Search NASA⌕ Search

SEARCH · Search NASA

Results for “sintering temperature”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

High-temperature deformation and microstructural analysis for silicon nitride-scandium(III) oxide

It was indicated that Si3N4 doped with Sc2O3 may exhibit high temperature mechanical properties superior to Si3N4 systems with various other oxide sintered additives. High temperature deformation of samples was studied by characterizing the microstructures before and after deformation. It was found that elements of the additive, such as Sc and O, exist in small amounts at very thin grain boundary layers and most of them stay in secondary phases at tripple and multiple grain boundary junctions. These secondary phases are devitrified as crystalline Sc2Si2O7. Deformation of the samples was dominated by cavitational processes rather than movements of dislocations. Thus the excellent deformation resistance of the samples at high temperature can be attributed to the very small thickness of the grain boundary layers and the crystalline secondary phase.

Cheong, Deock-Soo↗

An Aerosol Jet Printed Resistance Temperature Detector‐Micro Hotplate with Temperature Coefficient of Resistance Stabilized by Electrical Sintering

Abstract Aerosol jet printing (AJP) is an emerging direct write tool enabling rapid prototyping and fabrication of electronics components. AJP provides faster and less expensive production of devices with feature sizes of >10 microns compared to traditional MEMS processes. Herein, the fabrication of a resistance temperature detector‐micro hotplate (RTD‐µHP) is reported using AJP printed silver. AJP eliminates sophisticated MEMS processes such as masking, alignment, and etching. The compatibility of the AJP process with a broad range of materials is demonstrated by printing highly resolved lines on rigid and flexible substrates. Optimal thermal sintering conditions of AJP printed silver (Ag) lines are found by in situ resistance measurements. To stabilize the temperature coefficient of resistance (TCR) of the RTD‐µHP at high operating current levels, electrical sintering is performed on the RTD‐µHPs. Electrical sintering improves the conductivity of fully thermally sintered Ag RTD‐µHPs by 32% and provides a burn‐in mechanism for stabilizing the TCR. The TCR of the RTD‐µHPs after electrical sintering is 3.80 × 10 −3 at 22 °C, close to the value for bulk Ag. The performance of the RTD‐µHPs is tested using a reference thermocouple. The RTD‐µHPs show reliable and repeatable heating and temperature sensing up to 70 °C in air.

Sui, Yongkun↗

Method of fabricating rigid radiation reflectors

A rigid radiation reflector is fabricated from a powdered material transparent to light in a wavelength band extending from approximately 0.2 micrometers to at least 8 micrometers. The powdered material is dispersed in a liquid wherein the powdered material is at least 95% insoluble in the liquid. The resulting mixture is molded under pressure at room temperature and then sintered to generate a porous solid. The porous solid is cooled to room temperature. A surface of the porous solid is then coated with a light-reflecting metal.

Youngquist, Robert C.↗

Predicting sintering window during supersolidus liquid phase sintering of steels using feedstock analysis and CALPHAD

Binder jet 3D printing results in carbon pickup from the binder at the inter-particle regions during binder burnout. The excess carbon lowers the solidus temperature of the green part locally during supersolidus liquid phase sintering (SLPS). Currently, thermodynamic calculations rely on the use of bulk powder compositions to predict the sintering window. This can overestimate the sintering temperature since the local increase in carbon on powder surfaces is not accounted for, that can locally lower the solidus temperature during SLPS. Here we show that using the inputs from feedstock and binder analysis, the excess carbon and hence the sintering window for the alloy can be predicted using CALPHAD. We present a case study on applying the proposed approach for pressureless sintering of binder jet additive manufactured (BJAM) of H13 steel via SLPS.

36 MATERIALS SCIENCE↗

Understanding the effects of fabrication process on BaZr 0.9 Y 0.1 O 3– δ grain-boundary chemistry using atom probe tomography

