Search NASA⌕ Search

SEARCH · Search NASA

Results for “tensile behavior”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Failure mechanisms of 3-D woven SiC/SiC composites under tensile and flexural loading at room and elevated temperatures

Nicalon silicon carbide 3D yarn with silicon carbide matrix composites made through a chemical vapor infiltration (CVI) process were investigated under tensile and flexural loading at 23, 1200 and 1550 C in air. The effectiveness of a chemical vapor deposition (CVD) SiC surface coating was also evaluated in severe oxidizing environment. Acoustic emission sensors and in situ optical microscopy were used at room temperature to monitor the failure mechanisms. It is shown that the level of tensile stress at which nonlinear behavior begins is not drastically reduced at 1200 and 1550 C when composites were protected by a SiC surface coating. Extensive fiber pull-out was observed only in the 1550 C specimen. Similar behaviors were also found in flexural specimens.

Chulya, Abhisak↗

The Effect of Stabilization Treatments on Disk Alloy CH98

Gas turbine engines for future subsonic transports will probably have higher pressure ratios which will require nickelbase superalloy disks with 1300 to 1400 F temperature capability. Several advanced disk alloys are being developed to fill this need. One of these, CH98, is a promising candidate for gas turbine engines and is being studied in NASA s Advanced Subsonic Technology (AST) program. For large disks, residual stresses generated during quenching from solution heat treatments are often reduced by a stabilization heat treatment, in which the disk is heated to 1500 or 1600 F for several hours followed by a static air cool. The reduction in residual stress levels lessens distortion during machining of disks. However, previous work on CH98 has indicated that stabilization treatments can also decrease creep capability. In this study, a systematic variation of stabilization temperature and time was investigated to determine its effect on 1300 F tensile and, more importantly, creep behavior. Dwell crack growth rates were also measured for selected stabilization conditions. As these advanced disk alloys may be given a supersolvus solution or a subsolvus solution heat treatment for a given application, it was decided that both options would be studied.

Gayda, John↗

Advanced Ceramic Matrix Composites with Multifunctional and Hybrid Structures

Ceramic matrix composites are leading candidate materials for a number of applications in aeronautics, space, energy, and nuclear industries. Potential composite applications differ in their requirements for thickness. For example, many space applications such as "nozzle ramps" or "heat exchangers" require very thin (< 1 mm) structures whereas turbine blades would require very thick parts (> or = 1 cm). Little is known about the effect of thickness on stress-strain behavior or the elevated temperature tensile properties controlled by oxidation diffusion. In this study, composites consisting of woven Hi-Nicalon (trademark) fibers a carbon interphase and CVI SiC matrix were fabricated with different numbers of plies and thicknesses. The effect of thickness on matrix crack formation, matrix crack growth and diffusion kinetics will be discussed. In another approach, hybrid fiber-lay up concepts have been utilized to "alloy" desirable properties of different fiber types for mechanical properties, thermal stress management, and oxidation resistance. Such an approach has potential for the C(sub I)-SiC and SiC(sub f)-SiC composite systems. CVI SiC matrix composites with different stacking sequences of woven C fiber (T300) layers and woven SiC fiber (Hi-Nicalon (trademark)) layers were fabricated. The results will be compared to standard C fiber reinforced CVI SiC matrix and Hi-Nicalon reinforced CVI SiC matrix composites. In addition, shear properties of these composites at different temperatures will also be presented. Other design and implementation issues will be discussed along with advantages and benefits of using these materials for various components in high temperature applications.

Singh, Mrityunjay↗

Nicalon/siliconoxycarbide ceramic composites

A series of silsesquioxane copolymers was synthesized by acid hydrolysis and condensation of trimethoxysilanes of the form RSi(OCH3)3, where R = methyl or phenyl. By varying pH, water/methoxy and methyl/phenyl ratios, the molecular structure, polymer rheology and ceramic composition can be controlled. The polymers form an amorphous siliconoxycarbide on pyrolysis. Composites of Nicalon/siliconoxycarbide were fractured in four-point flexure and in tension to evaluate the influence of matrix composition, final fabrication temperature and use of filler on composite mode of failure, modulus, strain capability and strength. Incorporation of filler was found to increase matrix compressive strength. Employment of processing temperatures of 1375 to 1400 C enhanced strain to failure and reduced the tendency toward brittle fracture. Mixed mode (compression/shear and tension/shear) failures were observed in flexural samples processed to the higher temperatures, giving rise to nonlinear stress-strain curves. Tensile samples pyrolyzed to 1400 C showed linear-elastic behavior and failed by fracture of fiber bundles. Matrix material was found to be adherent to the fiber surface after failure. These results demonstrate the need for tensile testing to establish composite behavior.

