Analysis of Advanced Thermoelectric Materials and Their Functional Limits

The world's demand for energy is increasing dramatically, but the best energy conversion systems operate at approximately 30% efficiency. One way to decrease energy loss is in the recovery of waste heat using thermoelectric (TE) generators. A TE generator is device that generates electricity by exploiting heat flow across a thermal gradient. The efficiency of a TE material for power generation and cooling is determined by the dimensionless Figure of Merit (ZT): ZT = S(exp. 2)sigmaT/κ: where S is the Seebeck coefficient, sigma is the electrical conductivity, T is the absolute temperature, and κ is the thermal conductivity. The parameters are not physically independent, but intrinsically coupled since they are a function of the transport properties of electrons. Traditional research on TE materials has focused on synthesizing bulk semiconductor-type materials that have low thermal conductivity and high electrical conductivity affording ZT values of 1. The optimization of the σ/κ ratio is difficult to achieve using current material formats, as these material constants are complementary. Recent areas of research are focusing on using nanostructural artifacts that introduce specific dislocations and boundary conditions that scatter the phonons. This disrupts the physical link between thermal (phonon) and electrical (electron) transport. The result is that κ is decreased without decreasing σ. These material formats give ZT values of up to 2 which represent approximately 18% energy gain from waste heat recovery. The next challenge in developing the next generation of TE materials with superior performance is to tailor the interconnected thermoelectric physical parameters of the material system. In order to approach this problem, the fundamental physics of each parameter S, sigma, and κ need to be physically understood in their context of electron/phonon interaction for the construction of new high ZT thermoelectric devices. Is it possible to overcome the physical limit imposed by of the effect of phonon lattice oscillation and energetic electrons towards thermal conductivity? Is the Seebeck coefficient, based on the difference in voltage over temperature gradient ( deltaV/deltaT), an intrinsic parameter of each material? All these parameters were manipulated using nano-bridge and twin-lattice structural concepts at the NASA Langley Research Center. This talk will review the current trend of TE research to optimize the ZT and discuss about new approaches on increasing ZT within functional limits of each parameter.

Kim, Hyun Jung↗

Phase Sensitive X-Ray Diffraction Imaging Study of Protein Crystals

The study of defects and growth of protein crystals is of importance in providing a fundamental understanding of this important category of systems and the rationale for crystallization of better ordered crystals for structural determination and drug design. Yet, as a result of the extremely weak scattering power of x-rays in protein and other biological macromolecular crystals, the extinction lengths for those crystals are extremely large and, roughly speaking, of the order of millimeters on average compared to the scale of micrometers for most small molecular crystals. This has significant implication for x-ray diffraction and imaging study of protein crystals, and presents an interesting challenge to currently available x-ray analytical techniques. We proposed that coherence-based phase sensitive x-ray diffraction imaging could provide a way to augment defect contrast in x-ray diffraction images of weakly diffracting biological macromolecular crystals. I shall examine the principles and ideas behind this approach and compare it to other available x-ray topography and diffraction methods. I shall then present some recent experimental results in two model protein systems-cubic apofemtin and tetragonal lysozyme crystals to demonstrate the capability of the coherence-based imaging method in mapping point defects, dislocations, and the degree of perfection of biological macromolecular crystals with extreme sensitivity. While further work is under way, it is intended to show that the observed new features have yielded important information on protein crystal perfection and nucleation and growth mechanism otherwise unobtainable.