Proton-conducting oxides, such as BaZr 0.9 Y 0.1 O 3–δ (BZY10), are receiving significant scientific attention for application in a variety of electrochemical applications. It has been shown that the synthesis route has a significant effect on the ionic behavior of these materials, especially the grain boundaries (GB). In this study, laser-pulsed atom probe tomography (APT) is used to characterize the GB chemistry of BZY10 samples prepared by four different methods: (1) spark plasma sintering (SPS), (2) conventional sintering followed by high-temperature annealing (HT), (3) conventional sintering with NiO used as a sintering aid (SSR-Ni), and (4) solid-state reactive sintering of oxide precursor powders with NiO as a reactive sintering aid (SSRS-Ni). Oxygen depletion (corresponding to oxygen vacancy accumulation) was observed at every GB in this study, consistent with the positive space-charge GB region commonly assigned to these materials. In contrast to the consistent trends associated with oxygen depletion, cation constituents showed varying segregation/depletion behaviors. The samples that used NiO revealed Ni preferentially segregating to the GB. The most common impurities in BZY10 are Al, Fe, Mg, Si, and Sr, all of which generally accumulate at GBs. In order to quantify these chemical trends, the APT method was optimized for this material supplemented with understanding from density functional theory (DFT). Finally, this APT study reveals the complexity of BZY10 GB chemistry and shows that even adjacent GBs in the same material can sometimes show surprisingly different GB chemistry.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Thermally Driven Interfacial Degradation between Li 7 La 3 Zr 2 O 12 Electrolyte and LiNi 0.6 Mn 0.2 Co 0.2 O 2 Cathode

Solid-state batteries offer higher energy density and enhanced safety compared to the present lithium-ion batteries using liquid electrolytes. A challenge to implement them is the high resistances, especially at the solid electrolyte interface with the cathode. Sintering at elevated temperature is needed in order to get good contact between the ceramic solid electrolyte and oxide cathodes and thus to reduce contact resistances. Many solid electrolyte and cathode materials react to form secondary phases. It is necessary to find out which phases arise as a result of interface sintering and evaluate their effect on electrochemical properties. Herein, we assessed the interfacial reactions between LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) and Li 7 La 3 Zr 2 O 12 (LLZO) as a function of temperature in air. We prepared model systems by depositing thin-film NMC622 cathode layers on LLZO pellets. The thin-film cathode approach enabled us to use interface-sensitive techniques such as X-ray absorption spectroscopy in the near-edge as well as the extended regimes and identify the onset of detrimental reactions. We found that the Ni and Co chemical environments change already at moderate temperatures, on-setting from 500 °C and becoming especially prominent at 700 °C. By analyzing spectroscopy results along with X-ray diffraction, we identified Li 2 CO 3 , La 2 Zr 2 O 7 , and La(Ni,Co)O 3 as the secondary phases that formed at 700 °C. The interfacial resistance for Li transfer, measured by electrochemical impedance spectroscopy, increases significantly upon the onset and evolution of the detected interface chemistry. Our findings suggest that limiting the bonding temperature and avoiding CO 2 in the sintering environment can help to remedy the interfacial degradation.

36 MATERIALS SCIENCE↗

Mechanical characterization of fine-grain dispersion-strengthened tungsten as a plasma facing material

Field-Assisted Sintering Technology (FAST) was used to produce fine-grained, dispersion-strengthened tungsten (W) materials. Investigated materials 4138, 4353, and 4355 composed of 3 wt% ZrC sintered at 1800 °C, 5 wt% ZrC sintered at 1800 °C, and 3 wt% ZrC sintered at 2000 °C, respectively. They were compared against ITER-grade W. A series of mechanical and thermal property testing and microstructure studies were conducted to study them as a potential plasma facing material (PFM) for fusion reactors. Hardness testing showed that manufacturing conditions substantially altered hardness. Material 4355 had an average HV10 value of 497.2 ± 16.8, slightly higher than ITER-grade at 378.5 ± 40.3. However, material 4353 was substantially higher with an HV10 value of 738.9 ± 31.7 over the investigated temperature range. Electron Backscatter Diffraction (EBSD) analysis showed that FAST produced substantially smaller grains than the hot-rolled ITER-grade W material, offering notable control over grain size. Materials 4353 and 4355 had grain sizes of 0.44 ± 0.20 µm and 3.67 ± 0.89 µm, respectively, whereas ITER-grade 27.14 ± 19.76 µm at room temperature. The fine grain structures showed no net coarsening after 1 hr. anneals up to 1800 °C, several hundred degrees above the 1100 – 1500 °C recrystallization range reported for conventional W. Inverse application of the Zener pinning relationship to the measured grain sizes indicates that these two FAST sintering conditions produce markedly different effective dispersoid populations, with effective particle diameters of approximately 90 nm at a peak sintering temperature of 1800 °C and approximately 460 nm at 2000 °C, respectively. This result demonstrates that the FAST thermal condition itself, and not the nominal ZrC content alone, governs the pinning effectiveness of the dispersion. Thermal diffusivity measurements support this finding independently. Materials of identical composition sintered at different temperatures differ by approximately 19% in measured thermal diffusivity with statistically indistinguishable density, while materials of different composition and sintering temperature converge to within approximately 2%. At a representative divertor heat flux of 10 MW/m², the lower thermal conductivity of the fine-grained materials corresponds to approximately 28 to 33 °C per millimeter of armor thickness relative to ITER-grade W, traded against a substantially larger margin to recrystallization-driven degradation. While high temperature tensile testing revealed likely contamination that motivates refinement of the manufacturing process, FAST-produced, fine-grained, dispersion-strengthened W offers process-controlled microstructural stability well above the operating temperatures of conventional W and supports its continued development as a PFM for economically viable commercial fusion power.

