Search NASA⌕ Search

SEARCH · Search NASA

Results for “superalloy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Determination of Location-Specific Solidification Cracking Susceptibility for a Mixed Dissimilar Alloy Processed by Wire-Arc Additive Manufacturing

Solidification cracking is a major obstacle when joining dissimilar alloys using additive manufacturing. In this work, location-specific solidification cracking susceptibility has been investigated using an integrated computational materials engineering (ICME) approach for a graded alloy formed by mixing P91 steel and Inconel 740H superalloy. An alloy mixture of 26 wt.% P91 and 74 wt.% Inconel 740H, with high configurational and total entropy, was fabricated using wire arc additive manufacturing. Microstructure characterization revealed intergranular solidification cracks in the FCC matrix, which increased in length along with the enrichment of Nb (~27 to 56 wt.%) and Cu (~87 wt.%) in the middle and top regions. DICTRA simulations to model location-specific solidification cracking susceptibility showed that the top region with the highest cooling rate (270 K/s) has the highest solidification cracking susceptibility in comparison with the middle and bottom regions. This is in good agreement with the experimentally observed varying crack length. From Scheil simulations, it was deduced that enrichment of Nb and Cu affected the solidification range as high as ~77%, in comparison with the matrix composition. The overall solidification cracking susceptibility and freezing range was highest for the 26 wt.% P91 alloy amongst the mixed compositions between P91 steel and 740H superalloy, proving that solidification characteristics play a major role in alloy design for additive manufacturing.

20 FOSSIL-FUELED POWER PLANTS↗

Phase field modeling of shearing processes of a dual-lobed γ"|γ'|γ" coprecipitate

The Ni-based superalloy IN718 is one of the most widely used commercial alloy in the aerospace industry since its development in 1960s. The excellent mechanical properties have been attributed in a great deal to strengthening by coherent γ' and γ" precipitates. The deformation mechanisms of these two phases have been well studied individually. Recent experimental characterization has shown coprecipitates of these two phases in a variety of morphologies and it was argued that these coprecipitates may lead to improved strengthening as compared to their monolithic counterparts. However, the deformation mechanisms of these coprecipitates are still not well understood. In this study, we performed microscopic phase field simulations, with generalized-stacking-fault (GSF) energy surfaces from ab initio calculations as inputs, to systematically study the shearing processes of a periodical array of dual-lobed coprecipitates as well as monolithic precipitates. We found that the coupling between the γ' and γ" phases in the coprecipitates forces dislocations to take high energy shearing pathways in both phases that would not occur if they were in monolithic forms. The coupling also creates stacking fault configurations in the coprecipitates that require high stress to form. Thus, the presence of coprecipitates in general should increase the resistance to dislocation shearing and lead to higher strength levels. Various fault configurations observed during the shearing process are documented as a reference for future comparison with experimental observations. The link between stacking fault shearing and microtwinning is also discussed. Here, the mechanisms analyzed in this study deepens our understanding of coprecipitation effects on alloy strength and may form a cornerstone for multi-precipitate strengthened alloy design strategies.

36 MATERIALS SCIENCE↗

Dissolution zone model of the oxide structure in additively manufactured dispersion-strengthened alloys

The structural evolution of oxides in dispersion-strengthened superalloys during laser-powder bed fusion is considered in detail. Alloy chemistry and process parameter effects on oxide structure are assessed through a parameter study on the model alloy Ni-20Cr, doped with varying concentrations of Y 2 O 3 and Al. Small angle neutron scattering measurements of the dispersoid size distribution show the dispersoid size increases with higher laser power, slower scan speed, and increasing Y 2 O 3 and Al content. Complementary electron microscopy measurements reveal reactions between Y 2 O 3 and Al, even in nanoscale dispersoids, and the presence of micron-scale oxide slag inclusions in select specimens. A scaling analysis of mass and momentum transport within the melt pool, presented here, establishes that diffusional structural evolution mechanisms dominate for nanoscale dispersoids, while fluid forces and advection become significant for larger slag inclusions. These findings are developed into a theory of dispersoid structural evolution, integrating quantitative models of diffusional processes – dispersoid dissolution, nucleation, growth, coarsening – with a reduced order model of time-temperature trajectories of fluid parcels within the melt pool. Calculations of the dispersoid size in single-pass melting reveal a zone in the center of the melt track in which the oxide feedstock fully dissolves. Within this zone the final Y 2 O 3 size is independent of feedstock size and determined by nucleation and growth kinetics. If the dissolution zones of adjacent melt tracks overlap sufficiently with each other to dissolve large oxides, formed during printing or present in the powder feedstock, then the dispersoid structure throughout the build volume is homogeneous and matches that from a single pass within the dissolution zone. Gaps between adjacent dissolution zones result in oxide accumulation into larger slag inclusions. Predictions of final dispersoid size and slag formation using this dissolution zone model match the present experimental data and explain process-structure linkages speculated in the open literature.

