High-Temperature Oxidation Study in a Multi-Oxidant Environment Using 18 O Tracer

The goal of this study was to use 18 O-enriched water to better understand the role of H 2 O in high-temperature oxidation. Seven model and three commercial M-Cr and M-Cr-Al alloys were studied in air with 10% of H 2 O at 800 °C for 5 h. Oxygen from water vapor was more reactive than oxygen from the air and 18 O enriched at the outermost layers of the formed Cr- and Al-rich oxides. Alloys with Al and/or Ti additions showed signs of internal oxidation but 18 O was not enriched inside the alloy in locations with internal oxidation. In conclusion, depending on the alloy Al content, the oxide went from Al oxidation beneath a chromia scale to external alumina scale formation.

18O-enriched water↗

Effect of Water Vapor on Lifetime of 625 and 120 Foils During Oxidation Between 650 and 800 °C

In this work, the oxidation behavior of alloy 625 and 120 foils was studied at 650, 700 and 800 °C in dry air and flowing air + 10% H 2 O up to 10,000 h (alloy 625) or 30,000 h (alloy 120). The effect of water vapor on Cr loss was investigated. Manganese and iron in the 120 foil induced faster Cr depletion in the foil and breakdown of the Cr 2 O 3 scale into Fe and Cr-rich oxide compared to the alloy 625 foil. In the latter case, the presence of Nb led to the formation of Nb and Cr-rich oxide after breakdown of the Cr 2 O 3 scale. Simultaneous Cr loss due to oxidation and volatilization of the Cr 2 O 3 oxide scale was predicted and compared to experimental Cr loss measurements for exposures up to 30,000 h.

36 MATERIALS SCIENCE↗

Morphological and chemical characteristics of oxide scales formed on δ-phase plutonium metal alloys II: 2.0 at% Ga

The focused ion-beam scanning electron microscopy (FIB-SEM) and three-dimensional (3D) microscopy were applied to characterize the subsurface morphological features of oxide scales formed on an ~2.0 at. % Ga plutonium (Pu) metal alloy. Using the FIB-SEM technique, a number of morphological features formed in the interior of the oxide scale from Pu metal’s environmental exposure were observed and identified. Auger electron spectroscopy (AES) was utilized to characterize the cross-sectional composition and chemistry of the oxide scale. The oxide scale formed during inert storage and operational environments was found to be highly variable in thickness and morphology, presenting some regions with a thin (<400 nm), dense oxide layer and others with a thick (>2 µm) scale with substantial lateral cracking. After subsequent exposure to dry air environment, the oxide scale became thicker (~4 µm) and slightly more porous. The changes following aging in a moist air environment were observed to be more severe, with the formation of a highly porous internal structure containing significant lateral and transverse cracking. In comparison to the scale formed on an ~3.5 at. % Ga-Pu metal alloy, the oxide morphology of the lower gallium alloy investigated here exhibited greater variation in thickness and a noteworthy dependence on the presence of water vapor, particularly in terms of the internal porosity formed during growth of the oxide.

36 MATERIALS SCIENCE↗

Effect of surface segregation on the oxidation resistance of Cu 3 Pt ( 100 )

Alloying element segregation often occurs under a reactive environment but its interplay with the subsequent surface oxidation of the alloy remains unclear. Using synchrotron-based ambient-pressure x-ray photoelectron spectroscopy, we dynamically monitor the surface segregation in Cu 3 Pt(100) in response to temperature and oxygen gas. Vacuum annealing leads to surface segregation of Cu along with the enrichment of Pt in the subsurface region. Upon switching to the O 2 atmosphere, dissociative chemisorption of oxygen does not change the surface segregation profile from that under the vacuum annealing condition. A stepwise increase in the oxygen pressure results in the transformation pathway of Cu → Cu 2 O → CuO, in which the selective oxidation of Cu gives rise to further accumulation of Pt underneath the oxide/alloy interface that hinders the supply of Cu from the bulk to the oxide/alloy interface, thereby leading to the termination of the surface oxidation after the Cu 2 O → CuO conversion is completed. This differs from the transformation pathway of Cu → Cu 2 O → Cu 2 O/CuO for the oxidation of pure Cu and Cu-Au alloys, in which the oxidation of Cu continues and the Cu 2 O/CuO bilayer growth is constantly maintained. Furthermore, these key differences provide useful insight into alloy design for controlling the surface properties such as corrosion resistance and catalytic performance of Cu base alloys.

