Search NASA⌕ Search

SEARCH · Search NASA

Results for “WELDING MACHINE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

An evaluation of GTAW-P versus GTA welding of alloy 718

Mechanical properties were evaluated to determine statistically whether the pulsed current gas tungsten arc welding (GTAW-P) process produces welds in alloy 718 with room temperature structural performance equivalent to current Space Shuttle Main Engine (SSME) welds manufactured by the constant current GTAW-P process. Evaluations were conducted on two base metal lots, two filler metal lots, two heat input levels, and two welding processes. The material form was 0.125-inch (3.175-mm) alloy 718 sheet. Prior to welding, sheets were treated to either the ST or STA-1 condition. After welding, panels were left as welded or heat treated to the STA-1 condition, and weld beads were left intact or machined flush. Statistical analyses were performed on yield strength, ultimate tensile strength (UTS), and high cycle fatigue (HCF) properties for all the post welded material conditions. Analyses of variance were performed on the data to determine if there were any significant effects on UTS or HCF life due to variations in base metal, filler metal, heat input level, or welding process. Statistical analyses showed that the GTAW-P process does produce welds with room temperature structural performance equivalent to current SSME welds manufactured by the GTAW process, regardless of prior material condition or post welding condition.

Gamwell, W. R.↗

Simulation of Distortion and Residual Stress Development During Heat Treatment of Steel Castings

Heat treatment and associated processing, such as quenching, are critical during high strength steel casting production. These processes must be managed closely to prevent thermal and residual stresses that may result in distortion, cracking (particularly after machining), re-work, and weld repair. The risk of casting distortion limits aggressive quenching that can be beneficial to the process and yield an improved outcome. As a result of these distortions, adjustments must be made to the casting or pattern design, or tie bars must be added. Straightening castings after heat treatments can be both time-consuming and expensive. Residual stresses may reduce a casting's overall service performance, possibly resulting in catastrophic failure. Stress relieving may help, but expends additional energy in the process. Casting software is very limited in predicting distortions during heat treatment, so corrective measures most often involve a tedious trial-and-error procedure. An extensive review of existing heat treatment residual stress and distortion modeling revealed that it is vital to predict the phase transformations and microstructure of the steel along with the thermal stress development during heat treatment. After reviewing the state-of-the-art in heat treatment residual stress and distortion modeling, an existing commercial code was selected because of its advanced capabilities in predicting phase transformations, the evolving microstructure and related properties along with thermal stress development during heat treatment. However, this software was developed for small parts created from forgings or machined stock, and not for steel castings. Therefore, its predictive capabilities for heat treatment of steel castings were investigated. Available experimental steel casting heat treatment data was determined to be of insufficient detail and breadth, and so new heat treatment experiments were designed and performed, casting and heat treating modified versions of the Navy-C ring (a classical test shape for heat treatment experiments) for several carbon and low alloy steels in order to generate data necessary to validate the code. The predicted distortions were in reasonable agreement with the experimentally measured values. However, the final distortions in the castings were small, making it difficult to determine how accurate the predictions truly are. It is recommended that further validation of the software be performed with the aid of additional experiments with large production steel castings that experience significant heat treatment distortions. It is apparent from this research that the mechanical properties of the bonded sand used for cores and sand molds are key in producing accurate stress simulation results. Because of this, experiments were performed to determine the temperature-dependent elastic modulus of a resin-bonded sand commonly utilized in the steel casting industry. The elastic modulus was seen to vary significantly with heating and cooling rates. Also, the retained room temperature elastic modulus after heating was seen to degrade significantly when the sand was heated above 125°C. The elastic modulus curves developed in this work can readily be utilized in casting simulation software. Additional experiments with higher heating rates are recommended to determine the behavior of the elastic modulus in the sand close to the mold-metal interface. The commercial heat treatment residual stress and distortion code, once fully validated, is expected to result in an estimated energy savings of 2.15 trillion BTU's/year. Along with these energy savings, reduction of scrap and improvement in casting yield will result in a reduction of the environmental emissions associated with the melting and pouring of the metal which will be saved as a result of this technology.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

MCPC Friction Stir Welding (FSW) Process Data

Processing parameters and machine log data for the MCPC LDRD Agile investment is collected material samples processed. This dataset captures the selected processing parameters, machine logs captured during material processing, and descriptions of how characterization samples were extracted from processed plates of material. The collect characterization data is captured in other datasets.