36 MATERIALS SCIENCE↗

A theoretical calculation of stacking fault energy of Ni alloys: The effects of temperature and composition

Combining cluster expansion (CE) method with one dimensional axial Ising model, this work investigated the effects of alloying elements and configurational variations due to temperature on the stacking fault energy (SFE) of FCC Ni binary alloys. Ensembles of large numbers of atomistic structures, each with more than ~400 atoms, were generated to consider sufficient long-range chemical disorder and temperature effects due to configurational entropy. Here, a Monte Carlo Metropolis algorithm was used to generate these structures, whose energies were then evaluated based on the effective cluster interactions obtained from CE. As a baseline, this work had shown the SFE of pure Ni and Al to be 127 mJ/m 2 and 137 mJ/m 2 , respectively, which agreed with the experimental values of 125 mJ/m 2 and 150 mJ/m 2 reported in the literature. Additions of Al, Ti, Cr and Co to pure Ni were found to decrease the SFE to different extents. Although temperature does not strongly influence the SFE of the FCC Ni-Al and Ni-Cr binary alloys, it can lead to significant changes to the SFE of the FCC Ni-Ti and Ni-Co alloys. While effects of temperature and composition on SFE observed in this work were calculated from binary Ni alloys, the general trends are nonetheless expected to be valid in the γ phase of multicomponent Ni superalloys.

36 MATERIALS SCIENCE↗

Cyclic oxidation behavior of selected commercial NiCr-alloys for engine exhaust valves in wet air environment between 800 and 950 °C

In this work, the impact of water vapor on the cyclic oxidation behavior of four commercial Ni-based superalloys (N80A, N90, R41 and H282) was investigated between 800 and 950°C. Oxidation- and volatilization-induced Cr loss accelerated the transition from protective and adherent oxide formation (Cr 2 O 3 ) to mixed oxides that significantly spalled at 950°C for H282 and R41. The accelerated oxidation, Cr depletion, and spallation susceptibility for R41 and to a lesser extent for H282 compared to N80A and N90 was related to the higher fraction of γ’, which led to increased Ti incorporation into the Cr 2 O 3 scale in the presence of water vapor.

36 MATERIALS SCIENCE↗

Effect of pressure on high-temperature oxidation of Ni alloys in supercritical CO 2 containing impurities

Direct supercritical CO 2 (sCO 2 ) power cycles require structural materials compatible with hot sCO 2 containing high levels of water and oxygen impurities. Chromia-forming Ni-based superalloys, which are leading candidates at temperatures > 600 °C, have shown good compatibility in pure sCO 2 , however potential impurity effects are not well understood. In this report we exposed several commercial Ni-based alloys to 95%CO 2 -4%H 2 O-(1-3)%O 2 at 750 °C and 0.1 or 20 MPa for 2500 h. Protective chromia scales formed in all cases. Nevertheless, water vapor-assisted oxide volatilization clearly occurred at high pressure. The volatilization rates decreased with time, but still represent a potentially serious compatibility issue in real, high-velocity, sCO 2 systems.

