Search NASA⌕ Search

SEARCH · Search NASA

Results for “microstructural properties”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Mechanical properties and microstructure characterization of Eurofer97 steel variants in EUROfusion program

Under the framework of EUROfusion, we performed comprehensive mechanical and microstructure characterization of ten Eurofer97 steel variants with varying compositions and heat treatment conditions. Moreover, we characterized the pre-irradiation fracture toughness of the materials along with their Vickers hardness, tensile properties, and microstructure. Compared with standard Eurofer97, the ten variants didn’t show a comprehensive improvement of mechanical properties. In addition, the composition and microstructures in some variants are adverse to fracture toughness, such as low C contents, coarse grain sizes, partially tempered martensite, lack of precipitates, and non-uniform distributions of coarse precipitates. Additional studies will be performed on the same materials after neutron irradiation.

36 MATERIALS SCIENCE↗

Microstructure, mechanical properties and texture evolution of AZ31 alloy containing trace levels of strontium

The effect of low levels of Sr (0.01, 0.03, 0.05 wt.%) on the microstructure, mechanical properties and texture of AZ31 magnesium alloy has been investigated. Thermodynamic modeling has been used to study the effect of Sr on phase precipitation at different temperatures. Cooling curve analysis reveals a decrease in solidification superheat with the addition of 0.03 wt.% Sr to AZ31. The as-cast microstructures of the alloys have been studied using optical microscopy (OM) and electron probe micro analysis (EPMA). Results show the refining effect of Sr on the grain size and on the {beta}-Mg{sub 17}Al{sub 12} precipitates through growth poisoning and inoculation, respectively. To investigate the mechanical properties of the alloys, as-cast samples were compression tested at elevated temperatures. Hot compression peak stress ({sigma}{sub max}) and critical strain before recrystallization ({epsilon}{sub c}) initially drop but then increase. {sigma}{sub max} first decreases due to the depletion of Al from solid solution and then increases when the amount of the Al-Sr precipitates reach a significant amount. {epsilon}{sub c} drops due to the acceleration of dynamic recrystallization kinetics as a result of grain refinement. It increases with increasing Sr when the concentration Sr in solid solution is increased leading to dislocation pinning and retardation of recrystallization. X-ray texture measurements on the hot compressed and extruded samples show a decrease in maximum intensity of the basal pole figures with increasing Sr as a result of reduced twining and the changes in Al and Sr concentrations in solid solution. - Research Highlights: {yields} Microstructures/precipitates of AZ31+trace levels of Sr were examined by OM and EPMA. {yields} Thermodynamic calculations and cooling curve analysis were used to predict ppt formation. {yields} It has been shown that Sr refines the grains and Mg17Al12 precipitates. {yields} Mechanical properties and texture were studied using hot compression and X-ray diffraction. {yields} Different micro-mechanisms were responsible for mechanical and texture changes.

36 MATERIALS SCIENCE↗

Preparation, microstructure and properties of AlN/CBC composites

Highlights: • AlN/CBC composites can be prepared by gelcasting and pressureless sintering method. • Suitable sintering additive content and increasing sintering temperature help to improve properties of composite. • Relative density, C content and microstructure et al. have effect on properties of composite. - Abstract: Gelcasting method with nontoxic biopolymer as gel former can be used to prepare ceramics with complex shape. AlN ceramic bonded carbon (AlN/CBC) composites with light weight were fabricated by gelcasting and pressureless sintering method using nontoxic agarose as gel former with Y{sub 2}O{sub 3} + CaF{sub 2} as sintering additive. The effect of sintering additive content and sintering temperature on the microstructure, flexural strength and thermal conductivity of composites was investigated. The results reveal that, as the temperature decreases, the raw powders solidify into three-dimensional net structures through abundant hydrogen bonds in the agarose. High sintering temperature facilitates densification and improves mechanical and thermal properties of the composites. Increasing sintering additive content can also tune the density and raise flexural strength. The AlN/CBC composite containing 7 wt% sintering additive content, which was sintered at 2000 °C, exhibits the highest thermal conductivity. Relative density, C content and microstructure uniformity have effects on properties of AlN/CBC composite.

