Search NASA⌕ Search

SEARCH · Search NASA

Results for “coating”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

The Effect of Journal Roughness and Foil Coatings on the Performance of Heavily Loaded Foil Air Bearings

Foil air bearing load capacity tests were conducted to investigate if a solid lubricant coating applied to the surface of the bearing's top foil can function as a break-in coating. Two foil coating materials, a conventional soft polymer film (polyimide) and a hard ceramic (alumina), were independently evaluated against as-ground and worn (run-in) journals coated with NASA PS304, a high-temperature solid lubricant composite coating. The foil coatings were evaluated at journal rotational speeds of 30,000 rpm and at 25 C. Tests were also performed on a foil bearing with a bare (uncoated) nickel-based superalloy top foil to establish a baseline for comparison. The test results indicate that the presence of a top foil solid lubricant coating is effective at increasing the load capacity performance of the foil bearing. Compared to the uncoated baseline, the addition of the soft polymer coating on the top foil increased the bearing load coefficient by 120% when operating against an as-ground journal surface and 85 percent against a run-in journal surface. The alumina coating increased the load coefficient by 40% against the as-ground journal but did not have any affect when the bearing was operated with the run-in journal. The results suggest that the addition of solid lubricant films provide added lubrication when the air film is marginal indicating that as the load capacity is approached foil air bearings transition from hydrodynamic to mixed and boundary lubrication.

Radil, Kevin C.↗

Environmental Barrier Coatings for Silicon-Based Ceramics

Silicon-based ceramics, such as SiC fiber-reinforced SiC (SiC/SiC ceramic matrix composites (CMC) and monolithic silicon nitride (Si3N4), are prime candidates for hot section structural components of next generation gas turbine engines. Silicon-based ceramics, however, suffer from rapid surface recession in combustion environments due to volatilization of the silica scale via reaction with water vapor, a major product of combustion. Therefore, application of silicon-based ceramic components in the hot section of advanced gas turbine engines requires development of a reliable method to protect the ceramic from environmental attack. An external environmental barrier coating (EBC) is considered a logical approach to achieve protection and CP long-term stability. The first generation EBC consisted of two layers, mullite (3Al2O3-2SiO2) bond coat and yttria-stabilized zirconia (YSZ, ZrO2-8 Wt.% Y2O3) top coat. Second generation EBCs, with substantially improved performance compared with the first generation EBC, were developed in the NASA High Speed Research-Enabling Propulsion Materials (HSR-EPM) Program. The first generation EBC consisted of two layers, mullite (3Al2O3-2SiO2) bond coat and yttria-stabilized zirconia (YSZ, ZrO2-8 wt.% Y2O3) top coat. Second generation EBCs, with substantially improved performance compared with the first generation EBC, were developed in the NASA High Speed Research-Enabling Propulsion Materials (HSR-EPM) Program (5). They consist of three layers, a silicon first bond coat, a mullite or a mullite + BSAS (BaO(1-x)-SrO(x)-Al2O3-2SiO2) second bond coat, and a BSAS top coat. The EPM EBCs were applied on SiC/SiC CMC combustor liners in three Solar Turbines (San Diego, CA) Centaur 50s gas turbine engines. The combined operation of the three engines has accumulated over 24,000 hours without failure (approximately 1,250 C maximum combustor liner temperature), with the engine in Texaco, Bakersfield, CA, accumulating about 14,000 hours. As the commercialization of Si-based ceramic components in gas turbines is on the horizon, a major emphasis is placed on EBCs for two reasons. First, they are absolute necessity for the protection of Si-based ceramics from water vapor. Second, they can enable a major enhancement in the performance of gas turbines by creating temperature gradients with the incorporation of a low thermal conductivity layer. Thorough understanding of current state-of-the-art EBCs will provide the foundation upon which development of future EBCs will be based. Phase stability and thermal conductivity of EPM EBCs are published elsewhere. This paper will discuss the chemical/environmental durability and silica volatility of EPM EBCs and their impact on the coating's upper temperature limit.

