Search NASA⌕ Search

SEARCH · Search NASA

Results for “cracking temperature”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Removable fastener for insulating tiles

Fastening device that consists of internally threaded silica insert, silica plug, and molded rubber retainer, seals holes in ceramic tiles securely over wide temperature excursions without cracking from thermal stresses. Device proves useful in high-temperature industrial applications.

Brown, J. N.↗

Gaseous hydrogen-induced cracking of Ti-5Al-2.5Sn.

Study of the kinetics of hydrogen-induced cracking in the Ti-5Al-2.5Sn titanium alloy, which has a structure of acicular alpha platelets in a beta matrix. The crack-growth rate at low stress-intensity levels was found to be exponentially dependent on stress intensity but essentially independent of temperature. The crack-growth rate at intermediate stress-intensity levels was found to be independent of stress intensity but dependent on temperature in such a way that crack-growth rate was controlled by a thermally activated mechanism having an activation energy of 5500 cal/mole and varied as the square root of the hydrogen pressure. The crack-growth rate at stress-intensity levels very near the fracture toughness is presumed to be independent of environment. The results are interpreted to suggest that crack growth at high stress intensities is controlled by normal, bulk failure mechanisms such as void coalescence and the like. At intermediate stress-intensity levels the transport of hydrogen to some interaction site along the alpha-beta boundary is the rate-controlling mechanism. The crack-growth behavior at low stress intensities suggests that the hydrogen interacts at this site to produce a strain-induced hydride which, in turn, induces crack growth by restricting plastic flow at the crack tip.

Williams, D. P.↗

Temperature dependence of autogenous shrinkage of silica fume cement pastes with a very low water–binder ratio

Ultra-high-strength concrete with a large unit cement content undergoes considerable temperature increase inside members due to hydration heat, leading to a higher risk of internal cracking. Hence, the temperature dependence of autogenous shrinkage of cement pastes made with silica fume premixed cement with a water–binder ratio of 0.15 was studied extensively. Development of autogenous shrinkage showed different behaviors before and after the inflection point, and dependence on the temperature after mixing and subsequent temperature histories. The difference in autogenous shrinkage behavior poses problems for winter construction because autogenous shrinkage may increase with decrease in temperature after mixing before the inflection point and with increase in temperature inside concrete members with large cross sections.

36 MATERIALS SCIENCE↗

Development of surface modified Zr cladding by coating technology for ATF

It is expected that the accident tolerance fuels (ATF) will provide an enhanced fuel performance of active cooling in the reactor core for a longer time period during design-basis events as well as maintain or improve the fuel performance during normal operations and operational transients. Thus, various ATF cladding concepts have being suggested and developed in many countries. Among them, the coated cladding concept is studied in this work after the considerations of various performances in both the accidents and normal operation of LWRs. In the surface coated cladding concepts, the combination of coating material and coating method is a very important factor to determine the ATF cladding performance. As a new coating material, Cr-based alloy was developed to increase the corrosion resistance under normal operation as well as the oxidation resistance during an accident. From the high temperature oxidation test at 1200 Celsius degrees, the Cr-based alloy showed a superior oxidation resistance to Zircaloy-4 cladding, and showed more improved corrosion resistance than Zircaloy-4 cladding under 360 Celsius degrees PWR simulated loop conditions. The 3D laser coating and a combination of arc ion plating and laser beam scanning were developed to obtain a good adhesion property of corrosion resistance alloy coated on a Zr substrate. The corrosion resistance alloy (Cr-based alloy and FeCrAl alloy) coated layer used by two types of coating methods was maintained without peeling off during the ring compression test at room temperature, although some cracks were formed on the coated layer. After a high-temperature oxidation test at 1200 Celsius degrees for 2000 s, a very thin oxide layer, which was a few microns, was formed on the corrosion resistance alloy layer. However, the ZrO{sub 2} phase, which was thicker than 100 μm was formed on the Zr alloy cladding surface. Thus, it is known that the high-temperature oxidation resistance of commercial Zr alloy cladding can be considerably improved by the coating of corrosion resistant alloys. In addition, the partial oxide dispersion strengthened (ODS) treatment using a laser beam scanning (LBS) method was applied to decrease the ballooning and rupture opening during accident conditions. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fatigue Crack Growth Rate of Inconel 718 Sheet at Cryogenic Temperatures

Inconel 718 sheet material was tested to determine fatigue crack growth rate (FCGR) at cryogenic conditions representative of a liquid hydrogen (LH2) environment at -423 degree F. Tests utilized M(T) and ESE(T) specimen geometries and environments were either cold gaseous helium or submersion in LH2. The test results support a significant improvement in the fatigue crack growth threshold at -423 degree F compared to -320 degree F or 70 degree F.

