Search NASA⌕ Search

SEARCH · Search NASA

Results for “electrode aging”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

The Importance of Water Transport in High Conductivity and High-Power Alkaline Fuel Cells

High ionic conductivity membranes can be used to minimize ohmic losses in electrochemical devices such as fuel cells, flow batteries, and electrolyzers. Very high hydroxide conductivity was achieved through the synthesis of a norbornene-based tetrablock copolymer with an ion-exchange capacity of 3.88 meq/g. The membranes were cast with a thin polymer reinforcement layer and lightly cross-linked with N,N,N',N'-tetramethyl-1,6-hexanediamine. The norbornene polymer had a hydroxide conductivity of 212 mS/cm at 80°C. Light cross-linking helped to control the water uptake and provide mechanical stability while balancing the bound (i.e. waters of hydration) vs. free water in the films. The films showed excellent chemical stability with <1.5% conductivity loss after soaking in 1 M NaOH for 1000 h at 80°C. The aged films were analyzed by FT-IR before and after aging to confirm their chemical stability. A H 2 /O 2 alkaline polymer electrolyte fuel cell was fabricated and was able to achieve a peak power density of 3.5 W/cm 2 with a maximum current density of 9.7 A/cm 2 at 0.15 V at 80°C. The exceptionally high current and power densities were achieved by balancing and optimizing water removal and transport from the hydrogen negative electrode to the oxygen positive electrode. High water transport and thinness are critical aspects of the membrane in extending the power and current density of the cells to new record values.

08 HYDROGEN↗

Super-resolving microscopy images of Li-ion electrodes for fine-feature quantification using generative adversarial networks

Abstract For a deeper understanding of the functional behavior of energy materials, it is necessary to investigate their microstructure, e.g., via imaging techniques like scanning electron microscopy (SEM). However, active materials are often heterogeneous, necessitating quantification of features over large volumes to achieve representativity which often requires reduced resolution for large fields of view. Cracks within Li-ion electrode particles are an example of fine features, representative quantification of which requires large volumes of tens of particles. To overcome the trade-off between the imaged volume of the material and the resolution achieved, we deploy generative adversarial networks (GAN), namely SRGANs, to super-resolve SEM images of cracked cathode materials. A quantitative analysis indicates that SRGANs outperform various other networks for crack detection within aged cathode particles. This makes GANs viable for performing super-resolution on microscopy images for mitigating the trade-off between resolution and field of view, thus enabling representative quantification of fine features.

30 DIRECT ENERGY CONVERSION↗

Systems, methods and computer-readable media to model kinetic performance of rechargeable electrochemical devices

A system includes an electrochemical cell, monitoring hardware, and a computing system. The monitoring hardware samples performance characteristics of the electrochemical cell. The computing system determines cell information from the performance characteristics. The computing system also analyzes the cell information of the electrochemical cell with a Butler-Volmer (BV) expression modified to determine exchange current density of the electrochemical cell by including kinetic performance information related to pulse-time dependence, electrode surface availability, or a combination thereof. A set of sigmoid-based expressions may be included with the modified-BV expression to determine kinetic performance as a function of pulse time. The determined exchange current density may be used with the modified-BV expression, with or without the sigmoid expressions, to analyze other characteristics of the electrochemical cell. Model parameters can be defined in terms of cell aging, making the overall kinetics model amenable to predictive estimates of cell kinetic performance along the aging timeline.

