At least 217 records · Page 12

AN INITIAL ASSESSMENT OF THE CREEP-RUPTURE STRENGTHS FOR WELDMENTS WITH ALLOY 800H BASE METAL AND ALLOY 617 FILLER METAL

In Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, Alloy 800H is qualified for elevated-temperature nuclear construction for temperatures up to 760°C (1,400°F) and a maximum service life of 300,000 hours. There are two permissible filler metals for Alloy 800H weldments specified in Division 5: ENiCrFe-2 (Alloy A) and ERNiCr-3 (Alloy 82). Low creep-rupture strengths of these weldments at the upper limits of the qualified temperatures and service lives may restrict the design envelope for elevated-temperature nuclear construction with Alloy 800H. As a result, an alternative filler metal is desired to improve the creep-rupture strengths of Alloy 800H weldments for the qualified temperatures and service lives. This work investigates an overmatched filler metal. Specifically, a weldment with Alloy 800H base metal and Alloy 617 filler metal fabricated by semiautomated gas tungsten arc welding is investigated. A scoping creep-rupture test program was conducted of cross-weld specimens at temperatures ranging from 750 to 1,000°C (1,292 to 1,832°F). Preliminary results on the creep-rupture strengths of the Alloy 800H weldment with Alloy 617 filler metal do not show significant improvement compared to the filler metals currently qualified in Division 5 for Alloy 800H weldments. Consequently, work is in progress to investigate a matching filler metal.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Novel Dissimilar Joints Between Alloy 800H and 2.25%Cr and 1%Mo Steel

Dissimilar metal joints between ferritic steels and nickel base alloys are currently fabricated using conventional arc welding processes with selected filler metal combinations. The dissimilar metal joints contain abrupt changes in composition over a relatively small distance. Many years of service at elevated temperatures has shown that these welds are susceptible to creep and creep fatigue failures. The primary mechanism for these creep failures involves carbon diffusion from the ferritic steel to the nickel base alloy. As a result, a carbon depleted zone is created that contains very few stable carbides. This work used additive manufacturing (AM) technologies as a highly controllable means for reducing carbon migration through theoretically designed, compositionally graded transition joints guided by appropriate thermodynamic, kinetic and heat transfer and fluid flow modeling. The contents of the report include the objectives and tasks set forth by the PI and collaborators, major technical accomplishments throughout the research and additional details in the form of technical publications resulting from the NEUP grant and reports from the collaborating university and national laboratory.

36 MATERIALS SCIENCE↗

Experimental and Computational Studies of Stress Corrosion Cracking of Alloys 308/309 and 82/182 Weldments in Corrosive and Radiation Environment

The goal of the project was to determine factors that influence SCC and IASCC in weldments found in LWR nuclear power plants. We focused on a SA508-304L SS weldment fabricated by EPRI using gas tungsten arc welding and used an aggressive BWR normal water chemistry (NWC) immersion environment. This weldment used 309L butter and 308L groove filler material. The microstructure of the 309L butter was non-uniform, exhibiting a 20–30μm thick martensitic layer closest to the SA508 interface, a 1–4 mm thick single γ austenite phase dilution zone, and a γ–δ duplex region extending to the 308L groove filler. The 308L groove filler had an entirely γ–δ duplex microstructure. Two approximately 1-inch thick 304L and SA508 plates approximately 12 by 6 square inches were joined using standard nuclear grade welding techniques. This included a post weld heat treatment of the 309L butter after application, a 0.32 cm fit-up root opening, and 57 bead lines of 308L groove filler applied in 18 layers. A 60 degree weld bevel angle was used and the 309L butter was 1.5 cm thick. Displacement cascade damage was induced using proton irradiation at the Michigan Ion Beam Laboratory. The incident proton energy was 2 MeV, the sample temperature was 360 ºC, and the calculated dpa value at 10 μm (60% of the Bragg peak depth of ~18 μm) was 5 dpa using the quick Kinchin-Pease model. Proton irradiation to this damage level required approximately 125 hours of beam time. Two types of samples were irradiated, tensile specimens and TEM bars. Samples were selected from all regions of the weldment, including the SA508-309L butter interface, the 309L-308L interface, and 308L-304L interface. The stainless steel alloys (304L, 308L, and 309L) within the heat affected zone are characterized by a duplex skeletal morphology of δ-ferrite and γ-austenite resulting from the recrystallization associated with weld fabrication. Approximately 7 to 8 mm of length along the specimen was irradiated. The gauge volume surfaces were mechanically polished and then electro-polished to remove mechanical damage from the mechanical polishing step prior to irradiation. Immersion tests were performed in a recirculating autoclave under BWR NWC conditions (2000 ppb wt. dissolved oxygen, neutral pH, 288 ºC, 10 MPa, and inlet water conductivity <100 nS/cm) to accelerate corrosion. Constant strain rate tests were performed either to failure or to approximately 5% strain. Strain rates of 10 -7 to 10 -6 mm/mm/s were used and typical immersion testing required four to six weeks to achieve failure or strains near 5%. Analysis primarily used advanced electron microscopy techniques of FIB lift out specimens.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