36 MATERIALS SCIENCE↗

A macro-micro approach for identifying crystal plasticity parameters for necking and failure in nickel-based alloy haynes 282

Here, this work develops a two-scales macro-micro approach to address the challenge in calibrating crystal plasticity microstructural models when samples undergo necking prior to fracture. The crystal plasticity models are crucial for predicting the materials’ plastic deformation and failure at the microstructure level, identifying the materials’ intrinsic properties as well as investigating the microstructure-properties relationships. However, after necking occurs, the experimentally measured stress-strain curves fail to reflect the materials ‘true’ stress-strain behavior and cannot be directly fitted into crystal plasticity models. The proposed macro-micro approach employs a top-down strategy to address this challenge, which has been studied with experimental tests on precipitation-strengthened Ni-based superalloy Haynes® 282®. In this approach, a macro rate-dependent anisotropic plasticity model with Voce-type hardening and Rice-Tracey damage law is first utilized to model the deformation and failure of the tensile bar, and calibrated by matching the stress-strain curves, necking strain, and reduction of area. Especially, to match the testing results under different applied strain rates, the rate-sensitivity parameter m and saturation stress in the elasticity model are modified to incorporate dependence on the local strain rate. Then, the ‘true’ stress-strain behaviors are extracted from the necking zone of the macro-model, which are used to calibrate a micro-model with explicit microstructures and governed by an extended crystal plasticity law. The consistency between the micro-model and macro-model are enforced during calibration. The calibration outcomes from the crystal plasticity model elucidate the materials intrinsic properties for slip, hardening, and failure, which is vital for further investigations into the microstructure-properties relationship and for accurate prediction of the material behavior under various test and service conditions.

36 MATERIALS SCIENCE↗

Effect of heterogeneous microstructure on the tensile and creep performances of cast Haynes 282 alloy

Precipitation-strengthened Ni-based superalloys are leading candidate materials for advanced ultra-supercritical (A-USC) plants with steam conditions up to 760 °C (1400 °F) and 35 MPa (5 ksi). This study evaluates representative specimens from a large casting of Haynes 282 to study the effect of microstructural heterogeneity on the mechanical behavior of this alloy. The tensile test results of cast Haynes 282 over the temperature range 20–816 °C exhibited lower tensile strength and ductility in comparison with the reference wrought Haynes 282. However, the creep rupture tests of the cast alloy below 704–788 °C and 190–431 MPa presented a similar stress-Larson-Miller parameter to that of the wrought material. Microstructural and dislocation characterizations using scanning electron microscopy, conventional transmission electron microscopy, and scanning transmission electron microscopy in conjunction with energy dispersive X-ray spectroscopy were performed to understand the microstructural evolution before and after the mechanical tests. The heterogeneous microstructures of the cast Haynes 282 material, including the coarse grains, potential casting defects, and a bimodal size distribution of γ' precipitates, were detrimental to the tensile behavior, whereas the coarse-scale grains had a positive effect on the creep performance because diffusional creep was the dominant creep mechanism.

tensile testing↗

Elucidating texture and grain morphology contributions to the micromechanical response of additively manufactured Inconel 625

Microstructural variation of additively manufactured (AM) metal components in comparison to wrought counterparts makes certification for critical applications a challenge. Microscale simulations leveraging modern computational tools may be used to supplement testing of AM microstructures, thus accelerating certification by reducing the number of experiments needed. However, as micromechanical response is closely tied to critical properties like fatigue-life and fracture, utilization of these simulations with macroscale experimental data alone is insufficient. One means to attain microscale experimental data is in situ diffraction data collected from synchrotron X-ray sources. In this work, such data were collected during in situ compression of AM Inconel 625 superalloy. Interpretation of experimental results was assisted by massive (8M element) complementary micromechanical simulations performed on sets of virtual microstructures generated using cellular automata. Together, micromechanical data from diffraction experiments and simulations were used to probe the effects of textured “track” microstructures generated during laser powder bed fusion and directional strength-to-stiffness on micromechanical response. Though fiber-averaged directional strength-to-stiffness ratios were expected to dominate given the high elastic anisotropy of the material, the combination of small variations in texture and specific grain configurations unique to AM microstructures lead to significant variability in micromechanical response after yield. The findings emphasize the importance of high-fidelity microstructural representation that captures key texture components and AM-specific morphology for property prediction of AM metals.