36 MATERIALS SCIENCE↗

Microstructures and properties of high-entropy alloy films and coatings: a review

In the past 14 years, as a branch of high-entropy alloy (HEA) materials, HEA films and coatings have exhibited the attractive and unique properties, relative to the conventional film and coating materials. The recent research and development of HEA films and coatings are reviewed in this paper. At first, the basic concept of HEAs films and coatings are introduced. Then, their preparation technologies, microstructures and appealing properties are summarized. Moreover, the possible reasons and design criteria for achieving the excellent properties are discussed. Finally, the suggested future research work for the HEA films and coatings are outlined. Preparation technologies, microstructures, and properties of HEA films and coatings are reviewed in this paper. The design criteria and suggested research directions are further discussed and proposed.

36 MATERIALS SCIENCE↗

Microstructure and Properties of 5083 Al/1060 Al/AZ31 Composite Plate Fabricated by Explosive Welding

A 5083 Al/1060 Al/AZ31 composite plate was fabricated by explosive welding. The microstructure and properties of the composite plate were investigated after explosive welding. The results showed that all bonding interfaces were wavy interfaces. With an increasing distance from the detonation point, the wavelength and the amplitude also increased. The EDS results indicated that a 5-μm diffusion layer was observed at the 1060 Al/AZ31 layer, including the Mg{sub 2}Al{sub 3} phase. Adiabatic shear bands and twin structures were observed in AZ31. The shear bond strength of the 5083 Al/1060 Al interface was 60 MPa, and the shear bond strength of the 1060 Al/AZ31 interface was 84 MPa.

36 MATERIALS SCIENCE↗

Microstructure, mechanical properties and in vitro degradation behavior of novel Zn-Cu-Fe alloys

Highlights: • Zn-3Cu-xFe (x = 0, 0.5 and 1 wt%) alloys are proposed for the first time as candidate biodegradable materials. • The YS, UTS, and elongation of Zn-3Cu-0.5Fe alloy are 232 MPa, 284 MPa and 33%, respectively. • The in vitro degradation rate in SBF was successfully increased by about 52% by 1 wt% Fe addition for Zn-3Cu. - Abstract: Zn and Zn-based alloys as biodegradable material have drawn more and more attention in recent years due to their good mechanical properties, lower degradation rate than Mg and acceptable biocompatibility. However, too low degradation rate is a challenge for future application of Zn-based alloys. In this study, Zn-3Cu-xFe (x = 0, 0.5 and 1 wt%) alloys were proposed as candidate biodegradable materials. The microstructure, mechanical and in vitro biodegradable properties were investigated systematically. The Zn-3Cu alloy was composed of Zn matrix and CuZn{sub 5} phase, while the FeZn{sub 13} phase was newly formed with the addition of Fe. Due to the micro-galvanic effect produced by FeZn{sub 13} as a cathodic phase to the Zn matrix, in vitro degradation rate in simulated body fluid solution (SBF) was greatly increased by about 52.1%, from 45.3 ± 8.22 for Zn-3Cu alloy to 68.9 ± 7.34 μm/year for Zn-3Cu-1Fe alloy. Although the mechanical properties were decreased slightly due to the introduction of hard and brittle FeZn{sub 13} secondary phase to the Zn matrix, Zn-3Cu-0.5Fe alloy still exhibits good combined mechanical properties and the YS, UTS and elongation are 232 MPa, 284 MPa and 33%, respectively. Taken together, the mechanical properties and in vitro degradation behavior of the Zn-3Cu-xFe alloys are more suitable than Zn-3Cu alloy as candidate biodegradable materials.

