Search NASA⌕ Search

SEARCH · Search NASA

Results for “electron backscattered diffraction”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

A novel ultrafine-grained Fe−22Mn−0.6C TWIP steel with superior strength and ductility

A fully recrystallized ultrafine-grained (UFG) Fe−22wt.%Mn−0.6wt.%C twinning-induced plasticity (TWIP) steel with mean grain size of 576 nm was fabricated by cold rolling and annealing process. Tensile test showed that this UFG steel possessed high yield strength of 785 MPa, and unprecedented uniform elongation of 48%. The Hall-Petch relationship was verified from the coarse-grained (CG) regime to the ultrafine-grained (UFG) regime. The microstructures at specified tensile strains were characterized by electron backscattered diffraction (EBSD) and transmission electron microscopy (TEM). The microstructures and strain hardening behavior of the UFG TWIP steel were compared with the CG counterpart. The strong strain hardening capability of the UFG steel is supposed to be responsible for the high strength and good ductility. - Highlights: • A fully recrystallized Fe−22Mn−0.6C TWIP steel with mean grain size of 576 nm was fabricated. • The ultrafine-grained (UFG) steel exhibits strong strain-hardening capability, excellent strength and ductility. • The Hall-Petch relationship is fitted well from the CG regime to the UFG regime.

36 MATERIALS SCIENCE↗

Characterization of multilayer nitride coatings by electron microscopy and modulus mapping

This paper discusses multi-scale characterization of physical vapour deposited multilayer nitride coatings using a combination of electron microscopy and modulus mapping. Multilayer coatings with a triple layer structure based on TiAlN and nanocomposite nitrides with a nano-multilayered architecture were deposited by Cathodic arc deposition and detailed microstructural studies were carried out employing Energy Dispersive Spectroscopy, Electron Backscattered Diffraction, Focused Ion Beam and Cross sectional Transmission Electron Microscopy in order to identify the different phases and to study microstructural features of the various layers formed as a result of the deposition process. Modulus mapping was also performed to study the effect of varying composition on the moduli of the nano-multilayers within the triple layer coating by using a Scanning Probe Microscopy based technique. To the best of our knowledge, this is the first attempt on modulus mapping of cathodic arc deposited nitride multilayer coatings. This work demonstrates the application of Scanning Probe Microscopy based modulus mapping and electron microscopy for the study of coating properties and their relation to composition and microstructure. - Highlights: • Microstructure of a triple layer nitride coating studied at multiple length scales. • Phases identified by EDS, EBSD and SAED (TEM). • Nanolayered, nanocomposite structure of the coating studied using FIB and TEM. • Modulus mapping identified moduli variation even in a nani-multilayer architecture.

36 MATERIALS SCIENCE↗

Microstructure and texture evolution of Cu–Nb composite wires

The evolution of microstructure and texture in Cu–Nb composite wires fabricated by an accumulative drawing and bundling process was investigated by backscattered electron (BSE), electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM). Results indicate the onset of severe curling and shape changing occurred at the size of Nb ∼ 400 nm with a surface increase of about 6.91 μm{sup 2}/μm{sup 3} (the area per unit volume). Two kinds of grain boundaries in Nb are suggested: one is 20°–50° boundary with a rotate/tilt axis around <110> parallel to drawing direction (DD), and another is > 50° boundary with the axis perpendicular to DD. The curling phenomenon occurred at the Cu–Nb interface and is related not only to the deformation mechanism of Nb but also to the presence of interface. This result is distinct from reported works showing that curling takes place when BCC metals are heavily drawn (Area reduction > 73%). The variation in microstructure and texture evolution between Cu and Nb filaments was discussed based on the differences in deformation mechanisms of these two metals. - Highlights: • Microstructure and texture evolution were studied systematically by EBSD. • In Nb, grain boundaries of 20°–50° have a rotate/tile axis around <110>//DD. • The rotation axes of above 50° boundaries are concentrated around <111> ⊥ DD in Nb. • Curling is related to not only deformation mode of BCC but also Cu–Nb interface.

