Search NASA⌕ Search

SEARCH · Search NASA

Results for “Alumina”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

High Temperature Oxidation Behavior of Ni-based High Entropy Superalloys

A new class of polycrystalline gamma-prime strengthened superalloys with alloy compositions of (wt%) Ni-20Co-13Cr-6Fe-4Al-3W-2Mo-(4-x)Nb-(x)Ti (x = 0,1,2) were subjected to cyclic oxidation exposures in dry air at 800 °C for 3600 h. The alloys were borderline chromia/alumina formers, showing good oxidation resistance relative to commercially available materials of similar composition. While all alloys formed alumina scales initially, only the alloy with the lowest Ti/Nb ratio retained an alumina scale for the duration of the exposure. Formation of a continuous layer of rutile TiO 2 at the alumina/alloy interface is proposed to cause eventual alumina failure for the alloys containing Ti.

36 MATERIALS SCIENCE↗

Designing Ceria/Alumina for Efficient Trapping of Platinum Single Atoms

Cerium oxide (ceria) has been shown to be very effective at trapping platinum atoms, due to formation of stable surface complexes at step edges, where coordinatively unsaturated cerium cations are present. But ceria loses its effectiveness when heated to high temperatures, due to loss of surface area and growth in particle size associated with sintering of the oxide. Being a rare-earth, and with limited supplies worldwide, it is important to develop methods to improve the effectiveness of ceria as a catalyst support. Here we explore the performance for trapping Pt atoms when the ceria is supported on a high surface area alumina carrier. This helps create a more sustainable catalyst formulation, especially if we can retain the high dispersion of Pt seen on ceria supports. For this work, we studied the atom trapping efficacy of ceria/alumina samples with increasing ceria content (8 wt% - 50%) and contrasted the behavior with pure ceria. Electron microscopy reveals that when dispersed on alumina, ceria is present in the form of crystalline nanoparticles as well as isolated cerium ions. These two forms of ceria differ markedly in their ability to trap Pt atoms. Atomically dispersed cerium is present in the form of Ce 3+ cations on alumina, however this form of ceria is not effective for trapping Pt atoms. Our results show that the atom trapped Pt resides primarily on crystalline ceria nanoparticles. CO oxidation was used as a probe reaction to evaluate the performance of these Pt AT /ceria-alumina catalysts. As a result, we conclude that over the range of ceria loadings we investigated, 50% ceria/alumina represents the optimal catalyst support for achieving high surface area and atom trapping efficiency while helping reduce the total ceria content in this catalyst system.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Control of wetting and uniformity via ZrSi x formation in ceramic-to-metal joints fabricated using Ag-Zr brazes

The deposition of a 2.0 µm SiO 2 film on the alumina surface in Kovar TM /94% alumina joints enables the formation of a silicide reaction layer on the alumina during brazing with 97Ag2Zr1Cu. Additionally, the average and standard deviation of joint thickness decrease from 50 to 15 and 29 to 4 µm, respectively compared to joints without added SiO 2 . Finally, the average failure stress of these braze joints was 45 MPa, while that of similar joints without added SiO 2 was 90 MPa. Sessile drop experiments of 98Ag2Zr on SiO 2 and 99.6% Al 2 O 3 substrates show that the braze wets and spreads to 3x its original area on SiO 2 with a wetting angle near 0°, but remains the same area on 99.6% Al 2 O 3 with a wetting angle of 106.6°. Focused-ion-beam scanning electron microscopy analysis of a cross-section of the 98Ag2Zr sessile drop on the SiO 2 substrate has shown that Zr reacts with SiO 2 to form Zr oxide and silicide layers. Scanning transmission electron microscopy diffraction and energy dispersive X-ray spectroscopy analysis indicate this silicide layer contains tetragonal Zr 5 Si 4 . In conclusion, analysis shows the silicide layer enhances wetting and joint uniformity while unreacted SiO 2 embrittles the joint and degrades strength.

alumina↗

Validation of a Custom Ball-on-Ring Apparatus and Consideration of Common Issues for Use in Further Testing (SULI Deliverables)