316 Stainless Steel↗

Effect of copper-rich regions on tensile properties of VPPA weldments of 2219-T87 aluminum

This study examines the relations between tensile properties and microstructural features of variable polarity plasma arc (VPPA) weldments of 2219-T87 aluminum. Crack initiation and weld failure of transverse tensile specimens of single and multipass weldments were studied. The specimens fractured on the rising portion of the stress-strain curve prior to necking, signifying that an increase in strength would accompany an increase in ductility. Of particular interest is a shallow, typically 0.001-0.003-in. (0.03-0.08-mm) deep, copper-rich region located in the crown and root corners of the weld. This region is a primary source of crack initiation and growth, due to its brittle nature and highly strained location. The brittle regions were removed by electropolishing and machining to determine their effect on weld tensile properties. The removal increased the ductility of the weld specimens, and in the case of single pass welds, actually increased the load carrying capacity. Local strain measurements and metallographic and chemical analyses are presented.

Hartman, J. A.↗

NASA's National Center for Advanced Manufacturing

NASA has designated the Principal Center Assignment to the Marshall Space Flight Center (MSFC) for implementation of the National Center for Advanced Manufacturing (NCAM). NCAM is NASA s leading resource for the aerospace manufacturing research, development, and innovation needs that are critical to the goals of the Agency. Through this initiative NCAM s people work together with government, industry, and academia to ensure the technology base and national infrastructure are available to develop innovative manufacturing technologies with broad application to NASA Enterprise programs, and U.S. industry. Educational enhancements are ever-present within the NCAM focus to promote research, to inspire participation and to support education and training in manufacturing. Many important accomplishments took place during 2002. Through NCAM, NASA was among five federal agencies involved in manufacturing research and development (R&D) to launch a major effort to exchange information and cooperate directly to enhance the payoffs from federal investments. The Government Agencies Technology Exchange in Manufacturing (GATE-M) is the only active effort to specifically and comprehensively address manufacturing R&D across the federal government. Participating agencies include the departments of Commerce (represented by the National Institute of Standards and Technology), Defense, and Energy, as well as the National Science Foundation and NASA. MSFC s ongoing partnership with the State of Louisiana, the University of New Orleans, and Lockheed Martin Corporation at the Michoud Assembly Facility (MAF) progressed significantly. Major capital investments were initiated for world-class equipment additions including a universal friction stir welding system, composite fiber placement machine, five-axis machining center, and ten-axis laser ultrasonic nondestructive test system. The NCAM consortium of five universities led by University of New Orleans with Mississippi State University, Tennessee Technological University, Texas A&M University, and Virginia Polytechnic Institute and State University provided wide-ranging engineering research, new degree/curriculum programs, and a web-based lecture series. NCAM has fostered an important presence and leadership role within the national manufacturing community. Its progressive influence can be seen in government, industry and academia, and in national associations, professional organizations, conferences, workshops, and forums.

Vickers, John↗

Ares I Upper Stage Element

This slide presentation reviews the elements that make up the Ares I launch vehicle, with particular attention devoted to the upper stage of the vehicle. The upper stage elememnts, a lunar mission profile, and the upper stage objectives are reviewed. The work that Marshall Space Flight Center is doing is highlighted: work on the full scale welding process, the vertical milling machining, and the thermal protection system.

Chojnacki, Kent↗

Temporarily alloying titanium to facilitate friction stir welding

While historically hydrogen has been considered an impurity in titanium, when used as a temporary alloying agent it promotes beneficial changes to material properties that increase the hot-workability of the metal. This technique known as thermohydrogen processing was used to temporarily alloy hydrogen with commercially pure titanium sheet as a means of facilitating the friction stir welding process. Specific alloying parameters were developed to increase the overall hydrogen content of the titanium sheet ranging from commercially pure to 30 atomic percent. Each sheet was evaluated to determine the effect of the hydrogen content on process loads and tool deformation during the plunge phase of the friction stir welding process. Two materials, H-13 tool steel and pure tungsten, were used to fabricate friction stir welding tools that were plunged into each of the thermohydrogen processed titanium sheets. Tool wear was characterized and variations in machine loads were quantified for each tool material and weld metal combination. Thermohydrogen processing was shown to beneficially lower plunge forces and stabilize machine torques at specific hydrogen concentrations. The resulting effects of hydrogen addition to titanium metal undergoing the friction stir welding process are compared with modifications in titanium properties documented in modern literature. Such comparative analysis is used to explain the variance in resulting process loads as a function of the initial hydrogen concentration of the titanium.

