Search NASA⌕ Search

SEARCH · Search NASA

Results for “GAS WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

Prediction of Weld Penetration in FCAW of HSLA steel using Artificial Neural Networks

Flux-cored arc welding (FCAW) is a semiautomatic or automatic arc welding process that requires a continuously-fed consumable tubular electrode containing a flux. The main FCAW process parameters affecting the depth of penetration are welding current, arc voltage, nozzle-to-work distance, torch angle and welding speed. Shallow depth of penetration may contribute to failure of a welded structure since penetration determines the stress-carrying capacity of a welded joint. To avoid such occurrences; the welding process parameters influencing the weld penetration must be properly selected to obtain an acceptable weld penetration and hence a high quality joint. Artificial neural networks (ANN), also called neural networks (NN), are computational models used to express complex non-linear relationships between input and output data. In this paper, artificial neural network (ANN) method is used to predict the effects of welding current, arc voltage, nozzle-to-work distance, torch angle and welding speed on weld penetration depth in gas shielded FCAW of a grade of high strength low alloy steel. 32 experimental runs were carried out using the bead-on-plate welding technique. Weld penetrations were measured and on the basis of these 32 sets of experimental data, a feed-forward back-propagation neural network was created. 28 sets of the experiments were used as the training data and the remaining 4 sets were used for the testing phase of the network. The ANN has one hidden layer with eight neurons and is trained after 840 iterations. The comparison between the experimental results and ANN results showed that the trained network could predict the effects of the FCAW process parameters on weld penetration adequately.

36 MATERIALS SCIENCE↗

Titanium Wire Arc Additive Manufacturing Inert Enclosure and Material Handling Safety Considerations

Wire arc additive manufacturing (WAAM) via metal inert gas (MIG)/gas metal arc welding (GMAW) is a viable option for fabrication of large-scale titanium parts; however, it introduces new safety hazards associated with both the material and the additional system hardware required for the process. Localized gas shielding of the weld arc via standard GMAW torch is inadequate for titanium due to its affinity for oxygen; thereby requiring the use of an inert enclosure to protect the weld from entraining oxygen. The use of the inert enclosure presents potential safety hazards such as operator asphyxiation and brings up discussion of confined space considerations. In addition, the titanium welding process creates pyrophoric titanium soot residue around the deposit, which can undergo deflagration during part cleaning and part removal. This paper provides an overview of the titanium WAAM process along with safety considerations for the design and operation of the inert enclosure as well as functional solutions for the safe handling of the titanium soot by-product.

Walters, Alex↗

Fluid Flow Phenomena during Welding

MOLTEN WELD POOLS are dynamic. Liquid in the weld pool in acted on by several strong forces, which can result in high-velocity fluid motion. Fluid flow velocities exceeding 1 m/s (3.3 ft/s) have been observed in gas tungsten arc (GTA) welds under ordinary welding conditions, and higher velocities have been measured in submerged arc welds. Fluid flow is important because it affects weld shape and is related to the formation of a variety of weld defects. Moving liquid transports heat and often dominates heat transport in the weld pool. Because heat transport by mass flow depends on the direction and speed of fluid motion, weld pool shape can differ dramatically from that predicted by conductive heat flow. Temperature gradients are also altered by fluid flow, which can affect weld microstructure. A number of defects in GTA welds have been attributed to fluid flow or changes in fluid flow, including lack of penetration, top bead roughness, humped beads, finger penetration, and undercutting. Instabilities in the liquid film around the keyhole in electron beam and laser welds are responsible for the uneven penetration (spiking) characteristic of these types of welds.

