Heterogeneous solute segregation suppresses strain localization in nanocrystalline Ag-Ni alloys

Solute segregation to individual grain boundaries is used by design to produce strong and stable nanocrystalline metallic alloys. Grain-boundary segregation, however, is known to cause adverse embrittlement effects from a strain-localization failure mechanism that imposes significant material limitations for structural applications. Here, using atomistic simulations, it is discovered that heterogeneous Ni segregation in nanocrystalline Ni-mixed Ag alloys dramatically shuts down localized shear bands during plastic deformation, while simultaneously increasing the tensile strength. Nanocrystalline Cu-mixed Ag metals are predicted to exhibit standard homogeneous Cu segregation and a tensile strength that saturates above a solute concentration of 8 at.% due to glass-like shear localization induced by grain boundaries. By contrast, it is found that heterogeneous Ni segregation in nanocrystalline Ag-Ni alloys forms solute-rich clusters along interfaces leading to strain delocalization at high strain and continuous strengthening at high solute concentrations up to 15 at.%. As a result, this study reveals the importance of heterogeneous versus homogeneous segregation behaviors on strain localization and points to a fundamentally new strategy to design failure-resistant nanostructured materials through grain boundary segregation engineering.

36 MATERIALS SCIENCE↗

Understanding the effect of refractory metal chemistry on the stacking fault energy and mechanical property of Cantor-based multi-principal element alloys

Multi-principal-element alloys (MPEAs) based on 3d-transition metals show remarkable mechanical properties. In this study, the stacking fault energy (SFE) in face-centered cubic (fcc) alloys is a critical property that controls underlying deformation mechanisms and mechanical response. Here, we present an exhaustive density-functional theory study on refractory- and copper-reinforced Cantor-based systems to ascertain the effects of refractory metal chemistry on SFE. We find that even a small percent change in refractory metal composition significantly changes SFEs, which correlates favorably with features like electronegativity variance, size effect, and heat of fusion. For fcc MPEAs, we also detail the changes in mechanical properties, such as bulk, Young's, and shear moduli, as well as yield strength. A Labusch-type solute-solution-strengthening model was used to evaluate the temperature-dependent yield strength, which, combined with SFE, provides a design guide for high-performance alloys. We also analyzed the electronic structures of two down-selected alloys to reveal the underlying origin of optimal SFE and strength range in refractory-reinforced fcc MPEAs. These new insights on tuning SFEs and modifying composition-structure-property correlation in refractory- and copper-reinforced MPEAs by chemical disorder, provide a chemical route to tune twinning- and transformation-induced plasticity behavior in fcc MPEAs.

36 MATERIALS SCIENCE↗

Direct measurements of the 3D plasma velocity in single-helical-axis RFP plasmas

The first local velocity measurements of helical equilibrium plasmas in the Reversed Field Pinch (RFP) Single Helical Axis (SHAx) state using a Charge Exchange Recombination Spectroscopy (CHERS) diagnostic are presented. Measurements show strong axisymmetric and non-axisymmetric flow, with n ¼ 5 components of flow related to the ðm; nÞ¼ð1; 5Þ dominant magnetic mode on the order of the axisymmetric flow in certain regions of the plasma, as well as significant n > 5 flow. Flow measurements are compared with NIMROD simulations of visco-resistive, single-fluid MHD in toroidal and cylindrical geometries with limited axial periodicity. Both measurements and the simulation with toroidal geometry show stronger inboard flows relative to the outboard flows, which is attributed to the toroidal geometry of the device. In the experiment, the n ¼ 5 component of flow is phase shifted from the reconnection-like flow pattern observed in the single-fluid simulations, possibly due to decoupling of the ion and electron fluids over much of the plasma. Finally, the strength of the helical angular flow shear relative to the critical shear necessary to disrupt nonlinear coupling between tearing modes is calculated around the helical magnetic axis. The shear in the measured flow is on the order of the theoretical critical threshold needed to nonlinearly decouple modes, but the measurement uncertainty in the gradient of the flow is large.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Mechanical behavior and shear band of a powder-metallurgy-fabricated CoCrFeMnNi high-entropy alloy during high strain-rate deformation