36 MATERIALS SCIENCE↗

Platinum–Ruthenium Alloys Are Not Bifunctional CO Electro-Oxidation Catalysts: A Kinetic Analysis

Electro-oxidation of CO is a common kinetic bottleneck in many types of fuel cells and organic electrosynthesis processes. Alloys of Pt and Ru are often used as anode catalysts, with high activity attributed to bifunctionality; this suggests that Ru preferentially activates water to form surface hydroxyl groups that can react with Pt-bound CO. However, rigorous kinetic measurements have not confirmed this assertion under steady-state electro-oxidation conditions. Here, CO electro-oxidation is analyzed using several commercial Pt/C and Pt 100-x Ru x /C nanoparticle catalysts in acidic and alkaline electrolytes. Kinetic observables including apparent transfer coefficients and reaction orders are measured and evaluated using a degree of rate control analysis. The kinetic observables for both Pt and PtRu alloys are most consistent with competitive adsorption and Langmuir–Hinshelwood coupling across a single site-type, rather than two distinct sites. Furthermore, the role of Ru in CO electro-oxidation is assigned to be a purely electronic effect.

Alcohols↗

Challenges and opportunities to alloyed and composite fuel architectures to mitigate high uranium density fuel oxidation: uranium silicide

We report the challenges and opportunities to alloyed and composite fuel architectures designed and intended to mitigate oxidation of the fuel during a cladding breech of a water-cooled reactor are discussed in three review manuscripts developed in parallel, with the presented article focused on the oxidation performance of uranium silicide. Several high uranium density fuels are under consideration for deployment as accident tolerant and/or advanced technology nuclear reactor fuels, including UN, U 3 Si 2 , UC and UB 2 . Presented here are the literature for the U3Si2 degradation modes, thermodynamics, and oxidation performance of the pure compound and its reported alloyed and composite architectures. Furthermore, this review covers the materials and techniques for the incorporation of additives, dopants, or composite fuel architectures to improve the oxidation/corrosion behavior for high uranium density fuels for use in LWRs.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

PdCu Alloy Catalyst for Inhibition‐free, Low‐temperature CO Oxidation

Designing robust catalysts for low‐temperature oxidation is pertinent to the development of advanced combustion engines to meet increasingly stringent emissions limitations. Oxidation of CO, hydrocarbon, and NO pollutants over platinum‐group catalysts suffer from strong inhibition due to their competitive adsorption, while coinage metals are generally slow at activating O 2 . Through computational screening, we discovered a PdCu alloy catalyst that completely oxidizes CO below 150 °C without inhibition by NO, propylene or water. This is attributed primarily to geometric effects and the presence of CO bound to Pd sites within the Cu‐rich surface of the PdCu alloy. Here, we demonstrate that the novel PdCu catalyst can be used in tandem with a PtPd catalyst to achieve sequential, inhibition‐free, complete oxidation of CO in a two‐bed system, while also achieving 50 % NO conversion below 120 °C. Moreover, neither water nor propylene adversely affect the low temperature CO oxidation activity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Atomic-scale understanding of oxide growth and dissolution kinetics of Ni-Cr alloys

Aqueous corrosion of metals is governed by formation and dissolution of a passivating, multi-component surface oxide. Unfortunately, a detailed atomistic description is challenging due to the compositional complexity and the need to consider multiple kinetic factors simultaneously. To this end, we combine experiments with a first-principles-derived, multiscale computational framework that transcends thermodynamic descriptions to explicitly simulate the kinetic evolution of surface oxides of Ni-Cr alloys as a function of composition, temperature, pH, and applied voltage. In the absence of pitting, we identify three distinct voltage regimes, which are kinetically dominated by oxide growth, dissolution, and competitive dissolution and reprecipitation. Evolving compositional gradients and oxide thickness are revealed, including a transition between a metastable Ni-Cr mixed oxide and a thick, porous Ni-dominated oxide. Beyond elucidating the underlying physics, we highlight the need for competing kinetics in models to properly predict the transition from passivation to corrosion. Our results provide a key step towards co-design of alloy composition alongside environmental conditions for sustainable use across a variety of critical energy and infrastructure applications.