CHARACTERIZATION OF FATIGUE BEHAVIORS OF NOTCHED 316L DED AM SPECIMENS

ASME Codification of Additive Manufacturing • Integration of AM into ASME Codes and Standards • The ASME goal is to have AM requirements in ASME Code Cases preceding the 2025 Edition. • The ASME Special Committee on AM has drafted criteria for two Code Cases for Additive Manufacturing. • AM Construction of Pressure Equipment using the Direct Energy Deposition Process with Wire Feedstock. • Includes Gas Metal Arc Welding. • Time-independent material properties. • Status - Criteria endorsed by AM Committee. • AM Construction of Pressure Equipment using the Powder Bed Fusion AM Process. • Includes Laser and Electron Beam Energy Sources. • Austenitic and Nonferrous materials. • Time-independent material properties. • Status – Approval ballot circulating to the AM Committee.

Krentz, Timothy M.↗

Fabrication and Testing of Solid-Solution Strengthened Corrosion Resistant Alloys For Service in Molten Fluoride Environments

The demand for higher system thermal efficiencies requires the operation of power generation cycles and heat conversion systems at progressively higher temperatures. As the system operating temperature increases, existing materials may not provide adequate mechanical properties or environmental compatibility or both. There is an increasing commercial interest in the development and deployment of liquid-fueled Molten Salt Reactors (MSRs). Hastelloy®N, the highest performing candidate MSR structural alloy, is not capable of operations at temperatures above 700°C, thus limiting the performance of these systems. Using an Integrated Computational Materials Engineering (ICME)-approach and small laboratory scale heats, ORNL developed a class of patented alloys covered by U.S. Patent 9, 435, 011 B2, “Creep-resistant, Cobalt-free alloys for high temperature, liquid-salt heat exchanger systems,” similar to Hastelloy®N in that they are primarily solid solution strengthened. In contrast to precipitation strengthened alloys, the microstructure of solid solution alloys and hence the high temperature mechanical properties are stable for extended periods of time allowing long reactor operating life. The new alloys have shown to possess good resistance to liquid fluorides at temperatures up to 850°C and have significantly improved creep properties when compared to Hastelloy®N. The purpose of the CRADA project was for ORNL to collaborate with Haynes International- a materials producer, MetalTek International- a foundry, and Kairos Power – an advanced reactor developer – to scale-up selected alloys, evaluate their properties, and identify one solid solution strengthened alloy that can meet the property requirements for the reactor being developed by Kairos Power and other similar liquid fluoride-salt cooled reactors. As part of the project, eight alloys were down-selected and fabricated in larger industrial scale heats by Haynes International. Resistance to molten salt was evaluated in flowing FLiNaK and FLiBe by Kairos Power using their Rotating Cage Loop (RCL) system. Accounting for iron deposition during these tests, the new alloys displayed very low net mass change showing excellent corrosion performance in molten salt. Creep properties evaluated at ORNL were found to be better than that of Hastelloy®N and 316 stainless steel. Long-term stabilities of the alloys evaluated by Haynes International showed that these alloys have excellent thermal stability in the temperature range 704.4-815.6°C, with the change in strength and ductility being less than 10-15% after a 4000-hour exposure at 815.6°C. Autogenously Gas Tungsten Arc Welding (GTAW) welded samples showed less than 10% change in yield strength / ultimate tensile strength / total elongation compared to the basemetal, indicating that the alloys have excellent weldability. Three parts were successfully investment-cast using one alloy with very little voiding showing feasibility of fabricating parts using the casting process. This project enabled extensive interaction between the material producer Haynes International, casting supplier MetalTek, and reactor developer Kairos Power. This facilitated testing of materials and components produced using the newly developed alloys by the end-user. This allowed the generation of critical dataset required for down-selection of a few promising alloys for further development. This data is also currently being shared with other reactor designers for them to evaluate the suitability of this alloy for their reactor design. The availability of this alloy will ultimately enable the design and development and deployment of MSRs with increased temperature of operation and thus, improved efficiencies.

