Search NASA⌕ Search

SEARCH · Search NASA

Results for “irreversible capacity”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

191 records · Page 11

Contrasting magnetic properties of polymorphic TbPt 3

Here, in this work, we report the contrasting magnetic behaviour of a bimorphic intermetallic compound TbPt 3 that undergoes a structural phase transformation from cubic AuBe 5 -type structure to the cubic AuCu 3 -type structure on annealing at high temperature for a very short time. The magnetic ground state configuration of TbPt 3 changes from ferromagnetic (FM) in AuBe 5 -type crystalline phase to antiferromagnetic (AFM) in AuCu 3 -type phase. However, the AFM ground state of the AuCu 3 -type compound is unstable, as a moderate magnetic field can induce the FM character through metamagnetic transformation. To understand the said crystallographic as well as magnetic transformations, structural and magnetic ab-initio calculations have been carried out for both phases. From theoretical calculations we have proposed that although the AuBe 5 -type structure of TbPt 3 irreversibly transforms to the AuCu 3 -type TbPt 3 by a very short heat treatment, the application of moderate magnetic field on AuCu 3 -type structure may result in recovering the magnetic properties of AuBe 5 -type structure of TbPt 3 . As the two different polymorphs exist simultaneously at ambient condition, TbPt 3 thus provides us a great opportunity to study directly the effect of crystal structure on its physical properties and vice versa.

36 MATERIALS SCIENCE↗

Dual Passivation of Cathode and Anode through Electrode–Electrolyte Interface Engineering Enables Long-Lifespan Li Metal–SPAN Batteries

The reliability and durability of lithium metal (Li 0 )–sulfur batteries are largely limited by the undesired Li 0 plating-stripping irreversibility and the detrimental polysulfide dissolution, yet approaches that can simultaneously address the above anodic and cathodic problems are scarce. In this study, we report the stable operation of a Li 0 -SPAN (sulfurized polyacrylonitrile) battery via an anode–cathode dual-passivation approach. By combination of a fluorinated localized high concentration electrolyte (LHCE) and a Li 3 N-forming additive (TMS-N 3 ), robust and highly conductive electrode passivation layers are formed in situ on the surface of both the Li 0 anode and the SPAN cathode. The resulting highly reversible, dendrite-free, and high-density Li 0 plating morphology enables a high Coulombic efficiency of 99.4%. Advanced tender energy X-ray spectroscopy also reveals the eliminated Li 2 S formation and minimized polysulfide dissolution in SPAN cathodes, leading to a high capacity of 580 mAh/g SPAN and stable cycling with negligible capacity decay (0.7%) for 800 cycles. This electrode–electrolyte interphase engineering strategy has tackled the major limitations of Li–S batteries in both ether- and carbonate-based electrolyte systems and under a wide temperature range from –10 to +50 °C, thus providing insightful guidelines for the rational design of highly durable and high-energy-density Li 0 -S batteries.

25 ENERGY STORAGE↗

Materials and Approaches for Mitigation of SOFC Cathode Degradation in SOFC Power Systems