Lee, Kang N.↗

Furnace Cyclic Behavior of Plasma-Sprayed Zirconia-Yttria and Multi-Component Rare Earth Oxide Doped Thermal Barrier Coatings

Ceramic thermal barrier coatings will play an increasingly important role in advanced gas turbine engines because of their ability to enable further increases in engine temperatures. However, the coating performance and durability become a major concern under the increasingly harsh thermal cycling conditions. Advanced zirconia- and hafnia-based cluster oxide thermal barrier coatings with lower thermal conductivity and improved thermal stability are being developed using a high-heat-flux laser-rig based test approach. Although the new composition coatings were not yet optimized for cyclic durability, an initial durability screening of numerous candidate coating materials was carried out using conventional furnace cyclic tests. In this paper, furnace thermal cyclic behavior of the advanced plasma-sprayed zirconia-yttria-based thermal barrier coatings that were co-doped with multi-component rare earth oxides was investigated at 1163 C using 45 min hot cycles. The ceramic coating failure mechanisms were studied by using scanning electron microscopy combined with X-ray diffraction phase analysis after the furnace tests. The coating cyclic lifetime will be discussed in relation to coating phase structures, total dopant concentrations, and other properties.

Zhu, Dongming↗

Carbon-Based Wear Coatings: Properties and Applications

The technical function of numerous engineering systems - such as vehicles, machines, and instruments - depends on the processes of motion and on the surface systems. Many processes in nature and technology depend on the motion and dynamic behavior of solids, liquids, and gases. Smart surface systems are essential because of the recent technological push toward higher speeds, loads, and operating temperatures; longer life; lighter weight and smaller size (including nanotechnology); and harsh environments in mechanical, mechatronic, and biomechanical systems. If proper attention is not given to surface systems, then vehicles, machines, instruments, and other technical systems could have short lives, consume excessive energy, experience breakdowns, result in liabilities, and fail to accomplish their missions. Surface systems strongly affect our national economy and our lifestyles. At the NASA Glenn Research Center, we believe that proper attention to surface systems, especially in education, research, and application, could lead to economic savings of between 1.3 and 1.6 percent of the gross domestic product. Wear coatings and surface systems continue to experience rapid growth as new coating and surface engineering technologies are discovered, more cost-effective coating and surface engineering solutions are developed, and marketers aggressively pursue, uncover, and exploit new applications for engineered surface systems in cutting tools and wear components. Wear coatings and smart surface systems have been used widely in industrial, consumer, automotive, aerospace, and biomedical applications. This presentation expresses the author's views of and insights into smart surface systems in wear coatings. A revolution is taking place in carbon science and technology. Diamond, an allotrope of carbon, joins graphite, fullerenes, and nanotubes as its major pure carbon structures. It has a unique combination of extreme properties: hardness and abrasion resistance; adhesion and friction; thermal conductivity; chemical and thermal inertness; corrosion and wear resistance; radiation resistance and biocompatibility; electronic, acoustic, and electrochemical characteristics; and environmental compatibility. These properties make diamond attractive for a wide range of diverse applications. In particular, chemical-vapor-deposited (CVD) diamond coatings offer a broad potential, since size and cost are not as limiting. The production of large, superhard diamond films or sheets at low cost make designer materials possible. This presentation is divided into two sections: properties and applications of hard coatings. The first section is concerned with the fundamental properties of the surfaces of CVD diamonds and related materials. The surface properties of hard coatings with favorable coefficients of friction (less than or equal to 0.1) and dimensional wear coefficients (less than or equal to 10(exp -6) cubic millimeters/N.m) in specific environments are discussed. The second section is devoted to applications. Examples of actual, successful applications and of potential challenging applications of the coatings.such as CVD diamond, diamondlike carbon, and cubic boron nitride-are described. Cutting tools coated with CVD diamond are of immediate commercial interest. Other applications, such as microelectromechanical systems (MEMS), valves, and bearings of CVD diamond, are being developed, but at a slow pace. There is a continually growing interest in commercializing diamondlike carbon for wear parts applications, such as biomedical parts and implants, forming dies, transport guides, magnetic tapes and disks, valves, and gears. Cubic boron nitride films are receiving attention because they can be used on tools to machine ferrous materials or on wear parts in sliding contact with ferrous materials.

