Search NASA⌕ Search

SEARCH · Search NASA

Results for “WELDING, ARC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Mechanisms of Oxide Formation in the Self-Reacting Friction Stir Weld Process

The initial objective of this study was to evaluate the effect of an extended delay time between preweld cleaning and the completion of a self-reacting friction stir welding (SRFSW) process on the resulting quality of various thickness panels of AA2219-T87. The current NASA standard specifies no more than a 48 hour delay between preweld cleaning and actual welding. The concern is whether increasing the cleaning delay time results in development of the residual oxide defect (ROD) in SRFSW. This concern emanates from the possibility of increased time correlating with increased oxide layer thickness on the faying surfaces. Oxide content on the faying surfaces has been reported to correlate with the occurrence of the ROD which reduces mechanical properties. When the SRFSW process was first adopted by the NASA Marshall Space Flight Center (MSFC), unexpected low tensile values that resulted were attributed to oxides within the weld that appeared to follow the former faying surface contours. Mitigation of the ROD was achieved through a combination of modifications to the processing parameters, tool designs, and incorporation of a weld seam offset. Two operations are involved in preweld cleaning: the first is removal of oil and grease, and the second is removal of surface oxides. In arc welding, improper cleaning of the faying surfaces of aluminum welded joints can increase the sensitivity toward development of defects. As the aluminum is locally melted, these contaminants contribute toward the development of porosity, inclusions, entrapped oxides, and other discontinuities which can degrade the strength of the weld joint. For weldment of large structures, the weld joint is typically cleaned, fit-up, and tack welded prior to the final full penetration welding pass. Because of the stringent joint fit-up requirements for mismatch and peaking for launch vehicle structures, the joint fit-up can sometimes contribute to lengthy delays between cleaning and tack welding, especially for circumferential weld joints on large diameter components. When the conventional friction stir welding (CFSW) process was introduced at the NASA MSFC, there was no procedure for cleaning prior to the solid-state joining process. As the process expanded to include SRFSW, preparation of the faying, crown, and root surfaces were implemented to overcome the ROD. Although the solid-state process is not expected to reach temperatures high enough for dissociation of the native oxide layer, concern remained regarding the redeposition of the native oxide layer within the stir zone. NASA has previously established the allowable time at 48 hours between preweld cleaning and a SRFSW process. The effect of potential 2 contamination resulting from an extended delay to 188 hours was subsequently evaluated for SRFSWs using tensile testing and metallographic imaging. Tensile specimens were tested at room temperature (RT), and at cryogenic conditions of liquid nitrogen (LN2) and liquid hydrogen. No detrimental effect on weld quality, as determined by weld strength, was reported for cleaning delays of 48, 120, 168, 240 or 288 hours. While no trends were established in this study, which extended the delay from 48 to 188 hours, there were a few outliers in terms of ultimate tensile strength (UTS). According to M. Fisher's 2014 Boeing Company Memo no. EYBF-MAF-14-029, all outliers were above the minimum acceptance criteria, but out of family with respect to the average values. As the robustness and reliability of any process ultimately depends on the average values as well as the outliers, an understanding of the cause of these outliers will ultimately improve the process. This report examines those outliers and their possible causes.

Schneider, J. A.↗

Weldability Investigation of Crack Resistant Aluminum Filler Metals Developed for Large Scale Additive Manufacturing and Industrial Welding Applications

In this study the NASA MSFC welding and manufacturing team investigated a new-age aluminum filler wire designed for welding and additive manufacturing (AM) of high strength aluminum alloys. High strength aluminum alloys are known to exhibit hot cracking and hot tearing issues during fusion welding operations. The goal of this investigation was to determine whether this new-age family of alloys can suppress the hot cracking and hot tearing issues exhibited during welding of high strength aluminum alloys and to do an initial characterization of the mechanical performance of welds created using these filler wires. This study focuses on fusion welding of aluminum alloy 6061 and compares the weldability characteristics of five aluminum filler metals and two forms of 6061 base material. The MSFC team utilized manual gas tungsten arc welding (GTAW) to conduct all welding operations and carried out metallographic analysis accompanied with mechanical testing to evaluate the performance of the welds created during this study. During the study it was observed that the new-age filler wires facilitated grain refinement in the weld fusion zone and were capable of creating crack free welds in aluminum alloy 6061 while exhibiting properties that met or exceeded conventional off the shelf aluminum filler metals.

Welding↗

Identification Of Anomalies In Welds

Advanced techniques combined with conventional analytical methods. Combination of real-time radiography, scanning electron microscopy, and energy-dispersive spectrometry identify enigmatic features in radiographs of welds where standard tensile, hardness, and electrical-conductivity tests and visible-light microscopic and macroscopic examinations insufficient. New combination of techniques applied successfully to variable-polarity-plasma-arc welds of 2219 aluminum alloy. Joints subjected to penetration, fill, and weld-repair passes with 2319 aluminum weld wire.