36 MATERIALS SCIENCE↗

Prediction and Monitoring Systems of Creep-Fracture Behavior of 9Cr-1Mo Steels for Teactor Pressure Vessels

A recent workshop on next-generation nuclear plant (NGNP) topics underscored the need for research studies on the creep fracture behavior of two materials under consideration for reactor pressure vessel (RPV) applications: 9Cr-1Mo and SA-5XX steels. This research project will provide a fundamental understanding of creep fracture behavior of modified 9Cr-1Mo steel welds for through modeling and experimentation and will recommend a design for an RPV structural health monitoring system. Following are the specific objectives of this research project: Characterize metallurgical degradation in welded modified 9Cr-1Mo steel resulting from aging processes and creep service conditions; Perform creep tests and characterize the mechanisms of creep fracture process; Quantify how the microstructure degradation controls the creep strength of welded steel specimens; Perform finite element (FE) simulations using polycrystal plasticity to understand how grain texture affects the creep fracture properties of welds; Develop a microstructure-based creep fracture model to estimate RPVs service life; Manufacture small, prototypic, cylindrical pressure vessels, subject them to degradation by aging, and measure their leak rates; Simulate damage evolution in creep specimens by FE analyses; Develop a model that correlates gas leak rates from welded pressure vessels with the amount of microstructural damage; Perform large-scale FE simulations with a realistic microstructure to evaluate RPV performance at elevated temperatures and creep strength; Develop a fracture model for the structural integrity of RPVs subjected to creep loads; and Develop a plan for a non-destructive structural health monitoring technique and damage detection device for RPVs.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

ARIES Oxide Production Program Monthly Report – April 2014

A summary of the accomplishments, milestones, financial summary, project performance and issues facing the Oxide Production Program for the end of April 2014 is presented in this Executive Summary. PF-4 and ARIES operations remain paused in order to resolve issues and perform an extent-of-condition review for Criticality Safety and Conduct of Operations. On April 28th, Jeff Yarbrough issued a memorandum updating status on the “pause” of PF-4 programmatic operations. He reported that 150 of the procedures that control programmatic operations in PF-4 have successfully resumed. These 150 procedures represent about ½ of the total that will enable us to meet FY14 programmatic commitments. No formal letter of direction will be provided to LANS via the NNSA Field Office contracting officer to address the direction relative to shipments, analytical chemistry sampling and guidance for financial adjustments in FY14 and FY15. LANS will provide a revised plan based on the funding profile included in the President’s Budget Request for the remainder of FY14 and FY15 to include revised FY14 milestones and proposed FY15 milestones. The ARIES Pit Cutter project met the NNSA milestone (Complete Design of Simple Pit Disassembly Equipment [ARIES Pit Cutter] – Due 8/15/14) by completing the fabrication design on 4/3/14, well in advance of the 8/15/14 due date. The project team has started procurement of long-lead items in preparation of the prototype fabrication and cold testing. The fabrication is scheduled to complete in FY14 and the cold testing will begin in FY14 and complete in early FY15. LANL and PNNL met on April 14 to discuss the path forward for PNNL criticality support to the program. The consensus was that PNNL resources can be effectively applied to the generation of detailed CSEs to support the program independent of the current ESS strategy. FY15 program planning is underway. The team is working on planning/drafting the work packages and developing the schedule under the assumption that operations will begin October 1, 2014. A planning schedule has been finalized and the team is meeting regularly to discuss details at the work package and WBS levels. The FY15 PMP is also in the process of being updated. The goal is to have all the drafts reviewed/approved and finalized prior to the start of the FY. MQ personnel have completed ADPSM Management Assessment: Evaluate Quality Roles and Responsibility Agreements between ADPSM and LANL Technical Support Organizations (PFITS 2011-1943). Two findings and four opportunities for improvement were reported. The robotic lathe controller upgrade has entered the construction phase of the project. The controller cabling IWD pre-job meeting was completed. The initial robotic lathe functional test was completed. The existing controller power supply disconnect is scheduled for early May. The NDA Cage project team received notification on 3/28/14 to restart the NDA cage project. Since then the team have been busy with activities that include assigning a planner, getting the construction work package ready for construction and getting the USQ completed. The electrical services installation for the new welding skid for the Inner Can Welder was completed. A gas bottle rack, used to support welding operations, will be installed in early May. The Outer Can Welder design is complete and the IWD is in development to execute construction. Installation materials have been ordered. Work continues on the MD-2 preliminary design. The project engineer is performing a technical evaluation of the Project Management Plan that was submitted by the design agent in response to the LANL Request for Proposal. If all requirements have been captured, LANL procurement will develop a contract and give the design agent notice to proceed on the preliminary design. Estimated completion is scheduled for September 2014. The design for the TA-55 Bldg. 314 warehouse was issued at 90% complete and has begun the last review process. A constructability review is scheduled for early May. The Project Manager has been working with the LANL estimating group to get the class 3 estimate for review. The Oxide Production Cage Upgrade project has kicked-off efforts on the 30% design. Requirements documentation has been drafted. The floor space was walked-down with other project managers and stakeholders and the boundaries were agreed upon.