Miyoshi, Kazuhisa↗

Friction and Wear Characteristics of Cu-4Al Foil Bearing Coating at 25 and 650 degree C

The friction and wear performance of a Cu-4Al top foil coating has been investigated in Generation I foil air bearings. The copper alloy was applied by a novel deposition technique (ion diffusion) and the journal was coated with PS304, a plasma spray deposited high temperature composite solid lubricant coating. The ion diffusion coating process deposits a desirable smooth layer compared to other methods like cathodic arc deposition. The tribological performance of bearings with and without Cu-4Al foil coatings were evaluated through start-stop tests on an air bearing test rig at 25 and 650 C. The results indicate that the Cu-4Al assists during the initial break-in period, gives more stable friction performance with respect to temperature, and appears to prevent top foil wear at high temperature. The measured load capacity coefficient was 0.5, which was comparable to earlier testing of more advanced design Generation III bearings coated with standard cathodic arc deposited Cu-4Al. However, further studies are needed to determine if deeper penetration of the copper alloy into the foil would help make the transition in friction behavior from contact with the Cu-4Al coated foil to contact with the base foil material more gradual. Also, future work is recommended to assess the performance of ion diffusion coatings with different Cu-based alloy compositions and to investigate the effect the coating has on the elastic modulus of the foil material.

Stanford, Malcolm K.↗

Furnace Cyclic Oxidation Behavior of Multi-Component Low Conductivity Thermal Barrier Coatings

Ceramic thermal barrier coatings will play an increasingly important role in advanced gas turbine engines because of their ability to further increase engine operating temperatures and reduce cooling, thus helping achieve future engine low emission, high efficiency and improved reliability goals. Advanced multi-component zirconia-based thermal barrier coatings are being developed using an oxide defect clustering design approach to achieve the required coating low thermal conductivity and high temperature stability. Although the new composition coatings were not yet optimized for cyclic durability, an initial durability screening of the candidate coating materials was conducted using conventional furnace cyclic oxidation tests. In this paper, furnace cyclic oxidation behavior of plasma-sprayed zirconia-based defect cluster thermal barrier coatings was investigated at 1163 C using 45 min hot cycles. The ceramic coating failure mechanisms were studied using scanning electron microscopy (SEM) combined with X-ray diffraction (XRD) phase analysis after the furnace tests. The coating cyclic lifetime is also discussed in relation to coating processing, phase structures, dopant concentration, and other thermo-physical properties.

Zhu, Dong-Ming↗

Therma1 Conductivity and Durability of Advanced Thermal Barrier Coatings

Thermal barrier coatings (TBCs) will play a crucial role in advanced gas turbine engines because of their ability to further increase engine operating temperature and reduce cooling, thus helping to achieve engine emission and efficiency goals. Future TBCs must be designed with increased phase stability, lower thermal conductivity, and improved sintering and thermal stress resistance in order to effectively protect engine hot-section components. Advanced low conductivity TBCs are being developed at NASA by incorporating multi-component oxide dopants into zirconia-yttria or hafnia-yttria to promote the formation of thermodynamically stable defect clusters within the coating structures. This presentation will primarily focus on thermal conductivity and durability of the novel defect cluster thermal barrier coatings for turbine airfoil and combustor applications, determined by a unique CO2 laser heat-flux approach. The laser heat-flux testing approach emphasizes the real-time monitoring and assessment of the coating thermal conductivity under simulated engine temperature and thermal gradient conditions. The conductivity increase due to coating sintering (and/or phase change) and the conductivity decrease due to coating delamination have been determined under steady-state, cyclic, uniform or non-uniform heat-flux conditions. The coating radiation flux resistance has been evaluated by varying coating thermal gradients, and also by using a laser-heated radiative-flux source. Advanced multi-component TBC systems have been shown to have significantly reduced thermal conductivity and improved high temperature stability due to the nano-sized, low mobility defect clusters associated with the paired rare earth dopant additions. The effect of oxide defect cluster dopants on coating thermal conductivity, thermal stability and furnace cyclic durability will also be discussed. The current low conductivity TBC systems have demonstrated long-term cyclic durability at very high temperatures which is far beyond the baseline ZrO2-Y2O3 capabilities.

