Search NASA⌕ Search

SEARCH · Search NASA

Results for “atomic layer etching”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

Room temperature plasma enhanced atomic layer deposition for TiO{sub 2} and WO{sub 3} films

This paper presents a study on plasma enhanced atomic layer deposition (ALD) of TiO{sub 2} and WO{sub 3} films on silicon substrates. At low temperatures, ALD processes, which are not feasible at high temperatures, could be possible. For example, temperatures at 180 °C and above allow no WO{sub 3} ALD process with WF{sub 6} as a precursor because etching processes hinder film growth. Further low temperature deposition techniques are needed to coat temperature sensitive materials. For the deposition, WF{sub 6} and TiCl{sub 4} are used as metal precursors and O{sub 2} and H{sub 2}O as oxygen sources. The depositions were accomplished in the temperature range of 30 °C up to 180 °C for both metal oxides. Spectroscopic ellipsometry, x-ray reflection, and grazing incidence diffraction were used to investigate the deposited ALD thin films. Film growth, density, crystallinity, and roughness are discussed as functions of temperature after ensuring the ALD requirement of self-saturating adsorption. Growth rates and measured material properties are in good agreement with literature data.

36 MATERIALS SCIENCE↗

Synthesis of Cu Nanowires with Polycarbonate Template

Copper nanowires were fabricated into arrays of pores on ion-track etched polycarbonate membrane, using electrodeposition technique. We coated Au thin film layer on one side of membrane in order to have electrical contact. X-ray diffraction analysis shows that the Au layer has a strong (111) texture. The pores which have cylindrical shape with 6 micron length and 30 nm diameter were filled by copper atoms, fabricating Cu nanowires. Energy Disperse Spectrometry (EDS) indicated the picks of copper which filled the pores of substrate. The morphology and structure of Cu nanowires were characterized by SEM, TEM and XRD, respectively. The results show that although all the nanowires do not have uniform diameter, but all of them are continuous along the length.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Effect of Cl{sub 2}- and HBr-based inductively coupled plasma etching on InP surface composition analyzed using in situ x-ray photoelectron spectroscopy

A Cl{sub 2}-HBr-O{sub 2}/Ar inductively coupled plasma (ICP) etching process has been adapted for the processing of InP-based heterostructures in a 300-mm diameter CMOS etching tool. Smooth and anisotropic InP etching is obtained at moderate etch rate ({approx}600 nm/min). Ex situ x-ray energy dispersive analysis of the etched sidewalls shows that the etching anisotropy is obtained through a SiO{sub x} passivation mechanism. The stoichiometry of the etched surface is analyzed in situ using angle-resolved x-ray photoelectron spectroscopy. It is observed that Cl{sub 2}-based ICP etching results in a significantly P-rich surface. The phosphorous layer identified on the top surface is estimated to be {approx}1-1.3-nm thick. On the other hand InP etching in HBr/Ar plasma results in a more stoichiometric surface. In contrast to the etched sidewalls, the etched surface is free from oxides with negligible traces of silicon. Exposure to ambient air of the samples submitted to Cl{sub 2}-based chemistry results in the complete oxidation of the P-rich top layer. It is concluded that a post-etch treatment or a pure HBr plasma step may be necessary after Cl{sub 2}-based ICP etching for the recovery of the InP material.

36 MATERIALS SCIENCE↗

Polycrystalline indium phosphide on silicon by indium assisted growth in hydride vapor phase epitaxy

Polycrystalline InP was grown on Si(001) and Si(111) substrates by using indium (In) metal as a starting material in hydride vapor phase epitaxy (HVPE) reactor. In metal was deposited on silicon substrates by thermal evaporation technique. The deposited In resulted in islands of different size and was found to be polycrystalline in nature. Different growth experiments of growing InP were performed, and the growth mechanism was investigated. Atomic force microscopy and scanning electron microscopy for morphological investigation, Scanning Auger microscopy for surface and compositional analyses, powder X-ray diffraction for crystallinity, and micro photoluminescence for optical quality assessment were conducted. It is shown that the growth starts first by phosphidisation of the In islands to InP followed by subsequent selective deposition of InP in HVPE regardless of the Si substrate orientation. Polycrystalline InP of large grain size is achieved and the growth rate as high as 21 μm/h is obtained on both substrates. Sulfur doping of the polycrystalline InP was investigated by growing alternating layers of sulfur doped and unintentionally doped InP for equal interval of time. These layers could be delineated by stain etching showing that enough amount of sulfur can be incorporated. Grains of large lateral dimension up to 3 μm polycrystalline InP on Si with good morphological and optical quality is obtained. The process is generic and it can also be applied for the growth of other polycrystalline III–V semiconductor layers on low cost and flexible substrates for solar cell applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