36 MATERIALS SCIENCE↗

High- and Low-Temperature Deformation Behavior of Different Orientation Hot-Rolled Annealed Zircaloy-4

In this paper, the hot-rolled annealed Zircaloy-4 samples with different orientation were subjected to uniaxial compression with a strain rate of 0.001 s{sup −1} to obtain the stress-strain curves of different initial orientation samples at different temperatures. Electron backscatter diffraction (EBSD) technique and transmission electron microscope (TEM) technique were used to analyze the microstructures and textures of compressed samples. The mechanical properties and microstructural evolution of rolling directions (RD), transverse directions (TD) and normal directions (ND) were investigated under the conditions of – 150 °C low temperature, room temperature and 200 °C high temperature (simulated lunar temperature environment). The results show that the strength of Zircaloy-4 decreases with the increase in deformation temperature, and the strength in three orientations is ND > TD > RD. The deformation mechanism of hot-rolled annealed Zircaloy-4 with different orientation is different. In RD, {101̄0}〈a〉 prismatic slip has the highest Schmid factor (SF), so it is most easy to activate the slip, followed by TD orientation, and ND orientation is the most difficult to activate. The deformed grains abide slip→twinning→slip rule, and the different orientation Zircaloy-4 deformation mechanisms mainly are the twinning coordinated with the slip.

36 MATERIALS SCIENCE↗

Hardness and modulus of Fe2B, Fe3(C,B), and Fe23(C,B)6 borides and carboborides in the Fe-C-B system

Highlights: • Hardness and modulus of the Fe{sub 2}B, Fe{sub 3}(C,B), Fe{sub 23}(C,B){sub 6} and M{sub 7}C{sub 3} phases are analyzed. • Hardness and modulus of the Fe{sub 3}(C,B) phase are increasing with its B content. • Size effects are apparent for hardness of Fe{sub 2}B, Fe{sub 3}(C,B), Fe{sub 23}(C,B){sub 6} and M{sub 7}C{sub 3}. • The model of Nix and Gao was used to evaluate the load-independent hardness H{sub 0}. • Hardness ranking is Fe{sub 2}B > M{sub 7}C{sub 3} > Fe{sub 3}(C,B) > Fe{sub 23}(C,B){sub 6} - Abstract: This work provides a comparative and comprehensive study of the indentation hardness and indentation modulus of iron-rich borides and carboborides of types Fe{sub 2}B, Fe{sub 3}(C,B), and Fe{sub 23}(C,B){sub 6}. In addition, the hardness and elastic modulus of Cr-rich M{sub 7}C are investigated for comparative purposes. We investigated the impact of increasing B content and indentation size effect (ISE). The phases of interest were stabilized in cast Fe-C-B alloys that varied with respect to the B / (B + C) ratio and heat treatment. The resulting microstructures were characterized by means of X-ray diffraction (XRD), scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and wavelength X-ray spectroscopy (WDS). Dynamic in-situ nanoindentation experiments based on the method of continuous stiffness measurement (CSM) were coupled to SEM and EBSD investigations to determine the mechanical properties of the individual borides and carboborides as a function of the indentation depth. The results were compared to values obtained for the Cr-rich M{sub 7}C{sub 3} carbide. It was found that the hardness of the B-rich Fe{sub 3}(C{sub ,}B) phase is considerably higher than pure Fe{sub 3}C and increases with increasing B content. The ISE was present in all investigated phases, and the hardness decreased as a function of indentation depth. The hardness at infinite indentation depth H{sub 0} was estimated according to the model of Nix and Gao. The Fe{sub 2}B phase was found to be the hardest phase (H{sub 0} = 19.04 GPa), followed by M{sub 7}C{sub 3} (H{sub 0} = 16.43 GPa), Fe{sub 3}(C,B) (H{sub 0} = 11.18 to 12.24 GPa), and Fe{sub 23}(C,B){sub 6} (H{sub 0} = 10.39 GPa).

