Ultrasonic Gear Steel Fatigue at NASA

Gear tooth bending fatigue life is one of the main drivers of rotorcraft gear box weight and maintenance cost. Depending on rotorcraft gearbox speed, 10,000 flight hours can easily mean reaching gear tooth bending fatigue cycles in the 10^10 cycle regime. Traditionally gear fatigue life in the 10^10 cycle regime is estimated based on empirical correction factors applied to the traditional fatigue limit of 10^7 cycles. In order to improve on this method of life prediction, enable better gear box design, and reduce gear box maintenance cost, NASA has started an ultrasonic gear steel fatigue program to quantify the 10^10 life of gear steels. Ultrasonic fatigue testing makes use of piezo electric actuators and resonance to generate stress-strain cycles at 20 kHz. The ability to test gear steals at 20 kHz reduces test time for 10^10 cycles from roughly 16 years with traditional 20 Hz testing to 6 days. In this presentation, the establishment of NASA's ultrasonic test capability, results to date, and future testing plans will be discussed.

Tallerico, Thomas F.↗

Very High Cycle Fatigue Testing of AMS 6308 Steel

Lightweight and reliable gearboxes are required for helicopters and future electrical vertical take-off and landing aircraft. Mechanical gears in these applications experience more than 10 7 million fatigue cycles over their operating life and between maintenance intervals. Fatigue data for gear steels above 10 7 cycles is rare due to the testing time required to reach these cycle counts with traditional methods. In this paper, ultrasonic fatigue testing is used to collect mechanical fatigue data on AMS 6308 steel in the 10 7 to 1010 cycle regime.

Thomas Tallerico↗

Aluminum to Stainless-Steel Joints for Cryogenic Applications

Aluminum to stainless-steel joints are necessary for cryogenic applications such as cryogenic fluid management and combustion devices. Supplemental development in this area was required for a test program at NASA Marshall Space Flight Center (MSFC) of an Al6061-RAM2 additively manufacturing liquid rocket nozzle. The test program identified a risk for installing stainless-steel fluid fittings to aluminum manifolds. To address this, a literature search was completed for various joint designs, and three designs were down selected to be cryogenic pressure cycle tested at MSFC. The test pieces were subsequently burst tested with ambient temperature water. This paper provides an overview of the literature review, down selected designs, test setup, test results, and fractography. The test results informed design decisions for the Al6061-RAM2 nozzle, and the recommended design proved to be a robust option with no notable issues identified during hot-fire testing.

Tessa M. Fedotowsky↗

Changes Found on Run-In and Scuffed Surfaces of Steel Chrome Plate, and Cast Iron

A study was made of run-in and scuffed steel, chrome-plate, and cast-iron surfaces. X-ray and electron diffraction techniques, micro-hardness determinations, and microscopy were used. Surface changes varied and were found to include three classes: chemical reaction, hardening, and crystallite-size alteration. The principal chemical reactions were oxidation and carburization.

IRON, CAST - WEAR RESISTANCE↗