Search NASA⌕ Search

SEARCH · Search NASA

Results for “aluminide”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

A strainrange partitioning analysis of low cycle fatigue of coated and uncoated Rene 80

A strainrange partitioning analysis was conducted on ultrahigh vacuum, strain-controlled, low-cycle fatigue behavior of uncoated and aluminide coated Rene' 80 nickel-base superalloy at 1000 C (1832 F) and 871 C (1600 F). The results indicated little effect of coating or temperature on the fatigue resistance. There was, however, a significant effect on fatigue life when creep was introduced into the strain cycles. The effect of this creep component was analyzed in terms of the method of strainrange partitioning.

Kortovich, C. S.↗

Effect of grain orientation and coating on thermal fatigue resistance of a directionally solidified superalloy (MAR-M 247)

The effect of off-axis directionally solidified (DS) grain growth on thermal fatigue life of Mar-M 247 alloy was evaluated. Uncoated conventionally cast as well as DS wedge bars were cycled in a burner rig between 1070 C and room temperature. The longitudinal axis and leading edge of the specimen coincided. As the angle between the specimen longitudinal axis and growth axis increased, the thermal fatigue life decreased for both the uncoated and aluminide-coated bars. Life increases of about 50 cycles for the DS conditions were attributed to coating. The decrease in thermal fatigue life with increasing angle is primarily attributed to the increase in modulus of elasticity with increasing angle and not to the intersection of DS grain boundaries with the specimen leading edge. The thermal fatigue cracks were observed to be transgranular in the DS material. Limited tensile and stress-rupture properties of conventionally cast and off-axis DS Mar-M 247 alloy are also presented.

Bizon, P. T.↗

An experimental, low-cost, silicon slurry/aluminide high-temperature coating for superalloys

A duplex silicon-slurry/aluminide coating has been developed and cyclically tested in Mach 1 combustion gases for oxidation and thermal fatigue resistance at 1093 C and in Mach 0.3 gases for hot-corrosion resistance at 900 C. The base-metal superalloys were VIA and B-1900. The coated B-1900 specimens performed much better in oxidation than similar specimens coated with aluminides and almost as well as the more-expensive Pt-Al and MCrAlY (where M is Ni and/or Co) coatings deposited by the physical vapor deposition process. The coating also provided good hot-corrosion protection. Metallographic, X-ray, and electron microprobe studies were made to characterize the coating, determine failure mechanisms, and study some of the changes due to exposure.

Young, S. G.↗

Some considerations of the performance of two honeycomb gas path seal material systems

A standard Hastelloy-X honeycomb material and a pack aluminide coated honeycomb material were evaluated as to their performance as labyrinth seal materials for aircraft gas turbine engines. Consideration from published literature was given to the fluid sealing characteristics of two honeycomb materials in labyrinth seal applications, and their rub characteristics, erosion resistance, and oxidation resistance were evaluated. The increased temperature potential of the coated honeycomb material compared to the uncoated standard could be achieved without compromising the honeycomb material's rub tolerance, although there was some penalty in terms of reduced erosion resistance.

Bill, R. C.↗

Design, fabrication, and bench testing of a solar chemical receiver

Solar thermal energy can be effectively collected, transported, stored, and utilized by means of a chemical storage and transport system employing the reversible SO2 oxidation reaction. A solar chemical receiver for SO3 thermal decomposition to SO2 and oxygen was analyzed. Bench tests of a ten foot section of a receiver module were conducted with dissociated sulfuric acid (SO3 and H2O) in an electrical furnace. Measured percent conversion of SO3 was 85% of the equilibrium value. Methods were developed to fabricate and assemble a complete receiver module. These methods included applying an aluminide coating to certain exposed surfaces, assembling concentric tubes with a wire spacer, applying a platinum catalyst to the tubing wall, and coiling the entire assembly into the desired configuration.

Summers, W. A.↗

Internal coating of air-cooled gas turbine blades

Four modified aluminide coatings were developed for IN-792 + Hf alloy using a powder pack method applicable to internal surfaces of air-cooled blades. The coating compositions are Ni-19Al-1Cb, Ni-19Al-3Cb, Ni-17Al-20Cr, and Ni-12Al-20Cr. Cyclic burner rig hot corrosion (900 C) and oxidation (1050 C) tests indicated that Ni-Al-Cb coatings provided better overall resistance than Ni-Al-Cr coatings. Tensile properties of Ni-19Al-1Cb and Ni-12Al-20Cr coated test bars were fully retained at room temperature and 649 C. Stress rupture results exhibited wide scatter around uncoated IN-792 baseline, especially at high stress levels. High cycle fatigue lives of Ni-19Al-1Cb and Ni-12Al-20Cr coated bars (as well as RT-22B coated IN-792) suffered approximately 30 percent decrease at 649 C. Since all test bars were fully heat treated after coating, the effects of coating/processing on IN-792 alloy were not recoverable. Internally coated Ni-19Al-1Cb, Ni-19Al-3Cb, and Ni-12Al-20Cr blades were included in 500-hour endurance engine test and the results were similar to those obtained in burner rig oxidation testing.