Wells, Douglas↗

Spin-forming Project Report

In a second development order, spin-forming equipment was again evaluated using the test shape, a hemispherical shell. In this second development order, pure vanadium and alloy titanium (Ti-6Al-4V) were spin-formed, as well as additional copper and 21-6-9 stainless. In the first development order the following materials had been spin-formed: copper (alloy C11000 ETP), 6061 aluminum, 304L stainless steel, 21-6-9 stainless steel, and tantalum-2.5% tungsten. Significant challenges included properly adjusting the rotations-per-minute (RPM), cracking at un-beveled edges and laser marks, redressing of notches, surface cracking, non-uniform temperature evolution in the titanium, and cracking of the tailstock. Lessons learned were that 300 RPM worked better than 600 RPM for most materials (at the feed rate of 800 mm/min); beveling the edges to lower the stress reduces edge cracking; notches, laser marks, or edge defects in the preform doom the process to cracking and failure; coolant is required for vanadium spin-forming; increasing the number of passes to nine or more eliminates surface cracking for vanadium; titanium develops a hot zone in front of the rollers; and the tailstock should be redesigned to eliminate the cylindrical stress concentrator in the center.

36 MATERIALS SCIENCE↗

On the fatigue crack propagation behavior of superalloys at intermediate temperatures

Two superalloys used in gas-turbine disks, Rene 95 and IN-100 were tested in several forms at 0.33 Hz in air, and the results were compared with earlier data on Astroloy to gain a better understanding of the effects of grain size, strength, and alloy composition on the fatigue crack propagation behavior. In addition, selected forms of Rene 95 were tested at 0.33 Hz in vacuum and in air using a cycle with a 120-sec tensile dwell to evaluate the effects of environment and creep. Results of the study emphasize the beneficial effect of large grain size on the fatigue and crep-fatigue crack growth resistance of the superalloys in the temperature range corresponding to the operating temperatures of aircraft gas-turbine engine disk rims.

Gayda, J.↗

Active species in chloroaluminate ionic liquids catalyzing low-temperature polyolefin deconstruction

Abstract Chloroaluminate ionic liquids selectively transform (waste) polyolefins into gasoline-range alkanes through tandem cracking-alkylation at temperatures below 100 °C. Further improvement of this process necessitates a deep understanding of the nature of the catalytically active species and the correlated performance in the catalyzing critical reactions for the tandem polyolefin deconstruction with isoalkanes at low temperatures. Here, we address this requirement by determining the nuclearity of the chloroaluminate ions and their interactions with reaction intermediates, combining in situ 27 Al magic-angle spinning nuclear magnetic resonance spectroscopy, in situ Raman spectroscopy, Al K-edge X-ray absorption near edge structure spectroscopy, and catalytic activity measurement. Cracking and alkylation are facilitated by carbenium ions initiated by AlCl 3 - tert -butyl chloride (TBC) adducts, which are formed by the dissociation of Al 2 Cl 7 − in the presence of TBC. The carbenium ions activate the alkane polymer strands and advance the alkylation cycle through multiple hydride transfer reactions. In situ 1 H NMR and operando infrared spectroscopy demonstrate that the cracking and alkylation processes occur synchronously; alkenes formed during cracking are rapidly incorporated into the carbenium ion-mediated alkylation cycle. The conclusions are further supported by ab initio molecular dynamics simulations coupled with an enhanced sampling method, and model experiments using n-hexadecane as a feed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Castable hot corrosion resistant alloy

Some 10 wt percent nickel is added to an Fe-base alloy which has a ferrite microstructure to improve the high temperature castability and crack resistance while about 0.2 wt percent zirconium is added for improved high temperatur cyclic oxidation and corrosion resistance. The basic material is a high temperature FeCrAl heater alloy, and the addition provides a material suitable for burner rig nozzles.