Zhu, Dong-Ming↗

Thermal/environmental barrier coating system for silicon-based materials

A coating system for a substrate containing a silicon-based material, such as silicon carbide-containing ceramic matrix materials containing silicon carbide and used to form articles exposed to high temperatures, including the hostile thermal environment of a gas turbine engine. The coating system includes a layer of barium strontium aluminosilicate (BSAS) as a bond coat for a thermal-insulating top coat. As a bond coat, the BSAS layer serves to adhere the top coat to a SiC-containing substrate. The BSAS bond coat exhibits sufficient environmental resistance such that, if the top coat should spall, the BSAS bond coat continues to provide a level of environmental protection to the underlying SiC-containing substrate.

Spitsberg, Irene T.↗

High-absorptance high-emittance anodic coating

A colored anodic coating for use on surfaces of substrates, e.g. aluminum substrates in which it is desirable to maintain a high solar absorptance (.alpha.) and a high infrared emittance (.epsilon.), particularly in low earth orbit space environments. This anodic coating is preferably a dark colored coating, and even more preferably a black coating. This coating allows a touch temperature within an acceptable design range to preclude burning of an astronaut in case of contact, but also allows a solar radiation absorption in an amount such that an .alpha./.epsilon. ratio of unity is achieved. The coating of the invention comprises a first layer in the form of an acid anodized colored anodic layer for achieving a high solar absorptance and a second or high emittance layer in the form of a clear acid anodized layer for achieving a high emittance. The entire coating is quite thin, e.g. 1-2 mils and is quite stable in a hostile space environment of the type encountered in a low earth orbit. The coating is obtained by first creating the high emittance clear anodized coating on the metal surface followed by anodizing using a colored anodizing process.

Le, Huong Giang↗

High-absorptance high-emittance anodic coating

A colored anodic coating for use on surfaces of substrates, e.g. aluminum substrates in which it is desirable to maintain a high solar absorptance (a) and a high infrared emittance (e), particularly in low earth orbit space environments. This anodic coating is preferably a dark colored coating, and even more preferably a black coating. This coating allows a touch temperature within an acceptable design range to preclude burning of an astronaut in case of contact, but also allows a solar radiation absorption in an amount such that an a/e ratio of unity is achieved. The coating of the invention comprises a first layer in the form of an acid anodized colored anodic layer for achieving a high solar absorptance and a second or high emittance layer in the form of a clear acid anodized layer for achieving a high emittance. The entire coating is quite thin, e.g. 1-2 mils and is quite stable in a hostile space environment of the type encountered in a low earth orbit. The coating is obtained by first creating the high emittance clear anodized coating on the metal surface followed by anodizing using a colored anodizing process.

Le, Huong Giang↗

Thermal Residual Stress in Environmental Barrier Coated Silicon Nitride - Modeled

When exposed to combustion environments containing moisture both un-reinforced and fiber reinforced silicon based ceramic materials tend to undergo surface recession. To avoid surface recession environmental barrier coating systems are required. However, due to differences in the elastic and thermal properties of the substrate and the environmental barrier coating, thermal residual stresses can be generated in the coated substrate. Depending on their magnitude and nature thermal residual stresses can have significant influence on the strength and fracture behavior of coated substrates. To determine the maximum residual stresses developed during deposition of the coatings, a finite element model (FEM) was developed. Using this model, the thermal residual stresses were predicted in silicon nitride substrates coated with three environmental coating systems namely barium strontium aluminum silicate (BSAS), rare earth mono silicate (REMS) and earth mono di-silicate (REDS). A parametric study was also conducted to determine the influence of coating layer thickness and material parameters on thermal residual stress. Results indicate that z-direction stresses in all three systems are small and negligible, but maximum in-plane stresses can be significant depending on the composition of the constituent layer and the distance from the substrate. The BSAS and REDS systems show much lower thermal residual stresses than REMS system. Parametric analysis indicates that in each system, the thermal residual stresses can be decreased with decreasing the modulus and thickness of the coating.