Hsu, L. L.↗

Oxidation and hot corrosion of coated and bare oxide dispersion strengthened superalloy MA-755E

Cyclic hot corrosion and oxidation of an experimental oxide dispersion strengthened (ODS) superalloy MA-755E were conducted in a hot gas stream at Mach 0.3. The response of the ODS alloy, bare or with protective coatings, was similar to that of a conventional cast alloy, IN-792, in hot corrosion at 900 C. However, during oxidation at 1100 and 1150 C the ODS alloy differed from the cast alloy by developing a greater amount of subsurface porosity. Compared with a diffused aluminide coating, an electron beam vapor deposited NiCrAlY coating offered superior oxidation protection and decreased porosity formation. In additional testing, the tendency to form porosity was associated with the large grains of recrystallized powder metallurgy alloys but was independent of the presence of an oxide dispersion.

Glasgow, T. K.↗

Progress in Protective Coatings for Aircraft Gas Turbines: A Review of NASA Sponsored Research

Problems associated with protective coatings for advanced aircraft gas turbines are reviewed. Metallic coatings for preventing titanium fires in compressors are identified. Coatings for turbine section are also considered, Ductile aluminide coatings for protecting internal turbine-blade cooling passage surface are also identified. Composite modified external overlay MCrAlY coatings deposited by low-pressure plasma spraying are found to be better in surface protection capability than vapor deposited MCrAlY coatings. Thermal barrier coating (TBC), studies are presented. The design of a turbine airfoil is integrated with a TBC, and computer-aided manufacturing technology is applied.

Merutka, J. P.↗

High temperature deformation of NiAl and CoAl

The high temperature mechanical properties of the aluminides are reviewed with respect to their potential as high temperature structural materials. It is shown that NiAl and CoAl are substantially stronger than the pure metals Ni and Co at high temperatures and approach the strength of some superalloys, particularly when those superalloys are tested in "weak" directions. The factors that limit and control the high temperature strengths of NiAl and CoAl are examined to provide a basis for the development of intermetallic alloys of this type.

Nix, W. D.↗

The use of the PUCOT for elastic modulus measurements on intermetallics at high temperatures

The piezoelectric ultrasonic composite oscillator technique (PUCOT) is being applied to measure the elastic constants of the aluminides in the temperature ranges 300 to 1700 K (CoAl and NiAl) and 300 to 1500 K (FeAl). The PUCOT consists of piezoelectric quartz drive and gauge crystals to excite longitudinal or torsional ultrasonic (80 kHz) resonant stress waves in the specimen and alumina spacer rod of appropriate resonant lengths. The resonant system is driven by a closed loop oscillator which maintains a constant gauge voltage and hence constant strain amplitude in the specimen. While the specimen is heated at 20 K/h the resonant period is measured continuously. The elastic moduli are calculated from these values of the resonant period and accurate determinations of specimen length. The technique is described and some results given.

Wolfenden, A.↗

A brittle to ductile transition in NiAl of a critical grain size

Tensile tests have been carried out on the strongly ordered B2 aluminide NiAl at 400 C to investigate the effect of the grain size on the ductility of the material. It is found that the ductility is very low and essentially independent of the grain size for aggregates of grains larger than about 20 microns; for finer-grained aggregates, the ductility increases sharply with decreasing grain size. Thus, NiAl exhibits a critical grain size below which polycrystalline aggregates are ductile in tension. For all grain sizes, fracture occurs in a brittle manner through a combination of intergranular decohesion and transgranular cleavage.

Schulson, E. M.↗

Effects of surface chemistry on hot corrosion life

Baseline burner rig hot corrosion with Udimet 700, Rene' 80; uncoated and with RT21, Codep, or NiCoCrAlY coatings were tested. Test conditions are: 900C, hourly thermal cycling, 0.5 ppm sodium as NaCl in the gas stream, velocity 0.3 Mach. The uncoated alloys exhibited substantial typical sulfidation in the range of 140 to 170 hours. The aluminide coatings show initial visual evidence of hot corrosion at about 400 hours, however, there is no such visual evidence for the NiCoCrAlY coatings. The turbine components show sulfidation. The extent of this distress appeared to be inversely related to the average length of mission which may, reflect greater percentage of operating time near ground level or greater percentage of operation time at takeoff conditions (higher temperatures). In some cases, however, the location of maximum distress did not exhibit the structural features of hot corrosion.

Fryxell, R. E.↗

Effects of silver and group 2 fluorides addition to plasma sprayed chromium carbide high temperature solid lubricant for foil gas bearing to 650 deg C

A new self-lubricating coating composition of nickel aluminide-bonded chromium carbide formulated with silver and Group II fluorides was developed in a research program on high temperature solid lubricants. One of the proposed applications for this new coating composition is as a wide temperature spectrum solid lubricant for complaint foil gas bearings. Friction and wear properties were obtained using a foil gas bearing start/stop apparatus at temperatures from 25 to 650 C. The journals were Inconel 718. Some were coated with the plasma sprayed experimental coating, others with unmodified nickel aluminide/chromium carbide as a baseline for comparison. The addtitional components were provided to assist in achieving low friction over the temperature range of interest. Uncoated, preoxidized Inconel X-750 foil bearings were operated against these surfaces. The foils were subjected to repeated start/stop cycles under a 14-kPa (2-psi) bearing unit loading. Sliding contact occurred during lift-off and coastdown at surface velocities less than 6 m/s (3000 rpm). Testing continued until 9000 start/stop cycles were accumulated or until a rise in starting torque indicated the journal/bearing had failed. Comparison in coating performance as well as discussions of their properties and methods of application are given.