Perovskites such as doped lanthanum manganite and cobaltite have been used successfully as a cathode material in SOFC power systems operating between 700-1000°C. The electrodes, however, remain prone to degradation in presence of Cr containing gas atmosphere under systems operating conditions. Cathode in SOFCs is considered as one of the largest contributors of electrochemical performance degradations, leading to significant increase in ohmic and non-ohmic losses as well as interfacial compound formation. These degradations are mostly irreversible due to permanent changes to chemical and morphological alterations in the electrodes, resulting in the blockage of triple phase boundary (TPB) sites and decrease in oxygen reduction reactions (ORR). Fundamental mechanistic understanding has been developed to elucidate the reaction pathways of electrode poisoning in electronically conducting electrodes (LSM) as well as mixed ionic and electronically conducting electrodes (LSCF). The overall goal of this program has been identification and development of cost effective solutions to mitigate electrode degradations under “real world” systems operating conditions. The overall technological innovations and impact from this work are: The research provides an understanding of the degradation mechanism and cost-effective approaches for implementation in SOFC systems; Develop mitigation processes utilizing low cost getters using conventional synthesis and fabrication route; Develop tailored high surface area powders and coatings for high Cr capture capacity under systems operating conditions; >Developed computational models to understand mechanistic behavior; Experimentally measure rate of Cr evaporation from chromia and alumina forming alloys under SOFC operating conditions; Developed conditions to minimize Cr evaporation from balance-of-plant alloys; This innovation will support the development of getter platform to capture both intrinsic and extrinsic impurities present in air; and, Applications under wide operating temperature range (500-900°C) as well for wide high-temperature electrochemical systems (SOFC, SOEC, and OTM). The work has been successfully developed, validated experimentally and implemented. Successful technology transfer of this knowledge with industrial partners has been accomplished and the getters have been independently tested and validated under their systems operating conditions. The innovation will also find application in related high temperature electrochemical systems such as OTM and SOEC for the prevention of Cr assisted performance degradation. The proposed approach for Cr capture can also be applied to oxy-combustion and other advanced combustion techniques for the reduction of Cr vapor in the exhaust gas stream. This fundamental knowledge gained also has led to the path forward for developing advanced getters for capturing more than one contaminant in air.

01 COAL, LIGNITE, AND PEAT↗

Revealing the Nature of Binary-Phase on Structural Stability of Sodium Layered Oxide Cathodes

The emergence of layered sodium transition metal oxides featuring a multiphase structure presents a promising approach for cathode materials in sodium-ion batteries, showcasing notably improved energy storage capacity. However, the advancement of cathodes with multiphase structures faces obstacles due to the limited understanding of the integrated structural effects. Herein, the integrated structural effects by an in-depth structure-chemistry analysis in the developed layered cathode system Na x Cu 0.1 Co 0.1 Ni 0.25 Mn 0.4 Ti 0.15 O 2 with purposely designed P2/O3 phase integration, are comprehended. The results affirm that integrated phase ratio plays a pivotal role in electrochemical/structural stability, particularly at high voltage and with the incorporation of anionic redox. In contrast to previous reports advocating solely for the enhanced electrochemical performance in biphasic structures, it is demonstrated that an inappropriate composite structure is more destructive than a single-phase design. The in situ X-ray diffraction results, coupled with density functional theory computations further confirm that the biphasic structure with P2:O3 = 4:6 shows suppressed irreversible phase transition at high desodiated states and thus exhibits optimized electrochemical performance. Finally, these fundamental discoveries provide clues to the design of high-performance layered oxide cathodes for next-generation SIBs.

36 MATERIALS SCIENCE↗

Building interface bonding and shield for stable Li-rich Mn-based oxide cathode

Implementation of Li-rich Mn-based oxide cathode with high-energy-density has been restrained by capacity/voltage degradation that results from irreversible lattice oxygen loss and structure rearrangements. To resolve these challenges, in this work, Li 1.2 Mn 0.54 Ni 0.13 Co 0.13 O 2 encapsulated by amorphous Co x B (CB-LRM) is rationally designed via autocatalytic plating for highly reversible cationic/anionic hybrid cathode material. Band coherency is ingeniously evoked by interface-reconstruction between bulk structure and amorphous coating layer, which lower the energy of O $2p$ states. Furthermore, this is associated with strengthened orbital hybridization of O $2p$-Mn $3d$ and increased formation energy of oxygen vacancy, which mitigates the lattice oxygen loss considerably. Additionally, interface shielding effects that protect electrode against electrolyte corrosion and the reduction of surface oxygen are also present with fully coverage of amorphous Co x B coating layer. As a result, the as-designed CBLRM cathode exhibits excellent cycle stability after 100 loops with only 0.154% per cycle capacity fade and improved voltage degradation. Given this, this work provides a potential avenue for rational design of lattice oxygen-based electrode materials with high-energy-density.