Hurwitz, Frances I.↗

Flaw growth behavior in thick welded plates of 2219-T87 aluminum at room and cryogenic temperatures

Axial load fatigue and fracture tests were conducted on thick welded plates of 2219-T87 aluminum alloy to determine the tensile strength properties and the flaw growth behavior in electron beam, gas metal arc, and pulse current gas tungsten arc welds for plates 6.35 centimeters (2.5 in.) thick. The tests were conducted in room temperature air and in liquid nitrogen environments. Specimens were tested in both the as-welded and the aged after welding conditions. The experimental crack growth rate were correlated with theoretical crack growth rate predictions for semielliptical surface flaws.

Forman, R. G.↗

Evaluation of the Mechanical Properties of Electroslag Refined Fe-12Ni Alloys

Three Fe-12Ni alloys, individually alloyed with small amounts of V, Ti, and Al, were manufactured through different melting techniques, with special emphasis on electroslag remelting, in order to achieve different levels of metal purity and associated costs. The relative effectiveness of these melting techniques was evaluated from tensile and slow bend fracture toughness behavior at 25 C and -196 C after tempering the test specimens at various temperatures. The best melting procedure was vacuum induction melting (VIM) with or without electroslag remelting (ESR). VIM+ESR is the recommended procedure since ESR provides increased yield of plate product, a reduction of overall manufacturing costs and, depending on the alloy composition, improved tensile and fracture toughness properties.

Bhat, G. K.↗

Thermomechanical Behavior of Advanced SiC Fiber Multifilament Tows

In order to relate single fiber behavior to multiple fiber behavior in composites, fast-fracture tensile strength, creep, and stress-rupture studies were conducted on advanced SiC fiber multifilament tows in the temperature range from 20 to 1400 C in air as well as in inert environments. For conditions of small fiber creep (short times and low temperatures), the tow results of this study confirm the ability of limited single fiber data to model the strength behavior of multiple fibers in a bundle. For conditions of high creep (long times and high temperatures), further studies are needed to explain tow rupture behavior being better than average single fiber behavior.

Yun, Hee Mann↗

Copoly(Imide Siloxane) Abhesive Materials with Varied Siloxane Oligomer Length

Incorporation of PDMS moieties into a polyimide matrix lowered the surface energy resulting in enhanced adhesive interactions. Polyimide siloxane materials were generated using amine-terminated PDMS oligomers of different lengths to study changes in surface migration behavior, phase segregation, mechanical, thermal, and optical properties. These materials were characterized using contact angle goniometry, tensile testing, and differential scanning calorimetry. The surface migration behavior of the PDMS component depended upon the siloxane molecular weight as indicated by distinct relationships between PDMS chain length and advancing water contact angles. Similar correlations were observed for percent elongation values obtained from tensile testing, while the addition of PDMS reduced the modulus. High fidelity topographical modification via laser ablation patterning further reduced the polyimide siloxane surface energy. Initial particulate adhesion testing experiments demonstrated that polyimide siloxane materials exhibited greater abhesive interactions relative to their respective homopolyimides.

Wohl, Christopher J.↗

The fracture behavior of graphite/epoxy laminates

The results of uniaxial tensile tests conducted on a variety of graphite/epoxy laminates containing narrow rectangular slits and square or circular holes with various aspect ratios are discussed. The techniques used to study stable-crack or damage-zone growth - namely, birefringence coatings, COD gages, and microscopic observations are discussed. Initial and final-fracture modes are discussed as well as the effect of notch size and shape and laminate type on the fracture process. Characteristic lengths are calculated using the point, average and inherent flaw theories and comparisons with observations are discussed. Further, the effect of flaw geometry on stress states and deformations is assessed.

Yeow, Y. T.↗

Rate and time dependent failure of structural adhesives

Studies on two adhesives (Metlbond 1113 and 1113-2) identified as having important applications in the bonding of composite materials are presented. A testing program to ascertain stress-strain, strain-rate, time, yield, and/or failure behavior of these materials in bulk form using uniaxial tensile constant strain-rate, creep, and relaxation tests is described. The stress-strain behavior of each material is shown to be significantly rate dependent. A rate dependent stress whitening (crazing) phenomenon occurs prior to either yield or fracture. A region of linear elasticity, a region of viscoelasticity, and the onset of yielding are identified in the stress-strain behavior. The linear elastic limit and the yield point are shown to be rate dependent and agree well with an empirical equation proposed by Ludwik. A creep to failure phenomenon is shown to exist and is correlated with a delayed yield equation proposed by Crochet. Analytical predictions based on a modified Bingham model are shown to agree well with experimental stress-strain strain-rate data. Analytical predictions based on a modified Ramberg-Osgood equation are also shown for comparison purposes.

Brinson, H. F.↗

Development and Evaluation of Elastomeric Materials for Geothermal Applications

A material was formulated having about 250-350 psi tensile strength and 30-80 percent elongation at 260 C for at least 24 hours in simulated brine. The relationship between these laboratory test results and sealing performance in actual or simulated test conditions is not entirely clear; however, it is believed that no conventional formation or casing packer design is likely to perform well using these materials. The synthetic effort focused on high temperature block copolymers and development of curable polystyrene. Procedures were worked out for synthesizing these new materials. Initial results with heat-cured unfilled polystyrene 'gum' at 260 C indicate a tensile strength of about 50 psi. Cast films of the first sample of polyphenyl quinoxaline-polystyrene block copolymer, which has 'graft-block' structure consisting of a polystyrene chain with pendant polyphenyl quinoxaline groups, show elastomeric behavior in the required temperature range. Its tensile strength and elongation at 260 C were 220-350 psi and 18-36 percent, respectively. All of these materials also showed satisfactory hydrolytic stability.