Ali, Abdul-Aziz↗

Coating MCPs with AlN and GaN

A development effort underway at the time of reporting the information for this article is devoted to increasing the sensitivity of microchannel plates (MCPs) as detectors of photons and ions by coating the MCPs with nitrides of elements in period III of the periodic table. Conventional MCPs are relatively insensitive to slowly moving, large-mass ions for example, ions of biomolecules under analysis in mass spectrometers. The idea underlying this development is to coat an MCP to reduce its work function (decrease its electron affinity) in order to increase both (1) the emission of electrons in response to impingement of low-energy, large-mass ions and (2) the multiplying effect of secondary electron emission. Of particular interest as coating materials having appropriately low or even negative electron affinities are gallium nitride, aluminum nitride, and ternary alloys of general composition Al(x)Ga(1-x)N (where 0<x<1). These materials exhibit attractively high degrees of chemical, mechanical, and thermal stability plus acceptably high resistance to sputtering. The electron-excitation cross sections of these materials are expected to exceed those of several other materials (including diamond) that are, variously, in use or under development for the same purpose. Moreover, by doping these materials with silicon, one can render them partly electrically conductive, thereby suppressing the undesired accumulation of electric charge that could otherwise occur during bombardment by ions. For experiments, thin films of AlN and GaN both undoped and doped with Si were deposited on commercial MCPs by radio-frequency molecular-beam epitaxy (also known as plasma-assisted molecular-beam epitaxy) at temperatures <200 C. This deposition technique is particularly suitable because (1) MCPs cannot withstand the higher deposition-substrate temperatures used to decompose constituent compounds in some other deposition techniques and (2) in this technique, the constituent Al, Ga, and N are supplied in elemental form, so that there is no need for thermal decomposition at the substrate surface. The nitride films thus formed were, variously, amorphous or polycrystalline. The nitride films were coated with surface layers of gold <100 thick. The MCPs were tested in a standard configuration in which the output stage of a first MCP was coupled to the input stage of a second MCP. Each pair of MCPs was mounted in a standard holder that included front and back contact rings and an anode for collecting the output electrons of the second MCP. The MCP pairs were biased at potentials between 1.7 and 1.9 kV, and count rates measured after preamplification and discrimination. To enable a direct comparison, in one pair, the second MCP was uncoated while the first MCP was coated over half its surface. The coated and uncoated sides of the half-coated MCP were exposed to fluxes of argon ions at kinetic energies of 1.0 and 0.5 keV. At 1.0 keV, the count rate for the coated side was about 2.3 times greater than that for the uncoated side; at 0.5 keV, the count rate for the coated side was about 1.8 times greater than that for the uncoated side.

Bensaoula, Abdelhakim↗

Development of YAG:Dy Thermographic Phosphor Coatings for Turbine Engine Applications