99 GENERAL AND MISCELLANEOUS↗

Fabrication and Testing of Solid-Solution Strengthened Corrosion Resistant Alloys For Service in Molten Fluoride Environments

The demand for higher system thermal efficiencies requires the operation of power generation cycles and heat conversion systems at progressively higher temperatures. As the system operating temperature increases, existing materials may not provide adequate mechanical properties or environmental compatibility or both. There is an increasing commercial interest in the development and deployment of liquid-fueled Molten Salt Reactors (MSRs). Hastelloy®N, the highest performing candidate MSR structural alloy, is not capable of operations at temperatures above 700°C, thus limiting the performance of these systems. Using an Integrated Computational Materials Engineering (ICME)-approach and small laboratory scale heats, ORNL developed a class of patented alloys covered by U.S. Patent 9,435,011 B2, “Creep-resistant, Cobalt-free alloys for high temperature, liquid-salt heat exchanger systems,” similar to Hastelloy®N in that they are primarily solid solution strengthened. In contrast to precipitation strengthened alloys, the microstructure of solid solution alloys and hence the high temperature mechanical properties are stable for extended periods of time allowing long reactor operating life. The new alloys have shown to possess good resistance to liquid fluorides at temperatures up to 850°C and have significantly improved creep properties when compared to Hastelloy®N. The purpose of the CRADA project was for ORNL to collaborate with Haynes International- a materials producer, MetalTek International- a foundry, and Kairos Power – an advanced reactor developer – to scale-up selected alloys, evaluate their properties, and identify one solid solution strengthened alloy that can meet the property requirements for the reactor being developed by Kairos Power and other similar liquid fluoride-salt cooled reactors. As part of the project, eight alloys were down-selected and fabricated in larger industrial scale heats by Haynes International. Resistance to molten salt was evaluated in flowing FLiNaK and FLiBe by Kairos Power using their Rotating Cage Loop (RCL) system. Accounting for iron deposition during these tests, the new alloys displayed very low net mass change showing excellent corrosion performance in molten salt. Creep properties evaluated at ORNL were found to be better than that of Hastelloy®N and 316 stainless steel. Long-term stabilities of the alloys evaluated by Haynes International showed that these alloys have excellent thermal stability in the temperature range 704.4-815.6°C, with the change in strength and ductility being less than 10-15% after a 4000-hour exposure at 815.6°C. Autogenously Gas Tungsten Arc Welding (GTAW) welded samples showed less than 10% change in yield strength / ultimate tensile strength / total elongation compared to the basemetal, indicating that the alloys have excellent weldability. Three parts were successfully investment-cast using one alloy with very little voiding showing feasibility of fabricating parts using the casting process. This project enabled extensive interaction between the material producer Haynes International, casting supplier MetalTek, and reactor developer Kairos Power. This facilitated testing of materials and components produced using the newly developed alloys by the end-user. This allowed the generation of critical dataset required for down-selection of a few promising alloys for further development. This data is also currently being shared with other reactor designers for them to evaluate the suitability of this alloy for their reactor design. The availability of this alloy will ultimately enable the design and development and deployment of MSRs with increased temperature of operation and thus, improved efficiencies.

36 MATERIALS SCIENCE↗

Mitigating Scatter in Mechanical Properties in AISI 410 Fabricated via Arc-Based Additive Manufacturing Process

Wire-based metal additive manufacturing utilizes the ability of additive manufacturing to fabricate complex geometries with high deposition rates (above 7 kg/h), thus finding applications in the fabrication of large-scale components, such as stamping dies. Traditionally, the workhorse materials for stamping dies have been martensitic steels. However, the complex thermal gyrations induced during additive manufacturing can cause the evolution of an inhomogeneous microstructure, which leads to a significant scatter in the mechanical properties, especially the toughness. Therefore, to understand these phenomena, arc-based additive AISI 410 samples were fabricated using robotic gas metal arc welding (GMAW) and were subjected to a detailed characterization campaign. The results show significant scatter in the tensile properties as well as Charpy V-notch impact toughness data, which was then correlated to the microstructural heterogeneity and delta (δ) ferrite formation. Post-processing (austenitizing and tempering) treatments were developed and an ~70% reduction in the scatter of tensile data and a four-times improvement in the toughness were obtained. The changes in mechanical properties were rationalized based on the microstructure evolution during additive manufacturing. Based on these, an outline to tailor the composition of “printable” steels for tooling with isotropic and uniform mechanical properties is presented and discussed.