DNA translocation through an array of kinked nanopores

Synthetic solid-state nanopores are being intensively investigated as single-molecule sensors for detection and characterization of DNA, RNA and proteins. This field has been inspired by the exquisite selectivity and flux demonstrated by natural biological channels and the dream of emulating these behaviours in more robust synthetic materials that are more readily integrated into practical devices. So far, the guided etching of polymer films, focused ion-beam sculpting, and electron-beam lithography and tuning of silicon nitride membranes have emerged as three promising approaches to define synthetic solid-state pores with sub-nanometre resolution. These procedures have in common the formation of nominally cylindrical or conical pores aligned normal to the membrane surface. Here we report the formation of 'kinked' silica nanopores, using evaporation-induced self-assembly, and their further tuning and chemical derivatization using atomic-layer deposition. Compared with 'straight through' proteinaceous nanopores of comparable dimensions, kinked nanopores exhibit up to fivefold reduction in translocation velocity, which has been identified as one of the critical issues in DNA sequencing. Additionally, we demonstrate an efficient two-step approach to create a nanopore array exhibiting nearly perfect selectivity for ssDNA over dsDNA. We show that a coarse-grained drift-diffusion theory with a sawtooth-like potential can reasonably describe the velocity and translocation time of DNA through the pore. By control of pore size, length and shape, we capture the main functional behaviours of protein pores in our solid-state nanopore system.

36 MATERIALS SCIENCE↗

Epitaxial two dimensional aluminum films on silicon (111) by ultra-fast thermal deposition

Aluminum thin films are known for their extremely rough surface, which is detrimental for applications such as molecular electronics and photonics, where protrusions cause electrical shorts or strong scattering. We achieved atomically flat Al films using a highly non-equilibrium approach. Ultra-fast thermal deposition (UFTD), at rates >10 nm/s, yields RMS roughness of 0.4 to 0.8 nm for 30-50 nm thick Al films on variety of substrates. For UFTD on Si(111) substrates, the top surface follows closely the substrate topography (etch pits), indicating a 2D, layer-by-layer growth. The Al film is a mixture of (100) and (111) grains, where the latter are commensurate with the in-plane orientation of the underlying Si (epitaxy). We show the use of these ultra-smooth Al films for highly reproducible charge-transport measurements across a monolayer of alkyl phosphonic acid as well as for plasmonics applications by directly patterning them by focused ion beam to form a long-range ordered array of holes. UFTD is a one-step process, with no need for annealing, peeling, or primer layers. It is conceptually opposite to high quality deposition methods, such as MBE or ALD, which are slow and near-equilibrium processes. For Al, though, we find that limited diffusion length (and good wetting) is critical for achieving ultra-smooth thin films.

36 MATERIALS SCIENCE↗

Continuous polymer films deposited on top of porous substrates using plasma-enhanced atomic layer deposition and molecular layer deposition

Molecular layer deposition (MLD) is able to produce ultrathin polymer films with control over thickness, cross-linking, and chemical composition. With these capabilities, MLD should be useful in the fabrication of novel polymer membranes on porous supports. However, confining a continuous MLD film to the surface of porous substrates is difficult because of MLD film growth in the pores. The deposition in the pores lowers the conductance of the porous support. This paper presents a method to deposit continuous polymer films on top of porous substrates. In this method, Al2O3 plasma-enhanced atomic layer deposition (PE-ALD) using trimethylaluminum and oxygen plasma as the reactants was first used to cap the pores of the substrate. Subsequently, a polyamide MLD film was deposited on the Al2O3 PE-ALD capping layer using m-phenylenediamine and trimesoyl chloride as the reactants. The Al2O3 pore caps were then removed from the porous substrate by etching from the backside using a timed exposure to a dilute sodium hydroxide solution. This method was demonstrated using anodic aluminum oxide (AAO) and polyethersulfone (PES) porous substrates. Al2O3 PE-ALD film growth was limited to the top of the porous substrate, resulting in rapid surface recombination or high sticking coefficients for the reactive plasma species within the pores. Gas permeance measurements confirmed the pore capping of the AAO substrates. The reopening of the pores by dissolving the Al2O3 pore caps with a sodium hydroxide solution was monitored using gas permeance versus etch time. The removal of the Al2O3 pore caps from the PES substrates could also dissolve the Al2O3 layer underneath the MLD film. The loss of this Al2O3 layer led to the detachment of the MLD film from the PES substrate. However, the MLD film could be anchored to the PES support at fractures located in the Al2O3 film prior to the MLD. The Al2O3 film fracture allowed the MLD film to anchor firmly to the PES substrate by MLD in the pores of the PES porous substrate. The distance between the anchor points was a function of fracture density. This distance could be controlled by applying a tensile stress to the Al2O3 PE-ALD film to fracture the film through sample bending. This method produced firmly anchored polymer MLD films on top of the PES porous substrates.