Ceramic materials are well-known for their high hardness and strength but are limited in their application due to low toughness and sudden failure. As a potential solution, inspiration can be taken from dental enamel nanostructure, where undulating rods cause cracks to branch or deflect, increasing the energy needed to cause total fracture of a ceramic part. Following the dental enamel structure, a novel ceramic which uses 3D printed Yttria stabilized Zirconia rods in an alumina matrix was developed. To test this bio-inspired ceramic material, a proper testing apparatus needed to be created and tested to verify its accuracy. For this project, a bespoke ball on ring testing apparatus was created and tested using both conventionally sintered alumina disks and purchased alumina disks to validate its accuracy. By comparing the Weibull distribution of rupture strengths measured by the tests to literature values, it was shown that the testing frame had a wide distribution of strength which did not align with literature values on the lower end. Through fractography, it was found that some samples fractured from the contact stress induced by the ball indenter, which could not be used to calculate rupture strength. This fracture was often linked to low stress to failure, which was initiated by a flaw on the surface near the indenter which acted as a stress concentrator. Removal of these samples from the data set increased the accuracy of the reported rupture strength values for the ceramic. Considering the equations for the magnitude of contact and flexural strength, along with observations of initiating flaws, several measures can be taken for testing the bio-inspired composite. These measures include proper polishing of both sides of the sample, reducing sample thickness, and potentially using a softer indenter material.

36 - MATERIALS SCIENCE↗

Pre-Oxidation to Improve Liquid Metal Compatibility

Liquid metals represent an aggressive environment where selective degradation can attack structural alloys. Pre-oxidizing structural alloys, particularly those able to form alumina scales, have shown promise for Sn, Pb and Pb–Li concepts for fusion and fission applications. For Pb at 700 °C, a dramatic reduction in mass loss was observed for an alumina-forming austenitic (AFA) steel after pre-oxidation. Likewise, a ferritic FeCrAlMo alloy showed better compatibility in static Sn at 400–500 °C and flowing PbLi when pre-oxidized at 1000 °C to form α-Al2O3. Recent experiments with flowing PbLi at 675–700 °C has shown significant degradation suggesting that alumina-forming alloys are limited to ~ 650 °C in this environment. While the concept is promising, most experiments have been relatively short-term and long-term degradation mechanisms need to be evaluated.

Pint, Bruce↗

Engineering Assembly Kinetics and Line Roughness in Solvent Vapor-Annealed Block Copolymer/Homopolymer Blends

Block copolymer (BCP) directed self-assembly (DSA) is a promising route to enhance lithography resolution by multiplying nanopattern density and reducing feature roughness. Eliminating kinetically trapped self-assembly defects requires fast self-assembly. However, acceleration strategies like solvent vapor annealing or homopolymer blending broaden domain interfaces, implying a trade-off in increased feature roughness. In this work, we experimentally investigate this apparent dilemma between self-assembly kinetics and line roughness for solvent vapor-annealed thin films of a lamellar poly(styrene-block-2-vinylpyridine) (PS-b-P2VP) BCP blended with PS and P2VP homopolymers. Binary blends with PS or P2VP homopolymers and ternary blends incorporating both in equal weight fractions were solvent vapor annealed using acetone, a near-neutral solvent for PS and P2VP, followed by P2VP-selective vapor-phase infiltration with alumina (AlOx) and polymer etching. Binary blends with P2VP exhibit a modest kinetic enhancement but also higher line-edge and -width roughness due to the increased frequency of P2VP protrusions and bridge defects in the alumina line patterns. In contrast, binary blends with PS self-assemble noticeably faster, while domain asymmetry from the added PS homopolymer reduces roughness by curbing the number of alumina protrusions and bridge defects. Ternary blends maintain DSA line patterns across a wider composition window and, at higher homopolymer loadings, reduce roughness at length scales near the lamellar period, consistent with a reduced impact of intradomain compositional fluctuations. These findings provide important insights for codesigning blend compositions and process flows to achieve high-resolution, defect free patterns with minimal roughness through BCP DSA.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Unveiling the Stability of Encapsulated Pt Catalysts Using Nanocrystals and Atomic Layer Deposition