36 MATERIALS SCIENCE↗

Corrosion Resistance of 309L Stainless Steel Claddings on Carbon Steel Produced with Wire-Fed Directed Energy Deposition

Additive manufacturing (AM) tools are capable of applying overlay austenitic stainless steel (SS) claddings to carbon steel components. The benefits of this approach over arc welding include a smaller heat-affected zone, residual stress reduction, and material savings. In particular, wire-directed energy deposition is a suitable technique because of its low material cost and high rate of production compared to other AM methods. However, metallurgical variations in composition, phase fraction, and microsegregation can potentially influence the corrosion behavior of such claddings. In this work, 309L SS is clad on carbon steel substrates and electrochemical methods are used to measure their general and pitting corrosion resistance in simulated marine environments (3.5 wt% NaCl solutions). Two-layer claddings are fabricated with four laser powers to understand the effects of bulk chemical composition, austenite/δ-ferrite phase fractions, and individual phase compositions on corrosion behavior. The two-layer claddings are compared to a single-layer cladding, wrought 304 SS, and the carbon steel substrate for a comprehensive assessment of corrosion performance. The two-layer claddings are remarkably resistant to general corrosion in the 3.5 wt% NaCl environment because of their high Cr content (21.6 wt% to 23.3 wt% Cr). The single-layer cladding exhibits localized corrosion at unmixed Fe-rich peninsulas that originate at the dissimilar metal boundary and protrude into the first cladding layer. All two-layer claddings possess higher pitting corrosion resistance than wrought 304 SS, demonstrating their effectiveness as a corrosion-resistant barrier. Here, the pitting corrosion resistance is superior for claddings made with lower laser powers, due to low dilution and greater δ-ferrite contents.

36 MATERIALS SCIENCE↗

AMVOS: Additive Manufacturing Video Object Segmentation Dataset

This dataset provides labeled video frames from four additive manufacturing (AM) processes for video object segmentation (VOS) tasks. It contains 90 video segments comprising 900 individually annotated frames across five AM datasets: laser hot-wire directed energy deposition (LHW-DED), tungsten inert gas wire arc additive manufacturing (TIG-WAAM), plasma arc welding (PAW), visible-light polymer extrusion (visPolymer), and near-infrared polymer extrusion (irPolymer). Each video segment consists of 10 contiguous frames with corresponding pixel-level object instance annotations. Depending on the process, two of four object classes are labeled per frame: Melt Pool, Feed Wire, Nozzle, or Material. Raw frames are provided as .jpg files and annotations as palettized .png files. The dataset follows the directory structure of established VOS benchmarks (DAVIS, YouTube-VOS, MOSE), enabling direct integration into VOS model training and evaluation pipelines for foundation model fine-tuning, domain adaptation, or zero-shot performance benchmarking. Data was collected at Oak Ridge National Laboratory's Manufacturing Demonstration Facility.

Wetzel, Jon [ORNL]↗

Practical Challenges and Failure Modes During Fabrication of Haynes 230 Micro-Pin Solar Receivers for High Temperature Supercritical Carbon Dioxide Operation