Welch, Brian C. (ORCID:000000029747045X)↗

Non-destructive Quantitative Phase Analysis and Microstructural Characterization of Zirconium Coated U-10Mo Fuel Foils via Neutron Diffraction

This report uses neutron diffraction to investigate the crystal phase composition of uranium-molybdenum alloy foils (U-10Mo) for the CONVERT MP-1 Reactor Conversion Project, and determines the effect on alpha-uranium contamination following the deposition of a Zr metal diffusion layer by various methods: plasma spray deposition of Zr powders at LANL and hot co-rolling with Zr foils at BWXT. In summary, there is minimal decomposition of the gamma phase U-10Mo foil to alpha phase contamination following both plasma spraying and hot co-rolling. The average unit cell volume, i.e. lattice spacing, of the Zr layer can be mathematically extracted from the diffraction data; co-rolled Zr matches well with literature values of bulk Zr, while plasma sprayed Zr shows a slight increase in the lattice spacing, indicative of interstitial oxygen in the lattice. Neutron diffraction is a beneficial alternative to conventional methods of phase composition, i.e. x ray diffraction (XRD) and destructive metallography. XRD has minimal penetration depth in high atomic number materials, particularly uranium, and can only probe the first few microns of the fuel plate; neutrons pass completely through the foil, allowing for bulk analysis of the foil composition and no issues with addition of cladding layers, as in the final, aluminum-clad reactor fuel plates. Destructive metallography requires skilled technicians, cutting of the foil into small sections, hazardous etching conditions, long polishing and microscopy times, etc.; the neutron diffraction system has an automated sample loader and can fit larger foils, so there is minimal analysis preparation; the total spectrum acquisition time is ~ 1 hour per sample. The neutron diffraction results are limited by spectra refinement/calculation times and the availability of the neutron beam source. In the case of LANSCE at Los Alamos, the beam operates ~50% of the year. Following the lessons learned from these preliminary results, optimizations to the process and analysis can be made, and neutron diffraction can become a viable and efficient technique for gamma/alpha phase composition determination for nuclear fuels.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Low-Resistance, High-Yield Electrical Contacts to Atom Scale Si:P Devices Using Palladium Silicide

Scanning tunneling microscopy (STM) enables the fabrication of two-dimensional δ-doped structures in Si with atomistic precision, with applications from tunnel field-effect transistors to qubits. The combination of a very small contact area and the restrictive thermal budget necessary to maintain the integrity of the δ layer make developing a robust electrical contact method a significant challenge to realizing the potential of atomically precise devices. We demonstrate a method for electrical contact using Pd 2 Si formed at the temperature of silicon overgrowth (250 °C), minimizing the diffusive impact on the δ layer. Here, we use the transfer length method to show our Pd 2 Si contacts have very high yield (99.7% +0.2% –1.5%) and low resistivity (272 ± 41 Ω μm) in contacting mesa-etched Si:P δ layers. We also present three terminal measurements of low contact resistance (<1 kΩ) to devices written by STM hydrogen depassivation lithography with similarly high yield (100% +0% –3.2%).

