Search NASA⌕ Search

SEARCH · Search NASA

Results for “PV fields”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

Field retrieved photovoltaic backsheet survey from diverse climate zones: Analysis of degradation patterns and phenomena

Understanding the impact of climate stressors on photovoltaic (PV) backsheet degradation in real-use conditions is critical to improve the accelerated testing exposures, extend the backsheet lifetime, and increase the confidence in PV reliability. Here, in this work, a total of 33 PV module backsheets were retrieved from six climatic zones worldwide with 2 - 28 years of exposure. These modules included five types of backsheet air-side materials (or outer layer): poly(vinylidene fluoride) (PVDF), poly(tetrafluoroethylene-co-hexafluoropropylene-co-vinylidene fluoride) (THV), poly(vinyl fluoride) (PVF), poly(ethylene terephthalate) (PET), and polyamide (PA). Attenuated total reflection Fourier-transform infrared spectroscopy (ATR-FTIR) was used to identify air-side materials. The degradation induced color change, gloss loss, and chemical material changes analyzed using optical microscopy, differential scanning calorimetry (DSC), scanning electron microscopy (SEM), colorimetry (yellowness index (YI)), and gloss measurements. PVDF, THV, and PVF air-side layer backsheets, in particular PVF, had minimal degradation in the air-side layer appearance and chemical structures after exposure in different climatic zones. The PET air-side backsheets exhibited obvious color increase (22.55 YI units after about 9 years exposure) and the PA/PA/PA backsheets showed large gloss loss (up to 76.4 %) relative to the unexposed backsheets. Severe cracks between cells that penetrated through the entire thickness of backsheets are observed on PA/PA/PA backsheets after 4-6 years of exposure in 6 climatic zones. The current indoor exposure standards were not sufficient to identify this degradation type. However, fluoropolymer based PV backsheets showed lower levels of degradation predictors and increased climatic resistance. Specific samples (PVF) showed little change from baseline after 28 years of outdoor exposure.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

First principles modeling of polymer encapsulant degradation in Si photovoltaic modules

An outstanding issue in the longevity of photovoltaic (PV) modules is the accelerated degradation caused by the presence of moisture. Moisture leads to interfacial instability, de-adhesion, encapsulant decomposition, and contact corrosion. However, experimental characterization of moisture in PV modules is not trivial and its impacts can take years or decades to establish in the field, presenting a major obstacle to designing high-reliability modules. First principles calculations provide an alternative way to study the ingress of water and its detrimental effect on the structure and decomposition of the polymer encapsulant and interfaces between the encapsulant and the semiconductor, the metal contacts, or the dielectric layer. Here, we use density functional theory (DFT) computations to model single chain, crystalline and cross-linked structures, infrared (IR) signatures, and degradation mechanisms of ethylene vinyl acetate (EVA), the most common polymer encapsulant used in Si PV modules. IR-active modes computed for low energy EVA structures and possible decomposition products match well with reported experiments. The EVA decomposition energy barriers computed using the Nudged Elastic Band (NEB) method show a preference for acetic acid formation as compared to acetaldehyde, are lowered in the presence of a water solvent or hydroxyl ion catalyst, and match well with reported experimental activation energies. This systematic study leads to a clear picture of the hydrolysis-driven decomposition of EVA in terms of energetically favorable mechanisms, possible intermediate structures, and IR signatures of reactants and products.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Field‐Relevant Degradation Mechanisms in Metal Halide Perovskite Modules

Field testing, failure analysis, and understanding of degradation mechanisms are essential to advancing metal halide perovskite (MHP) photovoltaic (PV) technology toward commercialization. Here, we present performance data from up to 1 year of outdoor testing of MHP modules in Golden, Colorado. The module encapsulation architecture and encapsulant materials have a significant impact on module reliability, with modules containing a polyolefin elastomer (POE) in addition to a desiccated polyisobutylene (PIB) edge seal outlasting modules with only a PIB edge seal or PIB blanket. Nondestructive and destructive characterization of the field-tested modules points to module scribes and interfaces as areas of potential mechanical weakness and chemical migration, resulting in shunt pathways and increased series resistance. Finally, indoor accelerated stress testing with light and elevated temperatures is performed, demonstrating failure with similar scribe degradation signatures as compared to the field-tested modules. In conclusion, under both outdoor testing and light and elevated temperature conditions, electrochemical corrosion between the copper electrode and the mobile iodine ions appeared dominant, with a significant progression at the scribes that is speculated to result from an interplay between the initial laser damage and joule heating from enhanced ion diffusion under bias.