Printed circuit heat exchangers (PCHX) fabricated from high nickel alloys have shown promise as primary heat exchangers, recuperators, and solar receivers for high temperature and pressure supercritical carbon dioxide power cycles. There are numerous challenges in fabricating these devices including forming channel features, joining via diffusion or transient liquid phase bonding, and brazing/welding of headers. Commercial entities are understandably hesitant to share propriety best practices, and both commercial and non-commercial entities working on these components tend not to publically share failures and mistakes. However, sharing of this information could prevent similar costly errors and further the understanding of the coupled manufacturing, materials and mechanics issues in creating these components. Thus, in this paper, we document the challenges, failures, and mitigation methods uncovered in fabrication of prototype micro-pin based solar thermal receivers constructed of Haynes 230 and fabricated through a combination of photochemical machining (PCM), wire electrical discharge machining (EDM), transient liquid phase (TLP) bonding, vacuum brazing, and gas tungsten arc welding (GTAW). The receiver is designed to absorb concentrated solar fluxes greater than 140 W cm-2, while heating supercritical carbon dioxide from 550 °C to 720 °C at a pressure of 20 MPa to 25 MPa. The prototype receiver consists of a thin (~ 450 µm), Haynes 230 coversheet bonded to a 15 cm × 15 cm Haynes 230 micro-pin plate. The pieces are joined using a TLP bonding process with a nickel-phosphorus interlayer. Prior to bonding, micro-pins with height ~150 µm and diameter 300 µm are fabricated using PCM in the plate, and through slot features are made using wire EDM. Finally, flow headers are joined to the microchannel plate through a combination of vacuum brazing and GTAW. During hydrostatic proof testing, the prototype device failed when the coversheet delaminated from the pin array at a pressure of 290 bar. A failure analysis including scanning electron microscopy (SEM) to view failure sites and energy-dispersive X-ray spectroscopy (EDS) to evaluate elemental analysis of the failed areas was conducted. The failure modes can be broadly categorized as (1) failures potentially relating to reliquification of the transient liquid phase bonds between the micro-pins plate and coversheet during post-processing, (2) failures related to manufacturing defects, and (3) failures attributed to design.

14 SOLAR ENERGY↗

GCR: Development of Improved Alloy 800H Weldment

In Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, Alloy 800H is qualified for elevated-temperature nuclear construction for temperatures up to 760°C (1400°F) and a maximum service life of 300,000 hours. There are two permissible filler metals for Alloy 800H weldments specified in Division 5: ENiCrFe-2 (Alloy A) and ERNiCr-3 (Alloy 82). Low creep-rupture strengths of these weldments at the upper limits of the qualified temperatures and service lives may restrict the design envelope for elevated-temperature nuclear construction with Alloy 800H. As a result, an alternative filler metal is desired to improve the creep-rupture strengths of Alloy 800H weldments for the qualified temperatures and service lives. This work investigates an overmatched filler metal. Specifically, a weldment with Alloy 800H base metal and Alloy 617 filler metal fabricated by semiautomated gas tungsten arc welding is investigated. A scoping creep-rupture test program was conducted of cross-weld specimens at temperatures ranging from 750 to 1000°C (1292 to 1832°F). Preliminary results on the creep-rupture strengths of the Alloy 800H weldment with an Alloy 617 filler metal do not show significant improvement compared to the filler metals currently qualified in Division 5 for Alloy 800H weldments. Consequently, work is in progress to investigate a matching filler metal, UTP A 2133 Mn.

36 MATERIALS SCIENCE↗

Materials for Advanced Ultra-Supercritical (AUSC) Steam Turbines – AUSC Component Demonstration