2-dimensional systems↗

Selected Area Manipulation of MoS 2 via Focused Electron Beam-Induced Etching for Nanoscale Device Editing

Here we demonstrate direct-write patterning of single and multilayer MoS 2 via a focused electron beam-induced etching (FEBIE) process mediated with the XeF 2 precursor. MoS 2 etching is performed at various currents, areal doses, on different substrates, and characterized using scanning electron and atomic force microscopies as well as Raman and photoluminescence spectroscopies. Scanning transmission electron microscopy reveals a sub-40 nm etching resolution and the progression of point defects and lateral etching of the consequent unsaturated bonds. The results confirm that the electron beam-induced etching process is minimally invasive to the underlying material in comparison to ion beam techniques, which damage the subsurface material. Single-layer MoS 2 field-effect transistors are fabricated, and device characteristics are compared for channels that are edited via the selected area etching process. The source–drain current at constant gate and source–drain voltage scale linearly with the edited channel width. Moreover, the mobility of the narrowest channel width decreases, suggesting that backscattered and secondary electrons collaterally affect the periphery of the removed area. Focused electron beam doses on single-layer transistors below the etching threshold were also explored as a means to modify/thin the channel layer. The FEBIE exposures showed demonstrative effects via the transistor transfer characteristics, photoluminescence spectroscopy, and Raman spectroscopy. While strategies to minimize backscattered and secondary electron interactions outside of the scanned regions require further investigation, here, we show that FEBIE is a viable approach for selective nanoscale editing of MoS 2 devices.

36 MATERIALS SCIENCE↗

Nanoporous Atomically Thin Graphene Membranes for Desalting and Dialysis Applications

Dialysis is a ubiquitous separation process in biochemical processing and biological research. State-of-the-art dialysis membranes comprise a relatively thick polymer layer with tortuous pores, and suffer from low rates of diffusion leading to extremely long process times (often several days) and poor selectivity, especially in the 0–1000 Da molecular weight cut-off range. Here, the fabrication of large-area (cm 2 ) nanoporous atomically thin membranes (NATMs) is reported, by transferring graphene synthesized using scalable chemical vapor deposition (CVD) to polycarbonate track-etched supports. In this study, after sealing defects introduced during transfer/handling by interfacial polymerization, a facile oxygen-plasma etch is used to create size-selective pores (≤1 nm) in the CVD graphene. Size-selective separation and desalting of small model molecules (≈200–1355 Da) and proteins (≈14 000 Da) are demonstrated, with ≈1–2 orders of magnitude increase in permeance compared to state-of-the-art commercial membranes. Rapid diffusion and size-selectivity in NATMs offers transformative opportunities in purification of drugs, removal of residual reactants, biochemical analytics, medical diagnostics, therapeutics, and nano-bio separations.

36 MATERIALS SCIENCE↗

Layer-by-Layer Transfer of Multiple, Large Area Sheets of Graphene Grown in Multilayer Stacks on a Single SiC Wafer

Here we report a technique for transferring graphene layers, one by one, from a multilayer deposit formed by epitaxial growth on the Si-terminated face of a 6H-SiC substrate. The procedure uses a bilayer film of palladium/polyimide deposited onto the graphene coated SiC, which is then mechanically peeled away and placed on a target substrate. Orthogonal etching of the palladium and polyimide leaves isolated sheets of graphene with sizes of square centimeters. Repeating these steps transfers additional sheets from the same SiC substrate. Raman spectroscopy, scanning tunneling spectroscopy, low-energy electron diffraction and X-ray photoelectron spectroscopy, together with scanning tunneling, atomic force, optical, and scanning electron microscopy reveal key properties of the materials. The sheet resistances determined from measurements of four point probe devices were found to be ~2 kΩ/square, close to expectation. As a result, graphene crossbar structures fabricated in stacked configurations demonstrate the versatility of the procedures.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Low vacuum annealing of polymer at low temperatures towards direct and scalable growth of graphene

Highlights: • Low Temperature and pressure growth process. • Synthesis of transfer free single layer graphene in the absence of reducing gases. • Sandwich structure growth process. - Abstract: A transfer-free method is demonstrated for the synthesis of graphene flakes directly on insulating substrate (SiO{sub 2}/Si) by carbon decomposition and diffusion through a layer of nickel. The 100 nm nickel catalyst was deposited on the top of SiO{sub 2} (300 nm)/Si substrate. The sandwich structure was prepared wherein spin-coated polymer was used as a carbon source for the graphene formation. The carbon molecules decomposed and diffused into the nickel layer during annealing of sandwich structures in low vacuum (∼5 × 10{sup −1} Pa) at 600–750 °C for 10 min. When cooled to room temperature (25 °C), graphene is formed at the interface between Ni and SiO{sub 2}/Si, the nickel film was removed by chemical etching. The observed graphene on SiO{sub 2}/Si substrates is confirmed by optical microscopy, Raman spectroscopy and atomic force microscopy. The Raman spectroscopy mapping over a 55 × 55 μm{sup 2} area confirmed the good quality of graphene flakes obtained.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Cl atom recombination on silicon oxy-chloride layers deposited on chamber walls in chlorine-oxygen plasmas