36 MATERIALS SCIENCE↗

Magnetic properties and microstructure of bulk Nd-Fe-B magnets solidified in magnetic field

The Nd-Fe-B bulk magnets with a slab shape of 0.9 x 4 x 15 mm{sup 3} were prepared by injection casting into a copper mold. The effects of applying a magnetic field during the casting process on the magnetic properties and microstructure of Nd{sub 9.5}Fe{sub 71.5}Ti{sub 2.5}Zr{sub 0.5}Cr{sub 1}B{sub 14.5}C{sub 0.5} alloy have been studied. The results show that the sample cast with magnetic field has a stronger (00L) texture of Nd{sub 2}Fe{sub 14}B phase with the c-axis perpendicular to the slab plane than the sample cast without magnetic field. The intensity of the texture weakens from surface to inner region of the bulk magnets. Applying a magnetic field during the casting process is helpful to refine the grain size effectively. As a result, the magnetic properties are improved from B{sub r} = 5.8 kG, {sub i}H{sub c} = 6.5 kOe, and (BH){sub max} = 5.9 MGOe for thesample cast without magnetic field to B{sub r} = 6.1 kG, {sub i}H{sub c} = 10.3 kOe, and (BH){sub max} = 7.3 MGOe for the sample cast with a 3.7 kOe magnetic field.

36 MATERIALS SCIENCE↗

Effect of Minor Er on the Microstructure and Properties of Al-6.0Mg-0.4Mn-0.1Cr-0.1Zr Alloys

As-cast Al-6.0Mg-0.4Mn-0.1Cr-0.1Zr alloys containing different additions of Er were prepared. Then, the specimens were carried out homogenization heat treatment, hot rolling, cold rolling, and annealing. The effects of minor Er on the microstructure and properties of Al-6.0Mg-0.4Mn-0.1Cr-0.1Zr alloy were investigated. Results show that addition of Er can refine the microstructure and improve the mechanical properties of the alloys. As for the annealed alloys, the addition of 0.33%Er can increase the tensile strength by 29 MPa. Strength increment is mainly attributed to refinement and the precipitation of Al{sub 3}Er and Al{sub 3}(Er, Zr). Additionally, the minor Er can improve the corrosion resistance of the alloys, which can be attributed to the compact composite oxide film of Er-O and Al-O, purification, and modification.

36 MATERIALS SCIENCE↗

Effect of chip size on mechanical property and microstructure of AZ91D magnesium alloy prepared by solid state recycling

In this study, different kinds of AZ91D magnesium alloy chips were prepared by solid state recycling. Mechanical properties and microstructures of the recycled specimens were investigated. Various microstructural analyses were performed using the techniques of optical microscopy, scanning electron microscopy and oxygen-nitrogen analysis. Microstructural observations revealed that all the recycled specimens consisted of fine grains due to dynamic recrystallization. The oxide precipitate content is closely related to the recycled chip size. Accumulated oxygen concentration linearly increases with the total surface area of the machined chips in the recycled specimens. Ambient oxide in the recycled specimen contributes to a higher ultimate tensile strength and a higher elongation to failure; however, excessive oxide in the recycled specimen may adversely affect the elongation to failure.

36 MATERIALS SCIENCE↗

Effects of Overlapping Distances on Steel Microstructure and Properties After Multi-track Laser Quenching

In this study, multi-track laser quenching with different overlapping distances was used to assess SM45C microstructure and properties. Two overlapping distance types were evaluated, including overlapping distances in the transition and martensite regions, respectively. After multi-track quenching, hardness showed a threefold increase. With the overlapping distance in the transition region, surface hardness varied from 600 to 700 HV. There was a region of low hardness in each track. Hardness in the low hardness region was from 300 to 400 HV. The average hardness was basically over 500 HV with the overlapping distance in the martensite region, although there was a softening region. The increased hardness was mainly caused by the martensite. Microstructure in the overlapping region was self-tempered martensite, retained austenite and ferrite. Tempered sorbite and lowly tempered martensite were observed in heat-affected zones. Friction coefficients of quenched specimens varied between 0.275 and 0.325, with a 14% reduction relative to the base metal. The wear rate of the quenched specimen was only 40.8% of the base metal. With time, mass reduction in the quenched specimen was much smaller than that of the base metal. For specimens treated with laser quenching, slight fatigue wear was dominating.

