The Influence of Residual Stress on Fatigue Crack Growth Rates in Stainless Steel Processed by Different Additive Manufacturing Methods

The properties and microstructure of Type 304L stainless steel produced by two additive manufacturing (AM) methods—directed energy deposition (DED) and powder bed fusion (PBF)—are evaluated and compared. Localized heating and steep temperature gradients of AM processes lead to significant residual stress and distinctive microstructures, which may be process-specific and influence mechanical behavior. Test data show that materials produced by DED and PDF have small differences in tensile strengths but clear differences in residual stress and microstructural features. Measured fatigue crack growth rates (FCGRs) for cracks propagating parallel to and perpendicular to the build directions differ between the two AM materials. To separate the influences of residual stress and microstructure, K-control test procedures with decreasing and constant stress intensity factor ranges are used to measure FCGRs in the near-threshold regime (crack growth rates ≤ 1 × 10 −8 m/cycle). Residual stress is quantified by the residual stress intensity factor, K res , measured by the online crack compliance method. Correcting the FCGR data for differences in K res brings results for specimens of the two AM materials into agreement with each other and with results for wrought specimens, when the latter are corrected for crack closure. Differences in microstructure and tensile strength have an insignificant influence on FCGRs in these tests.

additive manufacturing↗

Preliminary Study on Machining of Additively Manufactured Ti-6Al-4V

We report additively manufactured metals differ from their conventionally produced counterparts due to the inherent material inhomogeneity, porosity, and thermal stress induced by the process. These differences make the machining of additively manufactured metals more difficult and cause premature tool failure or unexpected surface finish at certain conditions. This study takes the first step to investigate and identify the causes of these issues, particularly for Ti-6Al-4V. Printed and wrought samples, as well as heat treatment effect, are compared in a dry cutting condition at a cutting speed of 90 m/min in terms of cutting power, vibration, temperature, and produced surface finish. The results show a lower cutting power and more vibration for as-printed Ti samples, indicating a less ductile microstructure and inclusion of pores. Heat treatment can eliminate these phenomena. There is no significant difference found in the produced surface finish at the current cutting condition.

36 MATERIALS SCIENCE↗

Deformation and Fracture Behavior of Additively Manufactured 316L Stainless Steel

Tensile deformation and fracture behavior of an additively manufactured (AM) 316L stainless steel (SS) in the as-built, stress-relieved, and solution-annealed conditions was investigated using in situ tensile testing in a scanning electron microscope with an electron back scattering diffraction (SEM–EBSD) detector. Analyses were performed to discuss the characteristic deformation and fracture process of the fine-grained AM 316L SS with and without relaxation heat treatment. The as-built 316L showed the highest strength, and both post-build heat treatments lowered the strength of the alloy. Regardless of the post-build processing, the AM 316L SS showed overall higher strength but slightly lower ductility when compared to the wrought (WT) 316L SS. Analysis of EBSD data indicated that the characteristic microstructural features from AM, such as the complex and fine grain morphology, dislocation network, pores, and silicon-rich oxides, evolved and exerted various roles during the tensile deformation and fracture processes. Further, it was obvious that the interaction of dislocation slips with oxide particles and cavities (or pores) resulted in an accelerated cracking in AM 316L SS. Overall, however, their influence on mechanical behavior was limited, as the genuinely high ductility of 316L SS could help avoid any premature or brittle fracture.

36 MATERIALS SCIENCE↗

Mechanical Characteristics of Additively Manufactured ODS 316L and 316H Alloys with and Without Post-build Processing

This research aims to explore an accelerated development path for oxide dispersion-strengthened (ODS) alloys by integrating additive manufacturing (AM) technologies with recent advances in ODS materials and traditional manufacturing methods. Novel AM and post-build processing routes have been developed for ODS austenitic alloys, specifically Fe-Cr-Ni alloys like 316L and 316H. Electron microscopy and mechanical characterizations were conducted to evaluate the effects of process variables on microstructure and properties, aiming for an economically feasible route property optimization. Traditionally, ODS alloy production involves multi-day high-energy mechanical milling of alloy powder with yttria (Y 2 O 3 ) followed by powder consolidation via extrusion or other methods and additional thermomechanical processing (TMP) for property control. Here, to address these challenges associated with this complex and costly approach, we propose exploring alternative, cost-effective processing routes focusing on AM and traditional TMP methods. The new ODS alloy processing routes have achieved up to a 400% increase in yield strength and a 60% increase in ultimate tensile strength compared to wrought stainless steels while still maintaining significant ductility and fracture toughness. This paper details the novel and economical AM-based processing routes for ODS austenitic alloys, combined with post-build TMPs, and discusses the mechanical and microstructural characteristics of the developed materials.

