Degradation mechanisms of electron mobility in metal-oxide-semiconductor field-effect transistors with LaAlO{sub 3} gate dielectric
LaAlO{sub 3} is a promising candidate of gate dielectric for future very large scale integration devices. In this work, metal-oxide-semiconductor capacitors and transistors with LaAlO{sub 3} gate dielectric were fabricated and the electron mobility degradation mechanisms were studied. The LaAlO{sub 3} films were deposited by radio frequency magnetron sputtering. The LaAlO{sub 3} films were examined by x-ray diffraction, secondary ion mass spectroscopy, and x-ray photoelectron spectroscopy. The temperature dependence of metal-oxide-semiconductor field-effect transistors characteristics was studied from 11 K to 400 K. The rate of threshold voltage change with temperature (DELTAV{sub T}/DELTAT) is -1.51 mV/K. The electron mobility limited by surface roughness is proportional to E{sub eff}{sup -0.66} in the electric field of 0.93 MV/cm<E{sub eff}<2.64 MV/cm at 300 K and the phonon scattering is proportional to T{sup -5.6} between 300 and 400 K. Soft optical phonon scattering was used to explain the extra source of phonon scattering in LaAlO{sub 3}-gated n-channel metal-oxide-semiconductor field-effect transistors.