High-entropy alloys (HEAs) fabricated by powder metallurgy are considered to exhibit extremely-great potential application values in the field for high-speed impact deformation due to their uniform microstructures and compositions. The mechanical behavior of a powder-metallurgy-fabricated (PM) CoCrFeMnNi HEA was investigated at room temperature with strain rates ranging from 1200 s -1 to 2800 s -1 . It was found that the serration behavior and shear localization of the alloy under dynamic conditions occurred. Results also indicated that the serrated flow took place in the PM CoCrFeMnNi HEA during mechanical deformation at high strain rates (>1000 s -1 ) and became more pronounced as the strain rate increased. Furthermore, it was determined that the yield-strength values of the PM CoCrFeMnNi HEA were sensitive to strain rates, where the values increased from 500 MPa to 700 MPa when the strain rates increased from 1200 s -1 to 2800 s -1 . Shear bands with a width of about 20 μm were generated in the PM CoCrFeMnNi HEA after the shear stress reached a maximum value of 635 MPa, which corresponded to a nominal strain of about 8.71. Nanotwins and ultrafine-equiaxed grains with a diameter of about 150 nm also developed at the core of the shear band during deformation. The results revealed that the strength of the shear band was much higher than that of the matrix grain. Nanotwins in the shear band were composed of a single face-centered-cubic (FCC) structure with the twin plane of ($\bar{1}$1$\bar1$), which could be formed via a rotational dynamic recrystallization (RDR).

36 MATERIALS SCIENCE↗

Deformation behavior of nanoscale Al–Al 2 Cu eutectics studied by in situ micropillar compression

We report deformation behavior of nanoscale laser processed Al–Al 2 Cu eutectics at room temperature is characterized through in situ micro-pillar compression testing in a scanning transmission microscope. Interlamellar spacing of Al–Al 2 Cu eutectics varies from hundreds of nanometers to 20 nm. Three different sizes of micro-pillars are fabricated in order to study the deformation behaviors of single colony and multiple colonies, corresponding to the single crystal and polycrystal respectively. For single colonies, lamellar orientations parallel, normal or inclined to the loading direction were tested. The main findings are: 1) the plasticity mechanisms strongly depend on loading orientation: buckling and kinking in the parallel-loaded eutectics, planar sliding along Al–Al 2 Cu lamellar interfaces in the incline-loaded eutectics and localized shearing in the normal-loaded eutectics. 2) the incline-loaded eutectics exhibits the lowest compression flow strength, and the normal-loaded eutectics has the highest compression flow strength. 3) with decreasing inter-lamellar spacing, the strength increases and plasticity is uniformly distributed, as opposed to shear localization. Highest compressive plasticity is observed in polycrystalline eutectics with an ensemble of lamellar orientations with ~20 nm average spacing: 17.9% at flow stress of 1.63 GPa, and degenerate, bimodal morphology: 11.1% at flow stress of 1.36 GPa.

36 MATERIALS SCIENCE↗

Collapse of Reacted Fracture Surface Decreases Permeability and Frictional Strength