36 MATERIALS SCIENCE↗

Effect of heat input on the microstructure, residual stresses and corrosion resistance of 304L austenitic stainless steel weldments

Austenitic stainless steels are widely used in high performance pressure vessels, nuclear, chemical, process and medical industry due to their very good corrosion resistance and superior mechanical properties. However, austenitic stainless steels are prone to sensitization when subjected to higher temperatures (673 K to 1173 K) during the manufacturing process (e.g. welding) and/or certain applications (e.g. pressure vessels). During sensitization, chromium in the matrix precipitates out as carbides and intermetallic compounds (sigma, chi and Laves phases) decreasing the corrosion resistance and mechanical properties. In the present investigation, 304L austenitic stainless steel was subjected to different heat inputs by shielded metal arc welding process using a standard 308L electrode. The microstructural developments were characterized by using optical microscopy and electron backscattered diffraction, while the residual stresses were measured by X-ray diffraction using the sin{sup 2}ψ method. It was observed that even at the highest heat input, shielded metal arc welding process does not result in significant precipitation of carbides or intermetallic phases. The ferrite content and grain size increased with increase in heat input. The grain size variation in the fusion zone/heat affected zone was not effectively captured by optical microscopy. This study shows that electron backscattered diffraction is necessary to bring out changes in the grain size quantitatively in the fusion zone/heat affected zone as it can consider twin boundaries as a part of grain in the calculation of grain size. The residual stresses were compressive in nature for the lowest heat input, while they were tensile at the highest heat input near the weld bead. The significant feature of the welded region and the base metal was the presence of a very strong texture. The texture in the heat affected zone was almost random. - Highlights: • Effect of heat input on microstructure, residual stresses and corrosion is studied. • HAZ and width of dendrite in the welded region increase with heat input. • Residual stresses are tensile near the welded region after the highest heat input. • Welded region has the highest pit density after highest heat input. • Dendrites and δ-ferrite were highly oriented in the welded region.

36 MATERIALS SCIENCE↗

Martensitic Transformation in Fe x Mn 80-x Co 10 Cr 10 High-Entropy Alloy

High-entropy alloys and even medium-entropy alloys are an intriguing class of materials in that structure and property relations can be controlled via alloying and chemical disorder over wide ranges in the composition space. Employing density-functional theory combined with the coherent-potential approximation to average over all chemical configurations, we tune free energies between face-centered-cubic and hexagonal-close-packed phases in Fe x Mn 80 - x Co 10 Cr 10 systems. Within Fe-Mn-based alloys, we show that the martensitic transformation and chemical short-range order directly correlate with the face-centered-cubic and hexagonal-close-packed energy difference and stacking-fault energies, which are in quantitative agreement with recent observation of two phase region (face-centered cubic and hexagonal closed pack) in a polycrystalline high-entropy alloy sample at x = 40 at.%. Our predictions are further confirmed by single-crystal measurements on a x = 40 at.% using transmission-electron microscopy, selective-area diffraction, and electron-backscattered-diffraction mapping. The results herein offer an understanding of transformation-induced or twinning-induced plasticity in this class of high-entropy alloys and a design guide for controlling the physics at the electronic level.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure and In Situ Observations of Undercooling for Nucleation of [beta]-Sn Relevant to Lead-Free Solder Alloys

Difficult nucleation of {beta}-Sn during solidification of tin and tin-based lead-free solder alloys can result in high degrees of undercooling of the liquid prior to solidification. The undercooling can produce solder joints with large grains, anisotropic behavior, and undesirable mechanical properties. This paper describes our examination of the amount of undercooling of tin on both graphite (non-wetting) and copper (wetting) surfaces using in situ x-ray diffraction. The microstructure was further characterized by optical microscopy, scanning electron microscopy, and electron backscattering diffraction imaging microscopy. Undercoolings as high as 61 C were observed for Sn solidified on graphite, while lower undercoolings, up to 30 C, were observed for Sn solidified on copper. The microstructure of the high purity Sn sample solidified on graphite showed very few grains in the cross-section, while the commercially pure Sn sample solidified with only one grain and was twinned. Tin solidified on copper contained significant amounts of copper in the tin, intermetallic phase formation at the interface, and a eutectic microstructure.