Byun, Thak Sang [Oak Ridge National Laboratory (OR↗

Ending the Energy-Poverty Nexus: An Ethical Imperative for Just Transitions

Arguments for a just transition are integral to debates about climate change and the drive to create a carbon-neutral economy. There are currently two broad approaches rooted in ethics and justice for framing just energy transitions. The first can be described as internal to the transition and emphasizes the anticipation, assessment, and redressing of harms created by the transition itself and the inclusion in transition governance of groups or communities potentially harmed by its disruptions. In this article, we propose a second approach to ethics and justice in an energy transition, which we describe as systemic or societal in scope. This approach complements attention to the proximate dynamics and impacts of the transition process with a focus on the distant societal and economic outcomes the transition brings into being and how they compare to conditions prior to the transition. It poses the question: do the transformative social, economic, and technological changes wrought by energy systems create more just societies and economies, or do they instead reinforce or recreate long-standing injustices and inequalities? We illustrate this approach with an assessment of one of the most significant existing forms of energy injustice: the energy-poverty nexus. We argue that the energy-poverty nexus reflects configurations of socio-energy systems that create complex, extractive feedbacks between energy insecurity and economic insecurity and, over time, reinforce or exacerbate poverty. We further argue that just energy transitions should work to disentangle these configurations and re-design them so as to create generative rather than extractive feedbacks, thus ending the energy-poverty nexus and creating long-term outcomes that are more just, equitable, and fair.

14 SOLAR ENERGY↗

Effects of heat treatment and build orientation on the evolution of $ϵ$ and $α'$ martensite and strength during compressive loading of additively manufactured 304L stainless steel

In this paper, the effect of heat-treatment and build orientation on martensitic phase transformation in additively manufactured (AM) 304L stainless steel is studied and compared with conventionally produced wrought material. The relationships between observed martensitic transformations and material microstructures and their effects on mechanical strength are established through experimental observations. In situ high-energy X-ray powder diffraction measurements were performed to monitor the evolution of $ϵ$ and $α'$ martensite during compressive loading of stainless steel. Electron backscatter diffraction (EBSD) was used to provide insight on initial grain morphology, crystallographic misorientation within grains, and crystallographic texture. Heat treatment alters the microstructure of AM samples creating different initial conditions. This difference in starting microstructure resulted in variability in martensitic transformation during compressive deformation. The rate of martensitic transformation decreased for AM samples treated with temperatures up to 1100°C, after which the AM microstructures recrystallized, resulting in increased rate of martensitic transformation for those samples treated at higher temperatures. It was also observed that aligning the axis of compression with the AM build direction resulted in a lower rate of strain-induced martensite formation as opposed to aligning the compression axis perpendicular to it. More favorable distribution of crystal orientations in the latter loading orientation promoted martensitic transformation. These and additional experimental observations from EBSD in terms of kernel average misorientation, mean grain orientation spread, and mean crystallite size reveal strong microstructural effects on strength of additively manufactured metallic materials.

304L stainless steel↗

Microstructure and properties of a high temperature Al–Ce–Mn alloy produced by additive manufacturing

An Al–10Ce-8Mn (wt%) alloy was designed and fabricated by laser powder bed fusion additive manufacturing (AM). The rapid cooling rates of the AM process produced a refined microstructure with a large fraction of reinforcing intermetallic phases. The tensile properties of the alloy were characterized in the as-fabricated state and following thermal exposure. The properties of the as-fabricated microstructure showed exceptional high-temperature performance and strength retention at elevated temperatures up to 400 °C relative to benchmark wrought Al and AM Al alloy properties. Characterization of the microstructure and thermodynamic modeling of the ternary Al–Ce–Mn system rationalized the solidification and solid-state phase transformations. Finally, analysis of the relevant strengthening mechanisms for both the as-fabricated and thermally exposed conditions was performed.