14 SOLAR ENERGY↗

Resilience Metrics Framework for Solar Photovoltaics

This presentation was given at the Photovoltaic Specialist Conference (PVSC) 54 in New Orleans, Louisiana. Photovoltaic (PV) systems are routinely exposed to extreme weather, including wind and hail storms. Historically, most systems have proven to be resilient to such events, but some storms have damaged PV systems, leading to physical and financial loss. Storm hardening measures and specific system attributes can reduce this risk. This work introduces a set of resilience metrics and a framework for quantifying, comparing, and predicting PV system resilience. The framework is divided into two parts: 1) predictive, attribute metrics based on site and component characteristics, and 2) impact metrics that assess post-storm performance. Metrics are weighted and aggregated, producing hazard-specific resilience scores. We derive damage functions from storm-impacted PV systems, establishing a baseline against which post-storm performance can be compared. This damage was widely variable across hail and wind intensities, and field hail damage was less than predicted by laboratory tests, suggesting that system features - in addition to storm conditions - influence damage likelihood. Finally, the metrics framework is demonstrated using three case studies of storm damaged PV systems. Although additional data are needed to create attribute specific damage functions and establish metric weights, this study presents a methodology for evaluating PV resilience and contributes new damage functions to the literature.

14 SOLAR ENERGY↗

Non-contact Current-Voltage (I-V) Tracer for Photovoltaics

This report presents a non-contact approach to simultaneously obtain current-voltage (I-V) curves of photovoltaic (PV) substrings and modules in a string without the need of disconnecting the individual modules from the string. There are two types of I-V curve tracers currently available in the marketplace, capacitor-based and electronic load-based. The primary requirement of these conventional I-V tracers is the disconnection of individual modules in the string so the individual modules contacted through the connectors of the individual modules. These contact-tracers have three major limitations in the utility scale power plants: First limitation – Weather and Accuracy: The mass-produced commercial contact-tracers cannot obtain the I-V curves of both string and its modules (as high as 30 modules), almost simultaneously (within about 5 minutes) at, practically, a single irradiance level, a single module temperature, a single spectrum and a single AOI (angle of incidence). This inability of the contact-tracers forces the testing personnel to wait for an extended or multiple sunny (>800 W/m 2 ) duration(s) of a cloudy day. This is a serious limitation as waiting for the sunny conditions or days is a huge practical challenge in almost all locations, except desert locations. Also, since the I-V curves are obtained at different prevailing weather conditions, it becomes critical to translate all the measured I-V curves of 30 modules in the string to a single test condition, for example STC (standard test conditions), so the underperforming modules can be identified. The accuracy of translation equations is heavily influenced by the irradiance level and temperature, spectral and AOI ranges; Second limitation - Safety: The second limitation is related to the high voltage electrical safety of the test personnel during disconnecting and reconnecting of individual modules or cable connectors from the string under daylight conditions and damaging of the original module connectors (especially the field aged connectors) during the disconnecting and reconnecting process; Third limitation – Labor: The third limitation is related to the enormous amount of time and hardship for the test personnel under prevailing (often harsh) protracted field conditions. This project was executed by Arizona State University in collaboration with its industry partner, PV Measurements Inc. (PVM). To mitigate all the three challenges of the state-of-the-art equipment indicated above, we utilized a non-contact I-V (NCIV) tracer approach. In this approach, we utilized an electrostatic voltmeter (ESV) and voltage sensor/probe combination to obtain I-V curves. The ESV units are extensively used in the high voltage industry but not in the PV industry. To obtain the simultaneous I-V curves of the substrings and modules within a string, we utilized multiple commercial ESV-Probe sets. In this approach, we utilized a non-contact voltage sensor (called, Probe) placed on the glass surface of the module (above the last cell of the module). This probe senses the module voltage (with respect to ground) through measured capacitance which is dictated by the surface charges (which in turn is dictated by the module voltage) and transmits the sensed voltage to the voltmeter (called, ESV or NCV, non-contact voltmeter). The current is sensed by a non-contact hall sensor. In a 30-module string, the 30th probe obtains the entire string I-V along with the string I-V obtained by the electronic load. so that the I-V curves of the substrings and modules can be obtained by NCIV without the need of disconnecting the individual modules in the string. The string I-V curves obtained by the electronic load and NCIV can be compared for the accuracy determination. One can use 30 ESV units and 30 Probes to obtain 30 I-V curves of a 30-module string or use just 5 ESV units and 30 Probes in conjunction with 5 six-channel switchboxes (called, 6:1 switchboxes). To reduce the equipment cost, we utilized the 6:1 switchbox approach so the number of ESV units is reduced from 30 to 5. The approaches, achievements and challenges of this project are detailed in this report.