36 MATERIALS SCIENCE↗

Interrupted in situ EBSD study of texture evolution and mechanism of surface grains in electroformed Ni after annealing with an initially duplex <100> + <111> fiber texture during uniaxial tensile deformation

Highlights: • The texture evolution of the electroformed Ni was investigated by using an interrupted in situ electron backscattered diffraction. • The initial <100> fiber component evolved into the metastable cube component with a weaker copper component. • Only a few grains of the initial <111> fiber component evolved into the copper orientation. - Abstract: The texture evolution process and mechanism of surface grains in electroformed Ni after annealing with an initially duplex <100> + <111> fiber texture during uniaxial tensile deformation were investigated by using interrupted in situ electron backscattered diffraction. The results showed that the initially duplex <100> + <111> fiber texture evolved into the metastable Cube orientation with a weak Cu orientation during the uniaxial tensile deformation. The volume fractions of <100> and <111> fiber texture decreased from 54.0% to 29.3% and 16.6% to 6.6%, respectively. The volume of the Cube orientation remained almost stable at 12%, whereas that of the Cu orientation increased from 1% to 2.9%. A simulation of the final preferred orientation based on the Taylor model was a cubic texture, which qualitatively agreed well with the experimental result. The simulated results indicated that the formed Cube and Cu textures evolved from the initial <100> and <111> fiber textures, respectively.

36 MATERIALS SCIENCE↗

CHARACTERIZATION OF DEFECTS IN ALLOY 152, 52 AND 52M WELDS

Defect distributions have been documented by optical metallography, scanning electron microscopy and electron backscatter diffraction in alloy 152 and 52 mockups welds, alloy 52 and 52M overlay mockups and an alloy 52M inlay. Primary defects were small cracks at grain boundaries except for more extensive cracking in the dilution zone of an alloy 52 overlay on 304SS. Detailed characterizations of the dilution zone cracks were performed by analytical transmission electron microscopy identifying grain boundary titanium-nitride precipitation associated with the intergranular separations. I. INTRODUCTION Weldments continue to be a primary location of stress-corrosion cracking (SCC) in light-water reactor systems. While problems related to heat-affected-zone (HAZ) sensitization and intergranular (IG) SCC of austenitic stainless alloys in boiling-water reactors (BWRs) have been significantly reduced, SCC has now been observed in HAZs of non-sensitized materials and in dissimilar metal welds where Ni-base alloy weld metals are used. IGSCC in weld metals has been observed in both BWRs and pressurized water reactors (PWRs) with recent examples for PWR pressure vessel penetrations producing the most concern. This has led to the replacement of alloy 600/182/82 welds with higher Cr, more corrosion-resistant replacement materials (alloy 690/152/52/52M). Complicating this issue has been a known susceptibility to cracking during welding [1-7] of these weld metals. There is a critical need for an improved understanding of the weld metal metallurgy and defect formation in Ni-base alloy welds to effectively assess long-term performance. A series of macroscopic to microscopic examinations were performed on available mockup welds made with alloy 52 or alloy 152 plus selected overlay and inlay mockups. The intent was to expand our understanding of weld metal structures in simulated LWR service components with a focus on as-welded defects. Microstructural features, defect distributions, defect characteristics and weld residual strains were examined by optical metallography, scanning electron microscopy, electron backscatter diffraction and transmission electron microscopy. Industry-supplied mock-up welds were characterized including alloy 52 and 152 weldments, alloy 52M overlay and inlay welds, and an alloy 52 overlay. II. WELDMENTS II.A. Alloy 52 and 152 Weld Mockups The alloy 52 and 152 weld mockups were fabricated by MHI for the Kewaunee reactor and were obtained from the EPRI NDE Center. The mockups were U-groove welds joining two plates of 304SS as shown in Figure 1. Alloy 152 butter (heat 307380) was placed on the U-groove surface for both mockups by shielded metal arc welding (SMAW). For the alloy 152 weld mockup, the alloy 152 fill (heat 307380) was also applied using SMAW while for the alloy 52 weld mockup, the alloy 52 fill (heat NX2686JK) was applied using gas tungsten arc welding (GTAW). Welding parameters for the fill materials were substantially different with the alloy 152 SMAW having a deposition speed of 4-25 cm/min with a current of 95-145 A and the alloy 52 GTAW having a deposition speed of 4-10 cm/min with a current of 150-300 A. One prominent feature in these mockup welds is the presence of a crack starting at the 304SS butt joint at the bottom of the U-groove and extending up into the weld. It appears that the 304SS plate on either side of the butt joint acted as an anchor for the weld resulting in a stress rise across the slit that drove crack formation and extension up into the fill weld. As will be shown in the next section, the extent of the cracking around this stress riser was much greater in the MHI 52 weld mockup.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Influence of current density on microstructure of pulse electrodeposited tin coatings