36 MATERIALS SCIENCE↗

An additively-manufactured molten salt-to-supercritical carbon di-oxide primary heat exchanger for solar thermal power generation – Design and techno-economic performance

The design and techno-economic performance of a compact additively manufactured (AM) molten salt (MS)-to-supercritical carbon di-oxide (sCO2) primary heat exchanger (PHE) for solar thermal application is described. The PHE design consists of sCO2 flow through an array of microscale pin fins while the MS flows through mm-scale rectangular channels. Constraints imposed by AM using laser powder bed fusion method are considered in the design. Structural and fluid flow simulations are performed to arrive at a viable design of the core and headers. A simplified one-dimensional steady state model for the PHE is developed including the impact of surface roughness from the AM process. A process-based cost model is used to determine the tradeoff between thermofluidic design and manufacturing cost. A parametric study is performed using the thermo-fluidic and cost models to determine the set of geometrical and flow variables that result in high power density and low cost, while restricting the pressure drop on the sCO2 side to less than 2% of line pressure. Flow rates of MS and sCO2 were varied over heat capacity rate ratios ranging from 0.2 to 1. Results indicate that it is possible to design a low-pressure drop AM PHE with an effectiveness of 90% and a power density in excess of 10 MW/m3 (including headers). Fabrication of representative nickel superalloy specimens are shown to demonstrate that low-porosity parts with the requisite dimensional tolerance of PHE core can be generated.

14 SOLAR ENERGY↗

Combining synchrotron X-ray diffraction, mechanistic modeling and machine learning for in situ subsurface temperature quantification during laser melting

Laser melting, such as that encountered during additive manufacturing, produces extreme gradients of temperature in both space and time, which in turn influence microstructural development in the material. Qualification and model validation of the process itself and the resulting material necessitate the ability to characterize these temperature fields. However, well established means to directly probe the material temperature below the surface of an alloy while it is being processed are limited. To address this gap in characterization capabilities, a novel means is presented to extract subsurface temperature-distribution metrics, with uncertainty, from in situ synchrotron X-ray diffraction measurements to provide quantitative temperature evolution data during laser melting. Temperature-distribution metrics are determined using Gaussian process regression supervised machine-learning surrogate models trained with a combination of mechanistic modeling (heat transfer and fluid flow) and X-ray diffraction simulation. The trained surrogate model uncertainties are found to range from 5 to 15% depending on the metric and current temperature. The surrogate models are then applied to experimental data to extract temperature metrics from an Inconel 625 nickel superalloy wall specimen during laser melting. The maximum temperatures of the solid phase in the diffraction volume through melting and cooling are found to reach the solidus temperature as expected, with the mean and minimum temperatures found to be several hundred degrees less. The extracted temperature metrics near melting are determined to be more accurate because of the lower relative levels of mechanical elastic strains. However, uncertainties for temperature metrics during cooling are increased due to the effects of thermomechanical stress.

36 MATERIALS SCIENCE↗

Low Cost HIP Fabrication of Advanced Power Cycle Components and PM/Wrought Inconel 740H Weld Development (Final Technical Report)

The objective of this Phase 1 project is to demonstrate the feasibility of structures and components for advanced fossil energy power cycle by fusion welding powder metallurgy (PM) based near net shape (NNS) hot isostatic pressing (HIP) Nickel superalloy Inconel 740H (IN740H) components to wrought IN740H components. The outcome of the project includes a prototype pipe elbow demonstration of the NNS HIP process using IN740H powder, an initial assessment of IN740H PM/wrought weldability, and a manufacturing and capital cost analysis of IN740H NNS HIP components for advanced ultra-super critical steam (AUSC) power plants. The anticipated value proposition of NNS HIP manufacturing is ~50% cost reduction of large complex components in AUSC or super-critical carbon dioxide (sCO2) power cycles. This document is a final technical report for the project, covering efforts conducted from October 2019 to June 2021.