Platinum exhibits desirable catalytic properties, but it is scarce and expensive. Optimizing its use in key applications such as emission control catalysis is important to reduce our reliance on such a rare element. Supported Pt nanoparticles (NPs) used in emission control systems deactivate over time because of particle growth in sintering processes. Here, in this work, we shed light on the stability against sintering of Pt NPs supported on and encapsulated in Al 2 O 3 using a combination of nanocrystal catalysts and atomic layer deposition (ALD) techniques. We find that small amounts of alumina overlayers created by ALD on preformed Pt NPs can stabilize supported Pt catalysts, significantly reducing deactivation caused by sintering, as previously observed by others. Combining theoretical and experimental insights, we correlate this behavior to the decreased propensity of oxidized Pt species to undergo Ostwald ripening phenomena because of the physical barrier imposed by the alumina overlayers. Furthermore, we find that highly stable catalysts can present an abundance of under-coordinated Pt sites after restructuring of both Pt particles and alumina overlayers at a high temperature (800 °C) in C 3 H 6 oxidation conditions. The enhanced stability significantly improves the Pt utilization efficiency after accelerated aging treatments, with encapsulated Pt catalysts reaching reaction rates more than two times greater than those of a control supported Pt catalyst.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Promotion of adsorptive and catalytic properties of zeolitic Brønsted acid sites by proximal extra-framework Si(OH) x groups

Steric confinement in zeolites influences the catalytic conversion of alkanes. For zeolitic Brønsted acid sites, proximate extra-framework species introduce additional confinement to the pore constraints, enhancing the catalytic activity of alkane cracking. Although extra-framework alumina has been the most studied, here we report the element-specific impact of silica species. Further, by grafting extra-framework silica species close to Brønsted acid sites in H-ZSM-5 zeolite, the binding of bases like pyridine and amines is strengthened via van der Waals interactions with their aryl or alkyl chains. Brønsted acid sites close to extra-framework silica achieve a higher reaction rate of protolytic cracking of n-pentane via enthalpic (unlike entropic, as with extra-framework alumina) stabilization of the transition state by 24–51 kJ mol −1 . The lower activation energy points to an earlier transition state than in the presence of extra-framework alumina, with a better stabilization of the carbonium ions in the transition state compared to the parent zeolite.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Elimination of the bias-stress effect in ligand-free quantum dot field-effect transistors

Field-effect transistors (FETs) made from colloidal quantum dot (QD) solids commonly suffer from current–voltage hysteresis caused by the bias-stress effect (BSE), which complicates fundamental studies of charge transport in QD solids and the use of QD FETs in electronics. Here, we show that the BSE can be eliminated in n-channel PbSe QD FETs by first removing the QD ligands with a dose of H 2 S gas and then infilling the QD films with alumina by atomic layer deposition (ALD). The H 2 S-treated, alumina-infilled FETs have stable, hysteresis-free device characteristics (total short-term stability), indefinite air stability (total long-term stability), and a high electron mobility of up to 14 cm 2 V −1 s −1 , making them attractive for QD circuitry and optoelectronic devices. The BSE-free devices are utilized to conclusively establish the dependence of the electron mobility on temperature and QD diameter. We demonstrate that the BSE in these devices is caused by both electron trapping at the QD surface and proton drift within the film. The H 2 S/alumina chemistry produces ligand-free PbSe/PbS/Al 2 O 3 interfaces that lack the traps that cause the electronic part of the BSE, while full alumina infilling stops the proton motion responsible for the ionic part of the BSE. In conclusion, our matrix engineering approach should aid efforts to eliminate the BSE, boost carrier mobilities, and improve charge transport in other types of nanocrystal solids.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Development of a Stress Sensor for In-Situ High-Pressure Deformation Experiments Using Radial X-Ray Diffraction