The selection and development of thermographic phosphor coatings were pursued to meet the objective of demonstrating luminescence-decay-based temperature measurements up to 1300C on the surface of a vane in an operating demonstrator turbine engine. To meet this objective, YAG:Dy was selected based on the desirable luminescence performance observed for YAG:Dy powder: (1) excellent temperature sensitivity and intensity at operating turbine engine temperatures, (2) an emission peak at the relatively short wavelength of 456 nm, where the interference from background blackbody radiation is fairly low, and (3) its nearly single exponential decay which makes for a simple, reliable temperature calibration. However, implementation of YAG:Dy for surface temperature measurements required application of YAG:Dy as a coating onto the surface of a superalloy component with a preexisting yttria-stabilized zirconia (YSZ) thermal barrier coating (TBC). An inherent dilemma in producing a YAG:Dy coating is that coating processing is constrained to be performed at temperatures below (less than 1200C) what is considered safe for the superalloy component, much lower than temperatures used to produce the high quality crystalline powder. Therefore, YAG:Dy coatings tend to exhibit lower luminescence performance compared to well prepared YAG:Dy powder, and the luminescence performance of the coating will depend on the method of coating deposition. In this presentation, the luminescence performance of YAG:Dy coatings prepared by the different methods of (1) application of a binder-based YAG:Dy-containing paint, (2) solution precursor plasma spray (SPPS), and (3) electron-beam physical vapor deposition (EB-PVD) and the effect of post-deposition heat treatments will be discussed.

Eldridge, J. I.↗

Launch Pad Coatings for Smart Corrosion Control

Corrosion is the degradation of a material as a result of its interaction with the environment. The environment at the KSC launch pads has been documented by ASM International (formerly American Society for Metals) as the most corrosive in the US. The 70 tons of highly corrosive hydrochloric acid that are generated by the solid rocket boosters during a launch exacerbate the corrosiveness of the environment at the pads. Numerous failures at the pads are caused by the pitting of stainless steels, rebar corrosion, and the degradation of concrete. Corrosion control of launch pad structures relies on the use of coatings selected from the qualified products list (QPL) of the NASA Standard 5008A for Protective Coating of Carbon Steel, Stainless Steel, and Aluminum on Launch Structures, Facilities, and Ground Support Equipment. This standard was developed to establish uniform engineering practices and methods and to ensure the inclusion of essential criteria in the coating of ground support equipment (GSE) and facilities used by or for NASA. This standard is applicable to GSE and facilities that support space vehicle or payload programs or projects and to critical facilities at all NASA locations worldwide. Environmental regulation changes have dramatically reduced the production, handling, use, and availability of conventional protective coatings for application to KSC launch structures and ground support equipment. Current attrition rate of qualified KSC coatings will drastically limit the number of commercial off the shelf (COTS) products available for the Constellation Program (CxP) ground operations (GO). CxP GO identified corrosion detection and control technologies as a critical, initial capability technology need for ground processing of Ares I and Ares V to meet Constellation Architecture Requirements Document (CARD) CxP 70000 operability requirements for reduced ground processing complexity, streamlined integrated testing, and operations phase affordability. Researchers at NASA's Corrosion Technology Laboratory at KSC are developing a smart, environmentally friendly coating system for early corrosion detection, inhibition, and self healing of mechanical damage without external intervention. This smart coating will detect and respond actively to corrosion and mechanical damage such as abrasion and scratches, in a functional and predictable manner, and will be capable of adapting its properties dynamically. This coating is being developed using corrosion sensitive microcapsules that deliver the contents of their core (corrosion inhibiting compounds, corrosion indicators, and self healing agents) on demand when corrosion or mechanical damage to the coating occurs.

Calle, Luz M.↗

Optimization of a Wcl6 CVD System to Coat UO2 Powder with Tungsten

In order to achieve deep space exploration via Nuclear Thermal Propulsion (NTP), Marshall Space Flight Center (MSFC) is developing W-UO2 CERMET fuel elements, with focus on fabrication, testing, and process optimization. A risk of fuel loss is present due to the CTE mismatch between tungsten and UO2 in the W-60vol%UO2 fuel element, leading to high thermal stresses. This fuel loss can be reduced by coating the spherical UO2 particles with tungsten via H2/WCl6 reduction in a fluidized bed CVD system. Since the latest incarnation of the inverted reactor was completed, various minor modifications to the system design were completed, including an inverted frit sublimer. In order to optimize the parameters to achieve the desired tungsten coating thickness, a number of trials using surrogate HfO2 powder were performed. The furnace temperature was varied between 930 C and 1000degC, and the sublimer temperature was varied between 140 C and 200 C. Each trial lasted 73-82 minutes, with one lasting 205 minutes. A total of 13 trials were performed over the course of three months, two of which were re-coatings of previous trials. The powder samples were weighed before and after coating to roughly determine mass gain, and Scanning Electron Microscope (SEM) data was also obtained. Initial mass results indicated that the rate of layer deposition was lower than desired in all of the trials. SEM confirmed that while a uniform coating was obtained, the average coating thickness was 9.1% of the goal. The two re-coating trials did increase the thickness of the tungsten layer, but only to an average 14.3% of the goal. Therefore, the number of CVD runs required to fully coat one batch of material with the current configuration is not feasible for high production rates. Therefore, the system will be modified to operate with a negative pressure environment. This will allow for better gas mixing and more efficient heating of the substrate material, yielding greater tungsten coating per trial.