The work by the United States Department of Energy (U.S. DOE)/Ohio Coal Development Office (OCDO) Advanced Ultra-Supercritical (AUSC) Steam Boiler and Turbine Materials Consortia from 2001 through September 2015 was primarily focused on lab scale and pilot scale materials testing. The field testing included air-cooled probes and steam-cooled “loops” that were installed into existing utility boilers to gain exposure of these materials to realistic conditions of high temperature and corrosion due to the constituents in the coal ash. Successful research and development resulted in identification of metallic alloy materials and fabrication processes suited for power generation applications with metal temperatures up to approximately 1472°F (800°C). These materials or alloys have shown, in extensive laboratory tests and shop fabrication studies, to have excellent applicability for high-efficiency low CO2 transformational power generation technologies. However, as valuable as these material field tests have been for obtaining information, their scale is significantly below that required to minimize the risk associated with a power company building a multi-billion-dollar AUSC power plant. To decrease the identified risk barriers to full-scale implementation of these advanced materials, the U.S. DOE/OCDO AUSC Steam Boiler and Turbine Materials Consortia identified the key areas of the technology that need to be tested at a larger scale. Based upon the recommendations and outcome of a Consortia-sponsored workshop with the U.S.’s leading utilities, a Component Test (ComTest) Program for AUSC was proposed. The AUSC ComTest program would define materials performance requirements, plan for overall advanced system integration, design critical component tests, fabricate components for testing from advanced materials, and carry out the tests. A Pre-FEED evaluation of the test facility including the evaluation of three potential sites has been completed and previously reported. This report describes the Front-End Engineering Design (FEED), Detailed Engineering and the Environmental Assessment of the ComTest project. A significant amount of work was accomplished during Phase 1 to identity the components, as well as the component size, that would be manufactured from advanced alloys such as INCONEL 740H or HAYNES 282 alloys. Pathways to supply these components for ComTest have been identified as well as any further development that would be required. Every project of this nature has challenges and this project was no exception. The greatest challenge has been the project cost. Largely due to the infrastructure and balance of plant equipment upgrades required for Youngstown Thermal, the estimated project cost for the “base case” project was greater than originally budgeted. The project team spent a significant amount of time exploring opportunities for reducing the project cost. These options included: • Youngstown Thermal was exploring building a Combined Heat and Power (CHP) unit at their facility. The Youngstown Thermal staff, supported by Thermal Engineering Group, worked with the project team to determine whether it was economically desirable to supply ComTest with steam and other utilities, which would be supplied by the CHP project. • The project team also evaluated opportunities to optimize the project scope to reduce cost, such as reducing project scope by eliminating the Superheater Outlet Header test. • Southern Company had offered two sites as possible host locations for ComTest. Both sites had infrastructure in place such as steam from an existing unit, natural gas, cooling water and ample electrical power that would be required to be added at the Youngstown Thermal site. Utilizing this existing infrastructure could reduce the project cost. An additional project challenge was the departure of Babcock and Wilcox from the project in September 2016. This project setback was overcome by GE Power’s willingness to assume the design of the ComTest superheater. Since the project could not proceed without the superheater, this was a very positive project development. The merger of the GE Power and Alstom Power steam turbine divisions created synergies leading to the conclusion that instead of building a small-scale turbine, a more practical and useful endeavor would be to validate the manufacturing technology and supplier readiness for fabricating and machining full scale steam turbine components. Consequently, in March 2017, GE Power decided that a steam turbine test would not be necessary as part of the ComTest demonstration. Removing the operational testing of the steam turbine from ComTest further reduced the total project cost. Additionally, there was an opportunity to move ComTest from Youngstown Thermal to one of the Southern Company sites and operate ComTest at supercritical steam conditions and test the steam turbine main stop/control valve at a temperature and pressure that would be representative of the conditions of a high pressure steam turbine inlet valve. The steam could also possibly be returned to the host boiler so there would be no economic penalty of using this steam for ComTest. Relocating the project could further reduce the project cost due to the infrastructure already in place, including high pressure natural gas and cooling water, and the potential for heat integration, allowing a reduction of operating costs. Due to these potential cost reductions, it was decided to move the project away from Youngstown Thermal in March 2017. As integrating ComTest at the Southern Company site was explored, an issue was raised regarding the integration of the ComTest cycle with the plant steam cycle. Steam would be supplied to ComTest at nominally ~3865 psia and 775°F. The steam would be heated with natural gas to 1400°F for the valve test and then cooled to 1000°F so that the steam would be returned to the host boiler at the same conditions as their high pressure steam turbine inlet. However, there were concerns raised that the addition of the energy (natural gas) to the steam could trigger a New Source Review on the unit. Southern Company did not want ComTest to cause this review, so condensing all of the steam exiting ComTest and returning it to the host steam cycle as condensate was explored to insure there would be no implication that ComTest was adding energy to the host plant’s steam cycle. Ultimately, Southern Company decided that they wanted to “decouple” ComTest from the operating unit, making ComTest self-supporting, similar to the Youngstown Thermal “base case.” Without the steam turbine, the project team reached a consensus that operating the ComTest Superheater and steam turbine valves at the typical pressure of a package boiler (~1000 psig) would not generate enough useful technical information to justify the cost of the test. Therefore, it was decided in the December 2017 project quarterly meeting to cancel the operational phase of ComTest. Throughout the engineering phase of ComTest, manufacturing and supply chain challenges were identified. When GE Power recommended dropping the steam turbine test from ComTest, they identified many important manufacturing issues that should be evaluated and demonstrated. Other challenges had been raised by the GE Power group designing the superheater as well as those engineering components such as pressure relief and steam turbine bypass valves. In the December 2017 meeting, the project team decided that it was more beneficial to the AUSC technology to pursue these manufacturing and supply chain issues as Phase 2 of the ComTest project. This report is organized in the following manner: • Section 2 discusses the ComTest project background and organization. • Section 3 discussed project management. • Section 4 discusses the design of the ComTest AUSC components – the Superheater, steam turbine and Superheater Outlet Header. • Section 5 discusses the implementation of ComTest at Youngstown Thermal and the Southern Company site. • Section 6 discusses the development of the AUSC Supply Chain • Section 7 discusses the recommended plan for Phase 2 of ComTest