14 SOLAR ENERGY↗

Photovoltaic Cable Connectors: A Comparative Assessment of the Present State of the Industry [Slides]

The consequences of failure for balance of systems (BoS) components (such as PV cable connectors) include offline module string(s); low system voltage; arc, ground, insulation, and over-temperature faults; triggered fuse(s); system shutdown; and fire. The degradation modes for connectors are studied here through an industry survey and its subsequent examination, which are compared to field-degraded specimens. 117 specimens were obtained from a variety of locations and climates or accelerated tests. A failure analysis for connectors from PV installations was developed (and applied to 54 specimens) including nondestructive examinations (photography, a custom resistance-current scan, and X-ray computed tomography) and destructive examinations (featuring milling of the external plastic, extraction of the internal convolute spring, and potting and polishing in cross-section). Surface and through-thickness composition of the metal pins and springs was quantified using scanning electron microscopy with energy-dispersive X-ray spectroscopy. Fourier-transform infrared spectroscopy was used to verify the base polymer materials and compare the chemical structure of the connector body, bushing, end nut, and o-ring. Thermogravimetric analysis and differential scanning calorimetry were used to further verify the degradation of the same polymeric components. Updated from 2023 NIST/UL Workshop on Photovoltaic Materials Durability (website: https://events.ul.com/WPMogn?rt=aAuoWsl4E0KaORLCMeOgfA) and 2024 PVRW workshop (https://pvrw.nrel.gov/past-proceedings).

14 SOLAR ENERGY↗

Impact of duration and missing data on the long-term photovoltaic degradation rate estimation

Accurate quantification of photovoltaic (PV) system degradation rate (R D ) is essential for lifetime yield predictions. Although R D is a critical parameter, its estimation lacks a standardized methodology that can be applied on outdoor field data. The purpose of this paper is to investigate the impact of time period duration and missing data on R D by analyzing the performance of different techniques applied to synthetic PV system data at different linear R D patterns and known noise conditions. The analysis includes the application of different techniques to a 10-year synthetic dataset of a crystalline Silicon PV system, with emulated degradation levels and imputed missing data. Here, the analysis demonstrated that the accuracy of ordinary least squares (OLS), year-on-year (YOY), autoregressive integrated moving average (ARIMA) and robust principal component analysis (RPCA) techniques is affected by the evaluation duration with all techniques converging to lower R D deviations over the 10-year evaluation, apart from RPCA at high degradation levels. Moreover, the estimated R D is strongly affected by the amount of missing data. Filtering out the corrupted data yielded more accurate R D results for all techniques. It is proven that the application of a change-point detection stage is necessary and guidelines for accurate R D estimation are provided.

14 SOLAR ENERGY↗

Durable Module Materials (DuraMAT) Consortium (Final Technical Report)

The DuraMAT Consortium brings together DOE national lab and university research capabilities with the photovoltaic (PV) and supply-chain industries to accelerate a sustainable, just, and equitable transition to zero carbon electricity generation by 2035 through our five core objectives: development of a central data resource for PV modules, multi-scale and multi-physics modeling, disruptive acceleration science, forensic tools for fielded modules, and materials solutions for more durable, reliable, and resilient modules.

14 SOLAR ENERGY↗

Nextracker bifacial webinar in partnership with PV Evolution Labs

This presentation for a Nextracker-sponsored virtual symposium and webinar series leveraged PVEL's DOE-funded outdoor bifacial field study to explain potential for bifacial gain in dual-axis tracker mounting configurations. Data from PVEL's study also informed the modeling findings presented by Nextracker.