36 MATERIALS SCIENCE↗

Effect of process conditions and chemical composition on the microstructure and properties of chemically vapor deposited SiC, Si, ZnSe, ZnS and ZnS(x)Se(1-x)

Subatmospheric pressure CVD processes have been developed to produce theoretically dense, highly pure, void-free and large area bulk materials, SiC, Si, ZnSe, ZnS and ZnS(x)Se(1-x). These materials are used for optical elements, such as mirrors, lenses and windows, over a wide spectral range from the VUV to the IR. We discuss the effect of CVD process conditions on the microstructure and properties of these materials, with emphasis on optical performance. In addition, we discuss the effect of chemical composition on the properties of the composite material ZnS(x)Se(1-x). We first present a general overview of the bulk CVD process and the relationship between process conditions, such as temperature, pressure, reactant gas concentration and growth rate, and the microstructure, morphology and properties of CVD-grown materials. Then we discuss specific results for CVD-grown SiC, Si, ZnSe, ZnS and ZnS(x)Se(1-x).

Pickering, Michael A.↗

Microstructure and Properties of AlCoCrFeNiTi High-Entropy Alloy Coating on AISI1045 Steel Fabricated by Laser Cladding

AISI1045 steel is widely used in mechanical engineering. In spite of the favorable toughness and strength, the surface properties of AISI1045 steel, such as hardness, wear resistance and corrosion resistance, are not ideal. Therefore, surface modification of AISI1045 is necessary, especially for the parts suffering severe work condition. Laser cladding is a promising surface modification technology. In this work, the AlCoCrFeNiTi high-entropy alloy (HEA) coatings were prepared on the AISI1045 steel to improve its surface properties. Metallurgical bonding is obtained between the coating and the substrate. The microstructure and surface properties of the coating were characterized by scanning electron microscope, energy-dispersive spectrometry, x-ray diffraction, electrochemical workstation, microhardness tester and pin-on-ring wear tester. The microstructure of the coating produced by laser cladding is dendritic. The AlCoCrFeNiTi HEA coating is mainly composed of disordered body-centered cubic phase (Fe-Cr), ordered B2 phase (AlNi) and intermetallic phase (Ti-rich). The coating shows excellent abrasion resistance and corrosion resistance in comparison with the substrate. The maximum microhardness of the coating reaches approximately 865 HV, which is 4.5 times of AISI1045 steel.

36 MATERIALS SCIENCE↗

Effect of filling materials on the microstructure and properties of hybrid laser welded Al-Mg-Si alloys joints

Highlights: • A serious comparison was made on the hybrid laser welded AA6061-T6 joint with different filling materials. • The microstructure of the welded joint was characterized using EBSD and SEM. • A strength model was successfully built to predict the strength of the hybrid laser welded AA6061-t6 joint. • The study shed new insights on how to select appropriate filling materials when using hybrid laser welding. - Abstract: A serious investigation was conducted to examine the influence of filling materials on the microstructure and properties of hybrid laser welded AA6061-T6 joints. The results of the tensile tests showed that the welded joint with ER4043 filling materials had higher tensile strength than that with ER5356 filling material. Based on the results obtained a strength model was built to predict and explain the enhancement of the yield strength of the hybrid laser welded AA6061-T6 joint with different welding wires. In contrast to the tensile strength, the ER4043 joint showed lower fatigue strength than that of the ER5356 joint due to extensive presence of micropores in fusion zone. Further, the corrosion experiment illustrated that the ER4043 joint had poorer resistance to the corrosive attack under 3.5% NaCl solution. A summary was made on the performance of both welded joints to shed new insights on selecting appropriate filling materials when welding AA6061-T6 by hybrid laser welding method.