Pulse electrodeposited tin coatings on copper substrate have been synthesized from an aqueous solution containing sodium stannate (Na{sub 2}SnO{sub 3}.3H{sub 2}O) and sodium hydroxide (NaOH). The effect of current density on surface morphology of the deposits has been investigated. As deposited coatings are characterized by X-ray diffraction, scanning electron microscopy, electron backscatter diffraction, and line profile analysis. The X-ray diffraction analysis shows that the deposits consist of tetragonal ({beta}-Sn) structure with microcrystalline grains. The deposits plated at lower current density exhibit (110) texture which decreases with increasing current densities. The effects of current density on Cu-Sn diffusion and whisker growth of the electrodeposited tin coatings are also reported here. - Highlights: Black-Right-Pointing-Pointer Pulse electrodeposition of Sn from aqueous alkaline solution without adding any organic additive. Black-Right-Pointing-Pointer Effect of current density on morphology and whisker growth in tin coatings aged for 1 year. Black-Right-Pointing-Pointer Solution bath is stable and can be operated over a wide range of current density.

36 MATERIALS SCIENCE↗

Characterizing defect structures in AM steel using direct electron detection EBSD

The mechanical properties of additive and traditionally manufactured alloys are largely dependent on the characteristics and distribution of dislocation cell networks that develop during the fabrication process. This work demonstrates the ability to quantitatively characterize these dislocation structures by high angular resolution electron backscatter diffraction analysis using a direct electron detector. The defect structures are characterized in terms of the geometrically necessary dislocation density and the associated Burgers vector and line direction. Furthermore, the results are discussed in terms of potential defect formation mechanisms.

36 MATERIALS SCIENCE↗

High-cycle fatigue behavior of Ti-5Al-2.5Sn ELI alloy forging at low temperatures

High-cycle fatigue properties of Ti-5Al-2.5Sn Extra Low Interstitial (ELI) alloy forging were investigated at low temperatures. The high-cycle fatigue strength at low temperatures of this alloy was relatively low compared with that at ambient temperature. The crystallographic orientation of a facet formed at a fatigue crack initiation site was determined by electron backscatter diffraction (EBSD) method in scanning electron microscope (SEM) to understand the fatigue crack initiation mechanism and discuss on the low fatigue strength at low temperature. Furthermore, in terms of the practical use of this alloy, the effect of the stress ratio (or mean stress) on the high-cycle fatigue properties was evaluated using the modified Goodman diagram.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Assessing Manufacturability of the Oxide Dispersion Strengthened (ODS) 14YWT Alloy Fuel Cladding Tube Using SolidStir™ Technology