20 FOSSIL-FUELED POWER PLANTS↗

High Throughput Computational Framework of Materials Properties for Extreme Environments

This project aims to establish a framework capable of efficiently predicting the properties of structural materials for service in harsh environments over a wide range of temperatures and over long periods of time. The approach is to develop and integrate high throughput first-principles calculations in combination with machine learning (ML) methods, perform high throughput CALPHAD (calculations of phase diagrams) modeling, and carry out finite element method (FEM) simulations. Relevant to high temperature service in fossil power system, nickel-based superalloys such as Inconel 740 and Haynes 282 as well as the associated (Ni-Cr-Co)-Al-C-Fe-Mn-Mo-Nb-Si-Ti system, were investigated. The present framework was built on the concept of phase-based property data, in which properties of individual phases are modeled as a function of internal and external independent variables. This project established an open-source infrastructure with the following capabilities: (1) High throughput implementation of first-principles calculations at finite temperatures and variable compositions using both accurate phonon calculations and the efficient Debye model for thermodynamic properties, elastic constants, diffusion coefficients, vacancy formation, stacking and twin faults, and dislocation mobility; i.e., using the developed code DFTTK; (2) Machine learning capabilities to predict the above properties so that the number of first-principles calculations can be significantly reduced; e.g., using the developed code SIPFENN; (3) High throughput CALPHAD modeling of the above properties as a function of temperature and composition using our unique capability based on ESPEI and PyCalphad; (4) New capabilities to predict the stress-strain behavior of individual phases; and (5) New models for tensile strength prediction in common FEM software with the crystal plasticity finite element simulations (CPFEM).

, Ni-based superalloys↗

Environmental Compatibility Issues for Ni-Based Alloys in Direct-Fired Supercritical CO2 Power Cycles

Direct-fired supercritical CO2 (sCO2) power cycles offer potential for high-efficiency power generation from natural gas and other fossil fuels with built-in carbon capture. Ni-based superalloys are the leading candidates for the hottest portions of these systems, where they must endure long-term exposure to high-temperature, high-pressure, high-velocity, impure CO2-rich environments. Herein we describe results of various experimental testing campaigns conduced at NETL showing that under such conditions, several simultaneously occurring degradation modes may be active including surface oxidation, alloy carburization, and oxide volatilization. It will be shown that the rates of degradation can be strongly affected by the alloy composition, impurities in the CO2, manufacturing method (wrought vs additive), and other factors. The influence of these factors in controlling alloy degradation are discussed in the context of potential compatibility issues for components in real sCO2 systems, such as compact heat exchangers. Finally, as a potential remedial measure, ongoing work involving protective coatings suitable for complex geometries is presented.

alloy oxidation↗

Near-Net-Shape HIP Manufacturing for sCO2 Turbomachinery Cost Reduction

sCO2 turbomachinery that operates above 650°C requires the use of γ' strengthened Ni-based superalloys, leading to high cost and barrier of market adoption. Near-net-shape (NNS) HIP manufacturing with 282® alloy powder is being developed for sCO2 turbine components, with a significant estimated cost reduction. Tensile, creep, low cycle fatigue properties of argon gas atomized and plasma atomized powders were evaluated and compared to sand cast HAYNES® 282®. While tensile strength and fatigue life outperformed sand cast material, a 10~25% debit in the creep stress capability was observed due to the fine grain size and presence of prior particle boundaries (PPBs). Finite element model calibrated by powder rheological properties accurately predicted the nonuniform shrinkage during HIP, providing HIP tooling design to achieve the target dimension. A 20 lbs. turbine nozzle ring was successfully demonstrated within 0.01 inch dimensional tolerance at the vanes. A 1700lbs. turbine casing with complex internal struts and manifolds was also demonstrated being close to the target dimension.

14 SOLAR ENERGY↗

Assessing the interfacial corrosion mechanism of Inconel 617 in chloride molten salt corrosion using multi-modal advanced characterization techniques