We developed a stress sensor for in-situ deformation experiments using synchrotron radial X-ray diffraction. This stress sensor provided nearly diffraction-plane-independent stress that, when used in series with a sample, reduced the uncertainty of the average stress estimation acting on a sample. Here, we present the results of a study where pyrope was used as a stress sensor. Using a Deformation-DIA (D-DIA) high-pressure deformation apparatus, pyrope, olivine and alumina were deformed in the same run/cell assembly placed in series along the compression direction. Deformation experiments were conducted at pressures between 4 and 5 GPa and temperatures between 730 and 1273 K with strain-rates between 10 –5 and 10 –6 s –1 . Stresses estimated from various (hkl) planes in pyrope were nearly the same; i.e., pyrope is plastically isotropic with ≤10 % variation with (hkl). However, stresses from various (hkl) planes in olivine and alumina varied by approximately a factor of 3. Comparisons between average stresses inferred from pyrope and those from different diffraction planes in olivine and alumina showed that the average stress in these materials evolved from low-end stress, estimated from various (hkl) planes at small strain, to high-end stress at a large strain. This suggests that the rate-controlling slip system in these materials changes from the soft to the hard slip system with strain.

58 GEOSCIENCES↗

Layered catalyst structures and methods of making the same

A layered catalyst structure for purifying an exhaust gas stream includes a catalyst support and a palladium catalyst layer including an atomic dispersion of palladium ions electrostatically adsorbed onto an exterior surface of the catalyst support. The catalyst support includes an alumina substrate, a first ceria layer disposed on and extending substantially continuously over the alumina substrate, and a second colloidal ceria layer formed directly on the first ceria layer over the alumina substrate. The palladium catalyst layer is formed on the exterior surface of the catalyst support by applying a palladium-containing precursor solution to the exterior surface of the catalyst support and then heating the catalyst support and the palladium-containing precursor solution. The palladium-containing precursor solution includes a positively charged palladium complex in an aqueous medium and has a pH greater than a point of zero charge of the second colloidal ceria layer.

Gu, Yuntao↗

Influence of Joule Heating on the Stability of High Temperature Irradiation Resistant Thermocouples

Development of in-core instrumentation is driven by the pursuit of safer and more economic energy production from both existing nuclear reactors and Generation IV reactor designs. Idaho National Laboratory (INL) has developed high temperature irradiation resistant thermocouples (HTIR-TCs) for temperature sensing inside Generation IV nuclear reactors. These thermocouples are composed of phosphorus-doped niobium (Nb-P) and lanthana-doped molybdenum (Mo-LaO) thermoelements, an alumina (Al2O3) insulation, and a niobium sheath. HTIR-TCs require an initial heat treatment exceeding the maximum service temperature to stabilize the generated electromotive force (EMF) signal; however, the mechanism behind this stabilization is not well understood. This work evaluates the impact of Joule heating on the thermoelements' microstructures, chemical stability, and mechanical properties to determine the mechanisms by which the EMF signal stabilization occurs. Accordingly, during the Joule heat treatment, a secondary Nb3P phase coarsened along the length of the Nb-P thermoelement, along with the formation of an interaction region at the Al2O3/niobium interface. The interaction between the alumina insulation and the Nb-P thermoelement was also observed within the Mo-LaO thermoelement. Joule heating induced stability within the generated EMF signal of HTIR-TCs through the formation of secondary phases within the Nb-P and the interaction of the alumina insulation with the thermoelements.

46 - INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AN↗

Influence of Joule Heating on the Stability of High Temperature Irradiation-resistant Thermocouples