Hu, Z. W.↗

Preliminary Work in Obtaining Site-Directed Mutants of Hen Egg White Lysozyme

Protein crystal growth studies are recognized as a critical endeavor in the field of molecular biotechnology. The scientific applications of this field include the understanding of how enzymes function and the accumulation of accurate information of atomic structures, a key factor in the process of rational drug design. NASA has committed substantial investment and resources to the field of protein crystal growth and has conducted many microgravity protein crystal growth experiments aboard shuttle flights. Crystals grown in space tend to be larger, denser and have a more perfect habit and geometry. These improved properties gained in the microgravity environment of space result largely from the reduction of solutal convection, and the elimination of sedimentation at the growing crystal surface. Shuttle experiments have yielded many large, high quality crystals that are suitable for high resolution X-ray diffraction analysis. Examples of biologically important macromolecules which have been successfully crystallized during shuttle missions include: lysozyme, isocitrate lyase, gamma-interferon, insulin, human serum albumin and canavalin. Numerous other examples are also available. In addition to obtaining high quality crystals, investigators are also interested in learning the mechanisms by which the growth events take place. Crystallization experiments indicate that for the enzyme HEWL, measured growth rates do not follow mathematical models for 2D nucleation and dislocation-led growth of tetragonal protein crystals. As has been suggested by the laboratory of Marc L. Pusey, a possible explanation for the disagreement between observation and data is that HEWL tetraconal crystals form by aggregated units of lysozyme in supersaturated solutions. Surface measurement data was shown to fit very well with a model using an octamer unit cell as the growth unit. According to this model, the aggregation pathway and subsequent crystal growth is described by: monomer < ------ > dimer < ------- > tetramer < ------ > octamer < ------ > higher order. It is believed that multimer aggregation of lysozyme occurs by interaction at specific binding sites on the surface of the protein crystals. If the presence of discrete binding sites and the aggregation hypothesis is true, then it follows that the alteration of the binding site(s) should have significant effect on the measurements obtained during growth experiments. Site-directed mutagenesis allows the specific alteration of proteins by replacement, deletion or addition of specific amino acid residues. This report outlines the approach for this strategy and the progress made thus far toward that end.

Holmes, Leonard D.↗

Multiscale Modeling of Damage Processes in Aluminum Alloys: Grain-Scale Mechanisms

This paper has two goals related to the development of a physically-grounded methodology for modeling the initial stages of fatigue crack growth in an aluminum alloy. The aluminum alloy, AA 7075-T651, is susceptible to fatigue cracking that nucleates from cracked second phase iron-bearing particles. Thus, the first goal of the paper is to validate an existing framework for the prediction of the conditions under which the particles crack. The observed statistics of particle cracking (defined as incubation for this alloy) must be accurately predicted to simulate the stochastic nature of microstructurally small fatigue crack (MSFC) formation. Also, only by simulating incubation of damage in a statistically accurate manner can subsequent stages of crack growth be accurately predicted. To maintain fidelity and computational efficiency, a filtering procedure was developed to eliminate particles that were unlikely to crack. The particle filter considers the distributions of particle sizes and shapes, grain texture, and the configuration of the surrounding grains. This filter helps substantially reduce the number of particles that need to be included in the microstructural models and forms the basis of the future work on the subsequent stages of MSFC, crack nucleation and microstructurally small crack propagation. A physics-based approach to simulating fracture should ultimately begin at nanometer length scale, in which atomistic simulation is used to predict the fundamental damage mechanisms of MSFC. These mechanisms include dislocation formation and interaction, interstitial void formation, and atomic diffusion. However, atomistic simulations quickly become computationally intractable as the system size increases, especially when directly linking to the already large microstructural models. Therefore, the second goal of this paper is to propose a method that will incorporate atomistic simulation and small-scale experimental characterization into the existing multiscale framework. At the microscale, the nanoscale mechanics are represented within cohesive zones where appropriate, i.e. where the mechanics observed at the nanoscale can be represented as occurring on a plane such as at grain boundaries or slip planes at a crack front. Important advancements that are yet to be made include: 1. an increased fidelity in cohesive zone modeling; 2. a means to understand how atomistic simulation scales with time; 3. a new experimental methodology for generating empirical models for CZMs and emerging materials; and 4. a validation of simulations of the damage processes at the nano-micro scale. With ever-increasing computer power, the long-term ability to employ atomistic simulation for the prognosis of structural components will not be limited by computation power, but by our lack of knowledge in incorporating atomistic models into simulations of MSFC into a multiscale framework.

Hochhalter, J. D.↗

Transient Creep of a Composite Lower Crust: A Polymineralic Basis for Rapidly Evolving Postseismic Deformation Modes - 2