97 MATHEMATICS AND COMPUTING↗

Unexpected Analyte Oxidation during Desorption Electrospray Ionization - Mass Spectrometry

During the analysis of surface spotted analytes using desorption electrospray ionization mass spectrometry (DESI-MS), abundant ions are sometimes observed that appear to be the result of oxygen addition reactions. In this investigation, the effect of sample aging, the ambient lab environment, spray voltage, analyte surface concentration, and surface type on this oxidative modification of spotted analytes, exemplified by tamoxifen and reserpine, during analysis by desorption electrospray ionization mass spectrometry was studied. Simple exposure of the samples to air and to ambient lighting increased the extent of oxidation. Increased spray voltage lead also to increased analyte oxidation, possibly as a result of oxidative species formed electrochemically at the emitter electrode or in the gas - phase by discharge processes. These oxidative species are carried by the spray and impinge on and react with the sampled analyte during desorption/ionization. The relative abundance of oxidized species was more significant for analysis of deposited analyte having a relatively low surface concentration. Increasing spray solvent flow rate and addition of hydroquinone as a redox buffer to the spray solvent were found to decrease, but not entirely eliminate, analyte oxidation during analysis. The major parameters that both minimize and maximize analyte oxidation were identified and DESI-MS operational recommendations to avoid these unwanted reactions are suggested.

36 MATERIALS SCIENCE↗

A 500 KV INVERTED GEOEMTRY FEEDTHROUGH FOR A HIGH VOLT-AGE DC ELECTRON GUN

This contribution reports on the development of an unprecedented inverted-insulator with cable connector for reliably applying 500 kV dc to a future polarized beam photogun, to be designed for operating at 350kV without field emission. Such a photogun design could then be used for generating a polarized electron beam to drive a spin-polarized positron source as a demonstrator for high energy nuclear physics at JLab. There are no commercial cable connectors that fit the large inverted insulators required for that voltage range. Our proposed concept is based on a modified epoxy receptacle with intervening SF6 layer and a test electrode in a vacuum vessel.

Hernandez-Garcia, C.↗

INTER-DIGITAL CAPACITIVE SENSOR FOR EVALUATING CABLE INSULATION THROUGH JACKET

Interdigital capacitive (IDC) sensors have previously been used to measure cable-age/damage indicative dielectric properties of cable insulation when placed in direct contact with the insulation. Often cable insulation is covered by a polymer jacket precluding direct contact with the insulation. As part of a continuing program to develop and evaluate nondestructive examination methods that may be applied to cable condition assessment, an IDC to measure the effect of cable polymer dielectric change through a covering jacket has been developed. The IDC consists of two fork-like electrodes facing each other with the fork tines interspersed and separated by a small gap. On one electrode, the gap is 5 mm while on the other, the gap is 2 mm. Electric field depth-of-field penetrations are similar to the electrode gaps. The electrodes are printed on a flexible substrate that can be conformed to the outside jacketed surface of a cylindrical cable, with tines parallel to the cable axis. The electrodes are connected to a broad frequency-spectral impedance meter that senses the capacitance between the narrowly gapped electrode tines. This capacitance is known to vary as a function of the permittivity of any material in close proximity to the electrodes. For jacketed cable systems, the IDC response is dominated by the jacket but, by analyzing measurements from IDC sensors with different depths-of-field penetration into the cable under test, the influence of the cable jacket material (primarily influenced by the shallow-depth-of field IDC) can be separated from the deeper-depth-of-field IDC sensing the combined effects of both jacket and underlying insulation. No other NDE method is known that is capable of sensing insulation dielectric properties through an overlying jacket.