36 MATERIALS SCIENCE↗

Mechanical properties and strain localization of WA-DED printed P91 steel

This paper discusses a P91 steel block that was additively manufactured by wire arc direct energy deposition (WA-DED) followed by two types of post-process heat treatment (PPHT). Vickers microhardness and digital image correlation tensile tests were performed along the building direction. The global mechanical properties (i.e., microhardness and tensile properties) and the local mechanical responses (i.e., hardness fluctuation and strain localization) were systematically investigated. Results showed that (1) all P91 specimens showed higher strengths than American Society of Mechanical Engineers standard requirements for wrought P91 steel, (2) the as-printed P91 exhibited much higher average hardness and fluctuations than that after PPHT, (3) PPHT reduced P91 strengths but improved the ductility significantly, and (4) strain localization presented in the as-printed specimen during uniform deformation in tensile tests. The hardness fluctuation and strain localization along the building direction of the AP P91 were caused by different thermal histories received during WA-DED. The study indicated that PPHT, ideally tempering-only heat treatment, is necessary for the WA-DED printed P91 steel.

Mechanical properties↗

An additive manufacturing design approach to achieving high strength and ductility in traditionally brittle alloys via laser powder bed fusion

Additive Manufacturing (AM) presents unprecedented opportunities to enable design freedom in parts that are unachievable via conventional manufacturing. However, AM-processed components generally lack the necessary performance metrics for widespread commercial adoption. We present a novel AM processing and design approach using removable heat sink artifacts to tailor the mechanical properties of traditionally low strength and low ductility alloys. The design approach is demonstrated with the Fe-50 at.% Co alloy, as a model material of interest for electromagnetic applications. AM-processed components exhibited unprecedented performance, with a 300 % increase in strength and an order-of-magnitude improvement in ductility relative to conventional wrought material. These results are discussed in the context of product performance, production yield, and manufacturing implications toward enabling the design and processing of high-performance, next-generation components, and alloys.

36 MATERIALS SCIENCE↗

Microstructure and high temperature tensile properties of 316L fabricated by laser powder-bed fusion

316L stainless steel fabricated by laser powder-bed fusion (LPBF) has attracted significant attention due to a unique combination of strength and ductility at room temperature. Understanding of high temperature tensile properties of LPBF fabricated 316L is, however, limited. In the present investigation, tensile testing was conducted at 20–700ºC on LPBF 316L in as printed condition and after annealing for 5 h at 500–800ºC. Room temperature data confirmed the excellent ductility of the LPBF-processed 316L steel due to the cellular structure with high dislocation density. However, a significant decrease in ductility was observed at temperatures above 200ºC. These results are consistent with a change of deformation mechanisms observed in wrought 316L, with twinning playing a key role at room temperature. Finally, microstructure characterization and tensile testing revealed that the cellular structure is stable up to 500ºC, but a decrease of yield strength was observed at temperatures above 600ºC likely due to a decrease in dislocation density via annealing.

36 MATERIALS SCIENCE↗

Deformation and fracture behavior of a laser powder bed fusion processed stainless steel: In situ synchrotron x-ray computed microtomography study

Tensile plastic deformation and fracture behavior of a laser powder bed fusion processed 316L stainless steel alloy was investigated in situ using high-resolution synchrotron x-ray computed microtomography (sXCT). Three different cases were studied: (1) specimen A1, near full-density with initial porosity of 0.04%, (2) specimen B1, initial lack-of-fusion (LOF) porosity of about 3% with the major axis of defects aligned nearly perpendicular to the tensile loading direction (LD), and (3) specimen B, similar to B1 but with the major axis of LOF defects aligned nearly parallel to LD. The effects of type, density, and orientation of defects in as-printed samples on plastic deformation and failure modes were studied by analyzing sXCT image sequences and quantitative defect properties. Specifically, the evolutions of porosity, size, aspect ratio, and angle of gas pores and LOF defects were characterized as a function of applied strain. Moreover, interactions between as-printed defects and deformation-induced crack propagation were investigated. The tensile behavior of specimen A1 was comparable to that of a commercial wrought plate. Furthermore, the quantitative in-situ sXCT results showed a void-growth phenomenon in A1 but without noticeable coalescence, resulting in a ductile cup-cone failure. Specimen B1 showed damage-driven brittle failure with limited plasticity due to early and rapid propagation of open voids. On the other hand, specimen B, with a similar amount of LOF defects as B1, showed deceivingly strong and ductile tensile behavior similar to A1 without any major crack propagations due to the favorable orientation relationship between LOF defects and the LD.

