBS mineralization as fluorine, and anodic energy consumption). Our results correspond with literature and clearly identify the well-known tradeoff between energy consumption and complete mineralization. Intriguingly, partial PFBS decomposition and energy consumption demonstrate nonlinear dependencies in the current/supporting electrolyte concentration space and the current/PFBS concentration space, respectively. These findings highlight the utility of the response surface methodology model to efficiently interrogate a large parameter space, identifying both common results and less-obvious interactions between electrochemical parameters and their influences on reaction outcomes.
In this project, an engineered form of a Metal-Organic Framework (MOF) based material is developed for the removal of perfluorooctane sulfonate (PFOS) for real-world applications. The powdered MOF material has been demonstrated at the Pacific Northwest National Laboratory (PNNL) to selectively capture PFOS from distilled (DI) water with a large performance advantage over granulated activated carbon (GAC). In this project, the powdered material was transformed into an engineered form (using a polymer) to demonstrate PFOS adsorption capacity in tap water. PNNL developed and processed the MOF material in the engineering form (granules). After thorough characterization and stability testing, these engineered MOF granules were provided to an industrial collaborator, AVANTech, LLC, for testing and demonstration of continuous, long-term PFOS removal from tap water. The preliminary results showed PFOS sorption capacities at parts per billion (ppb) concentrations in tap water under a flow system. Also provided insight into sorbent-based material utilization in a continuous flow system. Further studies are required to optimize and understand sorption in such industrial-scale applications.
Desalination is considered a promising solution to alleviate water shortages, yet current methods are often restricted, due to challenges like high energy consumption, significant cost, or limited desalination capacity. In this study, we present a novel approach of redox flow desalination (RFD) utilizing the highly aqueous-soluble and reversible redox-active compound, potassium 1,1'-bis(sulfonate) ferrocene (1,1'-FcDS). This water-soluble organic compound yielded stable and rapid desalination, sustaining extended operation without notable decay and achieving an impressive desalination rate of up to 457.5 mmol·h -1 ·m -2 and energy consumption as low as 40.2 kJ·mol NaCl -1 . Specifically, the RFD device effectively desalinated a 50 mM NaCl solution to potable standards within 6000 s using 1,1'-FcDS. It maintained an average energy consumption of 178.16 kJ·mol NaCl -1 and exhibited negligible deterioration in desalination rate, energy efficiency, and charge efficiency throughout a rigorous 12,000 s cycling test. Furthermore, the versatility of this method was demonstrated by effectively treating saline water with varying initial concentrations from 10 mM to 50 mM, showcasing its potential across a broad spectrum of applications.
Ammonia (NH3) gas is a prominent air pollutant that is frequently found in industrial and livestock production environments. Due to the importance in controlling pollution and protecting public health, the development of new platforms for sensing NH3 at room temperature has attracted great attention. In this study, a sensitive NH3 gas device with enhanced selectivity is developed based on zinc oxide nanofibers (ZnO NFs) decorated with poly(styrene sulfonate) (PSS) and operated at room temperature. ZnO NFs were prepared by electrospinning followed by calcination at 500 °C for 3 h. The electrospun ZnO NFs are characterized to evaluate the properties of the as-prepared sensing materials. The loading of PSS to prepare ZnO NFs/PSS composite is also optimized based on the best sensing performance. Under the optimal composition, ZnO NFs/PSS displays rapid, reversible, and sensitive response upon NH3 exposure at room temperature. The device shows a dynamic linear range up to 100 ppm and a limit of detection of 3.22 ppm and enhanced selectivity toward NH3 in synthetic air, against NO2 and CO, compared to pure ZnO NFs. Additionally, a sensing mechanism is proposed to illustrate the sensing performance using ZnO NFs/PSS composite. Therefore, this study provides a simple methodology to design a sensitive platform for NH3 monitoring at room temperature.
A sample of polyether sulfone was evaluated for toxicity of pyrolysis gases, using the toxicity screening test method developed at the University of San Francisco. Animal response times were relatively short at pyrolysis temperatures of 600 to 800 C, with death occurring within 6 min. The principal toxicant appeared to be a compound other than carbon monoxide.
The strain-birefringence response of poly(bisphenol-A-diphenyl sulfone) is found to be independent of temperature at temperatures below -100 C; at higher temperatures, the response becomes slightly dependent on temperature, with lower birefringence seen at higher temperatures. The stress-strain behavior and the stress-birefringence response both depend on temperature over the entire testing temperature range (-179 C to 150 C) studied; this dependence, however, is not pronounced. The evidence is seen as suggesting that the polymer molecules respond to deformation by undergoing conformational rearrangements; the mode of the molecular deformation remains unchanged for temperatures of -100 C or lower. At higher temperatures, the average length of the chain segments involved in the rearrangement increases. The stress-strain response is attributed mainly to chain orientation. The entropic contribution deriving from chain orientation at temperatures below -100 C is still substantial. The modest temperature dependence of the stress-strain response suggests that the energy barriers for the chain segments involved in the rearrangement are relatively low.
Epoxy resin networks cured with DDS were modified by incorporating tough ductile thermoplastics such as the amine terminated polyether sulfones and amine terminated polyether ketones. Both linear copolymers were able to significantly improve the fracture toughness values at the 15 and 30 weight percent concentrations examined. These improvements in fracture toughness were achieved without any significant change in the flexural modulus.
Reactive diamino terminated oligomers of pre-determined molecular weights can be prepared by either of two synthetic routes depending upon the compound used to introduce the amine functionality. After characterization by spectroscopic and thermal methods, these oligomers can be used in several post-reactions to yield novel block and segmented copolymer systems. A potential application for these poly(arylene ether sulfone) oligomers exists in the curing or co-curing of epoxy resins for improving toughness. They can also be used to prepare toughened bismaleimide systems as well as producing copolymers with improved solvent resistance, especially with respect to chlorinated solvents.
Multifunctional epoxy resin networks were chemically modified with thermoplastic amine terminated poly(arylene ether sulfones) of controlled molecular weights. This system was then examined as both neat resin and as a matrix resin for carbon fiber composites. The neat resin displayed a significant increase in both fracture toughness and energy release rate values. This was attributed to the altered morphology, which could be varied from particles of polysulfone in an epoxy matrix to that of a quasi-continuous polysulfone phase.
The effects of Co-60 gamma radiation on a series of poly(arylene ether sulfones) prepared by nucleophilic activated aromatic substitution are investigated experimentally. The preparation of the test compounds is described, and the test results are presented in extensive tables and graphs. Radiation-induced degradation, as measured by SO2 production, was found to be lowest in compounds based on biphenol rather than bisphenol A; these findings were also well correlated with ultimate-tensile-strain measurements.
Copolymers of fluorinated polydienes and sulfonated polystyrene and their use in fuel cell membranes, batteries, breathable chemical-biological protective materials, and templates for sol-gel polymerization.