Cable NDE, Interdigital Capacitance, Insulation Pe↗

Highly Stable, Anion Conductive, Comb-Shaped Copolymers for Alkaline Fuel Cells

To produce an anion-conductive and durable polymer electrolyte for alkaline fuel cell applications, a series of quaternized poly(2,6-dimethyl phenylene oxide)s containing long alkyl side chains pendant to the nitrogen-centered cation were synthesized using a Menshutkin reaction to form comb-shaped structures. The pendant alkyl chains were responsible for the development of highly conductive ionic domains, as confirmed by small-angle X-ray scattering (SAXS). The comb-shaped polymers having one alkyl side chain showed higher hydroxide conductivities than those with benzyltrimethyl ammonium moieties or structures with more than one alkyl side chain per cationic site. The highest conductivity was observed for comb-shaped polymers with benzyldimethylhexadecyl ammonium cations. The chemical stabilities of the comb-shaped membranes were evaluated under severe, accelerated-aging conditions, and degradation was observed by measuring IEC and ion conductivity changes during aging. The comb-shaped membranes retained their high ion conductivity in 1 M NaOH at 80 degrees C for 2000 h. These cationic polymers were employed as ionomers in catalyst layers for alkaline fuel cells. The results indicated that the C-16 alkyl side chain ionomer had a slightly better initial performance, despite its low IEC value, but very poor durability in the fuel cell. In contrast, 90% of the initial performance was retained for the alkaline fuel cell with electrodes containing the C-6 side chain after 60 h of fuel cell operation.

Li, NW↗

Application of electron backscatter diffraction techniques to quantify effects of aging on sub-grain and spatial heterogeneity in NMC cathodes

Identification and evaluation of structural heterogeneity in spent cathode materials is crucial to developing appropriate remediation strategies for novel recycling processes. Native heterogeneities may be exacerbated during the cell's operational lifetime, as sub-particle-scale variations induce anisotropic expansion and contraction upon cycling. Structural transformations resulting from repeated cycling and calendar aging predominantly occur at the secondary particle surface and at the grain boundaries (GBs) between primary particles. However, the diffusion and stress build up around and across GBs are poorly understood. In this study, electron backscatter diffraction (EBSD) is employed to track sub-grain lattice structure across a statistically relevant number of Li(Ni0.33Mn0.33Co0.33)O2 (NMC-111) particles. Specifically, differences in lattice misorientation – measured as the deviation from the grain's average orientation – are tracked as a function of position within the electrode (near current collector, middle, and near separator) and as a function of electrochemical cycling. Further, a novel method of structural analysis is developed, offering insight into sub-grain diffusion behavior by comparing lattice misorientation near the grain boundary versus in the grain bulk. The present results suggest that electrode-scale spatial heterogeneity in lattice structure is induced by initial manufacturing conditions, and that radial gradients in lattice misorientation evolve at the primary particle scale with repeated electrochemical cycling.

25 ENERGY STORAGE↗

Early calendar life and health prediction of silicon batteries via machine learning with uncertainty quantification

Lithium-ion batteries with silicon anodes promise high energy density but are limited by calendar lifetime. Reducing the long iteration time to obtain experimental results requires predicting calendar lifetime early in a cell's life. In this study, we demonstrate that lightweight machine learning models with feature engineering can provide calendar lifetime estimates from early electrochemical signals. After 1 month of electrochemical aging, the best models achieve 10% error in calendar-life prediction and can separate "bad" from "good" lifetime cells with a mean F1 score of 0.857. As battery systems exhibit inherent variability, four methods for uncertainty quantification are compared, and confidence intervals are demonstrated with an uncertainty of +-3.6 months in lifetime prediction. A feature importance analysis indicates that early patterns in voltage decay are the strongest indicators of calendar lifetime. Finally, this modeling approach has high error when generalizing to new electrode chemistries or testing conditions but with appropriately low confidence.

25 ENERGY STORAGE↗

Characterization of physiochemical properties of polymeric and electrochemical materials for aerospace flight

Nickel-cadmium rechargeable batteries are a vital and reliable energy storage source for aerospace applications. As the demand for longer life and more reliable space batteries increases, the understanding and solving of cell aging factors and mechanisms become essential. Over the years, many cell designs and manufacturing process changes have been developed and implemented. Cells fabricated with various design features were life cycled in a simulated low-Earth orbit regime. Following the test program, a comprehensive electrochemical analysis of cell components was undertaken to study cell degradation mechanisms. Discharge voltage degradation or voltage plateau has been observed during orbit cycling, but, its cause and explanation have been the subject of much discussion. A Hg/HgO reference electrode was used to monitor the reference versus each electrode potential during the discharge of a cycled cell. The results indicate that the negative electrode was responsible for the voltage plateau. Cell analysis revealed large crystals of cadmium hydroxide on the surface of the negative electrode and throughout the separator.