Abstract Geochemical and geomechanical perturbations of the subsurface caused by the injection of fluids present risks of leakage and seismicity. This study investigated how acidic fluid flow affects hydraulic and frictional properties of fractures using experiments with 3.8‐cm‐long specimens of Eagle Ford shale, a laminated shale with carbonate‐rich strata. In low‐pressure flow cells, one set of samples was exposed to acidic brine and another set was exposed to neutral brine. X‐ray computed tomography and energy‐dispersive X‐ray spectroscopy revealed that samples exposed to acidic brine were calcite‐depleted and had developed a porous altered layer, while the other set showed no evidence of alteration. After reaction, samples were compressed and sheared in a triaxial cell that supplied normal stress and differential pore pressure at prescribed sliding velocities, independently measuring friction and permeability. During the initial compression, the porous altered layer collapsed into fine particles that filled the fracture. This effectively impeded flow and sealed the fracture, resulting in fracture permeability to decrease 1 to 2 orders of magnitude relative to the unaltered fractures. This is a favorable outcome in subsurface applications where the goal is to reduce leakage risks. However, during shear the reacted fracture had lower frictional strength because the fine‐grained particles in the collapsed layer prevented the formation of interlocking microasperities. Therefore, coupled geochemical and geomechanical processes that could favorably seal fractures could also increase the likelihood of induced seismicity. These findings have important implications for geological carbon sequestration, pressurized fluid energy storage, geothermal energy, and other subsurface technologies.

58 GEOSCIENCES↗

Fiber orientation and porosity in large-format extrusion process: The role of processing parameters

Controlling fiber orientation and porosity in short-fiber thermoplastic composites is important for enhancing mechanical, electrical and thermal properties in large-format additive manufacturing. This study employs a factorial design of experiments (DoE) to assess the effects of nozzle diameter (5.08 mm–10.16 mm), temperature (230–250 °C), and extruder screw speed (150–280 rpm) on flow rate, shear rate, porosity, fiber orientation, fiber length and tensile strength in 20 % carbon fiber-filled acrylonitrile butadiene styrene. ANOVA results show that screw speed significantly impacts flow rate, while nozzle diameter and temperature have lesser effects. Shear rate increases with smaller nozzles and higher speeds. Porosity decreases from 5.58 % with a 10.16 mm nozzle to 3.11 % with a 5.08 mm nozzle at 150 rpm due to increased shear rates, which induce shear thinning, reducing viscosity and facilitating gas escape. Larger nozzles (10.16 mm) produce larger, more heterogeneous pores, while smaller nozzles (5.08 mm) yield smaller, uniform pores. Beads produced with the 5.08 mm nozzle exhibit longer fiber lengths due to reduced residence time, lower shear stress, and better alignment. Fiber orientation improves with smaller nozzles due to higher shear rates but decreases with higher screw speeds (280 rpm) due to shorter residence times. The highest fiber alignment (A xx ∼ 0.65) and low porosity (∼3%) were achieved with a 5.08 mm nozzle at 150 rpm, while equivalent additive manufacturing-compression molding samples exhibited better tensile strength (∼93 MPa) under these conditions. In conclusion, these findings emphasize the importance of optimizing processing parameters to enhance fiber alignment and reduce porosity for improved mechanical performance.

Design of experiments↗

In situ study on the compression deformation of MoNbTaVW high-entropy alloy

The excellent mechanical properties of high-entropy alloys (HEAs) make them promising materials for advances in science and technology. However, the underlying mechanism of plastic deformation is not well understood. In situ experiments are urgently required to provide a fundamental understanding of the plastic deformation under high pressure. We performed in situ synchrotron X-ray diffraction (XRD) experiments to study compression deformation behavior of the HEA MoNbTaVW in a radial diamond anvil cell (rDAC). Our results show that the strength and ratio of the stress-to-shear modulus values are ~1.5 and 3 times that of pure tungsten (W), respectively. MoNbTaVW showed plastic deformation above 5 GPa and displayed a much stronger texture. In this work, we found that the active dislocation behavior is mainly responsible for the high strength in MoNbTaVW under compression. This unique technique opens a new avenue to investigate the in situ mechanical properties and their mechanism in other types of HEAs.