36 MATERIALS SCIENCE↗

Magnetic properties and microstructure of FePt/Au multilayers with high perpendicular magnetocrystalline anisotropy

FePt/Au multilayers were deposited on preheated 100 deg. C MgO (001) single crystal substrates by magnetron sputtering. Magnetic properties and microstructure of the films were studied. Results show that the film possesses high coercivity H{sub C}, excellent perpendicular magnetic anisotropy (PMA), and weak interparticle exchange coupling (IEC) after annealing. FePt and Au can grow epitaxially on MgO substrates along the [001] direction, leading to excellent PMA. Au atoms partly diffuse to the boundaries of FePt phases and function as grain refiners and particle isolators, which markedly decrease the FePt grain size and IEC. Moreover, the additional FePt/Au interface energy, the stress energy due to the mismatch between FePt and Au lattices, and the diffusion of Au atoms all promote the ordering process of FePt film. This leads to the decrease in ordering temperature by 150 deg. C and a considerable increase in H{sub C}.

36 MATERIALS SCIENCE↗

Influence of phase composition on microstructure and properties of Mg-5Al-0.4Mn-xRE (x = 0, 3 and 5 wt.%) alloys

The microstructure and mechanical properties investigations of two AME503 and AME505 experimental alloys in as-cast conditions were presented. The investigated materials were fabricated on the basis of the AM50 commercial magnesium alloy with 3 and 5 wt.% cerium rich mischmetal. In the as-cast condition, both experimental alloys were mainly composed of α-Mg, Al{sub 11}RE{sub 3} and Al{sub 10}RE{sub 2}Mn{sub 7} intermetallic phases. Additionally, due to non-equilibrium solidification conditions, a small amount of α + γ divorced eutectic and Al{sub 2}RE intermetallic phase were revealed. The obtained results also show a significant influence of rare earth elements on Brinell hardness, tensile and compression properties at ambient temperature and especially on creep properties at 473 K. Improved alloy properties with a rise in rare earth elements mass fraction results from an increase in Al{sub 11}RE{sub 3} phase volume fraction and suppression of α + γ eutectic volume fraction in the alloy microstructure. Additionally, the influence of rare earth elements on the dendrite arm space value was discussed. The presented results also proved the thermal stability of the intermetallic phases during creep testing. - Highlights: • Two different Mg-5Al-0.4Mn alloys containing 3 and 5 wt.% of rare earth elements were fabricated. • Addition of rare earth elements leads to a reduction of dendrite arm spaces. • Mechanical properties depend on the phase composition of the alloys. • The increase of the rare earth elements content causes rise of the creep resistance.

36 MATERIALS SCIENCE↗

Effect of Volumetric Energy Density on Microstructure and Properties of Grade 300 Maraging Steel Fabricated by Laser Powder Bed Fusion

Here this study investigated the effect of laser powder bed fusion process parameters on the microstructure and properties of maraging steel. The results show that the process parameters can be finetuned to achieve both a high build rate/low hardness and low build rate/high hardness during fabrication, enabling the co-design of components where property gradients are desirable such as an injection molding tool where surface hardness is desired to be higher than the bulk, which needs to have higher fracture toughness.

36 MATERIALS SCIENCE↗

Effect of Forging on Microstructure, Mechanical Properties and Acoustic Emission Characteristics of Al Alloy (2014): 10 wt.% SiC{sub p} Composite

In this paper a systematic study has been undertaken to study the effect of forging on microstructure, mechanical properties and acoustic emission (AE) characteristics of Al alloy (2014)—10 wt.% SiC metal-matrix composites. Hammer forging was carried out at a temperature of 470 °C in an open die, with a deformation ratio of 3.5:1. Microstructural analyses were carried out at three different positions of forged billet. Significant material flow was observed in the sample taken from the sides of the forged billet, but no appreciable material flow was observed at the center of the forged billet. The microstructural characterization showed that forging resulted in cracking of SiC particles in Al alloy (2014)—10 wt.% SiC composite. The AE results during forging showed an increase in AE signal intensity during the initial yielding period and a subsequent decrease in the intensity of AE signals with sudden burst at the end of the forging. The plastic deformation at room temperature was less ductile in nature but at high temperature, appreciable ductility was observed. The FESEM micrographs of fracture surfaces of the tensile specimens showed appreciable clustering of SiC particles during plastic deformation both at room and high temperature.

36 MATERIALS SCIENCE↗