08 HYDROGEN↗

Pacific Northwest National Laboratory Investigation of the Stress Corrosion Cracking in Nickel-Base Alloys (Volume 2)

The objective of this program is to evaluate the primary water stress corrosion cracking (PWSCC) susceptibility of high chromium alloy 690 and its weld metals, establish quantitative measurements of crack-growth rates and determine relationships among cracking susceptibility, environmental conditions and metallurgical characteristics. Stress-corrosion, crack-growth rates have been determined for 12 alloy 690 specimens, 11 alloy 152/52/52M weld metal specimens, 4 alloy 52M/182 overlay specimens and 2 alloy 52M/82 inlay specimens in simulated PWR primary water environments. The alloy 690 test materials included three different heats of extruded control-rod-drive mechanism (CRDM) tubing with variations in the initial material condition and degree of cold work for one heat. Two cold-rolled (CR) alloy 690 plate heats were also obtained and evaluated enabling comparisons to the CR CRDM materials. Weld metal, overlay and inlay specimens were machined from industry mock ups to provide plant-representative materials for testing. Specimens have been tested for one alloy 152 weld, two alloy 52 welds and three alloy 52M welds. The overlay and inlay specimens were prepared to propagate stress-corrosion cracks from the alloy 182 or 82 material into the more resistant alloy 52M. In all cases, crack extension was monitored in situ by direct current potential drop (DCPD) with length resolution of about +1 µm making it possible to measure extremely low growth rates approaching 5x10 -10 mm/s. Most SCC tests were performed at 325-360°C with hydrogen concentrations from 11-29 cc/kg; however, environmental conditions were modified during a few experiments to evaluate the influence of temperature, water chemistry or electrochemical potential on propagation rates. In addition, low-temperature (~50°C) cracking behavior was examined for selected alloy 690 and weld metal specimens. Extensive characterizations have been performed on material microstructures and stress-corrosion cracks by optical and electron microscopy techniques and linked to crack-growth test results to help define material and environmental parameters controlling SCC susceptibility.

Bruemmer, Stephen M.↗

Friction welding.

Results of an exploratory study of the structure and properties of friction welds in Udimet 700 (U-700) and TD-nickel (TD-Ni) bar materials, as well as dissimilar U-700/TD-Ni friction welds. Butt welds were prepared by friction welding 12.7-mm-diam U-700 bars and TD-Ni bars. Specimens for elevated temperature tensile and stress rupture testing were machined after a postweld heat treatment. Friction welding of U-700 shows great potential because the welds were found to be as strong as the parent metal in stress rupture and tensile tests at 760 and 980 C. In addition, the weld line was not detectable by metallographic examination after postheating. Friction welds in TD-Ni or between U-700 and TD-Ni were extremely weak at elevated temperatures. The TD-Ni friction welds could support only 9% as much stress as the base metal for 10-hour stress rupture life at 1090 C. The U-700/TD-Ni weld could sustain only 15% as much stress as the TD-Ni parent metal for a 10-hour stress rupture life at 930 C. Thus friction welding is not a suitable joining method for obtaining high-strength TD-Ni or U-700/TD-Ni weldments.