Postseismic horizontal strain and displacement following the June 28, 1992, Landers, California, earthquake (M(sub W) 7.3) is broad scale and cannot be explained solely by delayed afterslip located at the rupturing fault trace. Both the observed strain at Pifion Flat Observatory (PFO) and observed Global Positioning System receiver velocities evolve rapidly after the Landers-Big Bear earthquake sequence. The observed exponential decay of these motions, with timescales of 4-34 days, may reflect a soft creep rheology in the lower crust and brittle-ductile transition zone or even within the seismogenic crust itself. Here a simple model of a two-dimensional screw dislocation in a layered Maxwell viscoelastic Earth is employed in conjunction with a composite rheology to demonstrate that the short timescale transient response modes (approx. = 4-34 days) are consistent with the behavior of a biviscous lower crust. The lowest viscosity of this system is derivable from laboratory experimental data on the long-term creep of natural quarztites, and the highest viscosity is consistent with isostasy-related lower crustal flow in a continental extensional tectonic environment. The model predicts significant stress relaxation at the base of the seismogenic crust. Near the base of the seismogenic zone, and about 4 km away from the mainshock, the rate of predicted relaxation is of the order of 0.01 MPa/ d during the first 20 days of postseismic flow. Oblate spheroidal inclusions at 5% concentration levels that are both aligned and fairly flat in shape and that have a viscosity of 3-4 x 10(exp 15) Pa s are consistent with both the amplitude and decay time of horizontal crustal strain observed at PFO after the Landers mainshock. It is speculated that the structures exposed in cross sections and in seismic reflection profiles of the lower crust that have mylonitic associations are, in part, the cause of such rapid postseismic evolution in southeastern California. Unmylonitized quartz-rich rock at sufficiently elevated temperatures could also contribute to the rapid decay modes.

Ivins, Erik R.↗

Fatigue Behavior and Deformation Mechanisms in Inconel 718 Superalloy Investigated

The nickel-base superalloy Inconel 718 (IN 718) is used as a structural material for a variety of components in the space shuttle main engine (SSME) and accounts for more than half of the total weight of this engine. IN 718 is the bill-of-material for the pressure vessels of nickel-hydrogen batteries for the space station. In the case of the space shuttle main engine, structural components are typically subjected to startup and shutdown load transients and occasional overloads in addition to high-frequency vibratory loads from routine operation. The nickel-hydrogen battery cells are prooftested before service and are subjected to fluctuating pressure loads during operation. In both of these applications, the structural material is subjected to a monotonic load initially, which is subsequently followed by fatigue. To assess the life of these structural components, it is necessary to determine the influence of a prior monotonic load on the subsequent fatigue life of the superalloy. An insight into the underlying deformation and damage mechanisms is also required to properly account for the interaction between the prior monotonic load and the subsequent fatigue loading. An experimental investigation was conducted to establish the effect of prior monotonic straining on the subsequent fatigue behavior of wrought, double-aged, IN 718 at room temperature. First, monotonic strain tests and fully-reversed, strain-controlled fatigue tests were conducted on uniform-gage-section IN 718 specimens. Next, fully reversed fatigue tests were conducted under strain control on specimens that were monotonically strained in tension. Results from this investigation indicated that prior monotonic straining reduced the fatigue resistance of the superalloy particularly at the lowest strain range. Some of the tested specimens were sectioned and examined by transmission electron microscopy to reveal typical microstructures as well as the active deformation and damage mechanisms under each of the loading conditions. In monotonically strained specimens, deformation during the subsequent fatigue loading was mainly confined to the deformation bands initiated during the prior monotonic straining. This can cause dislocations to move more readily along the previously activated deformation bands and to pile up near grain boundaries, eventually making the grain boundaries susceptible to fatigue crack initiation. The mechanisms inferred from the microstructural investigation were extremely valuable in interpreting the influence of prior monotonic straining on the subsequent fatigue life of Inconel 718 superalloy.

Source record↗

Diffraction and imaging study of imperfections of crystallized lysozyme with coherent X-rays

Phase-contrast X-ray diffraction imaging and high-angular-resolution diffraction combined with phase-contrast radiographic imaging were employed to characterize defects and perfection of a uniformly grown tetragonal lysozyme crystal in the symmetric Laue case. The full-width at half-maximum (FWHM) of a 4 4 0 rocking curve measured from the original crystal was approximately 16.7 arcsec and imperfections including line defects, inclusions and other microdefects were observed in the diffraction images of the crystal. The observed line defects carry distinct dislocation features running approximately along the <1 1 0> growth front and have been found to originate mostly in a central growth area and occasionally in outer growth regions. Inclusions of impurities or formations of foreign particles in the central growth region are resolved in the images with high sensitivity to defects. Slow dehydration led to the broadening of a fairly symmetric 4 4 0 rocking curve by a factor of approximately 2.6, which was primarily attributed to the dehydration-induced microscopic effects that are clearly shown in X-ray diffraction images. The details of the observed defects and the significant change in the revealed microstructures with drying provide insight into the nature of imperfections, nucleation and growth, and the properties of protein crystals.