Knichen, David G.↗

Tool For Friction Stir Tack Welding of Aluminum Alloys

A small friction-stir-welding tool has been developed for use in tack welding of aluminum-alloy workpieces. It is necessary to tack-weld the workpieces in order to hold them together during friction stir welding because (1) in operation, a full-size friction-stir-welding tool exerts a large force that tends to separate the workpieces and (2) clamping the workpieces is not sufficient to resist this force. It is possible to tack the pieces together by gas tungsten arc welding, but the process can be awkward and time-consuming and can cause sufficient damage to necessitate rework. Friction stir tack welding does not entail these disadvantages. In addition, friction stir tack welding can be accomplished by use of the same automated equipment (except for the welding tool) used in subsequent full friction stir welding. The tool for friction stir tack welding resembles the tool for full friction stir welding, but has a narrower shoulder and a shorter pin. The shorter pin generates a smaller workpiece-separating force so that clamping suffices to keep the workpieces together. This tool produces a continuous or intermittent partial-penetration tack weld. The tack weld is subsequently consumed by action of the larger tool used in full friction stir welding tool.

Bjorkman, Gerald W.↗

Robotic and automatic welding development at the Marshall Space Flight Center

Welding automation is the key to two major development programs to improve quality and reduce the cost of manufacturing space hardware currently undertaken by the Materials and Processes Laboratory of the NASA Marshall Space Flight Center. Variable polarity plasma arc welding has demonstrated its effectiveness on class 1 aluminum welding in external tank production. More than three miles of welds were completed without an internal defect. Much of this success can be credited to automation developments which stabilize the process. Robotic manipulation technology is under development for automation of welds on the Space Shuttle's main engines utilizing pathfinder systems in development of tooling and sensors for the production applications. The overall approach to welding automation development undertaken is outlined. Advanced sensors and control systems methodologies are described that combine to make aerospace quality welds with a minimum of dependence on operator skill.

Jones, C. S.↗

Gray-Scale Processing For Tracking Of Welds

Digital analysis of video-image-processing system contributes to automation of weld-seam tracking. Makes no contact with seam. Small television camera views seam just ahead of point currently being welded. Arc provides illumination. Periodically frame grabber digitizes video image and stores in computer memory as gray-scale values. Seam located by analyzing Hough-transform arrays of derivatives of digitally-filtered image data. Information on location and orientation of seam used as feedback by welding robot to correct deviations of electrode from seam as welding continues.

Gutow, David A.↗

Vision Systems Illuminate Industrial Processes

When NASA designs a spacecraft to undertake a new mission, innovation does not stop after the design phase. In many cases, these spacecraft are firsts of their kind, requiring not only remarkable imagination and expertise in their conception but new technologies and methods for their manufacture. In the realm of manufacturing, NASA has from necessity worked on the cutting-edge, seeking new techniques and materials for creating unprecedented structures, as well as capabilities for reducing the cost and increasing the efficiency of existing manufacturing technologies. From friction stir welding enhancements (Spinoff 2009) to thermoset composites (Spinoff 2011), NASA s innovations in manufacturing have often transferred to the public in ways that enable the expansion of the Nation s industrial productivity. NASA has long pursued ways of improving upon and ensuring quality results from manufacturing processes ranging from arc welding to thermal coating applications. But many of these processes generate blinding light (hence the need for special eyewear during welding) that obscures the process while it is happening, making it difficult to monitor and evaluate. In the 1980s, NASA partnered with a company to develop technology to address this issue. Today, that collaboration has spawned multiple commercial products that not only support effective manufacturing for private industry but also may support NASA in the use of an exciting, rapidly growing field of manufacturing ideal for long-duration space missions.

Source record↗

Welding Curtains

Concept of transparent welding curtains made of heavy duty vinyl originated with David F. Wilson, President of Wilson Sales Company. In 1968, Wilson's curtains reduced glare of welding arc and blocked ultraviolet radiation. When later research uncovered blue light hazards, Wilson sought improvement of his products. He contracted Dr. Charles G. Miller and James B. Stephens, both of Jet Propulsion Laboratory (JPL), and they agreed to undertake development of a curtain capable of filtering out harmful irradiance, including ultraviolet and blue light and provide protection over a broad range of welding operation. Working on their own time, the JPL pair spent 3 years developing a patented formula that includes light filtering dyes and small particles of zinc oxide. The result was the Wilson Spectra Curtain.