36 MATERIALS SCIENCE↗

Strengthening mechanisms for microstructures containing unimodal and bimodal γ' precipitates in ATI 718Plus

Here, the influence of γ' precipitate size distribution on the deformation mechanisms under tensile loading in ATI 718Plus was studied. A set of aging treatments within the temperature range of 720 °C–900 °C was performed on solution-treated samples to obtain various γ' precipitate size distributions. Unimodal and bimodal γ' precipitate size distributions were achieved through single-step and two-step aging sequences, respectively, and such microstructures were tensile tested to failure to assess their yield strength, ultimate tensile strength, and elongation-to-failure. Some of the tensile samples were interrupted after achieving 3–4 % plastic strain, and the deformed microstructures were examined using transmission electron microscopy to investigate the γ' precipitate-dislocation interactions. For the unimodal γ' precipitate size distribution samples with the smaller γ' precipitates (radius ~ 7 nm), dislocations sheared through the precipitates. Both dislocation loops and paired dislocations were observed for the microstructures containing larger γ' precipitates (radius ~ 24 nm). The microstructure containing a bimodal γ' precipitate size distribution, which included average γ' precipitate radii of ~6 nm and ~28 nm, exhibited shearing as the dominant deformation mechanism, and this microstructure exhibited the highest strength values. The experimental observations were rationalized based on the theoretically-calculated critical resolved shear stress values for shearing and looping and a modified model for predicting the yield strength for bimodal microstructures was introduced.

36 MATERIALS SCIENCE↗

Shock physics in warm dense matter: A quantum hydrodynamics perspective

Abstract Warm dense matter (WDM), an exotic, highly compressed state of matter between solid and plasma phases, is of high current interest, in particular for astrophysics and inertial confinement fusion. For the latter, in particular the propagation of compression shocks is crucial. The main unknown in the shock propagation in WDM is the behaviour of the electrons since they are governed by correlations, quantum and spin effects that need to be accounted for simultaneously. Here we describe the shock dynamics of the warm dense electron gas using a quantum hydrodynamic model. From the numerical hydrodynamic simulations, we observe that the quantum Bohm pressure induces shear force that weakens the formation and strength of the shock. In addition, the Bohm pressure induces an electron density response that takes the form of oscillations. This is confirmed by the theoretical analysis of the early stage of the shock formation. Our theoretical and numerical analyses allow us to identify characteristic dimensionless shock propagation parameters at which the effect of the Bohm force is important.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Kelvin–Helmholtz instability under stabilizing parallel magnetic field in nonhomogeneous compressible MHD flows

We study the Kelvin–Helmholtz instability (KHI) for the general case of a compressible, nonhomogeneous, magnetized plasma flow. The study is limited to a vortex sheet interface with an imposed parallel magnetic field. We introduce a new formalism based on a convective Mach number M c , a convective Alfvénic Mach number M Ac , and a total convective Mach number that combines the two. We derive an analytic expression of the KHI growth rate for a homogeneous flow (i.e., zero Atwood number, A=0) that converges toward both the expression for unmagnetized compressible flow and Chandrasekhar's expression for magnetized incompressible flow. Otherwise, the dispersion relation is solved numerically and allows deriving general stability diagrams of magnetized KHI for the triplet (A, M c , β −plasma) parameters. We show these parameters uniquely define all configurations for a parallel magnetic field. We also construct diagrams with respect to the convective Alfvénic Mach number, the β − plasma parameter, or the magnetic field showing which magnetic field strength is required for stabilizing a given shear flow. The theoretical growth rates are compared with 18 simulations made with the GAMERA code, currently used for 3D magnetospheric simulations. Finally, we apply our results to the analysis of a past KHI experiment performed at the OMEGA laser facility, showing linear theory succeeds to provide accurate estimates of the growth rate at early times. We further discuss how our results can inform future experiments in the high-Mach magnetized regime at the National Ignition Facility. Possible limitations of the study due to resistive, mixing, or turbulence effects are discussed.

compressible flows↗

Evaluating Effects of Shear Processing on 2D Crystalline Materials in 3D Metal Matrices: Atomistic Understanding of High Shear Deformation of Copper Graphene Composites