36 MATERIALS SCIENCE↗

Use of Modeling and Experiments to Assess the Effect of Minor Alloying Additions on Alumina Scale Formation during High-Temperature Oxidation

During the last decades, new generations of Ni-based superalloys have emerged with judiciously controlled chemistries. These alloys heavily rely on the addition of refractory elements to enhance their mechanical properties at elevated temperatures; however, a clear interpretation of the influence of these minor-element additions on the alloy's high-temperature oxidation behavior is still not well understood, particularly from the standpoint of predicting the transition from internal to external alumina formation. In this context, the present investigation describes a systematic study that addresses the intrinsic effects that minor element additions of Nb, Ta, and Re have on the oxidation behavior of alumina-scale forming γ-Ni alloys. By combining a novel simulation approach with high-temperature oxidation experiments, the present study evidences the generally positive effect associated with 2 at. % addition of Ta and Re as well as the detrimental consequences of Nb additions on the 1100 °C oxidation of (in at. %) Ni-6Al-(0,4,6,8)Cr alloys.

Rodriguez, Rafael↗

Potential Dependent Mn Oxidation and Its Role in Passivation of Ni 38 Fe 20 Cr 22 Mn 10 Co 10 Multi-Principal Element Alloy Using Multi-Element Resolved Atomic Emission Spectroelectrochemistry

The identity of passivating oxides on multi-principal element alloys is of great interest as their optimization offers the potential for exceptional corrosion resistance in aqueous solutions over a broad range of potential and pH. This study focuses on a non-equiatomic Ni 38 Fe 20 Cr 22 Mn 10 Co 10 solid solution alloy and tracks the fate of each alloying element during linear sweep voltammetry, low and intermediate potential holds in the passive potential domain as well as during open circuit relaxation after anodic polarization in slightly acidified Cl − solution. Ni dissolves at all potentials investigated in this work, Fe and Co are incorporated into oxides or hydroxides in low concentrations whilst Cr and Mn are enriched at passive potentials. At low passivating potentials, Mn(II) dissolves and is incorporated in minor amounts in oxides containing large concentrations of Cr(III). Considerable enrichment in Mn(II)-species occurs relative to Cr(III) in the oxide at 0.1 V vs SCE. Electrochemical impedance spectroscopy suggests the presence of layered oxides with marginal passivation at high Mn(II) levels. The formation of these oxides depends on a combination of thermodynamic and kinetic factors as well as the sequence of passivation.

Han, Junsoo (ORCID:0000000192952954)↗

Challenges and opportunities to alloyed and composite fuel architectures to mitigate high uranium density fuel oxidation: Uranium mononitride

We see the challenges and opportunities to alloyed and composite fuel architectures designed and intended to mitigate oxidation of the fuel during a cladding breech of a water-cooled reactor are discussed in three review manuscripts developed in parallel, with the presented article focused on the oxidation performance of uranium mononitride. Several high uranium density fuels are under consideration for deployment as accident tolerant and/or advanced technology nuclear reactor fuels, including one on each: UN, U 3 Si 2 , UC and UB 2 . Presented here is the research motivation for the incorporation of additives, dopants, or composite fuel architectures to improve the oxidation/corrosion behavior of high uranium density nuclear fuels for use in LWRs. Furthermore, this review covers the literature on the degradation modes, thermodynamics, and oxidation performance of pure UN and UN-compounds as well as reported alloyed and composite architectures.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Site-Selective Doping and Oxidation State Control of Copper in Gold Nanorods