Parker, Gabe [ORNL] (ORCID:0000000190394100)↗

Improving the Fracture Toughness and Ductility of Liquid-Phase Sintered WNiFe Tungsten Heavy Alloys by High-Temperature Annealing

Tungsten heavy alloys (WHAs) are candidates for use in fusion reactor divertors. Here, we characterize liquid-phase sintered WHAs with 90, 92.5, 95, and 97 (wt.%) tungsten (W), with a balance of a 0.7Ni–0.3Fe ductile phase. These WHAs show remarkable room temperature (RT) fracture toughness at the maximum load, K Jm , ranging from ≈ 38 to 107 MPa√m, compared to a monolithic W toughness of ≈ 8 MPa√m. In most cases, the fracture of WHAs occurs through stable crack tearing. However, the 97W WHA has the lowest toughness and fracture elastically in all but the smallest specimens. As lower Ni contents are desirable for fusion application, we explore the potential for improving the ductility and K Jm of WHAs using vacuum annealing at 1300 °C for 24 h. The microstructural observations reveal negligible changes in the WHA microstructure and constituent compositions. While annealing reduces the Vickers microhardness (HV), it does not significantly change the RT yield (σ y ) and ultimate (σ u ) strengths but results in beneficial increases in total elongation in the 95 and 97W WHAs by a factor of 2. RT tests on the precracked three-point-bend (3PB) bars show that annealing increases the K Jm of these WHAs, and in the case of the 97W WHA, the increase is from 42 to 92%, depending on the size of the specimen. Toughening is due to enhanced crack tip process zone microcracking and dilatation.

36 MATERIALS SCIENCE↗

Indirect measurement of the viscosity of the intergranular glass phase in yttria-sintered silicon nitride

Dense, sintered Si3N4 possesses a residual intergranular glass phase which softens at high temperatures, resulting in degradation of the ceramic's mechanical properties at high temperatures. An important parameter in the determination of the high temperature mechanical properties of sintered Si3N4 is the temperature-viscosity relationship of the intergranular glass. A method for indirectly measuring the intergranular glass viscosity at a given temperature using physical modelling of a two phase glass crystal microstructure and beam bending viscometry measurements of Si3N4 is described. Intergranular glass viscosities obtained by this method are presented for a yttria sintered Si3N4.

Dittmar, Mark B.↗

Report Summarizing the Mechanical Properties of a Large ODS Ferritic Alloy Ingot by Forging at High Temperatures for Future Mother Tube Production

Oxide dispersion strengthened (ODS) ferritic alloys are considered the benchmark fuel cladding and core structural material in advanced nuclear energy reactors that require high-temperature strength and creep properties and resistance to radiation damage. The ODS ferritic alloys including 14YWT are produced by mechanical alloying (MA), which is time-consuming and is associated with high manufacturing costs that are not beneficial to being used in advanced nuclear energy reactors. This report summarizes the accomplishments in FY24 in the INM program for producing an ODS ferritic alloy by high-deformation, high-temperature processing of reactive and ferritic alloy powders for advanced reactor fuel cladding applications. Following four hot forging experiments, it was concluded that several significant challenges were encountered that were difficult to overcome. These challenges were related to using high annealing temperatures for pressure assisted sintering processes to produce dense microstructures, but the high annealing temperatures result in long range diffusion of Ti through the bcc Fe lattice and react with the YIG particles that are distributed on the prior surfaces of the ferritic alloy powders. In addition, it was determined that the high deformations induced by forging at high temperatures were not very effective for fracturing the reactive YIG particles into smaller particles and distributing them into the interior of the ferritic alloy powders. Spark plasma sintering was attempted for shortening the time at high temperatures, which led to full densification but the microstructure characterization results still showed that Ti atoms diffused over long distances in the bcc Fe lattice and reacted with the YIG particles. Finally, a short 30 minute high intensity ball milling experiment was conducted on blended 14WT and YIG powders for inducing severe deformations that caused the initially spherical powders of 14WT decorated with the YIG particles on the surfaces to transform to flakes and fracturing of YIG particles into smaller particles that were incorporated into the bcc Fe lattice. Two forgings were performed with the high intensity milled powders: first annealing for 20 minutes at 850ºC followed by forging and second annealing for 20 minutes at 1,100ºC followed by forging. At 850ºC, Ti atoms are effectively immobile, thus allowing for densification albeit incomplete. The deformation by forging after annealing for 20 minutes at 1,100ºC favored dynamic recrystallization processes that led to nano-size grains with very high stored energy due to high dislocation density. The corresponding VH data showed significant hardening that correlated with estimated strengthening of ~1650 MPa. This hybrid processing approach combining high intensity ball milling of powder with annealing and forging showed the most promise for producing an oxide dispersing strengthened ferritic alloy.

