Search NASA⌕ Search

SEARCH · Search NASA

Results for “CdTe solar cell”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

203 records · Page 12

Hands-On PV Experience (HOPE) Workshop, Final Technical Report FY22-FY24

The Hands-On Photovoltaics Experience, or HOPE, is a one-week school held at NLR each summer to educate graduate student photovoltaic researchers in the fundamentals of photovoltaics (PV) as well as specific cell technologies and measurement & characterization techniques. The program brings students from universities across the U.S. and their faculty advisors to spend a week in an in-depth, intensive program, including hands-on lab experiences in solar cell fabrication and testing. This program is intended to educate the students and increase collaboration among the students, their advising faculty, and staff at NLR. Our survey results consistently indicate high satisfaction with this program and good student outcomes post-HOPE. HOPE is a selective program with a competitive application process and is limited to 12-20 students each year. Keeping the program small enables a high level of interaction among the students and individualized attention from the faculty and staff.

14 SOLAR ENERGY↗

Low-Temperature Gold Deposition Improves CdTe Back Contacts

Improved back contacts can benefit CdTe photovoltaics (PV). In this work, Cd(Se,Te) PV absorbers are cooled during Au evaporation to thermally quench a chemical reaction occurring between gold and CdTe and the generation of a reaction product that lowers device efficiency. Reducing substrate temperature enhances PV power conversion efficiency via open-circuit voltage and fill factor increases. X-ray photoelectron spectroscopy (XPS) reveals that lower temperature also reduces chemical perturbations of the CdTe, potentially linking back contact formation to a CdTe degradation product that hinders PV performance. Comparing reaction enthalpy and substrate heating energy shows that back contact formation by sputtering elemental metals onto ZnTe may exhibit a degradation pathway analogous to that of CdTe/Au reported here. Degradation-diminishing contact formation processes are therefore of general interest for optoelectronic devices, and the reduced substrate temperature in this study is one example.

14 SOLAR ENERGY↗

Data for "Gold-Induced Chemical Perturbations in CdTe-Based Photovoltaic Cells"

Back contacting p-type CdTe has been identified as one of the major areas of loss in CdTe photovoltaic (PV) power conversion efficiency (PCE). In research settings, Au is a common contact material due to its ease of use and decent performance. This work provides a detailed investigation into using gold for back contacting As-doped, CdCl2 treated, polycrystalline CdTe that has been exposed to air after absorber processing, another routine practice. First, X-ray photoemission spectroscopy (XPS) is used to determine the native oxide to be 1.6 nm of CdTeO3 using a combination of angle-resolved XPS and the cadmium modified Auger parameter. During gold metallization of CdTe, oxygen and oxidized tellurium are eliminated from the thin CdTeO3 native oxide. The fate of the released oxygen and possibly cadmium and tellurium are not known, but these reaction byproducts can enter the absorber bulk or grain boundaries, stay at the interface, or dissolve in the Au. Interfacial hole barriers between CdTe and Au are measured for samples with and without the native oxide present prior to metallization. Results show that the thin CdTeO3 alleviates the downward band bending by 40 meV from 470 meV to 430 meV even though it is consumed during interface formation. The implications of these chemical reactions on the device are assessed through photoluminescence (PL) spectroscopy which shows losses in internal open circuit voltage (iVoc) from 820 meV to 795 meV, carrier lifetime from 123 ns to 45 ns, and PL quantum yield from 2.9x10-5 to 1.2x10-5. Modeling time-resolved PL lifetimes demonstrates the back surface recombination velocity due to metallization reduces minority carrier lifetimes. These results identify the native oxide and show that it plays an important role in mediating downward band bending along with how the back interface reaction can negatively impact device-scale parameters and reduce PV PCE.

14 SOLAR ENERGY↗

Gold-Induced Chemical Perturbations in CdTe-Based Photovoltaic Cells

Back-contacting p-type CdTe has been identified as one of the major areas of loss in CdTe photovoltaic (PV) power conversion efficiency (PCE). In research settings, Au is a common contact material due to its ease of use and decent performance. This work provides a detailed investigation into using gold for back contacting As-doped, CdCl 2 -treated, polycrystalline CdTe that has been exposed to air after absorber processing, another routine practice. First, X-ray photoemission spectroscopy (XPS) is used to determine the native oxide to be 1.6 nm of CdTeO 3 by using a combination of angle-resolved XPS and the cadmium-modified Auger parameter. During gold metallization of CdTe, oxygen and oxidized tellurium are eliminated from the thin CdTeO 3 native oxide. The fates of the released oxygen and possibly cadmium and tellurium are not known, but these reaction byproducts can enter the absorber bulk or grain boundaries, stay at the interface, or dissolve in the Au. Interfacial hole barriers between CdTe and Au are measured for samples with and without the native oxide present prior to metallization. Results show that the thin CdTeO 3 alleviates the downward band bending by 40 meV from 470 to 430 meV even though it is consumed during interface formation. The implications of these chemical reactions on the device are assessed through photoluminescence (PL) spectroscopy, which shows losses in internal open circuit voltage (iVoc) from 820 to 795 meV, carrier lifetime from 123 to 45 ns, and PL quantum yield from 2.9 × 10 −5 to 1.2 × 10 −5 . Modeling timeresolved PL lifetimes demonstrates the back surface recombination velocity due to metallization reduces minority carrier lifetimes. These results identify the native oxide and show that it plays an important role in mediating downward band bending along with how the back interface reaction can negatively impact device-scale parameters and reduce PV PCE.

14 SOLAR ENERGY↗

Understanding ERE and iVOC Metrics for Graded CdSeTe Absorbers

PL-based external radiative efficiency (ERE) and implied open-circuit voltage (iVOC) metrics were introduced for thin-film solar absorbers to better understand the voltage deficit and diagnose losses in solar cells. Traditionally, elevated ERE and iVOC measurements are associated with diminished recombination within the solar device, a rationale heavily reliant on the assumption of a uniform bandgap and high carrier mobilities in the absorber. Recently, very low mobilities in CdSeTe absorbers (< 1 cm2/(V.s)) were measured using the light-induced transient grading technique. In this study, we use a detailed numerical model of iVOC to investigate the possible reasons of elevated iVOC in realistic CdSeTe absorbers with a graded Se profile. In particular, we examine how the bandgap nonuniformity and the reduced hole mobility in graded CdSeTe absorbers affect iVOC measurements. We show that high iVOC may result from inflated quasi-Fermi level splitting in the high-Se region in the front part of a CdSeTe absorber with slow hole transport. We reproduce the experimentally reported 360 mV increase in iVOC-VOC gap with reduced doping using a model with sub-1 cm2/(V.s) hole mobility in the high-Se region. Based on our results, we conclude that the iVOC metric (or ERE metric) should not be used as a sole metric of CdSeTe absorber quality. We discuss possible ways to extract useful information from the iVOC-VOC gap by supplementing the front-side illumination measurements with back-side illumination measurements.

14 SOLAR ENERGY↗