Rock, M.↗

Performance and lifetime of intercalative water deionization cells for mono- and divalent ion removal

We report intercalative deionization (IDI) uses two cation intercalation electrodes separated by an anion exchange membrane in a symmetric cell design that has the potential to deliver electrochemically desalinated water in an energy- and water-efficient way. Here, we define and measure metrics to describe the performance and lifetime of IDI cells and compare them for NaCl and CaCl 2 feed solutions. With 20 mM NaCl, NiHCF/AEM/NiHCF flow cells achieve 10 mM average concentration change at a productivity of 20 l/h/m 2 and 5 mM average concentration change at 130 l/h/m 2 . In both cases the cells are operated at a 3C current rate and consume ~30 Wh/m 3 of energy. With 10 mM CaCl 2 , the specific capacity and salt removal of IDI flow cells is ~4 times lower. NiHCF/NiHCF beaker cells with CaCl 2 electrolyte suffer from strong capacity fade, while the same cells with NaCl electrolyte achieve 500 cycles without any capacity fade. Our post-mortem analysis using X-ray diffraction, secondary electron microscopy, energy dispersive X-ray spectroscopy, synchrotron-based X-ray absorption spectroscopy and micro X-ray fluorescence mapping reveals that NiHCF dissolves upon repeated intercalation with Ca 2+ , releasing residual K + , Ni 2+ and Fe(CN) 6 3 , which precipitates as a crystalline decomposition product on the electrodes. This side reaction deprives the active material NiHCF of charge compensating Fe, and thus accounts for the observed capacity fade.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Quantifying the impact of operating temperature on cracking in battery electrodes, using super-resolution of microscopy images and stereology

There are numerous factors that can have an impact on the degradation behavior of batteries, such as the number of recharge cycles or the charge rate. Here, we investigate the influence of operating temperature on the structural degradation of the microstructure in lithium-ion positive electrodes. For that purpose, the microstructure is characterized for cathodes which have been cycled for 200 cycles under 6C (10-minute) charging at different operating temperatures, namely, 20°C, 30°C, 40°C, and 50°C. For each operating condition scanning electron microscopy (SEM) images of cross-sectioned Li x Ni 0.5 Mn 0.3 Co 0.2 O 2 (NMC532) electrodes have been analyzed, to determine structural descriptors such as global particle porosity, crack size/length/width distribution, and porosity and specific surface area distribution of individual particles. Additionally, a stereological method has been deployed to investigate the local particle porosity as a function of distance to the particle center. Results show that particle porosity increases with increasing cycling temperature. Particle porosity is greatest at the particle center and decreases along the particle radius to the exterior. Particle surface area is similar across the four cycling-temperature aging conditions.

25 ENERGY STORAGE↗

Section IV.D.3 for DOE 2013 Annual Report: Novel Phosphazene-based Compounds to Enhance Safety and Stability of Cell Chemistries for High Voltage Applications (INL)

Electrolytes play a central role in performance and aging in most electrochemical systems. As automotive and grid applications place a higher reliance on electrochemical stored energy, it becomes more urgent to have electrolyte components that enable optimal battery performance while promoting battery safety and longevity. Safety remains a foremost concern for widespread utilization of Li-ion technology in electric-drive vehicles, especially as the focus turns to higher voltage systems (5V). This work capitalizes on the long established INL expertise regarding phosphazene chemistry, aimed at battery-viable compounds for electrolytes and electrodes that are highly tolerant to abusive conditions. This report showcases our 2013 work for the DOE applied battery research (ABR) program, wherein testing results are summarized for INL electrolytes and alternative anode materials.