36 MATERIALS SCIENCE↗

High-temperature compressive creep tests of U 3 Si 2 with spark plasma sintering: Experiments and finite element modeling

This paper reports a systematic high-temperature creep behavior of dense U 3 Si 2 pellets using a spark plasma sintering (SPS) apparatus at elevated temperatures and pressures under vacuum conditions. The stress exponent was subsequently derived to be 3.21 at 1173 K and 2.17 at 1223 K, respectively, indicating a grain boundary sliding creep mechanism. The creep activation energy was determined to be 203.6 ± 19.0 kJ/mol, which agrees well with the literature. Finite element modeling was performed using the creep parameters fitted from the strain-time plot. Additionally, the results suggest an excellent match with the experimental data, confirming the validity of the experiments. Microstructure characterizations indicate that the main phase of the specimens after creep tests remains to be U 3 Si 2 , with a 4 μm thick layer of nano-sized particles induced from the diffusion between U 3 Si 2 and alumina disc used to avoid electric current passing through the sample. The successful conduct of creep experiments demonstrates the great potential of SPS to perform high-temperature mechanical testing of nuclear fuels under vacuum conditions. The subsequent finite element modeling exhibits excellent capabilities for accurately predicting material performance in the creep tests and provides a practical tool in evaluating nuclear fuels’ performance for a much-extended time scale.

36 MATERIALS SCIENCE↗

Improved silicon carbide for advanced heat engines. II - Pressureless sintering and mechanical properties of injection molded silicon carbide

The influence on density and strength of pressureless sintering in vacuum and argon environments has been evaluated with injection molded SiC materials. Main effects and two factor interactions of sintering (cycle variables temperature, time, heating rate, and atmosphere) were assessed. An improved understanding of the influence of the processing flaws and sintering conditions has been obtained. Strength and density have improved from a baseline level of 299 MPa (43.3 Ksi) and 94 pct of theoretical density to values greater than 483 MPa (70 Ksi) and 97 pct.

Whalen, Thomas J.↗

Crystallization and properties of Sr-Ba aluminosilicate glass-ceramic matrices

Powders of roller quenched (Sr,Ba)O-Al2O3-2SiO2 glasses of various compositions were uniaxially pressed into bars and hot isostatically pressed at 1350 C for 4 hours or cold isostatically pressed and sintered at different temperatures between 800 to 1500 C for 10 or 20 hours. Densities, flexural strengths, and linear thermal expansion were measured for three compositions. The glasss transition and crystallization temperatures were determined by Differential Scanning Calorimetry (DSC). The liquidus and crystallization temperature from the melt were measured using high temperature Differential Thermal Analysis (DTA). Crystalline phases formed on heat treatment of the glasses were identified by powder x ray diffraction. In Sr containing glasses, the monoclinic celsian phase always crystallized at temperatures above 1000 C. At lower temperatures, the hexagonal analog formed. The temperature for orthorhombic to hexagonal structure transformation increased monotonically with SrO content, from 327 C for BaO-Al2O3-2SiO2 to 758 C for SrO-Al2O3-2SiO2. These glass powders can be sintered to almost full densities and monoclinic celsian phase at a relatively low temperature of 1100 C.