25 ENERGY STORAGE↗

Structure and Interface Design Enable Stable Li-Rich Cathode

Li-rich layered-oxide cathodes have the highest theoretical energy density among all the intercalated cathodes, which have attracted intense interests for high energy Li-ion batteries. However, O3-structured layered-oxide cathodes suffer from a low initial Coulombic efficiency (CE), severe voltage fade, and poor cycling stability because of the continuous oxygen release, structural rearrangements due to irreversible transition-metal migration, and serious side reactions between the delithiated cathode and electrolyte. In this work, we report that these challenges are migrated by using a stable O2-structured Li 1.2 Ni 0.13 Co 0.13 Mn 0.54 O 2 (O2-LR-NCM) and all-fluorinated electrolyte. The O2-LR-NCM can restrict the transition metals migrating into the Li layer and the in situ formed fluorinated cathode electrolyte interphase (CEI) on the surface of the O2-LR-NCM from the decomposition of all-fluorinated electrolyte during initial cycles effectively restrains the structure transition, suppresses the O2 release, and thereby safeguards the transition metal redox couples, enabling a highly reversible and stable oxygen redox reaction. O2-LR-NCM in all fluorinated electrolytes achieves a high initial CE of 99.82 % and cycling CE of and cycling CE of >99.9%, high reversible capacity of 278 mAh/g, and high capacity retention of 83.3% after 100 cycles. The synergic design of electrolyte and cathode structure represents a promising direction to stabilize high-energy cathodes.

25 ENERGY STORAGE↗

Directing High-Efficiency Na Plating with Carbon–Aluminum Junction Interfaces for Anode-Free Na Metal Batteries

Anode-free sodium metal batteries are highly promising for future energy storage but suffer from much faster cycling degradation as they are sensitive to even trace levels of irreversible side reactions. This work focuses on the most practical Al foil current collectors and systematically examined the effect of nano-sized carbon coating on improving the Na plating and stripping stability. We identified that the carbon-Al junction interface generated by carbon coating enabled more uniform Na depositing with lower overpotentials, delivering higher than 99.8% Faradaic efficiencies for a wide range of cycling currents between 0.5 and 3.0 mA cm -2 . This performance is much better than the 96.4% efficiency observed on uncoated Al foils under the same conditions, and was also confirmed under lean electrolyte and freezing electrolyte conditions, and can be attributed to the stronger interfacial binding and enhanced sodiophilic properties of the carbon-aluminum junction sites. Furthermore, these sites not only ensure uniform Na plating but also eliminates side reactions that would otherwise cause electrolyte depletion. As a result, Na-metal free full cells assembled with high capacity Na 3 V 2 (PO 4 ) 3 cathode delivered ~ 85% capacity retention for 100 cycles, higher than the 73% of retention of uncoated Al foil.

25 ENERGY STORAGE↗

Mapping Competitive Reduction upon Charging in LiNi 0.8 Co 0.15 Al 0.05 O 2 Primary Particles

Side reactions involving surface reduction play a critical role in the failure of LiNi 0.8 Co 0.15 Al 0.05 O 2 to reach its theoretical capacity as a cathode material for Li-ion batteries. While macroscopic consequences are known, the underlying nanoscopic mechanisms are not fully elucidated. By coupling X-ray spectroscopy with several X-ray microscopy modalities, we have spatially resolved the extent of Ni oxidation at several states of charge and uncovered heterogeneity that is hidden when considering ensemble measurements alone. The use of morphologically controlled particles enabled high-resolution imaging of these materials, uncovering gradients of Ni oxidation states within individual primary particles. At high states of charge, these gradients revealed regions of possible oxygen deficiency extending deeper into the particle than previously observed. Surface-sensitive X-ray coupled scanning tunneling microscopy allows oxidation states to be measured at the material's surface, showing predominantly Ni II in the first atomic layer and mixtures of Ni II with Ni III /Ni IV already appearing 1.5 nm into the particle. These results reveal the subtle interplay between irreversible surface transformations and the bulk reactions that ultimately define function, which will refine strategies of surface passivation that are key to overcoming current performance limitations.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ameliorating the sodium storage performance of hard carbon anode through rational modulation of binder