Development of in-core instrumentation is driven by the pursuit of safer, more economic energy production from the perspective of both existing nuclear reactors and Generation IV reactor designs. Idaho National Laboratory has developed high-temperature irradiation-resistant thermocouples (HTIR-TCs) for temperature sensing inside Generation IV nuclear reactors. These thermocouples are composed of phosphorus-doped niobium (Nb-P) and lanthana-doped molybdenum (Mo-LaO) thermoelements, an alumina (Al2O3) insulation, and a niobium sheath. HTIR-TCs require an initial heat treatment exceeding the maximum service temperature to stabilize the generated electromotive force (EMF) signal. The mechanism behind the stabilization of the HTIR-TCs through traditional heat treatment methods is understood; however, the traditional heat treatment method is expensive, time consuming, and results in a heterogeneous microstructure. Therefore, we investigated a rapid method for stabilization and microstructure homogeneity, through Joule heating. This work evaluates the impact of Joule heating on the thermoelements’ microstructures, chemical stability, and mechanical properties so as to determine the mechanisms by which stabilization of the EMF signal occurs. Accordingly, during the Joule heat treatment, a secondary Nb3P phase coarsened along the length of the Nb-P thermoelement, along with the formation of an interaction region at the Al2O3/niobium interface. The interaction between the alumina insulation and the Nb-P thermoelement was also observed within the Mo-LaO thermoelement. Joule heating induced stability within the generated HTIR-TC EMF signal via the formation of secondary phases within the Nb-P and the interaction between the alumina insulation and the thermoelements.

46 - INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AN↗

High‐Field NMR, Reactivity, and DFT Modeling Reveal the γ‐Al 2 O 3 Surface Hydroxyl Network**

Abstract Aluminas are strategic materials used in many major industrial processes, either as catalyst supports or as catalysts in their own right. The transition alumina γ‐Al 2 O 3 is a privileged support, whose reactivity can be tuned by thermal activation. This study provides a qualitative and quantitative assessment of the hydroxyl groups present on the surface of γ‐Al 2 O 3 at three different dehydroxylation temperatures. The principal [AlOH] configurations are identified and described in unprecedented detail at the molecular level. The structures were established by combining information from high‐field 1 H and 27 Al solid‐state NMR, IR spectroscopy and DFT calculations, as well as selective reactivity studies. Finally, the relationship between the hydroxyl structures and the molecular‐level structures of the active sites in catalytic alkane metathesis is discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Role of Lewis Acid Sites in γ-Al 2 O 3 Oligomerization

Olefin oligomerization by γ-Al 2 O 3 has recently been reported, and it was suggested that Lewis acid sites are catalytic. The goal of this study is to determine the number of active sites per gram of alumina to confirm that Lewis acid sites are indeed catalytic. Addition of an inorganic Sr oxide base resulted in a linear decrease in the propylene oligomerization conversion at loadings up to 0.3 wt %; while, there is a >95 % loss in conversion above 1 wt % Sr. Additionally, there was a linear decrease in the intensity of the Lewis acid peaks of absorbed pyridine in the IR spectra with an increase in Sr loading, which correlates with the loss in propylene conversion, suggesting that Lewis acid sites are catalytic. Characterization of the Sr structure by XAS and STEM indicates that single Sr 2+ ions are bound to the γ-Al 2 O 3 surface and poison one catalytic site per Sr ion. The maximum loading needed to poison all catalytic sites, assuming uniform surface coverage, was ~0.4 wt % Sr, giving an acid site density of ~0.2 sites per nm2 of γ-Al 2 O 3 , or approximately 3 % of the alumina surface.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Revisiting the influence of Ni particle size on the hydrogenation of CO 2 to CH 4 over Ni/CeO 2

Nickel nanoparticles were supported on CeO 2 and evaluated in the hydrogenation of CO 2 to CH 4 at 538 K and 1 atm. Chemisorption of H 2 was used to estimate the average Ni particle size, which ranged from 1.3 to 17 nm. The apparent activation energy for CH 4 formation and turnover frequency for CO 2 conversion was independent of Ni particle size. The smallest Ni particles (1.3 nm) were less selective to CH 4 . Comparisons to alumina-supported Ni reveal the same performance as Ni/CeO 2 when normalized to active Ni atoms counted by H 2 chemisorption. A beneficial effect of ceria relative to alumina is the enhanced reducibility of Ni as evaluated by H 2 temperature-programmed reduction. The constancy of the turnover frequency on Ni particles suggests the acid-base and/or redox properties of the support do not play a significant role in the CO 2 methanation reaction under the conditions of study, which contrasts many earlier works.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