The United States Department of Energy (DOE) has committed to expanding the domestic clean energy portfolio in response to the rising challenges of energy security in the wake of climate change. Accordingly, the construction of a series of Generation IV reactor technologies are being demonstrated, including sodium-cooled, small modular, and molten chloride fast reactors (MCFRs). To date, there are no fully qualified structural materials for constructing MCFRs. A number of commercial structural alloys have been considered for the construction of MCFRs, including alloys from the Inconel and Hastelloy series. Informed qualification of structural materials for the construction of MCFRs in the future can only be ensured by expanding the current fundamental knowledgebase of information pertaining to material performance under environmental stressors relevant to operation of the reactor, including corrosion susceptibility. The purpose of this investigation is to illustrate how a correlative multi-modal electron microscopy characterization approach, including the novel application of focused-ion beam 3D reconstruction capabilities, can elucidate the corrosion mechanism of a candidate structural material Inconel 617 for MCFR in NaCl-MgCl 2 eutectic salt at 700°C for 1,000 h. Evidence of intergranular corrosion, Ni and Fe dealloying, and Cr-O enrichment along the grain boundary, which most likely corresponds to Cr 2 O 3 , is a phenomenon that has been documented in other Ni-based superalloys exposed to chloride molten salt systems. Additional corrosion products, including the formation of insoluble MgAl 2 O 4 , within the porous network produced by the salt attack is a novel observation. In addition, Mo 3 Si 5 and τ 2 precipitates are detected in the alloy bulk and are dissolved by the salt. Furthermore, the lack of detection of design γ' precipitates in Inconel 617 after 1,000 h could indicate that the molten salt corrosion mechanism has indirectly induced a phase transformation of Al 2 TiNi (τ 2 ) and Ni 3 (Al,Ti) (γ’) phase. This investigation provides a comprehensive understanding of molten salt corrosion mechanisms in a complex material system such as a commercial structural alloy for applications in MCFRs.

36 MATERIALS SCIENCE↗

Solid-State Transformation of an Additive Manufactured Inconel 625 Alloy at 700 °C

Inconel 625, a nickel-based superalloy, has drawn much attention in the emerging field of additive manufacturing (AM) because of its excellent weldability and resistance to hot cracking. The extreme processing condition of AM often introduces enormous residual stress (hundreds of MPa to GPa) in the as-fabricated parts, which requires stress-relief heat treatment to remove or reduce the internal stresses. Typical residual stress heat treatment for AM Inconel 625, conducted at 800 °C or 870 °C, introduces a substantial precipitation of the δ phase, a deleterious intermetallic phase. In this work, we used synchrotron-based in situ scattering and diffraction methods and ex situ electron microscopy to investigate the solid-state transformation of an AM Inconel 625 at 700 °C. Our results show that while the δ phase still precipitates from the matrix at this temperature, its precipitation rate and size at a given time are both smaller when compared with their counterparts during typical heat treatment temperatures of 800 °C and 870 °C. A comparison with thermodynamic modeling predictions elucidates these experimental findings. Our work provides the rigorous microstructural kinetics data required to explore the feasibility of a promising lower-temperature stress-relief heat treatment for AM Inconel 625. The combined methodology is readily extendable to investigate the solid-state transformation of other AM alloys.

36 MATERIALS SCIENCE↗

Study of the Printability, Microstructures, and Mechanical Performances of Laser Powder Bed Fusion Built Haynes 230

The nickel-based superalloy, Haynes 230 (H230), is widely used in high-temperature applications, e.g., heat exchangers, because of its excellent high-temperature mechanical properties and corrosion resistance. As of today, H230 is not yet in common use for 3D printing, i.e., metal additive manufacturing (AM), primarily because of its hot cracking tendency under fast solidification. The ability to additively fabricate components in H230 attracts many applications that require the additional advantages leveraged by adopting AM, e.g., higher design complexity and faster prototyping. In this study, we fabricated nearly fully dense H230 in a laser powder bed fusion (L-PBF) process through parameter optimization. The efforts revealed the optimal process space which could guide future fabrication of H230 in various metal powder bed fusion processes. The metallurgical analysis identified the cracking problem, which was resolved by increasing the pre-heat temperature from 80 °C to 200 °C. A finite element simulation suggested that the pre-heat temperature has limited impacts on the maximum stress experienced by each location during solidification. Additionally, the crack morphology and the microstructural features imply that solidification and liquation cracking are the more probable mechanisms. Both the room temperature tensile test and the creep tests under two conditions, (a) 760 °C and 100 MPa and (b) 816 °C and 121 MPa, confirmed that the AM H230 has properties comparable to its wrought counterpart. The fractography showed that the heat treatment (anneal at 1200 °C for 2 h, followed by water quench) balances the strength and the ductility, while the printing defects did not appreciably accelerate part failure.

14 SOLAR ENERGY↗