Moore, T. J.↗

CRACK GROWTH RESPONSE OF ALLOY 152 AND 52 WELD METALS IN SIMULATED PWR PRIMARY WATER

The crack growth response of alloy 152 and 52 weld metals has been measured in simulated PWR primary water at both high (325-350 C) and low (50 C) temperatures. Tests were performed on samples machined from alloy 152 or 52 mockup welds. Propagation rates under cycle + hold and constant K conditions at high temperatures show stable, but extremely low SCC growth rates. The most significant intergranular cracking occurred during cycling at 50 C, particularly for the alloy 152 weld metal at high stress intensity.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Quality status display for a vibration welding process

A method includes receiving, during a vibration welding process, a set of sensory signals from a collection of sensors positioned with respect to a work piece during formation of a weld on or within the work piece. The method also includes receiving control signals from a welding controller during the process, with the control signals causing the welding horn to vibrate at a calibrated frequency, and processing the received sensory and control signals using a host machine. Additionally, the method includes displaying a predicted weld quality status on a surface of the work piece using a status projector. The method may include identifying and display a quality status of a suspect weld. The laser projector may project a laser beam directly onto or immediately adjacent to the suspect welds, e.g., as a red, green, blue laser or a gas laser having a switched color filter.

36 MATERIALS SCIENCE↗

The Effects of Laser Peening and Shot Peening on Mechanical Properties in Friction Stir Welded 7075-T7351 Aluminum

Peening techniques like laser peening and shot peening were used to modify the surface of friction stir welded 7075-T7351 Aluminum Alloy specimens. The tensile coupons were machined such as the loading was applied in a direction perpendicular to the weld direction. The peening effects on the global and local mechanical properties through the different regions of the weld were characterized and assessed. The surface hardness levels resulting from various peening techniques were also investigated for both sides of the welds. Shot peening resulted in an increase to surface hardness levels, but no improvement was noticed on the mechanical properties. In contrast, mechanical properties were improved by laser peening when compared to the unpeened material.

Hatamleh, Omar↗

Effect of Martensite Content on Failure Behavior of Laser Welded Dual-Phase Steel Joints During Deformation

Laser welding was applied to three types of dual-phase (DP) steel sheets (DP590, DP780, and DP980) with different martensite contents. The microstructure of laser welded joints was observed by optical microscope and scanning electron microscope, and the hardness of welded joints was measured by a microhardness tester. The tensile testing machine and the Erichsen test machine were employed to measure the tensile properties and forming properties of welded joints, respectively. The microstructure model showed that the welded joints of three different materials all contained a hardened zone (HZ) that was composed of a fusion zone, a coarse-grained heat-affected zone, and fine-grained heat-affected zone. The microstructure of the HZ contained mainly martensite such that the average martensite content of welded joints was increased by 1.9-9.8%, and the microhardness of the HZ was 1.2-1.9 times that of the base metal (BM). Moreover, the elongation of welded joints decreased with decreasing martensite content in the BM, and the effect was severe for the DP590 welded joint (21.8%) compared to the other two welded joints. During the Erichsen test, deformation failure varied among the welded joints with different martensite contents, and it was determined by the HZ and softened zone. The fracture occurred in the softened zone and ran parallel along the zone for DP980 welded joints, whereas the fracture occurred in the HZ and ran perpendicular to this zone for the other two welded joints. The Erichsen values of the DP590, DP780, and DP980 welded joints were 81.1, 91.7, and 85.0% of the BM, respectively.

36 MATERIALS SCIENCE↗

Pitting behavior of friction stir repair-welded 304L stainless steel in 3.5% NaCl solution at room temperature: role of grain and defect structures

Stainless steel (SS) canisters used for storing spent nuclear waste are prone to chloride-induced stress corrosion cracking. Friction stir welding (FSW), being a low heat input process, can be used for repair welding of these canisters. In this study, an artificial crack was introduced on the 304L SS coupons by an electric discharge machining process. The artificial crack was repair-welded by FSW by maintaining the tool temperature a constant at two levels (725 and 825 °C). Friction stirring significantly reduced the grain size of the stirred zone (SZ) from about 47 to 2–4 μm. The fraction of low-angle grain boundaries increased in the SZ from 2 to 37–43%. Here, on the other hand, the fraction of special grain boundaries (Σ3 and Σ9) that was ~ 50% in the base metal reduced to < 10% in the SZ. During friction stirring, the oxide layer of artificial crack was broken and aligned to form a spiral defect called lazy-S structure. All these microstructural changes affected the corrosion behavior of the FSW specimens when tested in 3.5% NaCl at room temperature using cyclic polarization, chronoamperometry, and electrochemical impedance spectroscopy. The FSW specimens showed lower polarization resistance and lower transpassive potential than those of the base metal specimens. However, the pitting protection potentials of the FSW specimens were higher than that of the base metal. The pitting behavior of the FSW specimens was influenced more by the preferential attack on the lazy-S region than by passive film breakdown. The flat band potentials of the passive film formed on the FSW specimens were more positive than that of base metal. The charge carrier density of passive film formed on the FSW specimens was higher than that of the base metal. The higher fraction of low-angle grain boundaries present in the FSW specimens could supply more number of misorientation dislocations at the metal/film interface which could form anion vacancies by a climb process leading to formation of oxide at these locations without stressing the substrate. Therefore, low-angle boundaries are considered helpful for formation of stress-free passive films that will be highly stable and enhance both pitting and stress corrosion cracking resistance.