The 14YWT (Fe–14Cr–3W–0.4Ti–0.3Y2O3 (wt.%)) alloy is a potential candidatematerial for fabricating fuel cladding tubes and other structural components to be used in next-generation advanced nuclear reactors. Due to inherent limitations of current processing routes, this research explored a new variant of friction stir processing, commercially referred to as SolidStir™ Extrusion (patent pending) technology from Enabled Engineering to consolidate and extrude 14YWT powder into a fuel cladding tube. Several single-layer and multiple-layer consolidation experiments were carried out in an Inconel 625 die to determine the suitable processing parameters for SolidStir™ extrusion of the 14YWT alloy cladding tube. With these processing parameters, a 16–18 mm long tube of the 14YWT alloy with no visible defects was successfully extruded using this novel technology. Microstructural characterization results obtained using optical microscopy, scanning electron microscopy, energy dispersive spectroscopy, electron backscatter diffraction, and transmission electron microscopy will be presented.

Advanced Materials and Manufacturing Technology↗

The Influence of Microstructure on Oxidation Rate Of V–Cr–Ta–Zr Alloy During Its Chemical-Heat Treatment

Using the methods of scanning (electron backscatter diffraction) and transmission electron microscopy, an investigation of the influence of microstructure of a V–Cr–Ta–Zr alloy on the rate of surface oxide scale formation in the course of its chemical-heat treatment using oxidation in air is performed. It is shown that a preliminary plastic deformation, ensuring a multiple increase in the density of dislocations and misorientation boundaries, results in a 10% thicker surface oxide layer and a respective increase in the concentration of oxygen in the alloy during the final stage of its chemical-heat treatment. The role of this factor in developing the chemical-heat treatment regimes is discussed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Interfacial Microstructural Evolution and Metallurgical Bonding Mechanisms for IN718 Superalloy Joint Produced by Hot Compressive Bonding

The novel metallurgical joining process for bonding IN718 superalloy was investigated by hot compressive bonding (HCB) process under the deformation temperature range of 1000 °C to 1150 °C and true strains ranging from 0 to 0.5 at a strain rate of 0.001 s{sup −1}. The effect of HCB process parameters on the tensile strength was analyzed. Both the as-deformed and the interfacial microstructures were characterized using the optical microscope, electron backscattered diffraction and transmission electron microscope (TEM) analysis. The results of tensile property revealed that the degree of metallurgical bonding is promoted by increasing deformation temperature and strain. The evolution of the interfacial microstructure showed that the migration of interfacial grain boundary (IGB), which is characterized by discontinuous dynamic recrystallization, is the dominant metallurgical bonding mechanism in the early stages of bonding. TEM analysis indicated that the dislocation density is distributed heterogeneously over both sides of IGB, which is the significant reason for the migration of IGB, during the initial stage of HCB process.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded Dual-Phase Brass

Friction stir welding (FSW) is an ideal process to join brass to avoid the evaporation of zinc. In the present investigation, 6-mm-thick dual-phase brass plates were joined efficiently using FSW at various tool rotational speeds. The microstructures were studied using optical microscopy, electron backscattered diffraction and transmission electron microscopy. The optical micrographs revealed the evolution of various zones across the joint line. The microstructure of the heat-affected zone was similar to that of base metal. The weld zone exhibited finer grains due to dynamic recrystallization. The recrystallization was inhomogeneous and the inhomogeneity reduced with increased tool rotational speed. The dual phase was preserved in the weld zone due to the retention of zinc. The severe plastic deformation created a lot of dislocations in the weld zone. The weld zone was strengthened after welding. The role of tool rotational speed on the joint strength is further reported.

36 MATERIALS SCIENCE↗