Composites made of copper and graphene demonstrate high strength, lubricity and enhanced electrical and thermal conductivity compared pure copper. However, manufacturing these composites at bulk volumes for industrial applications has been a big challenge. Shear deformation assisted processing is an effective method for manufacturing materials such as copper-graphene composites demonstrating ultra-fine grain structures and compositional homogeneity. Nevertheless, microstructural evolution of the composites and their property development under such conditions is not clearly understood currently. To rectify this gap in literature, high strain shear deformation of copper coated graphene foils was performed using a tribometer pin in this study. Changes in microstructure of the composite as well as the constituent components under shear deformation was correlated to process conditions. A sharp increase in the coefficient of friction attributed to rupture and smearing of graphene layer into copper substrate was observed during the shear processing. The coefficient of friction of the sheared copper/graphene composite was lower than that of pure copper, suggesting that partially worn graphene is effectively lubricious at the macroscale. A multimodal characterization of the processed region further revealed a shear deformation-induced ultrafine two-phase grain-structure consisting of copper and graphitic domains. Shear deformation reduced the copper grain size from around 50 – 100 µm to ~200 nm on an average and ~2 – 5 nm in some locations. The semicrystalline graphene films were observed to fracture into 10 – 50 µm size flakes. Oxygen enrichment was observed in the processed region. Finally, graphitic domain were identified for the first time in the copper matrix and not just at the grain boundaries providing evidence for a metastable composite microstructure as a result of solid phase processing at room temperature.

36 MATERIALS SCIENCE↗

Investigation of interlayer adhesion of 3D printable cementitious material from the aspect of printing process

The safety of structure printed by extrusion-based 3D concrete printing (3DCP) is significantly influenced by interlayer bonding, which is governed by fresh material properties and processes, including mixing, printing, and post-processing phases. Much literature focused on improving interlayer bond strength via material tailoring/bonding agent addition but gave insufficient attention to other phases' impacts. This study investigates the effects of parameters on interlayer bond strength from different phases in 3DCP, including superplasticizer dosage, printing speed, and curing condition. In the mixing phase, the superplasticizer dosage was increased to reduce I{sub thix} and increase surface moisture content (SMC), consequently improving interface microstructure and interlayer bond strength. In the printing phase, similar results were observed by increasing pumping speed to increase material shear rate. In the post-processing phase, proper curing also improved interlayer bond strength. While SMC has a critical impact on interlayer bond strength, material thixotropic index (I{sub thix}) probably has a stronger influence.

36 MATERIALS SCIENCE↗

Extent of interlocking and metallurgical bonding in friction riveting of aluminum alloy to steel

In this study, the joining of 6061-T6 aluminum alloy and DP590 steel using a M42 steel rivet via friction riveting technique is investigated. The surface morphology and microstructure characterization reveal the formation of an anchor zone that imparts mechanical interlock as well as the formation of metallurgical bonds at the interface of aluminum and steel. A combination of interlocking and bonding results in the achievement of a high load-carrying capacity of 5.7 kN during lap shear testing at room temperature. A finite element-based computational model was developed which accurately predicted the lap shear response of the joint. The model revealed that the metallurgical bond formed during fric-riveting adds 39% peak load strength to the joint. An extensive microstructural investigation, post-lap-shear fractography, and the modeling results, together provided insights on the joint failure mechanism. In conclusion, this study highlights that friction riveting is a promising method for aluminum-to-steel dissimilar joining, which is important for lighweighing automotive vehicles for energy efficiency.

36 MATERIALS SCIENCE↗

Molecular dynamics study on interface formation and bond strength of impact-welded Mg-steel joints

It was recently demonstrated that the vaporizing foil actuator welding (VFAW) method can directly join immiscible magnesium and steel alloys without coating or a third chemical element based intermetallic compound layer. The VFAW Mg/steel joint exhibits a mixed interface layer of up to 200μm thickness consisting of Mg matrix and Fe particles. Computer simulations have suggested the formation of the interlayer is from the high-velocity frictional shearing between the Mg/steel substrates during the oblique impact in the VFAW process. This paper investigates the formation of Mg-Fe interlayer under VFAW condition with different shearing velocities using molecular dynamics (MD) model, and studies the bonding strength under different scenarios. Finally, the results elucidate the critical role of shearing velocity and surface roughness in achieving Mg/Fe joint.