36 MATERIALS SCIENCE↗

Phase transformation dynamics guided alloy development for additive manufacturing

Fusion-based additive manufacturing technologies enable the fabrication of geometrically and compositionally complex parts unachievable by conventional manufacturing methods. However, the non-uniform and far-from-equilibrium heating/cooling conditions pose a significant challenge to consistently obtaining desirable phases in the as-printed parts. Here, in this study, we report a martensite stainless steel development guided by phase transformation dynamics revealed by in-situ high-speed, high-energy, high-resolution X-ray diffraction. This developed stainless steel consistently forms desired fully martensitic structure across a wide range of cooling rates (10 2 –10 7 °C/s), which enables direct printing of parts with fully martensitic structure. The as-printed material exhibits a yield strength of 1157 ± 23 MPa, comparable to its wrought counterpart after precipitation-hardening heat-treatment. The as-printed property is attributed to the fully martensitic structure and the fine precipitates formed during the intrinsic heat treatment in additive manufacturing. The phase transformation dynamics guided alloy development strategy demonstrated here opens the path for developing reliable, high-performance alloys specific for additive manufacturing.

17–4 PH stainless steel↗

Using post-processing heat treatments to elucidate precipitate strengthening of additively manufactured superalloy 718

The poor machinability and extensive work hardening of Ni-based superalloys makes additive manufacturing an attractive option for producing geometrically complex components with distinct microstructures. Although previous studies show recovery of high strength at room temperature, very few studies demonstrate successful properties at elevated temperatures required for industrial applications. Here, the objectives of this study are to present a post-build heat treatment for high strength across a wide temperature range, determine the strength contribution of nanoscale precipitating phases to the overall mechanical properties of superalloy 718, and from these, provide a comprehensive microstructure-property relationship for wrought and AM 718 to guide efforts to simulate the properties of AM components. Laser powder bed fusion–produced superalloy 718 was characterized at multiple length scales using scanning electron microscopy and transmission electron microscopy in the as-built condition and with multiple heat treatments designed to form combinations of γ', γ", and δ precipitates. Uniaxial tensile tests performed from room temperature to 600 °C on subsize specimens determined the yield strength, elastic modulus, ultimate tensile strength, fracture stress, and uniform elongation. Precipitates in this work proved to be weak barriers to dislocation motion through a dispersed barrier model, but they provided strength to the alloy through their consistent high density. The relative contribution to the yield strength from γ" remained consistent between 48% and 57% of the total strength up to 600 °C, the primary influence on the high temperature strength of superalloy 718. The strength factors for γ" and δ precipitates were found to trend inversely with tensile test temperature and may be attributable to the differences in precipitate coherency. A post-build heat treatment is recommended to maintain high strength at elevated temperatures. A quantitative microstructure-property relationship, dependent on precipitate size, density, and morphology, was derived and can estimate the yield strength across a wide temperature range applicable to the operational regimes for superalloy 718.

36 MATERIALS SCIENCE↗

Anisotropic spall failure of additively manufactured 316L stainless steel

The dynamic high strain rate tensile (spall) failure of additively manufactured (AM) materials is an area of great interest but much less understood than material failure under other loading regimes. The research presented here examines the effects of microstructure anisotropy in 316L stainless steel fabricated by laser powder bed fusion (LPBF) on its spall failure and properties. In this work, plate-on-plate impact experiments were performed using an 80-mm gas gun to investigate the spall behavior of AM fabricated sample discs with impact along the perpendicular and parallel orientations relative to build directions. Experiments were also performed on wrought 316L stainless steel as baseline material with uniform equiaxed grain microstructure for comparison with the AM material of same composition. The spall experiments involved free-surface velocity profiles measured using Photon Doppler Velocimetry (PDV) to capture the spall pull-back signals, combined with post-mortem analysis of the microstructure of soft-recovered impacted samples. In the case of AM samples, spall failure initiated preferentially at melt pool boundaries in both impact directions. The spall plane location and spall strength, however, were both heavily influenced by the orientation of the impact direction relative to the build direction in the AM samples. The spall behavior is also observed to be more complex in the samples impacted perpendicular to the build (through-thickness) direction, due in large part to the orientation of the microstructural features such as melt pool boundaries, laser scan tracks, and general grain morphology.