Chlorine atom recombination coefficients were measured on silicon oxy-chloride surfaces deposited in a chlorine inductively coupled plasma (ICP) with varying oxygen concentrations, using the spinning wall technique. A small cylinder embedded in the walls of the plasma reactor chamber was rapidly rotated, repetitively exposing its surface to the plasma chamber and a differentially pumped analysis chamber housing a quadruple mass spectrometer for line-of-sight desorbing species detection, or an Auger electron spectrometer for in situ surface analysis. The spinning wall frequency was varied from 800 to 30 000 rpm resulting in a detection time, t (the time a point on the surface takes to rotate from plasma chamber to the position facing the mass or Auger spectrometer), of {approx}1-40 ms. Desorbing Cl{sub 2}, due to Langmuir-Hinshelwood (LH) Cl atom recombination on the reactor wall surfaces, was detected by the mass spectrometer and also by a pressure rise in one of the differentially pumped chambers. LH Cl recombination coefficients were calculated by extrapolating time-resolved desorption decay curves to t = 0. A silicon-covered electrode immersed in the plasma was either powered at 13 MHz, creating a dc bias of -119 V, or allowed to electrically float with no bias power. After long exposure to a Cl{sub 2} ICP without substrate bias, slow etching of the Si wafer coats the chamber and spinning wall surfaces with an Si-chloride layer with a relatively small amount of oxygen (due to a slow erosion of the quartz discharge tube) with a stoichiometry of Si:O:Cl = 1:0.38:0.38. On this low-oxygen-coverage surface, any Cl{sub 2} desorption after LH recombination of Cl was below the detection limit. Adding 5% O{sub 2} to the Cl{sub 2} feed gas stopped etching of the Si wafer (with no rf bias) and increased the oxygen content of the wall deposits, while decreasing the Cl content (Si:O:Cl = 1:1.09:0.08). Cl{sub 2} desorption was detectable for Cl recombination on the spinning wall surface coated with this layer, and a recombination probability of {gamma}{sub Cl} = 0.03 was obtained. After this surface was conditioned with a pure oxygen plasma for {approx}60 min, {gamma}{sub Cl} increased to 0.044 and the surface layer was slightly enriched in oxygen fraction (Si:O:Cl = 1:1.09:0.04). This behavior is attributed to a mechanism whereby Cl LH recombination occurs mainly on chlorinated oxygen sites on the silicon oxy-chloride surface, because of the weak Cl-O bond compared to the Cl-Si bond.

36 MATERIALS SCIENCE↗

Interfacial study and energy-band alignment of annealed Al{sub 2}O{sub 3} films prepared by atomic layer deposition on 4H-SiC

Al{sub 2}O{sub 3} films were prepared by atomic layer deposition using trimethylaluminum and H{sub 2}O at 250 Degree-Sign C on 4H-SiC substrates and annealed at 1000 Degree-Sign C in N{sub 2}. The as-deposited and annealed Al{sub 2}O{sub 3} films were measured and analyzed near the Al{sub 2}O{sub 3}/SiC interfaces by using an X-ray photoelectron spectroscopy (XPS) with etching processing. The XPS results showed that as-deposited Al{sub 2}O{sub 3} films were O-rich and converted to anhydride Al{sub 2}O{sub 3} films after annealed at 1000 Degree-Sign C in N{sub 2}. Si suboxides were found both at as-deposited and annealed Al{sub 2}O{sub 3}/SiC interfaces. Energy band shift between Al{sub 2}O{sub 3} and 4H-SiC was found after annealing. The conduction band offsets of as-grown and annealed Al{sub 2}O{sub 3}/SiC were 1.90 and 1.53 eV, respectively. These results demonstrated that Al{sub 2}O{sub 3} can be a good candidate to be applied in SiC metal-oxide-semiconductor devices.