Bansal, Narottam P.↗

Crystallization and properties of Sr-Ba aluminosilicate glass-ceramic matrices

Powders of roller quenched (Sr,Ba)O-Al2O3-2SiO2 glasses of various compositions were uniaxially pressed into bars and hot isostatically pressed at 1350 C for 4 hours or cold isostatically pressed and sintered at different temperatures between 800 to 1500 C for 10 or 20 hours. Densities, flexural strengths, and linear thermal expansion were measured for three compositions. The glass transition and crystallization temperatures were determined by Differential Scanning Calorimetry (DSC). The liquidus and crystallization temperature from the melt were measured using high temperature Differential Thermal Analysis (DTA). Crystalline phases formed on heat treatment of the glasses were identified by powder X ray diffraction. In Sr containing glasses, the monoclinic celsian phase always crystallized at temperatures above 1000 C. At lower temperatures, the hexagonal analog formed. The temperature for orthorhombic to hexagonal structural transformation increased monotonically with SrO content, from 327 C for BaO-Al2O3-2SiO2 to 758 C for SrO-Al2O3-2SiO2. These glass powders can be sintered to almost full densities and monoclinic celsian phase at a relatively low temperature of 1100 C.

Bansal, Narottam P.↗

An electrochemically stable homogeneous glassy electrolyte formed at room temperature for all-solid-state sodium batteries

All-solid-state sodium batteries (ASSSBs) are promising candidates for grid-scale energy storage. However, there are no commercialized ASSSBs yet, in part due to the lack of a low-cost, simple-to-fabricate solid electrolyte (SE) with electrochemical stability towards Na metal. In this work, we report a family of oxysulfide glass SEs (Na 3 PS 4-x O x , where 0 < x ≤ 60) that not only exhibit the highest critical current density among all Na-ion conducting sulfide-based SEs, but also enable high-performance ambient-temperature sodium-sulfur batteries. By forming bridging oxygen units, the Na 3 PS 4-x Ox SEs undergo pressure-induced sintering at room temperature, resulting in a fully homogeneous glass structure with robust mechanical properties. Furthermore, the self-passivating solid electrolyte interphase at the Na|SE interface is critical for interface stabilization and reversible Na plating and stripping. The new structural and compositional design strategies presented here provide a new paradigm in the development of safe, low-cost, energy-dense, and long-lifetime ASSSBs.

25 ENERGY STORAGE↗

Effects of mechanically alloying Al 2 O 3 and Y 2 O 3 additives on the liquid phase sintering behavior and properties of SiC

In order to improve the sintering of SiC, mixtures of Al 2 O 3 and Y 2 O 3 powders are commonly included as sintering additives. The aim of this work was to use mechanically alloyed Al 2 O 3 –Y 2 O 3 mixtures as sintering additives to promote liquid phase sintering of SiC using spark plasma sintering. The results showed that milling reduced the particle size of the powders and led to the formation of complex oxide phases (YAP, YAM, and YAG) at low temperatures. As the ball milling time increased, the mass loss of specimens sintered with mechanically alloyed Al 2 O 3 –Y 2 O 3 mixtures decreased, and accordingly the relative density increased. However, the hardness and flexural strength of sintered SiC specimens first increased and then decreased. Because the specimens prepared with oxides milled for a long time contained too much YAG/YAP and accordingly too much liquid at sintering temperature. This negatively affected the mechanical properties of the SiC specimens because of the increased volume of the complex oxide phases, which have inferior mechanical properties to SiC, in the sintered specimens. In conclusion, when the ball milling time was 6h, the hardness (24.02 GPa) and flexural strength (655.61 MPa) of the SiC specimens reached maximum values.

36 MATERIALS SCIENCE↗

Aerosol jet printed 3 omega sensors for thermal conductivity measurement

The 3 omega (3ω) method is a trusted technique for measuring thermal conductivity—a fundamental material property of critical importance in a broad range of applications. However, traditional 3ω sensor processing requires some form of physical vapor deposition, such as metal evaporation or sputtering. These 3ω sensor deposition techniques limit the materials and sample sizes applicable to the 3ω method. This work demonstrates an aerosol jet printing method to directly print silver 3ω sensors that yield accurate temperature-dependent measurement up to 300 °C on materials with thermal conductivity ranging from 1 to 150 W/m K. The interrelationship between printed sensor geometry, sensor thermal stability, and applicability to the 3ω method is examined. Thermal conductivity measurement with 3ω sensors conventionally sintered at 300 °C agrees to independent laser flash measurement within 4% from room temperature to 150 °C. An unconventional rapid high-temperature sintering method is shown to produce sensors that agree within 3% of the laser flash measurements from room temperature to 300 °C. The rapid sintering profiles also reduced the sensor–substrate thermal boundary resistance of the printed sensors by as much as 88%. The direct printing of 3ω sensors creates opportunities for measurement of thermal transport properties in applications previously inapplicable to the 3ω method.

47 OTHER INSTRUMENTATION↗