ARIES↗

Creep and Creep-Fatigue of Alloy 617 Weldments

Alloy 617 is the primary candidate material for the heat exchanger of a very high temperature gas cooled reactor intended to operate up to 950°C. While this alloy is currently qualified in the ASME Boiler and Pressure Vessel Code for non-nuclear construction, it is not currently allowed for use in nuclear designs. A draft Code Case to qualify Alloy 617 for nuclear pressure boundary applications was submitted in 1992, but was withdrawn prior to approval. Prior to withdrawal of the draft, comments were received indicating that there was insufficient knowledge of the creep and creep-fatigue behavior of Alloy 617 welds. In this report the results of recent experiments and analysis of the creep-rupture behavior of Alloy 617 welds prepared using the gas tungsten arc process with Alloy 617 filler wire. Low cycle fatigue and creep-fatigue properties of weldments are also discussed. The experiments cover a range of temperatures from 750 to 1000°C to support development of a new Code Case to qualify the material for elevated temperature nuclear design. Properties of the welded material are compared to results of extensive characterization of solution annealed plate base metal.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Development of Fiber Laser Weld Parameters for Stainless Steel and Refractory Metals

Laser welds were made in 21-6-9 stainless steel, vanadium and tantalum using LLNL's new 6kW fiber laser to target 1 mm penetration depths. The materials were machined into flat coupon samples with standard step-joint geometries, and were welded in a continuous wave mode. The laser was characterized using the Primes laser beam diagnostic system so that the beams can be reproduced in the future. The optical configuration consisted of a 200 {micro}m fiber, 200 mm collimator and 250 mm focusing lens, which delivered electron-beam level power densities in the 5 to 20 kW/mm2 range. The three different materials required different power densities to produce the desired penetration, and this report summarizes the results of this screening study that was directed at developing a first approximation to the proper welding parameters for future work. The results show that 1 mm penetrations can be achieved using a 400W beam for 21-6-9 stainless steel, a 600W beam for vanadium, and a 1,100W beam for tantalum using sharp focus and a travel speed of 40 inch/min. Future welds should incorporate a trailing gas shield to prevent discoloration of the surface and to prevent oxygen and nitrogen pickup in the welds.

36 MATERIALS SCIENCE↗

Effect of Welding Processes on the Microstructure, Mechanical Properties and Residual Stresses of Plain 9Cr-1Mo Steel Weld Joints

9Cr-1Mo steel designated as P9 is widely used in the construction of power plants and high-temperature applications. It is chosen for fabricating hexcan fuel subassembly wrapper components of fast breeder reactors. Arc welding processes are generally used for fabricating 9Cr-1Mo steel weld joints. A-TIG welding process is increasingly being adopted by the industries. In the present study, shielded metal arc (SMA), tungsten inert gas (TIG) and A-TIG welding processes are used for fabricating the 9Cr-1Mo steel weld joints of 10 mm thickness. Effect of the above welding processes on the microstructure evolution, mechanical properties and residual stresses of the weld joints has been studied in detail. All the three weld joints exhibited comparable strength and ductility values. 9Cr-1Mo steel weld joint fabricated by SMAW process exhibited lower impact toughness values caused by coarser grain size and inclusions. 9Cr-1Mo steel weld joint fabricated by TIG welding exhibited higher toughness due to finer grain size, while the weld joint fabricated by A-TIG welding process exhibited adequate toughness values. SMA steel weld joint exhibited compressive residual stresses in the weld metal and HAZ, while TIG and A-TIG weld joint exhibited tensile residual stresses in the weld metal and HAZ.