Meydbray, Jenya↗

Thermomechanical fatigue resistance of low temperature solder for multiwire interconnects in photovoltaic modules

Novel interconnect technologies leveraging low melting temperature solders, such as multiwire interconnects, are being deployed in photovoltaic (PV) modules for improved reliability through interconnect redundancy and lower thermal loads during interconnection and lamination. However, the equivalency of standardized accelerated testing to field conditions has not yet been established for these emerging technologies. In this study, the thermomechanical fatigue resistance of low temperature solder alloys is investigated and compared to that of conventional SnPb to assess the acceleration behavior of these alloys. While InSn is shown to have sufficient thermomechanical fatigue resistance on the order of that of SnPb, these results indicate Sn–Bi alloys may have poor thermomechanical fatigue resistance at field conditions. The results also show that Sn–Bi alloys have thermal cycling acceleration factors of less than one. This indicates that the standardized accelerated thermal cycling test, such as that in IEC 61215, will produce misleading results for Sn–Bi alloys and that unique testing is required for this PV module architecture. Though accelerated thermal cycling may be a meaningful qualification test for SnPb solder joints, these results suggest that mechanical loading may be a more appropriate test for Sn–Bi multiwire interconnects. This is due to the distinct processing and geometry of multiwire interconnects which may allow for mechanical, rather than strictly metallurgical interconnections.

14 SOLAR ENERGY↗

Photovoltaic Cable Connectors: A Comparative Assessment of the Present State of the Industry

The consequences of failure for balance-of-systems components (such as photovoltaic (PV) cable connectors) include offline module string(s); low system voltage; arc, ground, insulation, and overtemperature faults; triggered fuse(s); system shutdown; and fire. The degradation modes for connectors are studied here through an industry survey and its subsequent examination, which are compared with field-degraded specimens. A total of 117 specimens were obtained from a variety of locations and climates or accelerated tests. A failure analysis for connectors from PV installations was developed (and applied to 54 specimens), including nondestructive examinations (photography, a custom resistance-current scan, and X-ray computed tomography) and destructive examinations (featuring milling of the external plastic, extraction of the internal convolute spring, and potting and polishing in cross section). Surface and through-thickness composition of the metal pins and springs was quantified using scanning electron microscopy with energy-dispersive X-ray spectroscopy. Fourier transform infrared spectroscopy was used to verify the base polymer materials and compare the chemical structure of the connector body, bushing, end nut, and o-ring. Thermogravimetric analysis and differential scanning calorimetry were used to further verify the degradation of the same polymeric components.

cable connectors↗

Photovoltaic (PV) System Levelized Cost of Energy (LCOE) Evaluation with Grid Support Function Valuation and Service Lifetime Estimation

Photovoltaic (PV) systems play a critical role in renewable energy resource grid integration, and levelized cost of energy (LCOE) is commonly used to evaluate PV system feasibility in modern power grids. In this work, a revised PV system LCOE calculation model is derived to quantify the potential of LCOE reduction. Particularly, the grid support functions are valuated to offset the investment and operation costs of PV systems, which thereby reduces the LCOE. Meanwhile, PV system service lifetime is also estimated with the derived PV inverter reliability model, considering the critical components (i.e., semiconductor devices and capacitors). The case studies with field datasets are conducted to validate the effectiveness of the developed LCOE calculation model.

Zhao, Shijia↗

Impacts of PV Module Connector Failures on Cost and Performance of Utility Scale Photovoltaic Systems