Source record↗

Proof-of-Concept Experiments on a Gallium-Based Ignitron for Pulsed Power Applications

Ignitrons are electrical switching devices that operate at switching times that are on the order of microseconds, can conduct high currents of thousands of amps, and are capable of holding off tens of thousands of volts between pulses. They consist of a liquid metal pool within an evacuated tube that serves both the cathode and the source of atoms and electrons for an arc discharge. Facing the liquid metal pool is an anode suspended above the cathode, with a smaller ignitor electrode tip located just above the surface of the cathode. The ignitron can be charged to significant voltages, with a potential difference of thousands of volts between anode and cathode. When an ignition pulse is delivered from the ignitor electrode to the cathode, a small amount of the liquid metal is vaporized and subsequently ionized, with the high voltage between the anode and cathode causing the gas to bridge the gap between the two electrodes. The electrons and ions move rapidly towards the anode and cathode, respectively, with the ions liberating still more atoms from the liquid metal cathode surface as a high-current plasma arc discharge is rapidly established. This arc continues in a self-sustaining fashion until the potential difference between the anode and cathode drops below some critical value. Ignitrons have been used in a variety of pulsed power applications, including the railroad industry, industrial chemical processing, and high-power arc welding. In addition, they might prove useful in terrestrial power grid applications, serving as high-current fault switches, quickly shunting dangerous high-current or high-voltage spikes safely to ground. The motivation for this work stemmed from the fact that high-power, high-reliability, pulsed power devices like the ignitron have been used for ground testing in-space pulsed electric thruster technologies, and the continued use of ignitrons could prove advantageous to the future development and testing of such thrusters. Previous ignitron designs have used mercury as the liquid metal cathode, owing to its presence as a liquid at room temperatures and a vapor pressure of 10 Pa (75 mtorr) at room temperature. While these are favorable properties, there are obvious environmental and personal safety concerns with the storage, handling, and use of mercury and its compounds. The purpose of the present work was to fabricate and test an ignitron that used as its cathode an alternate liquid metal that was safe to handle and store. To that end, an ignitron test article that used liquid gallium as the cathode material was developed and tested. Gallium is a metal that has a melting temperature of 29.76 C, which is slightly above room temperature, and a boiling point of over 2,300 C at atmospheric pressure. This property makes gallium the element with the largest relative difference between melting and boiling points. Gallium has a limited role in biology, and when ingested, it will be subsequently processed by the body and expelled rather than accumulating to toxic levels. The next section of this Technical Memorandum (TM) provides background information on the development of mercury-based ignitrons, which serves as the starting point for the development of the gallium-based variant. Afterwards, the experimental hardware and setup used in proof-of-concept testing of a basic gallium ignitron are presented. Experimental data, consisting of discharge voltage and current waveforms as well as high-speed imaging of the gallium arc discharge in the gallium ignitron test article, are presented to demonstrate the efficacy of the concept. Discussion of the data and suggestions on improvements for future iterations of the design are presented in the final two sections of this TM.

Ali, H. K.↗

Fabrication techniques for thoria-dispersed /TD/ nickel

Metal spinning forms combustion chamber sections and nozzle sections, arc welding joints sections to form rocket motor. Hastelloy-X as filler results in slightly weaker weld than the TD nickel weld, but permits formation of larger rocket motor than is otherwise possible.

Source record↗

Electrical termination techniques

A technical review of high reliability electrical terminations for electronic equipment was made. Seven techniques were selected from this review for further investigation, experimental work, and preliminary testing. From the preliminary test results, four techniques were selected for final testing and evaluation. These four were: (1) induction soldering, (2) wire wrap, (3) percussive arc welding, and (4) resistance welding. Of these four, induction soldering was selected as the best technique in terms of minimizing operator errors, controlling temperature and time, minimizing joint contamination, and ultimately producing a reliable, uniform, and reusable electrical termination.

Oakey, W. E.↗

High energy density capacitors for vacuum operation with a pulsed plasma load

Results of the effort of designing, fabricating, and testing of a 40 joules/lb (88.2 joules/Kg) high voltage energy storage capacitor suitable for operating a pulsed plasma thruster in a vacuum environment for millions of pulses are presented. Using vacuum brazing and heli-arc welding techniques followed by vacuum and high pressure helium leak tests it was possible to produce a hermetically sealed relatively light weight enclosure for the dielectric system. An energy density of 40 joules/lb was realized with a KF-polyvinylidene fluoride dielectric system. One capacitor was D.C. life tested at 4 KV (107.8 joules/lb) for 2,000 hours before it failed. Another exceeded 2,670 hours without failure at 38.3 joules/lb. Pulse life testing in a vacuum exceeded 300,000 discharges with testing still in progress. The D.C. life test data shows a small decrease in capacitance and an increase in dissipation factor with time. Heat transfer from the load to the capacitor must also be considered besides the self-heat generated by the capacitor.

Guman, W. J.↗