25 ENERGY STORAGE↗

Chemical “Pickling” of Phosphite Additives Mitigates Impedance Rise in Li Ion Batteries

The use of high-voltage, high-capacity positive electrodes in lithium-ion batteries presents a challenge, given their tendency to degrade organic electrolytes. To prevent this damage, electrolyte additives modifying the cathode surface are required. Tris(trimethylsilyl) phosphite (TMSPi) is one of such electrolyte additives. However, the mechanism for its protective action (similarly to other phosphite, borate, and boroxane compounds) remains not completely understood. In LiPF6 containing carbonate electrolytes, TMSPi undergoes reactions yielding numerous products. Here we demonstrate that one of these products, PF2OSiMe3, is responsible for mitigation of impedance rise that occurs in aged cells during charge/discharge cycling. This same agent can also be responsible for reducing parasitic oxidation currents and transition metal loss during prolonged cell cycling. Mechanistic underpinnings of this protective action are examined using computational methods. Our study suggests that this beneficial action originates mainly through inhibition of catalytic centers for electrolyte oxidation that are present on the cathode surface, by forming capping ligands on the transition metal ions that block solvent access to such centers.

capacity fade↗

The effect of charging rate on the graphite electrode of commercial lithium-ion cells: A post-mortem study

Increased charging rates negatively affect the lifetime of lithium-ion cells by increasing cell resistance and reducing capacity. This work is a post-mortem study of 18650 cells subjected to charge rates of 0.7-, 2-, 4-, and 6-C. For cells charged at 0.7-C to 4-C, this performance degradation is primarily related to surface film thickness with no observable change in surface film chemical composition. However, at charge rates of 6-C, the chemical composition of the surface film changes significantly, suggesting that this change is the reason for the sharper increase in cell resistance compared to the lower charge rates. In addition, we found that surface film formation was not uniform across the electrode. Surface film was thicker and chemically different along the central band of the electrode “jelly roll”. This result is most likely attributable to an increase in temperature that results from non-uniform electrode wetting during manufacture. As a result, this non-uniform change further resulted in active material delamination from the current collector owing to chemical changes to the binder for the cell charged at 6-C.

30 DIRECT ENERGY CONVERSION↗

Surface heterogeneity propagation and homogenization for pouch cell-scale Li metal anodes

Li metal anode is a promising candidate for next-generation energy storage systems and is widely explored in Li-ion and solid-state batteries. Despite its potential, Li metal anodes face instabilities during long-term cycling, especially when paired with NMC or sulfur-based cathodes, where Li is cycled at high capacities of 6-8 mAh/cm2, equivalent to a thickness of 30-40 µm. During such extensive utilization, degradation mechanisms such as excessive solid electrolyte interphase (SEI), dendrites, and dead Li emerge, and ultimately lead to sudden failure and reduced cycle life. The origin of the degradation mechanisms stem from surface heterogeneities introduced during Li foil manufacturing and storage [1, 2]. As cycling progresses, the local heterogeneities propagate, resulting in uneven Li utilization and degradation-prone regions across the electrode [3], which consequently induce performance variations at the cell level. This heterogeneity propagation is particularly pronounced in large-format pouch cells in practical applications, where the surface effects are magnified. Without a clear understanding of the multi-scale heterogeneities and the development of surface homogenization methods, the performance consistency will be compromised, hindering the commercialization of Li metal batteries. In this presentation, we investigate the evolution of surface heterogeneity propagation on commercially available Li foils. We discover that inhomogeneous Li utilization appears as early as the first half-cycle of formation, manifesting as localized clusters and pits. In pouch cell configurations, these features exhibit areal density variations across the electrode on a scale of millimeters. To improve Li utilization homogeneity, a scalable mechanical brushing method is introduced to remove the chemically heterogeneous surface passivation layer. Furtherore, the influence of utilization homogeneity on cell-to-cell consistency is evaluated using 32 Li-NMC811 pouch cells divided into as-received and brushed Li groups. On the brushed Li, clusters and pits are no longer observable, and the cells exhibit significantly improved consistency in discharge capacity trajectories and cycle lifetime. Overall, this study highlights the role of Li surface utilization homogeneity on long-term cycling performance. Our research provides a pathway for improving large-area electrode uniformity and establishing evaluation methods for cell-to-cell consistency, both are key steps toward the commercialization of Li metal batteries and beyond. [1] Otto, Svenja-K., et al. "In-depth characterization of lithium-metal surfaces with XPS and ToF-SIMS: toward better understanding of the passivation layer." Chemistry of Materials 33.3 (2021): 859-867. [2] Hatzell, Kelsey, et al. "Aligning lithium metal battery research and development across academia and industry." Joule (2024). [3] Kim, Sangwook, et al. "Calendar life of lithium metal batteries: Accelerated aging and failure analysis." Energy Storage Materials 65 (2024): 103147.

