At least 199 records · Page 11

MAT 332: Recyclable-By-Design Carbon Fiber Composites for Battery Enclosures

This work aims to fabricate a small-scale battery module with the baseline RBD-CFRC and conduct mechanical crush test to develop an initial thermal runaway model. Test the adhesive properties of the RBD-CFRCs using their resin constituent, ultrasonic welding, and other resins employed today. Recommend a future direction for resin development to enable the welding of RBDCFRCs to dissimilar materials. Time and Cost Permitting. Iterate on resin development for flame resistance and adhesive properties, demonstrating how thermal runaway can be reduced or joining properties can be improved.

33 ADVANCED PROPULSION SYSTEMS↗

The Significance of Multi-Size Carbon Fibers on the Mechanical and Fracture Characteristics of Fiber Reinforced Cement Composites

One of the main challenges of using a high fiber volume content in a cement composite is the narrow margin of fiber volume content beyond which fibers can cause an adverse effect on the mechanical properties. In this paper, the significance of fiber size distribution and fiber volume content of different proportions of chopped and milled carbon microfibers are investigated. The mixes’ flowability showed improvement with altering the fiber size distribution despite having a high fiber content. Uniaxial compression cylinders and unnotched and notched beams were cast and then tested at 7 and 28 days of age. It was found that the compressive strength is significantly affected by fiber size distribution more than fiber volume content. On the other hand, the modulus of rupture and fracture toughness are proportional to the fiber volume content with little effect of fiber size distribution. Finally, neither high fiber volume content nor altered fiber size distribution significantly affected the elastic modulus of the fiber cement composites.

Abdellatef, Mohammed↗

Degradation in interfacial shear strength of carbon fiber/ vinyl ester composites due to long-term exposure to seawater using push-out tests

Here, in this study, single fiber (~7-μm diameter) push-out tests are conducted to evaluate hygrothermal effects on the interfacial shear strength (IFSS) of carbon fiber/vinyl ester (CF/VE) composites. Hygrothermal conditioning is achieved by saturating samples in simulated seawater at 40 °C for two years. An investigation has been conducted on the preparation, validity, and interpretation of the push-out test results. First, the authors present a polishing methodology that results in thin films of CF/VE composites in the thickness range of 15–120 μm and produces an average 41.2% drop in IFSS due to long-term hygrothermal exposure. Using scanning electron microscopy (SEM), we show that during the push-out tests, the failure initiates locally at the zone of minimum bond strength at the bottom (away from the indenter), then propagates along the length of the interface. The influence of radial tensile stresses originating due to bending is found to be negligible. Using the SEM imaging of the pushed-out fibers, we validate the failure of the interface to be the primary source of failure. The associated results are found to depend on the thickness of the interface. We then reevaluate the results using the Weibull distribution, knowing that the failure mechanism is analogous to the weakest link theory. The results show a 25.5% drop in the IFSS of the CFVE composite, measured at an infinitesimal scale due to long-term to hygrothermal conditioning at 40 °C. A significant drop in IFSS was observed after reheating above glass transition temperature (T g ) and cooling.

36 MATERIALS SCIENCE↗

Binder-Stabilized Carbon Fiber Hosts for High-Utilization Sodium–Polysulfide Flow Catholytes

Sodium-sulfur (Na-S) batteries hold promise as high-energy-density batteries for long-duration energy storage due to their high open circuit voltage and Earth-abundant active materials. However, low utilization of the sulfur active material limits the achievable specific capacity, especially when a liquid polysulfide catholyte is utilized. High-surface-area carbon materials demonstrate promise to increase sulfur utilization in a Na-S battery. To make the carbon host material applicable for a flow battery application, a binder is required to bind the carbon materials together and to a porous substrate. Here, we utilize a composite carbon paper electrode coated by polymer,carbon nanofibers (CNFs) and carbon black (CB). By varying the mass ratios of CNF to CB, we found that a 70/20/10 mass ratio of CNF/CB/binder provided the highest capacity (260 mAh g −1 compared to the baseline of 156 mAh g −1 ) and stable battery performance over 100 cycles. Analysis of the composite electrode and full cells reveals that the amount of CB in the composite electrode influences binder distribution, cell resistance, and full cell performance.

Lehmann, Michelle L. [Oak Ridge National Laborator↗