01 COAL, LIGNITE, AND PEAT↗

Nondestructive ultrasonic characterization of a triple-weld-bead wire arc additively manufactured ER70S-6 S-curved wall

Understanding build-scale microstructural variation in wire arc additive manufacturing (WAAM) of low-carbon steels is essential for ensuring consistent structure–property relationships throughout large components. Conventional destructive characterization techniques, such as scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD), are time-intensive and limited to localized regions, making comprehensive evaluation of large WAAM structures challenging. In this study, a nondestructive ultrasonic approach was employed to characterize a 252 mm tall ER70S-6 S-curved WAAM wall produced using a triple-bead deposition strategy. Optical and SEM analysis revealed a repeating dual-region microstructure consisting of uniform polygonal ferrite at melt pool centers and heterogeneous ferrite with coarse and fine grains near melt pool boundaries, attributed to cyclic thermal conditions. Longitudinal ultrasonic backscatter imaging was used to evaluate the continuity of this periodicity along the full build height. The ultrasonic response exhibited a consistent repeating pattern that correlated with the observed layer-wise microstructural variation. X-ray computed tomography confirmed the absence of detectable porosity, indicating that ultrasonic contrast is primarily governed by grain morphology. Overall, the results indicate that longitudinal backscatter ultrasound is a promising nondestructive characterization technique for validating microstructural variations along the s-curved WAAM wall, with significant potential for microstructure optimization and process control.

36 MATERIALS SCIENCE↗

Fluid Flow Phenomena during Welding

MOLTEN WELD POOLS are dynamic. Liquid in the weld pool in acted on by several strong forces, which can result in high-velocity fluid motion. Fluid flow velocities exceeding 1 m/s (3.3 ft/s) have been observed in gas tungsten arc (GTA) welds under ordinary welding conditions, and higher velocities have been measured in submerged arc welds. Fluid flow is important because it affects weld shape and is related to the formation of a variety of weld defects. Moving liquid transports heat and often dominates heat transport in the weld pool. Because heat transport by mass flow depends on the direction and speed of fluid motion, weld pool shape can differ dramatically from that predicted by conductive heat flow. Temperature gradients are also altered by fluid flow, which can affect weld microstructure. A number of defects in GTA welds have been attributed to fluid flow or changes in fluid flow, including lack of penetration, top bead roughness, humped beads, finger penetration, and undercutting. Instabilities in the liquid film around the keyhole in electron beam and laser welds are responsible for the uneven penetration (spiking) characteristic of these types of welds.

36 MATERIALS SCIENCE↗

Non-Intrusive Load Monitoring of EBW Processes A Second Study [Slides]

The Objective is to Determine if induced off-nominal welding disturbances: (1) Beam arc out (weld on high vapor pressure aluminum plate); (2) Pulsed beam voltage; (3) Pulsed beam current; and (4) Pulsed beam focus current can be observed in the input power to the high-voltage cabinet powering the EB gun, ie Non-Instrusive Load Monitoring (NILM).

36 MATERIALS SCIENCE↗

Transition of creep damage region in dissimilar welds between Inconel 740H Ni-based superalloy and P92 ferritic/martensitic steel