The reliability, cost and performance of electrical connectors are a concern in all types of electrical systems, and demands on connectors used on photovoltaic (PV) systems include that connectors maintain electrical conductivity and physical strength, endure ultraviolet sunlight and high ambient temperature, and resist moisture and chemical intrusion over a very long (>25 year) performance period. Connector failures increase operation and maintenance (O&M) costs and reduce plant production, but connector failure can also cause safety and liability problems, which are of greater concern. This work results from a three-year collaboration between Sandia National Laboratories (SNL), the Electric Power Research Institute (EPRI), and the National Renewable Energy Laboratory (NREL) and funded by the U.S. Department of Energy (DOE) Solar Energy Technology Office (SETO) under Agreements #39035 and #38531 "Connector Reliability Across the US Solar Sector." a multi-pronged investigation of PV connector health across the US (see https://energy.sandia.gov/pvconnectors/). This report presents derivation of a Techno-Economic Analysis (TEA) that models failure modes and frequencies (how often failure occurs), estimates O&M costs and lost production associated with connector failures, and then calculates the effect that PV module connectors can have on Levelized Cost of Energy (LCOE). The model is informed with initial data from quantitative assessment of failure rates, root causes and mechanisms, in-situ diagnostics and data collection, lab-based forensics, and interviews with PV connector manufacturers and plant operators. SNL conducted site inspections at multiple utility-scale sites in different climates and subjected field samples of new, used, and degraded connectors to visual and electrical characterization. EPRI conducted metallurgical analysis of the pin and sleeve conductors to study failure-induced morphological and compositional changes. There is in general a shortage of statistically valid data, but data from PVROM database maintained by SNL was sufficient to ascertain failure rates and lost production as well as provide qualitative insight in its curated maintenance records. This report details the structure of the mathematical model but the sources of data to inform the model will continue to evolve. Analysis of a 100 MW PV plant is provided as an example of the use of the model, with results indicating that connectors are responsible for Annualized O&M Costs of $\$$71,933/year; Annualized Unit O&M Costs of $\$$0.72/kW/year; that a Reserve Account of $\$$187,220 should be available to fund repairs related to connectors; that connectors add $\$$1,494,004 to the Net Present Value of the O&M Costs (project life); and that O&M related to connectors adds about $\$$0.00088/kWh to the Levelized Cost of Energy. The impact of this model is to provide a tool to make the US solar sector more robust by quantifying and monetizing the reliability risks to utility-scale PV systems posed by poorly installed, mismatched and/or poorly designed and manufactured connectors. The TEA provides a model incorporating failure statistics, O&M cost data, and lost production into a single figure of merit, informing decisions and enabling practitioners to optimize cost and performance trade-offs. Stakeholders include connector manufacturers, system designers and equipment specifiers, standards bodies, installers and O&M providers, investors and insurance underwriters. This report supports continued growth of PV predicated on assurances that properly installed and maintained PV system connectors are safe and reliable. The project team is proposing future work including accelerated testing of connectors and expanding the approach taken here to other PV system components, such as TEA for rapid shut-down devices.

14 SOLAR ENERGY↗

Adaptive Protection and Validated Models to Enable Deployment of High Penetrations of Solar PV (PV-MOD)