We report the synthesis of plasmonic gold–copper nanostructures with tunable copper spatial distribution and oxidation state. Au–Cu alloy shells were deposited in aqueous solution onto colloidal gold nanorods that functioned as seeds, and the resulting shell morphology was found to depend strongly on the nanorod aspect ratio. For relatively fat gold nanorods (16 x 31 nm), Au–Cu growth was preferentially localized near the rod midsections, forming belt-like structures, whereas for skinnier nanorods (9 x 32 nm), Au–Cu growth produced patchy surface coverage around the entire rod. The shell thickness was tuned from 1 to 4 nm; upon air exposure, thicker shells exhibited a higher Cu(I) fraction compared to the initial shell. Incorporation of the Au–Cu shell led to pronounced shifts in the plasmonic features of the gold nanorods. These tunable plasmonic Au–Cu nanorods provide a materials basis for Cu-based plasmonic materials in the context of electrochemical CO₂ reduction.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Oxidation mechanism in a refractory multiple-principal-element alloy at high temperature

Refractory multiple-principal-element alloys (RMPEAs) are promising structural materials to enable increased power efficiency in high-temperature oxidation environments, but the oxidation behavior and microstructures of the oxides, especially at the beginning of the oxidation, have received limited attention. Here, the oxidation mechanism in an equimolar W-Mo-Ta-Nb-V was investigated at 1300 °C and compared with the equimolar W-Mo-Ta-Nb alloy without V. The oxide scale on WMoTaNbV after 1 min exposure is shown to be composed of a degradation layer at the interface of the alloy/oxide, an initial oxide transition layer, followed by the main phase aggregate oxide layer, and an outermost oxide layer. At the early stage of oxidation, the absorption of oxygen by the RMPEA substrate forms a solid solution. Vanadium accelerates the initial degradation process as it forms VO. The initial oxidation-induced degradation of RMPEA follows a sequence governed by the free energy change accompanied by local element segregation. Liquid V-Mo oxides aggregate in the intermediate oxide layer. The inward growth of the oxide scale is controlled by the local composition changes, the orientation of the substrate, the crystal structure, and physical properties such as melting points of the oxides.

36 MATERIALS SCIENCE↗

Cyclic oxidation behavior of selected commercial NiCr-alloys for engine exhaust valves in wet air environment between 800 and 950 °C

In this work, the impact of water vapor on the cyclic oxidation behavior of four commercial Ni-based superalloys (N80A, N90, R41 and H282) was investigated between 800 and 950°C. Oxidation- and volatilization-induced Cr loss accelerated the transition from protective and adherent oxide formation (Cr 2 O 3 ) to mixed oxides that significantly spalled at 950°C for H282 and R41. The accelerated oxidation, Cr depletion, and spallation susceptibility for R41 and to a lesser extent for H282 compared to N80A and N90 was related to the higher fraction of γ’, which led to increased Ti incorporation into the Cr 2 O 3 scale in the presence of water vapor.

36 MATERIALS SCIENCE↗

High-throughput oxidation screening and down-selection of refractory high entropy alloys in the Al-Cr-Mo-Nb-Ta-Ti system

Rapid experimentation and characterization are ever-present needs in the discovery of high entropy alloys. High entropy alloy systems are difficult to survey with systematic composition sweeps using traditional synthesis methods. The number of distinct compositions in even a four-element system is experimentally intractable. Exploration of these, and higher-element systems, necessitates thermodynamic prediction coupled with an automated sample creation method and a rapid screening methodology to effectively down-select alloys with targeted properties. As a result, a high-throughput method for evaluating the oxidation performance of refractory high entropy alloys was developed and tested. The six-element system of aluminum, chromium, molybdenum, niobium, tantalum, and titanium was evaluated for single phase stability and short-duration oxidation resistance. Target compositions were initially determined via thermodynamic predictions of single-phase stability across a wide temperature range. A twenty-five-sample build plate was produced using directed energy deposition additive manufacturing. After fabrication, the twenty-five 1 cm 3 samples were heat treated and characterized for composition and phase identification. The build plate was exposed to a high temperature oxidizing environment at 1000 °C for three hours. After oxidation, the composition, morphology, and chemistry of the oxides formed were characterized. Of the twenty-five samples produced, nine exhibited a favorable oxidation response, from which a single-phase BCC alloy at a composition of Al 13 Cr 7 Mo 19 Nb 18 Ta 26 Ti 17 was identified as the alloy with the most protective oxidation coating with a thin, adherent oxide scale. Finally, the complete experimental down-selection—from machine setup to final alloy identification—required approximately 45 labor hours, demonstrating a rapid validation for alloy discovery.

Additive manufacturing↗