Highlights: • The fresh martensite formed in P92-sided CGHAZ during PWHT due to high Ni content. • Transition from type I to type IV cracking was observed with increasing temperature. • Creep damaged area changed depending on the dominant creep mechanism. • The transition value of Larson-Miller parameter would be within 25,063–26,168. - Abstract: Characterization of microstructures and creep fracture characteristics of dissimilar welds between Ni-based Inconel 740H superalloy and ferritic/martensitic P92 steel has been investigated. The welds were produced by shielded metal arc (SMA) welding process with the AWS A5.11 Class ENiCrFe-3 filler metal, commonly known as Inconel 182 superalloy. Postweld heat treatment (PWHT) at 760 °C for 4 h was conducted to temper the martensite in heat-affected zone (HAZ) of P92 and to form γ′ strengthener in Inconel 740H. The deposited Inconel 182 austenitic weld metal had a columnar microstructure, and grew epitaxially from the Inconel 740H base metal. The weld interface between P92 and weld metal was characterized by the discrete line with a minimal inter-diffusion, where the fresh untempered martensite was found to be formed during PWHT due to higher Ni contents diffused from Inconel 182 into P92. The P92 base metal and Inconel 182 weld metal displayed low hardness values (~240 Hv), and the sharp hardness increase was detected at coarse-grained HAZ of P92 while the hardness minimum occurred at the fine-grained HAZ (FGHAZ). Fracture location after creep was found to shift from the P92-sided fusion line to the FGHAZ of P92 with increasing creep temperature. The carbon migration from the P92 into the weld metal was not significant at lower creep temperature (600 °C), where the crack initiation at the P92-sided fusion line appeared to be related with a significant strain incompatibility across the fusion line. At both 650 °C and 700 °C where diffusion-controlled creep was more pronounced, the type IV cracking was observed. This may be attributed to the strain localization at the weak grain boundaries of FGHAZ due to the smaller grain size as well as the lack of grain boundary strengthening by carbides.

36 MATERIALS SCIENCE↗

Methodology for Estimating Thermal and Neutron Embrittlement of Austenitic Stainless Steel Welds During Service in Light Water Reactors

The effect of thermal aging on the degradation of fracture toughness and Charpy-impact properties of austenitic stainless steel (SS) welds has been characterized at reactor temperatures. The solidification behavior and the distribution and morphology of the ferrite phase in SS welds are described. Thermal aging of the welds results in moderate decreases in Charpy-impact strength and fracture toughness. The upper-shelf Charpy-impact energy of aged welds decreases by 50–80 J/cm2. The decrease in fracture toughness J-R curve, or JIc is relatively small. Thermal aging has minimal effect on the tensile strength. The fracture properties of SS welds are insensitive to filler metal; the welding process has a significant effect. The large variability in the data makes it difficult to establish the effect of the welding process on fracture properties of SS welds. Consequently, the approach used for evaluating thermal and neutron embrittlement of austenitic SS welds relies on establishing a lower-bound fracture toughness J-R curve for unaged and aged, and non-irradiated and irradiated, SS welds. The existing fracture toughness J-R curve data for SS welds have been reviewed and evaluated to define lower-bound J-R curve for submerged arc (SA)/shielded metal arc (SMA)/manual metal arc (MMA) welds and gas tungsten arc (GTA)/tungsten inert gas (TIG) welds in the unaged and aged conditions. At reactor temperatures, the fracture toughness of GTA/TIG welds is a factor of about 2.3 higher than that of SA/SMA/MMA welds. Thermal aging decreases the fracture toughness by about 20%. The potential combined effects of thermal and neutron embrittlement of austenitic SS welds are also described. Lower-bound curves are presented that define the change in coefficient C and exponent n of the power-law J-R curve and the JIc value for SS welds as a function of neutron dose. The potential effects of reactor coolant environment on the fracture toughness of austenitic SS welds are also discussed.

Chopra, O. K.↗

LDRD 19A42-015, Multi-Wire Arc Additive Manufacturing

Additive manufacturing (AM) techniques can efficiently and cost-effectively fabricate components with both geometrical and compositional complexities, where functionally-graded compositions in a component allow multiple service requirements to be simultaneously addressed, such as corrosion and high temperature structural requirements. High cost alloy compositions need only be deposited in local areas where they are needed. A multi-wire arc additive manufacturing (m-WAAM) system was developed to enable functionally-graded, additively manufactured complex structures. The m-WAAM system utilizes multiple filler wire alloys, allowing control of composition and composition gradients in the component during additive fabrication. Ultimately, this project successfully developed a high deposition rate, arc-based, additive manufacturing process with the truly novel capability of enabling spatial composition tailoring during the build of the component. System capabilities and process science will be studied in a follow-on LDRD starting next year.

36 MATERIALS SCIENCE↗