36 MATERIALS SCIENCE↗

2017 Accomplishments – Tritium Aging Studies on Stainless Steel Weldments and Heat-Affected Zones

In this study, the combined effects tritium and decay helium in forged and welded Types 304L and 21-6-9 stainless steels were studied. To measure these effects, fracture mechanic specimens were thermally precharged with tritium and aged for approximately 17 years to build in decay helium from tritium decay prior to testing. The results are compared to earlier measurements on the same alloys and weldments (4-5, 8-9). In support of Enhanced Surveillance, “Tritium Effects on Materials”, the fracture toughness properties of long-aged tritium-charged stainless-steel base metals and weldments were measured and compared to earlier measurements. The fracture-toughness data were measured by thermally precharging as-forged and as-welded specimens with tritium gas at 34.5 MPa and 350°C and aging for approximately 17 years to build-in decay helium prior to testing. These data result from the longest aged specimens ever tested in the history of the tritium effects programs at Savannah River and the fracture toughness values measured were the lowest ever recorded for tritium-exposed stainless steel. For Type 21-6-9 stainless steel, fracture toughness values were reduced to less than 2-4% of the as-forged values to 41 lbs / in specimens that contained more than 1300 appm helium from tritium decay. The fracture toughness properties of long-aged weldments were also measured. The fracture toughness reductions were not as severe because the specimens did not retain as much tritium from the charging and aging as did the base metals. For Type 304L weldments, the specimens in this study contained approximately 600 appm helium and their fracture toughness values averaged 750 lbs / in. The results for other steels and weldments are reported and additional tests will be conducted during FY18.

36 MATERIALS SCIENCE↗

Assessing Gaseous Hydrogen Assisted Fatigue Crack Growth Susceptibility of Pipeline Steel Weld Fusion Zones and Heat Affected Zones

The objective of this work was twofold: (1) measure reliable fatigue crack growth relationships for X65 steel and its girth weld in high-pressure hydrogen gas to enable structural integrity assessments of hydrogen pipelines, and (2) evaluate the hydrogen accelerated fatigue crack growth susceptibility of the weld fusion zone and heat-affected zone relative to the base metal. Fatigue crack growth relationships (da/dN versus ΔK) were measured for girth welded X65 pipeline steel in high pressure hydrogen gas (21 MPa) and in air. Hydrogen assisted fatigue crack growth was observed for the base metal (BM), fusion zone (FZ), and heat-affected zone (HAZ), and was manifested through crack growth rates reaching nearly an order of magnitude acceleration over rates in air. Addditionally, at higher ΔK values, crack growth rates of BM, FZ, and HAZ were coincident; however, at lower ΔK, the fatigue crack growth relationships exhibited some divergence with the fusion zone having the highest crack growth rates. These relative fatigue crack growth rates in the BM, FZ, and HAZ were provisional, however, since both crack closure and residual stress contributed to the crack-tip driving force in specimens extracted from the HAZ. Despite the relatively high applied R-ratio (R = 0.5), crack closure was detected in the heat affected zone tests, in contrast to the absence of crack closure in the base metal tests. Crack closure corrections were performed using the adjusted compliance ratio method and the effect of residual stress on K max was determined by the crack-compliance method. Crack-tip driving forces that account for closure and residual stress effects were quantified as a weighted function of ΔK and K max (i.e., K norm ), and the resulting da/dN versus K norm relationships showed that the HAZ exhibited higher hydrogen accelerated fatigue crack growth rates than the BM at lower K norm values.