Mueller, W. A.↗

Thermal treatment and mechanical properties of aluminum-2021

Mechanical properties, after thermal treatments, are summarized for sheet and plate of copper-rich, high-strength, heat-treatable aluminum-2021. The alloy is quench sensitive, quench rate and variations in aging affect corrosion behavior. Aging effects on yield strength, tensile strength, and elongation of sheet and plate are compared.

Brennecke, M. W.↗

Mechanical property determination of high conductivity metals and alloys

Pertinent mechanical properties of three high conductivity metals and alloys; namely, vacuum hot pressed grade S-200E beryllium, OFHC copper and beryllium-copper alloy no. 10 were determined. These materials were selected based on their possible use in rocket thrust chamber and nozzle hardware. They were procured in a form and condition similar to that which might be ordered for actual hardware fabrication. The mechanical properties measured include (1) tension and compression stress strain curves at constant strain rate (2) tensile and compressive creep, (3) tensile and compressive stress-relaxation behavior and (4) elastic properties. Tests were conducted over the temperature range of from 75 F to 1600 F. The resulting data is presented in both graphical and tabular form.

Harrod, D. L.↗

High temperature, low-cycle fatigue of copper-base alloys for rocket nozzles. Part 2: Strainrange partitioning and low-cycle fatigue results at 538 deg C

Low-cycle fatigue tests of 1/2 Hard AMZIRC Copper and NARloy Z were performed in argon at 538 C to determine partitioned strain range versus life relationships. Strain-controlled low-cycle fatigue tests of a Zr-Cr-Mg copper-base alloy were also performed. Strain ranges, lower than those employed in previous tests, were imposed in order to extend the fatigue life curve out to approximately 400,000 cycles. An experimental copper alloy and an experimental silver alloy were also studied. Tensile tests were performed in air at room temperature and in argon at 538 C. Strain-controlled low-cycle fatigue tests were performed at 538 C in argon to define the fatigue life over the regime from 300 to 3,000 cycles. For the silver alloy, three additional heat treatments were introduced, and a limited evaluation of the short-term tensile and low-cycle fatigue behavior at 538 C was performed.

Conway, J. B.↗

Studies of new perfluoroether elastomeric sealants

Channel and filleting sealants were developed successfully from cyano and diamidoxime terminated perfluoro alkylene ether prepolymers. The prepolymers were polymerized, formulated and tested. The polymers and/or formulations therefrom were evaluated as to their physical, mechanical and chemical properties (i.e., specific gravity, hardness, nonvolatile content, corrosion resistance, stress corrosion, pressure rupture resistance, low temperature flexibility, gap sealing efficiency, tensile strength and elongation, dynamic mechanical behavior, compression set, fuel resistance, thermal properties and processability). Other applications of the formulated polymrs and incorporation of the basic prepolymers into other polymeric systems were investigated. A cyano terminated perfluoro alkylene oxide triazine was formulated and partially evaluated. The channel sealant in its present formulation has excellent pressure rupture resistance and surpasses present MIL specifications before and after fuel and heat aging.

Basiulis, D. I.↗

Tensile buckling of advanced turboprops

Theoretical studies were conducted to determine analytically the tensile buckling of advanced propeller blades (turboprops) in centrifugal fields, as well as the effects of tensile buckling on other types of structural behavior, such as resonant frequencies and flutter. Theoretical studies were also conducted to establish the advantages of using high performance composite turboprops as compared to titanium. Results show that the vibration frequencies are not affected appreciably prior to 80 percent of the tensile speed. Some frequencies approach zero as the tensile buckling speed is approached. Composites provide a substantial advantage over titanium on a buckling speed to weight basis. Vibration modes change as the rotor speed is increased and substantial geometric coupling is present.

Chamis, C. C.↗

Design and fabrication of realistic adhesively bonded joints

Eighteen bonded joint test specimens representing three different designs of a composite wing chordwise bonded splice were designed and fabricated using current aircraft industry practices. Three types of joints (full wing laminate penetration, two side stepped; midthickness penetration, one side stepped; and partial penetration, scarfed) were analyzed using state of the art elastic joint analysis modified for plastic behavior of the adhesive. The static tensile fail load at room temperature was predicted to be: (1) 1026 kN/m (5860 1b/in) for the two side stepped joint; (2) 925 kN/m (5287 1b/in) for the one side stepped joint; and (3) 1330 kN/m (7600 1b/in) for the scarfed joint. All joints were designed to fail in the adhesive.

Shyprykevich, P.↗