The availability and validation of various PV models in commercial tools differ, with some models not yet thoroughly validated for advanced inverter functionalities and reliable performance under weak system conditions. Many existing models do not fully incorporate new inverter control functions, which can affect system stability. The increasing deployment of solar PV and other inverter-based resources (IBRs), including distributed energy resources (DERs), is influencing the reliable operation of protection schemes in distribution systems and microgrids. Emerging adaptive protection schemes (APS) offer new opportunities for protecting these systems during varying configurations and DER operating conditions, though their demonstration and validation remain limited. Adaptive protection schemes face similar challenges, as they are typically designed for specific configurations. There is a growing need for tools and methodologies to streamline the deployment of adaptive protection for safe and reliable DER integration. The project main objective was to develop and validate high-fidelity generic models of solar PV facilities for stability, protection, EMT, and QSTS analyses. This objective was achieved, and these models can now be integrated into commercial software tools, enabling utilities, vendors, and developers to study high-penetration PV systems more confidently. The project also demonstrated advanced applications of these models, including the design and deployment of adaptive protection schemes in high-penetration field applications and microgrids, supporting grid safety and reliability. Several milestones were reached by the end of the project. A sophisticated inverter test plan was developed, and inverters representative of the North American marketplace were selected. EPRI and NREL tested various inverters, conforming to IEEE standards. Improvements were made to existing generic models of IBR units, IBR plants, and aggregated feeders for various analyses. The first generic electromagnetic transient (EMT) model for a solar PV plant was developed, conforming to IEEE Std 2800™-2022 and validated against laboratory measurements of a 2.2 MVA large-scale battery energy storage system (BESS) inverter. That model was then used to produce reference responses illustrating examples of validated and verified IBR plant models that pass or fail tests for technical minimum capability and performance as specified in the IEEE standard. The developed, tested, and validated generic models can be used for transmission planning, stability assessments, expansion planning, and evaluating potential future IBR interconnection requirements. They can also support interconnection screens and conformity assessments of IBR plants, including solar PV. The project significantly contributed to the ongoing standardization and model-based representation and verification of IBR responses. The project further addressed challenges of common distribution protection schemes with increasing deployment of DER by developing, validating, and demonstrating adaptive protection schemes (APS) that can improve the reliable and safe integration of DER into distribution systems. New APS were designed using improved DER models for three common distribution systems: a radial feeder, a meshed network, and a microgrid. Modeling and hardware-in-the-loop (HIL) testing of the APS were conducted, successfully showing their effectiveness and selectivity. Proof-of-concept field demonstration was achieved for two APS, i.e., one on a radial feeder and another one in a microgrid. Field demonstration could not be achieved for the APS on a meshed network, primarily due apprehension of one utility partner and also due to limited access to the protective algorithms in the network protectors. Guidelines developed from the lessons learned in the project lay out the general process followed in the design, installation, and commissioning of APS for various distribution systems. Distribution utility partners’ apprehension about field demonstration of the new APS were addressed—with varying success—by taking a stepped risk-management approach of modeling of a wide range of sensitivities first, performing in-depth proof-of-concept testing in the laboratory including HIL next, and finally deliberately implementing and commissioning the actual protection equipment and algorithms into parts of—or in parallel operation to—the three real distribution systems. Future work should include pilot projects that further show the acceptable performance of the developed APS before these schemes be rolled out more widely. Inclusion of both utility and original equipment manufacturers (OEMs) in future projects could increase chances of successful field demonstration. Despite challenges in achieving the field demonstration goal of the project for all three APS, the research significantly contributed to the innovation of adaptive protection solutions for scalable and reliable DER integration into distribution systems. This project significantly enhances the understanding of the impact of using appropriate inverter models on distribution and transmission (T&D) systems. By addressing the limitations of existing generic models, the project introduces high-fidelity models for stability, protection, electromagnetic transient (EMT), and quasi-static time series (QSTS) analyses. These models, integrated into commercial software tools, enable utilities, vendors, and developers to confidently study high-penetration PV systems. The project also demonstrates advanced applications, including adaptive protection schemes (APS) for distribution systems and microgrids, ensuring grid safety and reliability. The technical effectiveness and economic feasibility of the methods are evident through the development and validation of sophisticated inverter test plans and the selection of representative inverters. Testing by EPRI and NREL on retail, commercial, and utility-scale inverters, conforming to IEEE standards, underscores the robustness of the models. Improvements to existing generic models for various analyses further enhance their validity and applicability. The project also identifies gaps in common distribution protection schemes and designed new APS using improved DER models, demonstrating their effectiveness through modeling and hardware-in-the-loop (HIL) testing. The project’s benefits to the public are manifold. By advancing the standardization and model-based representation of IBR response, it supports transmission planning, stability assessments, and future IBR interconnection requirements. The generic models can facilitate better communication between transmission planners and developers, supporting expected IBR plant capability and performance. Additionally, the development of APS for radial feeders, meshed networks, and microgrids supports the integration of distributed energy resources (DERs) into distribution systems, enhancing grid reliability and safety. The project’s emphasis on thorough testing and simplicity in design ensures practical and scalable solutions for DER integration.

14 SOLAR ENERGY↗

Development of Mission Profiles for Humidity Models in the Reliability Testing of PV Inverters: Preprint

To understand the impacts of humidity on PV inverters, mission profiles were developed to accurately describe the different processes and rates based on the environmental factors of temperature, relative humidity, and irradiance. The operating environment of the device introduces stress factors dependent on component temperature, relative humidity, and component voltage. The development of profiles started from looking at historical climate conditions at Cocoa, Florida, a hot and humid location. The profile developed from field location was compared with existing humidity test profiles in industrial and military standards to determine acceleration factors. Prior to the evaluation of the mission profiles, critical components in the PV inverter were identified based on vendor discussions along with failure modes of interest. The profiles considered in this study was demonstrated using a 4-kVA string inverter. The measurements from the devices were substituted in device manufacturer specified equation to determine the severity of each test. The severity of each test was compared against the severity of the 24-hour result to determine the acceleration factor of each test. The acceleration factors were determined to be over a range of 1.2-6 for the existing humidity tests from standards, when compared against the mission profile developed from field data. This optimal humidity/thermal profile will be passed to the IEC standards development for inverter qualification testing.

humidity models↗

Surface Stress Characterization and Trends in Thermally Strengthened Photovoltaic Module Glass

Simultaneous changes in photovoltaic (PV) module architecture-such as increased area, replacing the polymeric backsheet with a glass backsheet, and reducing glass thickness from 3.2 to 2.0 mm-have resulted in a novel failure called spontaneous glass breakage. Spontaneous glass breakage results in front and/or rear glass failure without any obvious cause. The resulting low-energy fracture patterns have raised concerns about the thermal strengthening in 2.0-mm glass. We present validation of a nondestructive method for measuring the glass surface stress in PV modules. We use a scattered light polariscope to examine the glass properties of 11 modules from 6 solar fields, with and without spontaneous glass breakage. Based on a Mann-Whitney test p-value of 1.4 x 10-6, we conclude that there is a correlation between lower surface stress and susceptibility to spontaneous breakage. A Kendall's Tau test p-value of 2.0 x 10-4 indicates a correlation between increased module area and lower surface stress. We find that 2.0-mm glass can be, and often is, fully tempered (surface stress ≥69 MPa), but inspecting the fracture pattern is not a reliable way to assess the amount of thermal strengthening. A combination of factors, not just surface stress, influences glass breakage.