36 MATERIALS SCIENCE↗

Tailoring grain growth and solid solution strengthening of single-phase CrCoNi medium-entropy alloys by solute selection

In the present study, we selected solutes to be added to the CrCoNi medium-entropy alloy (MEA) based on the mismatch of self-diffusion activation energy (SDQ) between the alloying elements and constituent elements of the matrix, and then investigated their grain growth behavior and mechanical properties. Mo and Al were selected as the solutes for investigation primarily because they have higher and lower SDQ, respectively, than those of the matrix elements; a secondary factor was their higher and lower shear modulus. Their concentrations were fixed at 3 at.% each because previous work had shown these compositions to be single-phase solid solutions with the face-centered cubic structure. Three alloys were produced by arc melting, casting, homogenizing, cold rolling and annealing at various temperatures and times to produce samples with different grain sizes. They were (a) the base alloy CrCoNi, (b) the base alloy plus 3 at.% Mo, and (c) the base alloy plus 3 at.% Al. The activation energies for grain growth of the CrCoNi, CrCoNi-3Mo and CrCoNi-3Al MEAs were found to be ~251, ~368 and ~219 kJ/mol, respectively, consistent with the notion that elements with higher SDQ (in this study Mo) retard grain growth (likely by a solute-drag effect), whereas those with lower values (Al) accelerate grain growth. The room-temperature tensile properties show that Mo increases the yield strength by ~40% but Al addition has a smaller strengthening effect consistent with their relative shear moduli. The yield strength as a function of grain size for the three singlephase MEAs follows the classical Hall-Petch relationship with much higher slopes (> 600 MPa μm -0.5 ) than traditional solid solutions. Furthermore, this work shows that the grain growth kinetics and solid solution strengthening of the CrCoNi MEA can be tuned by selecting solute elements that have appropriate diffusion and physical properties.

36 MATERIALS SCIENCE↗

Improved Calculation of the Young’s Modulus of Rectangular Prisms from Their Resonant Frequency Overtones by Identifying Appropriate Shear Constants

Young’s modulus is an important parameter for characterizing the strength of, and wave propagation through, a given material. This study improves the estimation of Young’s modulus using the impulse excitation technique based on an experimental analysis of 19 borosilicate glass bars. Analysis of the frequency equations relating Young’s modulus to the out-of-plane and in-plane flexural resonant frequencies of rectangular prisms has been conducted for both the fundamental frequency and its overtones at higher orders of vibration. Furthermore, the Young’s moduli of three novaculite rocks with various porosities were then measured up to the seventh order of vibration to validate the optimum shear constant equation for estimating Young’s modulus. Young’s modulus was found to be nearly frequency independent for these rock samples.

Impulse excitation↗

Joining of Thermoset Carbon Fiber Reinforced Polymer and AZ31 Magnesium Alloy Sheet Via Friction Stir Interlocking

A new technique called friction stir interlocking (FSI) was applied for lap-joining of AZ31 magnesium sheet and thermoset carbon fiber reinforced polymer (TS-CFRP) sheet. Instead of directly joining AZ31 and TS-CFRP, a series of magnesium interlocks were used to friction stir weld with AZ31 sheet to enable joining with TS-CFRP. Microstructural characterization of joint cross sections showed that a tool rotation rate of 800 rpm produced incomplete mixing of magnesium interlocks and the top AZ31 sheet, while 1200 rpm achieved sufficient material mixing to avoid unwelded regions. Mechanical property characterization showed that AZ31/TS-CFRP dissimilar joints failed through the magnesium interlock shanks during lap shear tensile testing, with a maximum normalized joint strength reaching ~100 MPa.

Wang, Tianhao↗