Hard carbon anodes have emerged as promising candidates for sodium-ion batteries due to their inherent advantages. Nevertheless, the surface imperfections in these materials often culminate in irreversible electrolyte consumption, fostering the development of a heterogeneous and fragile solid electrolyte interface (SEI), thereby compromising the initial Coulombic efficiency (ICE). Here, drawing inspiration from the catalytic potential of C=O (carbonyl) bonds in directing preferential salt reduction, we introduce a novel strategy that leverages the modulation of the binder, a long-term overlooked pivotal components in the electrode process. Specifically, Polymethyl methacrylate (PMMA), abundant in C=O groups, is partially substituted for PVDF, ensuring robust adhesion of the electrode material to the current collector while preserving superior mechanical properties. The accurate combination of two binders with delightful compatibility in the state-of-art electrode process, can promote a uniform formation of the SEI on the hard carbon surface enriched in inorganic components, which can ensure long-term interfacial stability and suppresses excessive solvent decomposition and facilitates Na + transfer at the interface. Consequently, the initial Coulombic efficiency of the hard carbon anode with 70 %PMMA binder achieves 86 %, with prominent cycling stability (88 % capacity retention over 500 cycles) at a high current density of 1.2 A g −1 . When paired with high loading cathodes to assemble the pouch cell, it also demonstrates stable operational scenarios.

25 ENERGY STORAGE↗

Anion modification for stable solid electrolyte interphase in anode-free lithium metal batteries

The durability of anode-free Li metal batteries is largely limited by the undesired Li plating/stripping irreversibility on the current collector due to the infinite volume change, uncontrollable Li dendrite growth, and continuous parasitic reactions between Li metal and the electrolyte. To address these challenges, the formation of a stable and robust solid electrolyte interphase (SEI) with high ionic conductivity and strong mechanical strength is critical. Here, we developed an advanced electrolyte by introducing LiNO 3 into the localized high concentration electrolyte (LHCE) with lithium bis(fluorosulfonyl)imide (LiFSI) salt, 1,2-dimethoxyethane (DME) solvent, and 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropylether (TFTE) diluent to in situ construct a LiF and Li x N y O z co-enriched passivation layer on the Cu current collector. The synergetic effect of high mechanical strength of LiF and high ionic conductivity of Li x N y O z endows the Li metal anode with a high Coulombic efficiency (CE) of 99.35%. In conclusion, in anode-free Li metal pouch cell using LiFePO 4 (LFP) as a cathode holds an exceptionally improved capacity retention under the charging/discharging rate of 1/3 C, demonstrating great promise for developing dendrite-free and safe Li metal batteries.

25 ENERGY STORAGE↗

Achieving SEI preformed graphite in flow cell to mitigate initial lithium loss

The irreversible lithium loss due to the formation of solid electrolyte interphase (SEI) in the initial cycle on the graphite anode greatly reduces the overall cell energy density of lithium ion batteries, that is, the lost Li ions from forming SEI lead to the decrease of Li ions for the intercalation. The method of cathode prelithiation has been widely explored to compensate this lithium loss. However, these cathode additives with high lithium contents inevitably lower the loading of the cathode active materials. In this work, we report a novel approach to solve this challenge, a facile graphite prelithiation method by preforming SEI layers on the surface of graphite powders (Pre-SEI graphite) utilizing a specially designed flow cell. The Li accommodation in the graphite anode can be controlled by the operating time and current density in the flow cell for the electrochemical SEI formation. As a result, we demonstrate a 10% initial Columbic efficiency increase of the LiFePO 4 electrode in a full cell configuration using the Pre-SEI graphite, compared with the pristine graphite anode. The electrochemical preformation of SEI on the graphite powders offers a complete solution to offset initial lithium loss without a sacrifice of active cathode material loading.

25 ENERGY STORAGE↗