14 SOLAR ENERGY↗

Failure Analysis of a New Polyamide-Based Fluoropolymer-Free Backsheet After Combined-Accelerated Stress Testing

The viability of novel coextruded, fluoropolymer-free backsheets for photovoltaic (PV) modules has been questioned as a result of a large number of early-life backsheet failures in PV installations containing one of the earliest co-extruded polyamide (PA)-based backsheet to reach the market, “AAA.” New PV reliability testing protocols have been recently developed and applied to backsheets to reproduce failures observed in the field and evaluate the durability of novel backsheet materials and designs prior to commercialization. A new co-extruded PA-based backsheet was tested using combined-accelerated stress testing (C-AST) and demonstrated a greater lifetime than AAA, and some other fluoropolymer-based backsheets such as polyvinylidene fluoride. The improved PA-based backsheet also eventually failed by through-thickness cracking. Using surface and bulk material characterization techniques, we performed a comprehensive study of material properties before and after the stress testing. Aging of the backsheet resulted in an increase of surface roughness by erosion of the outer PA layer. However the failure is more likely related to an increase in crystallinity of the polyolefin core layer reducing the backsheet tearing energy. The analysis can ultimately inform on the specific weaknesses of the materials so that the manufacturer can improve the backsheet design to extend its lifetime.

14 SOLAR ENERGY↗

Reducing module soiling with scalable and robust photocatalytic coatings

The air-glass interface at the front of a photovoltaic (PV) module reflects approximately 4% of incident light, decreasing the potential power output of the module by the same amount. Today’s modules reduce this loss by adding a low-refractive-index (1.25-1.30) SiO2 coating to the sunward side of the module glass; this antireflection coating recovers approximately 3% of the 4% light that would otherwise be lost. While such antireflection coatings work very well on clean, new modules, they do not inhibit soiling—the accumulation of soilants such as dust, pollen, soot, or other foreign material—on the module glass, and soilants reflect and scatter incident light. An improved coating would serve provide not only an antireflection effect, but also an anti-soiling effect. The goal of this project was to develop such a coating and provide a path for it to be manufactured in the U.S. The project successfully designed and fabricated coatings that provided >3% transmittance gain compared to bare glass (matching the performance of commercial antireflection coatings) and displayed anti-soiling behavior in standard laboratory soiling effects. This was achieved by using a Swift Coat proprietary coating deposition technique, aerosol impact-driven assembly (AIDA), to control the porosity and thus refractive index of coatings of photocatalytic materials—such as TiO2—that would otherwise increase (instead of decrease) reflection. These combined antireflection/anti-soiling coatings passed PV industry standard module reliability tests as well as coating-specific abrasion tests, showing that they have the durability needed for decades in the field. Swift Coat scaled the AIDA hardware and deposition process to make mini-modules that were monitored for nearly two years during field tests administered by a third party, as well as demonstrated scaling to the widths of full-sized modules. The fielded mini-modules outperformed reference modules (with commercial antireflection coatings) in two locations, providing a 1% absolute average performance boost and larger increases during periods of heavier soiling. Swift Coat’s cost analysis indicated a coating manufacturing cost below the sales price of today’s antireflection coatings. More than five module manufacturers sampled and assessed the coatings, and three provided letters of support. The coating developed in this project increases the energy output of PV modules, thereby decreasing the cost per kilowatt-hour of solar energy generated. Cheaper solar electricity benefits the public by accelerating the transition to a stable, affordable, carbon-free energy economy. In addition, for select applications in which PV modules are highly visible—such as on residential rooftops—the coating provides an aesthetic benefit because it stays cleaner than today’s modules. Finally, Swift Coat and its prospective customers are U.S. companies, and successful commercialization of this technology will provide U.S. jobs and a secure solar supply chain.

14 SOLAR ENERGY↗