36 MATERIALS SCIENCE↗

Additively manufactured Al-Ce-Ni-Mn alloy with improved elevated-temperature fatigue resistance

Here, the high cycle fatigue behavior of an additively manufactured (AM) Al-10.5Ce-3.1Ni-1.2Mn wt% alloy was evaluated at 350 °C. The measured fatigue strength of 50 MPa at this temperature is comparable to the most fatigue resistant wrought Al alloys (2618-T6 and 7079-T6) at 315 °C. Refinement of pore populations through advanced AM processing in the examined alloy led to oxide inclusions becoming dominant fatigue crack initiation sites. The distribution of microstructural features that determine crack initiation was measured by X-ray computed tomography and served as input to make fatigue strength model predictions with various methodologies. A Monte-Carlo based approach that was previously applied to predict the fatigue strength of cast aluminum alloys through pore size distributions yielded accurate predictions for the fatigue strength of this AM alloy. Given the tunability of defect distributions in AM alloys, the sensitivity of the Al-Ce-Ni-Mn alloy fatigue behavior to defect distributions and outstanding elevated-temperature fatigue resistance of this alloy; the results together suggest the possibility of a new generation of fatigue-resistant alloys produced by the additive manufacturing route.

36 MATERIALS SCIENCE↗

Additive manufacturing enabled synergetic strengthening of bimodal reinforcing particles for aluminum matrix composites

An additive manufactured TiB 2 /Al-Cu-Mg-Ni composite with a minor amount of Sc was fabricated by laser powder bed fusion (LPBF). The composite shows a yield strength of ~370 MPa, almost doubling the strength of its wrought matrix counterpart, and an elongation of ~7 %. The superior mechanical properties are attributed to a unique micro-nano hierarchical microstructure, consisting of nanoscale and microscale TiB 2 particles dispersed in a matrix of fine aluminum grains (3 µm) together with intragranular intermetallic nanoparticles and nano-cellular networks (cell size 30 nm). The formation of the TiB 2 nanoparticles is the consequence of partial dissolution of the TiB 2 particulates and the enrichment of Sc in the newly formed nanoparticles. Remarkable strengthening effects are achieved by the bimodal TiB 2 particles, intermetallic nanoparticles and intragranular nano-cellular networks. Finally, this study provides new insights into the role of additive manufacturing in tailoring the microstructure of particulate reinforced metal matrix composites (MMCs) with advanced properties.

36 MATERIALS SCIENCE↗

High temperature air oxidation behavior of Hastelloy X processed by Electron Beam Melting (EBM) and Selective Laser Melting (SLM)

The microstructure and oxidation behavior of Laser Beam Melted, Electron Beam Melted and wrought Hastelloy X were studied at 950 °C in dry air, 50 h cycles, up to 1000 h. The variability of processing parameters and powder compositions strongly impacted the oxidation and spallation behavior. Finally, the alloys with high Mn and Si were associated with higher oxidation rates, finer Cr 2 O 3 grain microstructure and increased spallation was observed for the alloys with large elongated grain microstructures (aspect ratio of 10 ± 3).

36 MATERIALS SCIENCE↗

High Temperature Oxidation Behavior of Aluminized Haynes 230

The effect of reactive air aluminizing (RAA) on the high-temperature oxidation behavior of the H230 superalloy is studied at 850 °C for 600 hours. Mass gain values are measured and microstructure is studied by XRD, SEM, and EDX. Post oxidation mass gain for the aluminized alloy is reduced compared to wrought alloy. A three-zone microstructure of diffusion coating is observed in RAA H230. Formation and growth of alumina scale during RAA process and oxidation is attributed to the complementary roles of ß-NiAl + ?'-Ni3Al phases in the composite coating.

Rashidi, S↗