36 MATERIALS SCIENCE↗

Cold Trap Replacement Project Report

This report documents the replacement of the Mechanisms Engineering Test Loop (METL) cold trap. The work involved preparation of the facility to replace the cold trap, removal of the existing welded cold trap from the sodium purification circuit, installation of a new replacement cold trap, completion of associated welds and examinations, restoration of instrumentation and heaters, and controlled return of the cold trap circuit to service. The replacement represented a significant maintenance evolution because the cold trap is an integral welded component of the sodium system. As a result, the work required coordinated control of sodium chemistry, deliberate formation of freeze plugs, inert gas management, precision cutting and welding, and a staged reheating and refill sequence. The activity was executed using procedural controls intended to protect personnel, preserve system cleanliness, and maintain the integrity of the sodium boundary throughout the work. This report provides a narrative summary of the milestone, including the purpose of the work, the pre-job system condition, the major field activities performed, observations made during execution, and the resulting post-work condition of the METL cold trap circuit.

42 ENGINEERING↗

An experimental investigation of the effectiveness of Ar-CO 2 shielding gas mixture for the wire arc additive process

Wire arc additive manufacturing (AM) is the process by which a large, metallic structure is built layer-by-layer using a welding arc to melt a wire feedstock. A novel opportunity exists to alter the shielding gas composition to fabricate distinct geometrical features without altering the other AM parameters. In this paper, shielding gases with varied concentrations of Argon (Ar) and CO 2 was used to deposit three distinct geometric shapes (walls, infill, and overhang) using a wire-based additive manufacturing system utilizing the gas metal arc welding (GMAW) surface tension transfer (STT) process. Computer-aided design (CAD) models were sliced with a custom-built slicer, and the sliced algorithm was converted into optimal robotic toolpaths. A custom virtual instrument (VI) was built in LabVIEW to compare the temperature profiles on the surface during each deposition process. After each deposition, the geometric features were scanned, and the surface waviness value was evaluated. Tensile and Charpy impact coupons were extracted from the wall geometries in the longitudinal and transverse directions and tested. The results indicated that a higher CO 2 content produced higher melt pool temperatures to an extent, while lower contents of CO 2 resulted in a dimensionally accurate geometry. The data also indicated that the 2%/98% CO 2 /Ar blend produced scatter in tensile strength and the analysis of variance (ANOVA) shows significant difference. However, the intermediate range of CO 2 (5–10%) resulted in uniform tensile properties. Altogether, these results indicate that a 5%/95% CO 2 /Ar blend is the ideal shielding gas for lowering process temperatures and improving mechanical properties in wire arc additive manufacturing using the gas metal arc welding surface tension transfer process. Additionally, varying concentrations of Ar/CO 2 can be used within the same part in order to modify the local properties or process parameters such as strength, toughness, temperature, or dimensional features. This may improve overall manufacturing quality without sacrificing specific properties.

42 ENGINEERING↗

Alternative PWHT to Improve High-Temperature Mechanical Properties of Advanced 9Cr Steel Welds

Creep-resistant 9Cr steels are extremely important in thermal power generation industry due to their marked resistance to creep and corrosion. The weldability of these alloys is critical since they are used in welded construction equipment. The required mechanical properties are achieved after post-weld heat treatment. This study examined the effect of different post-weld heat treatments on microstructure and mechanical properties of creep strength-enhanced 9Cr steel welding deposits. It was obtained with an experimental flux-cored arc welding wire used under protective gas (Ar-20% CO{sub 2}). The heat treatments used were: (1) tempering (760 °C × 2 h), (2) solubilizing (1050 °C × 1 h) + tempering (760 °C × 2 h) and (3) solubilizing (1150 °C × 1 h) + first tempering (660 °C × 3 h) + second tempering (660 °C × 3 h). All-weld metal chemical composition was analyzed, and hot tensile tests were carried out at different temperatures. Charpy-V impact tests and Vickers microhardness measurements were also performed. Microstructures were studied using x-ray diffraction and optical and scanning electron microscopy. In all cases, a martensitic matrix with intergranular and intra-granular precipitates was detected. In the as-welded condition, δ-ferrite was also found. Microhardness dropped, and the impact energy increased with post-weld heat treatments. The highest hot tensile strength result was achieved with samples submitted to austenization at 1150 °C and double tempering at 660 °C.