Charles A. Barrett↗

Sensitivity of Liquation Cracking to Deposition Parameters and Residual Stresses in Laser Deposited IN718 Alloy

The laser deposited IN718 alloys were fabricated with laser cladding system under different conditions to estimate the sensitivity of weld metal liquation cracking. The microstructure and the crack characterization of the laser deposited IN718 alloy were investigated, and the effect of metallurgical factors and residual stress on the crack sensitivity was analyzed. The results showed that the continuous dendritic Laves was precipitated and formed a Lave–austenite interface with ambiguous nanohardness distribution. The weld metal liquation cracking was propagated along the laser scanning direction and the buildup direction in the laser deposited IN718 alloy simultaneously, and the Nb-/Mo-riched fine granular clusters were formed in the crack surface. The precipitation amount of the coarse eutectic phases, presented as dendrite or network, was increased in the laser deposited alloy fabricated with IN718/C-Fe-Cr composite powder and slow cooling rate. The total crack length and the maximum crack length were decreased by increasing cooling rate, and the transverse residual stress was increased with increasing buildup layer number. The crack sensitivity of the laser deposited IN718 alloy was increased by the crack initiation provided by the metallurgical defects and the eutectic phases with low melting temperatures, and then, crack propagated along the continuous phase under the transverse residual stress.

36 MATERIALS SCIENCE↗

Crack Growth Rate and Large Plate Demonstration of Chloride-induced Stress Corrosion Cracking in Spent Nuclear Fuel Storage Canisters

This report describes the body of work involving testing and analyses performed in FY18 and FY19 at the Savannah River National Laboratory and at Korea University to determine chloride-induced stress corrosion crack (CISCC) growth rates in weldments of austenitic stainless steel plate material. The primary work involved: several separate crack growth rate test campaigns with new testing setups using laboratory-scale corrosion specimens; analyses to estimate the stress intensity factors for flaws postulated to be present in the residual stress fields of axial and circumferential weldments in a prototypic dry storage canister; and establishment of a “large plate” (approximately 51×46 cm with thickness 16 mm and weight about 30 kg) CISCC test that uses a plate with a circumferential weldment harvested from the Sandia National Laboratories’ full-size mockup dry storage canister. The tests for crack growth rate were conducted on ASTM E1861 bolt-load compact tension specimens in a setup designed to allow initially dried salt deposits to deliquesce and infuse the brine to the crack front under conditions relevant to the canister storage environments (e.g., temperature and humidity). The crack growth rate test results matched previous experimental data in the open literature. These literature data had been compiled by SNL and EPRI to develop a temperature-dependent (K-insensitive) crack growth rate model to support flaw disposition in the ASME Boiler and Pressure Vessel Section XI Code Case N-860, “Examination Requirements and Acceptance Standards for Spent Nuclear Fuel Storage and Transportation Containment Systems.” The knowledge of the salt, temperature, humidity conditions for CISCC including the threshold stress intensity factor, $K_{ISCC}$, were used to setup the large plate test in which a set of partthrough- wall and through-wall electrical discharge machined (EDM) defects were positioned in the weld residual stress field of the welded plate material from the mockup canister. A salt solution was applied to this plate specimen with an air-brush spray, then dried, and then exposed to a constant 75% RH condition at an ambient room temperature of 22 °C. The salt loading and environmental condition is expected to be aggressive to cause CISCC. The visual results at the surface of the plate show corrosion product staining (brown rust appearance) but with no CISCC emanating from the machined notches after approximately 5 months exposure to date. The plate test will continue in FY20 and phased-array ultrasonic testing and other NDE techniques will be applied to identify and characterize CISCC that may emanate from the machined defects. The notches and any CISCC from them will be sectioned at the conclusion of the test to verify NDE characterization, and to develop effective through-wall crack growth rates from cracks that would likely be branched.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Microcracking in composite laminates under thermal and mechanical loading