Wagner, R. C.↗

Modulus measurements in ordered Co-Al, Fe-Al, and Ni-Al alloys

The composition and/or temperature dependence of the dynamic Young's modulus for the ordered B2 Co-Al, Fe-Al, and Ni-Al aluminides has been investigated using the piezoelectric ultrasonic composite oscillator technique (PUCOT). The modulus has been measured in the composition interval 48.49 to 52.58 at. pct Co, 50.87 to 60.2 at. pct Fe, and 49.22 to 55.95 at. pct Ni for Co-Al, Fe-Al, and Ni-Al, respectively. The measured values for Co-Al are in the temperature interval 300 to 1300 K, while those for the other systems are for ambient temperature only. The data points show that Co-Al is stiffer than Fe-Al, which is stiffer than Ni-Al. The data points for Fe-Al and Ni-Al are slightly higher than those reported in the literature.

Harmouche, M. R.↗

The effects of grain size on the flow and fracture of long-range ordered alloys

The effects of grain size on the mechanical properties of long-range ordered alloys are examined with reference to the short-term behavior of aluminide intermetallics. It is shown that in those L1(2) alloys which exhibit anomalous thermal strengthening, the grain size affects the magnitude of the strengthening. In some cases it also affects ductility, whereby the tensile elongation and the tensile strength increase as the grain size decreases below a critical point. It is also believed that grain size may affect the partitioning of microalloying elements, such as boron, in Ni3Al.

Schulson, E. M.↗

Life prediction and constitutive models for engine hot section anisotropic materials

The development of directionally solidified and single crystal alloys is perhaps the most important recent advancement in hot section materials technology. The objective is to develop knowledge that enables the designer to improve anisotropic gas turbine parts to their full potential. Two single crystal alloys selected were PWA 1480 and Alloy 185. The coatings selected were an overlay coating, PWA 286, and an aluminide diffusion coating, PWA 273. The constitutive specimens were solid and cylindrical; the fatigue specimens were hollow and cylindrical. Two thicknesses of substrate are utilized. Specimens of both thickness (0.4 and 1.5 mm) will be coated and then tested for tensile, creep, and fatigue properties.

Swanson, G. A.↗

Thermal barrier coating life prediction model

This is the first report of the first phase of a 3-year program. Its objectives are to determine the predominant modes of degradation of a plasma sprayed thermal barrier coating system, then to develop and verify life prediction models accounting for these degradation modes. The first task (Task I) is to determine the major failure mechanisms. Presently, bond coat oxidation and bond coat creep are being evaluated as potential TBC failure mechanisms. The baseline TBC system consists of an air plasma sprayed ZrO2-Y2O3 top coat, a low pressure plasma sprayed NiCrAlY bond coat, and a Rene'80 substrate. Pre-exposures in air and argon combined with thermal cycle tests in air and argon are being utilized to evaluate bond coat oxidation as a failure mechanism. Unexpectedly, the specimens pre-exposed in argon failed before the specimens pre-exposed in air in subsequent thermal cycles testing in air. Four bond coats with different creep strengths are being utilized to evaluate the effect of bond coat creep on TBC degradation. These bond coats received an aluminide overcoat prior to application of the top coat to reduce the differences in bond coat oxidation behavior. Thermal cycle testing has been initiated. Methods have been selected for measuring tensile strength, Poisson's ratio, dynamic modulus and coefficient of thermal expansion both of the bond coat and top coat layers.

Hillery, R. V.↗

Life prediction and constitutive models for engine hot section anisotropic materials

The results are presented of a program designed to develop life prediction and constitutive models for two coated single crystal alloys used in gas turbine airfoils. The two alloys are PWA 1480 and Alloy 185. The two oxidation resistant coatings are PWA 273, an aluminide coating, and PWA 286, an overlay NiCoCrAlY coating. To obtain constitutive and fatigue data, tests were conducted on uncoated and coated specimens loaded in the CH76 100 CH110 , CH76 110 CH110 , CH76 111 CH110 and CH76 123 CH110 crystallographic directions. Two constitutive models are being developed and evaluated for the single crystal materials: a micromechanic model based on crystallographic slip systems, and a macroscopic model which employs anisotropic tensors to model inelastic deformation anisotropy. Based on tests conducted on the overlay coating material, constitutive models for coatings also appear feasible and two initial models were selected. A life prediction approach was proposed for coated single crystal materials, including crack initiation either in the coating or in the substrate. The coating initiated failures dominated in the tests at load levels typical of gas turbine operation. Coating life was related to coating stress/strain history which was determined from specimen data using the constitutive models.

Swanson, G. A.↗