Dry storage canister↗

A Comparative Analysis on Microstructure and Fracture Mechanism of X100 Pipeline Steel CGHAZ Between Laser Welding and Arc Welding

The objective of this study is to compare and contrast the differences in microstructure and fracture mechanism between CGHAZ of laser welding and submerged arc welding in X100 pipeline steel. The single-pass welding thermal simulation test of laser welding and submerged arc welding was carried out in MMS-200 thermal simulation test machine using self-made fixtures. The results indicated that the microstructure of laser welding CGHAZ and submerged arc welding CGHAZ was lath martensite and granular bainite, respectively. The impact energy of laser welding CGHAZ was 27 J, and the fracture mode was ductile fracture; the impact energy of submerged arc welding CGHAZ was 7.7 J, and the fracture mode was brittle fracture. The nucleation and propagation mechanism of cracks in different welding modes was established. Microcracks nucleated at the position of dislocation accumulation and remained austenite suppressed crack nucleation in laser welding CGHAZ. The nucleation site was at the M–A constituents in submerged arc welding CGHAZ. The main crack of laser welding CGHAZ was formed by one or a small number of microcracks. The main crack in submerged arc welding CGHAZ was formed by a large number of microcracks. The difference between crack nucleation and propagation mechanism is the reason why the impact energy of laser welding CGHAZ is higher than of submerged arc welding CGHAZ.

36 MATERIALS SCIENCE↗

Weld preparation tool for pipes and tubing

Improved scarfing tool consists of a mount-table, roller-guided assembly. It converts a conventional routing machine for relatively precise field preparation of pipes for welding.

Wallace, E. D.↗

Welding Process Development for Spent Nuclear Fuel Canister Repair

The potential for stress corrosion cracking (SCC) of welded stainless-steel interim storage containers for spent nuclear fuel (SNF) has been identified as a high priority data gap. This paper presents a fusion welding process that was developed for SNF canister repair. Submerged arc welding (SAW) was developed to weld 12.7 mm (0.5 in.) thick 304L stainless steel plates to simulate the initial welds on SNF canisters. The SAW procedure was qualified following ASME Boiler and Pressure Vessel Code requirements. During SAW, the welding temperature was recorded at various locations by using thermocouples. After SAW, weld microstructures were characterized, joint mechanical properties were tested, and the maximum tensile residual stress direction was identified. After SAW procedure qualification, artificial cracks were excavated perpendicular to the maximum tensile residual stress direction in the SAW heat affected zone. Machine cold-wire gas tungsten arc welding (CW-GTAW) was developed and used for repair welding at cracked locations.

Tang, Wei↗

The microstructure of aluminum A5083 butt joint by friction stir welding

This study presents the microstructure of the aluminum A5083 butt joint surface after it has been joined by friction stir welding (FSW) process. The FSW process is a unique welding method because it will not change the chemical properties of the welded metals. In this study, MILKO 37 milling machine was modified to run FSW process on 4 mm plate of aluminum A5083 butt joint. For the experiment, variables of travel speed and tool rotational speed based on capability of machine were used to run FSW process. The concentrated heat from the tool to the aluminum plate changes the plate form from solid to plastic state. Two aluminum plates is merged to become one plate during plastic state and return to solid when concentrated heat is gradually further away. After that, the surface and cross section of the welded aluminum were investigated with a microscope by 400 x multiplication zoom. The welding defect in the FSW aluminum was identified. Then, the result was compared to the American Welding Society (AWS) FSW standard to decide whether the plate can be accepted or rejected.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