Composites used in space structures are exposed to both extremes in temperature and applied mechanical loads. Cracks in the matrix form, changing the laminate thermoelastic properties. The goal of the present investigation is to develop a predictive methodology to quantify microcracking in general composite laminates under both thermal and mechanical loading. This objective is successfully met through a combination of analytical modeling and experimental investigation. In the analysis, the stress and displacement distributions in the vicinity of a crack are determined using a shear lag model. These are incorporated into an energy based cracking criterion to determine the favorability of crack formation. A progressive damage algorithm allows the inclusion of material softening effects and temperature-dependent material properties. The analysis is implemented by a computer code which gives predicted crack density and degraded laminate properties as functions of any thermomechanical load history. Extensive experimentation provides verification of the analysis. AS4/3501-6 graphite/epoxy laminates are manufactured with three different layups to investigate ply thickness and orientation effects. Thermal specimens are cooled to progressively lower temperatures down to -184 C. After conditioning the specimens to each temperature, cracks are counted on their edges using optical microscopy and in their interiors by sanding to incremental depths. Tensile coupons are loaded monotonically to progressively higher loads until failure. Cracks are counted on the coupon edges after each loading. A data fit to all available results provides input parameters for the analysis and shows them to be material properties, independent of geometry and loading. Correlation between experiment and analysis is generally very good under both thermal and mechanical loading, showing the methodology to be a powerful, unified tool. Delayed crack initiation observed in a few cases is attributed to a lack of preexisting flaws assumed by the analysis. Some interactions between adjacent ply groups are attributed to local stress concentrations. These two effects are not captured by the analysis due to its global nature. The analysis is conservative in these cases and agrees well with data after the observed onset of cracking.

Maddocks, Jason R.↗

Transition of creep damage region in dissimilar welds between Inconel 740H Ni-based superalloy and P92 ferritic/martensitic steel

Highlights: • The fresh martensite formed in P92-sided CGHAZ during PWHT due to high Ni content. • Transition from type I to type IV cracking was observed with increasing temperature. • Creep damaged area changed depending on the dominant creep mechanism. • The transition value of Larson-Miller parameter would be within 25,063–26,168. - Abstract: Characterization of microstructures and creep fracture characteristics of dissimilar welds between Ni-based Inconel 740H superalloy and ferritic/martensitic P92 steel has been investigated. The welds were produced by shielded metal arc (SMA) welding process with the AWS A5.11 Class ENiCrFe-3 filler metal, commonly known as Inconel 182 superalloy. Postweld heat treatment (PWHT) at 760 °C for 4 h was conducted to temper the martensite in heat-affected zone (HAZ) of P92 and to form γ′ strengthener in Inconel 740H. The deposited Inconel 182 austenitic weld metal had a columnar microstructure, and grew epitaxially from the Inconel 740H base metal. The weld interface between P92 and weld metal was characterized by the discrete line with a minimal inter-diffusion, where the fresh untempered martensite was found to be formed during PWHT due to higher Ni contents diffused from Inconel 182 into P92. The P92 base metal and Inconel 182 weld metal displayed low hardness values (~240 Hv), and the sharp hardness increase was detected at coarse-grained HAZ of P92 while the hardness minimum occurred at the fine-grained HAZ (FGHAZ). Fracture location after creep was found to shift from the P92-sided fusion line to the FGHAZ of P92 with increasing creep temperature. The carbon migration from the P92 into the weld metal was not significant at lower creep temperature (600 °C), where the crack initiation at the P92-sided fusion line appeared to be related with a significant strain incompatibility across the fusion line. At both 650 °C and 700 °C where diffusion-controlled creep was more pronounced, the type IV cracking was observed. This may be attributed to the strain localization at the weak grain boundaries of FGHAZ due to the smaller grain size as well as the lack of grain boundary strengthening by carbides.

36 MATERIALS SCIENCE↗

RECENT PROGRESS IN THE DEVELOPMENT OF DUCTILE-PHASE TOUGHENED TUNGSTEN FOR PLASMA-FACING MATERIALS

A promising approach to increasing fracture toughness and decreasing the DBTT of a W-alloy is by ductile-phase toughening (DPT) [1-3]. In this method, a ductile phase is included in a brittle matrix to prevent fracture propagation by crack bridging. To examine the prospect of DPT, W-Cu three-point bend samples were deformed at several strain rates and temperatures. Data from these tests is used for the calibration of a dynamic crack-bridging model that can effectively predict elevated temperature crack growth in W-composites. The development and initial testing of a Cu-ligament bridging model based on a micromechanical flow stress model of Cu is discussed. Good agreement with the 3-point bend testing data is demonstrated along with future plans to improve the model.

Henager, Charles H.↗