36 MATERIALS SCIENCE↗

Experimental Investigation and Numerical Study on the Elimination of Porosity in Aluminum Alloy Laser Welding and Laser–GMA Welding

Keyhole-induced porosity can strongly weaken the joint strength during aluminum alloy laser welding. Two factors are proposed to be responsible for the porosity formation: bubble formation caused by the instability of the keyhole and bubble captured by the solidification interface. Based on numerical and experimental results, the porosity is suppressed with preheating, due to the capillary stability of the keyhole and easy escape of bubble. N{sub 2} shielding gas has a minor effect on keyhole stability, but it reduces the porosity number as N{sub 2} bubble can dissolve into the liquid aluminum alloy melt pool quickly. The laser–gas metal arc (laser–GMA) welding process can stabilize the metallic plume and enlarge the weld pool. As a result, few spatters and bubbles are formed, and bubbles are easily escaped, both of which contribute to the suppression of porosity.

36 MATERIALS SCIENCE↗

Low-Cost Efficient Manufacturing of Pressurized Conformable Compressed Natural Gas Storage Tanks

The project goal was to combine welding and superplastic forming (SPF) processes to develop a conformal pressure vessel with >90% conformability, >12 MJ/kg energy density, and <$\$$1500 tank cost. PNNL investigated an extensive set of geometries and materials showing that reinforcement geometries based on the Schwarz-P minimal surface spanning a volume produced the highest flexibility in tank geometry, conformability, and nearly met the energy density target (11.9 vs. 12 MJ/kg) based on Titanium 6Al-4V material strength. The idealized geometry proved very challenging to achieve using welding and SPF of either tubing or sheet metal. PNNL demonstrated that full Schwarz-P shapes could be formed from titanium tubing using hot metal gas forming. However, that approach was discontinued because of the many components which required joining to assemble a tank structure. Superplastic blow-forming of a welded, multi-sheet pack was further developed using PNNL’s E-beam welding and SPF capabilities. Several sheet-pack designs were welded and formed, culminating in a small demonstration tank designed to withstand the design burst pressure. X-rays confirmed that the modeled internal structure was achieved during forming. During pressure tested the tank leaked (short of the required burst pressure) at thin spots in irregular E-beam welds connecting the outer pressure boundary to the inner reinforcing layers. However, the tank did not burst and the flat sides of the conformal tank were maintained, confirming the integrity of the internal reinforcements. Further refinement of the weld energy and speed plus the control of an automated welding machine would improve weld quality and increase the pressure to leak or burst.

03 NATURAL GAS↗

Control of Weld Residual Stress in a Thin Steel Plate through Low Transformation Temperature Welding Consumables

Low transformation temperature welding (LTTW) consumables are characterized by a low martensite start temperature and a large fraction of martensite forming in the weld. It can efficiently reduce the tensile residual stress because the volume expansion associated with the martensitic transformation compensates for the thermal contraction during cooling. In this work, a LTTW wire, designated as EH200B, was created for the arc welding of advanced high-strength steel thin plates. In comparison to conventional ER70S-3 wires, this LTTW wire generated an opposite distortion pattern. Neutron diffraction measurements along the center thickness of the welded plates showed the maximum residual stress along the longitudinal direction (LD) in the weld region, and the heat-affected zone (HAZ) immediately adjacent to the weld region was reduced from ~330 MPa to below 240 MPa by using the LTTW wire. A finite element (FE) model was developed to predict the residual stress distributions of the plates welded under these two wires. The simulation results showed reasonable agreement with the volume-average neutron diffraction data. Compressive residual stress in the weld region using the LTTW wire was predicted by the FE method. Electron backscattered diffraction and x-ray diffraction measurements confirmed ~90% martensite was present in the LTTW weld. The fatigue life of DP980 steel lap joint panels using EH200B wire nearly doubled that of ER70S-3 wire. This improvement was attributed to the high strength and low LD residual stress in the weld and HAZ immediately adjacent to the weld.

36 MATERIALS SCIENCE↗