Muramidase/chemistry↗

Influence of Containment on Defects in GeSi Crystals

Crystals grown without being in contact with a container have superior quality to otherwise similar crystals grown in direct contact with a container, especially with respect to impurity incorporation, formation of dislocations, and residual stress in crystals. "Detached" or "dewetted" Bridgman growth is similar to regular Bridgman growth in that most of the melt is in contact with the crucible wall, but the crystal is separated from the wall by a small gap, typically of the order of 10(exp -5) m. A small meniscus bridges the gap between the top of the crystal and the wall. Key parameters involved in achieving detached growth are the contact angle between the melt and crucible and the pressure differential across the meniscus. Sessile drop measurements were used to determine the wetting angles of Ge(sub 1-x)Si(sub x) melts on a variety of substrates and found that the highest wetting angles were achieved with pyrolitic boron nitride (pBN). GeSi crystals have been repeatedly grown detached in pBN crucibles but only occasionally in crucibles with lower wetting angles. Experiments have been conducted to assess the effect of pressure differential across the meniscus in sealed crucibles. This was done by adjusting the temperature profile after partial melting of the starting material. In a separate set of experiments, the pressure was controlled by connecting the volume below the meniscus to a regulated gas supply. The experiments were in agreement with calculations which predicted that stable detachment will only occur in crucibles with a low wetting angle over a relatively narrow range of pressure differential. Detached-grown crystals exhibited superior structural quality as evidenced by measurements of etch pit density, synchrotron white beam X-ray topography and double axis X-ray diffraction.

Volz, M. P.↗

New AFM Techniques for Investigating Molecular Growth Mechanisms of Protein Crystals

Atomic Force Microscopy (AFM) has emerged as a powerful technique for investigating protein crystal growth. Earlier AFM studies were among the first to demonstrate that these crystals grew by dislocation and 2D nucleation growth mechanisms [1]. These investigations were restricted to the micron range where only surface features, such as dislocation hillocks and 2D islands are visible. Most AFM instruments can scan at higher resolutions and have the potential to resolve individual protein molecules at nanometer ranges. Such scans are essential for determining the molecular packing arrangements on crystal faces and for probing the growth process at the molecular level. However, at this resolution the AFM tip influences the image produced, with the resulting image being a convolution of the tip shape and the surface morphology [2]. In most studies this problem is resolved by deconvoluting the image to obtain the true surface morphology. Although deconvolution routines work reasonably well for simple one- dimensional shapes, for complex surfaces this approach does not produce accurate results. In this study we devised a new approach which takes advantage of the precise molecular order of crystal surfaces, combined with the knowledge of individual molecular shapes from the crystallographic data of the protein and the AFM tip shape. This information is used to construct expected theoretical AFM images by convoluting the tip shape with the constructed crystal surface shape for a given surface packing arrangement. By comparing the images from actual AFM scans with the constructed ones for different possible surface packing arrangements, the correct packing arrangement can be conclusively determined. This approach was used in this study to determine the correct one from two possible packing arrangements on (I 10) faces of tetragonal lysozyme crystals. Another novel AFM technique was also devised to measure the dimension of individual growth units of the crystal faces. Measuring these units was not attempted before and most studies have assumed that the growth unit consisted of individual protein molecules. The linescan mode of AFM instruments allows the crystal surface to be scanned along a single line. By scanning across a growth step an image showing the motion of the step is obtained. Normally such an image shows a straight line for continuous and constant step velocity. In this study by increasing the scan rate and by decreasing the step velocity (by decreasing the supersaturation), we were able to capture images of individual growth events, shown by jump discontinuities in the step line. By suitable integration of the image the growth unit dimension in the scanned direction can be obtained. Since multiple units can be involved in the growth process it is necessary to collect a statistically relevant sample before drawing conclusions about the growth mechanism. This technique was successfully employed to obtain the dimensions of growth units for the (110) face, showing that they consisted of various aggregates corresponding to the 43 helices in the crystal structure.

Li, Huayu↗