36 MATERIALS SCIENCE↗

Method of transferring strained semiconductor structure

The transfer of strained semiconductor layers from one substrate to another substrate involves depositing a multilayer structure on a substrate having surface contaminants. An interface that includes the contaminants is formed in between the deposited layer and the substrate. Hydrogen atoms are introduced into the structure and allowed to diffuse to the interface. Afterward, the deposited multilayer structure is bonded to a second substrate and is separated away at the interface, which results in transferring a multilayer structure from one substrate to the other substrate. The multilayer structure includes at least one strained semiconductor layer and at least one strain-induced seed layer. The strain-induced seed layer can be optionally etched away after the layer transfer.

36 MATERIALS SCIENCE↗

Nanomechanical properties of platinum thin films synthesized by atomic layer deposition

The nanomechanical properties of Pt thin films grown on Si (100) using atomic layer deposition (ALD) were investigated using nanoindentation. Recently, atomic layer deposition (ALD) has successfully demonstrated the capability to deposit ultra-thin films of platinum (Pt). Using (methylcyclopentadienyl) trimethylplatinum (MeCpPtMe3) as chemical platinum precursor and oxygen (O2) as the oxidizing agent, the ALD synthesis of Pt can be achieved with high conformity and excellent film uniformity. The ALD process window for Pt films was experimentally established in the temperature range between 270 °C and 320 °C, where the sheet conductance was constant over that temperature range, indicating stable ALD Pt film growth rate. ALD growth of Pt films exhibits very poor nucleation and adhesion characteristics on bare Si surfaces when the native oxide was removed by 2% HF etch. Pt adhesion improves for thermally oxidized Si wafers and for Si wafers covered with native oxide. Three ALD Pt films deposited at 800, 900, and 1000 ALD deposition cycles were tested for the structural and mechanical properties. Additionally, the sample with 900 ALD deposition cycles was further annealed in forming gas (95% N2 and 5% H2) at 450 °C for 30 min in order to passivate dangling bonds in the grain boundaries of the polycrystalline Pt film. Cross-sectional transmission electron microscopy (TEM), X-ray diffraction (XRD), atomic force microscopy (AFM), and scanning electron microscope (SEM) were employed to characterize the films' surface structure and morphology. Nanoindentation technique was used to evaluate the hardness and modulus of the ALD Pt films of various film thicknesses. The results indicate that the films depict comparable hardness and modulus results; however, the 800 and 1000 ALD deposition cycles films without forming gas annealing experienced significant amount of pileup, whereas the 900 ALD deposition cycles sample annealed in forming gas resulted in a smaller pileup.

Mamun, M.A.↗

Characterizing the Three-Dimensional Structure of Block Copolymers via Sequential Infiltration Synthesis and Scanning Transmission Electron Tomography

Understanding and controlling the three-dimensional structure of block copolymer (BCP) thin films is critical for utilizing these materials for sub-20 nm nanopatterning in semiconductor devices, as well as in membranes and solar cell applications. Combining an atomic layer deposition (ALD) based technique for enhancing the contrast of BCPs in transmission electron microscopy (TEM) together with scanning TEM (STEM) tomography reveals and characterizes the three-dimensional structures of poly(styrene-block-methyl methacrylate) (PS-b-PMMA) thin films with great clarity. Sequential infiltration synthesis (SIS), a block-selective technique for growing inorganic materials in BCPs films in ALD, and an emerging tool for enhancing the etch contrast of BCPs, was harnessed to significantly enhance the high-angle scattering from the polar domains of BCP films in the TEM. The power of combining SIS and STEM tomography for three dimensional (3D) characterization of BCPs films was demonstrated with the following cases: self-assembled cylindrical, lamellar, and spherical PS-PMMA thin films. In all cases, STEM tomography has revealed 3D structures that were hidden underneath the surface, including: 1) the 3D structure of defects in cylindrical and lamellar phases, 2) non-perpendicular 3D surface of grain boundaries in the cylindrical phase, and 3) the 3D arrangement of spheres in body centered cubic (BCC) and hexagonal closed pack (HCP) morphologies in the spherical phase. The 3D data of the spherical morphologies was compared to coarse-grained simulations and assisted in validating the simulations’ parameters. STEM tomography of SIS-treated BCP films enables the characterization of the exact structure used for pattern transfer, and can lead to better understating of the physics which is utilized in BCP lithography.

Block copolymers↗