25 - ENERGY STORAGE↗

Multifunction Hydrophobic Ligand Engineered Cd(S, Se)/ZnS Quantum Dots for Stabilizing Highly Efficient Carbon‐Based Perovskite Solar Cells

The long-term operational stability of perovskite solar cells (PSCs) remains a key challenge impeding their commercialization, particularly due to ambient environments (e.g., moisture, oxygen, heat)-induced degradation. Carbon electrode-based PSCs have emerged as cost-effective and relatively stable alternatives to metal electrode-based devices due to carbon materials' hydrophobic behavior, yet they still lag in both long-term durability and power conversion efficiency (PCE). In this work, an ultrathin hydrophobic ligand-modified core–shell Cd(S,Se)/ZnS quantum dots (QDs) capping layer is introduced as a multifunctional interfacial modifier for carbon-electrode-based PSCs. This oleic acid ligand-modified QDs capping layer exhibits inherent hydrophobicity, effectively serving as a moisture barrier to retard perovskite degradation under ambient conditions. Furthermore, the strong interfacial bonding between the QDs and perovskite halide surfaces leads to efficient trap state passivation, reducing trap density and creating a more uniform electrical contact. The modified QDs/perovskite interface also features an elevated conduction band edge, promoting improved charge extraction. As a result, devices incorporating this quantum dot capping layer retain 98% of their initial PCE after 450 h of ambient aging and achieve a champion efficiency of 20.74%. As a result, this strategy highlights the potential of hydrophobic ligand-modified chalcogenide QDs as surface modifiers to enhance both the stability and performance of carbon-based PSCs, offering a promising route toward scalable fabrication of durable perovskite solar modules.

14 SOLAR ENERGY↗

Physical Interpretation of Early Battery Life Prediction Models

Early battery life prediction models are most useful for R&D if they help us understand the early changes in battery electrochemical response that correspond with long-term degradation and failure. Linear regression models such as Fused lasso and Partial Least Squares can fit coefficients directly to high-dimensional electrochemical data like capacity-voltage and ΔV–state-of-charge, i.e., Q(V) and ΔV(SOC) curves, learning coefficients that can be physically interpreted. We leverage the ISU-ILCC battery aging data set to learn high-dimensional coefficients for early battery life prediction from traditional slow-rate capacity check data, demonstrating learning on Q(V), d Q· d V −1 , and ΔV(SOC) curves. A thorough study on the dependence of coefficient values on train/test size and data preprocessing methods is made, demonstrating the reliability of high-dimensional regression approaches unless very small amounts of data are used for model training. For this data set, coefficients from Q(V) and d Q· d V −1 models highlight changes in electrode stoichiometry due to lithium loss, while ΔV(SOC) coefficients highlight changes in positive electrode diffusivity due to particle cracking as well as electrode stoichiometry shifts. By directly interpreting the coefficients of a regression model, we make physical insights into battery degradation mechanisms without requiring the assumptions of traditional battery data analysis methods.

25 ENERGY STORAGE↗