Belancik, Grace A.↗

Temperature Mapping at the Thermal Barrier Coating/Bond Coat Interface by Luminescence Lifetime Imaging Using Integrated Erbium-Doped Sublayers

Full-field temperature mapping of thermal barrier coated components by either infrared thermography or phosphor thermometry has been limited to surface temperature mapping even though temperature mapping at the thermal barrier coating (TBC)/bond coat interface is more relevant for evaluating the TBC thermal protection performance. For the first time, 2D temperature mapping at the TBC/bond coat interface has now been achieved by full-field luminescence lifetime imaging measurements of emission from a thin erbium-doped yttria-stabilized zirconia (YSZ) sensing layer integrated into the TBC below the overlying undoped YSZ. This new capability was applied to map temperatures at the TBC/bond coat interface for TBC-coated specimens subjected to a heat flux produced by the NASA Glenn high heat flux laser facility. In particular, thermal gradients at the TBC/bond coat interface were mapped in regions where the TBC was subjected to erosion or to mechanically induced delamination crack propagation. Finally, temperature mapping of the TBC/bond coat interface was used to evaluate the effectiveness of surface air film cooling at the TBC/bond coat interface.

Eldridge, Jeffrey I.↗

Application and Development of Atomic Layer Deposition Techniques to Improve Thermo-Optical Coatings for Spacecraft Thermal Control and Advanced Optical Instruments

A key technology development driver in environmental control systems and next generation optics are discussed utilizing thin film development borrowed from the semiconductor industry. The optical and physical properties of spacecraft radiator coatings are dictated by orbital environmental conditions. For example, coatings must adequately dissipate charge buildup when orbital conditions, such as polar, geostationary or gravity neutral, result in surface charging. Current dissipation techniques include depositing a layer of ITO (indium tin oxide) on the radiator surface in a high temperature process. The application of these enhanced coatings must be such that the properties in question are tailored to mission-specific requirements. The multi-billion-dollar semiconductor industry has adopted Atomic Layer Deposition (ALD) for self-assembly and atomic-scale placement. ALD is a cost-effective nanoadditive-manufacturing technique that allows for the conformal coating of substrates with atomic control in a benign temperature and pressure environment. By using ALD, modification of these coatings can be accomplished during coating application preprocessing. The preprocessing is rendered directly on the coating dry pigment before binding. Through the introduction of paired precursor gases, thin films can be deposited on a myriad of substrates ranging from glass, polymers, aerogels, metals, powders, and other high aspect-ratio micro- and nano- structures. By providing atomic-level control, where single layers of atoms can be deposited, the fabrication of metal transparent films, precise nano-laminates, and coatings of nano-channels and pores is achievable. A method has been demonstrated for the ALD of In2O3 and films on a variety of substrates from Si(100) wafers, glass slides, and on Z93P pigments resulting in a direct spaceflight application. Results will be presented that verify the chemical composition of ALD pigments and charge dissipation properties when the pigment goes through its binding and coating process and we present early results of ALD for carbon nanotube formation and encapsulation.

Dwivedi, Vivek H.↗

Durability of YSZ Coated Ti2AlC in 1300 °C Mach 0.3 Burner Rig Tests

A thermal barrier coating system survived burner rig testing at 1300 °C for 500 h. A 160 µm thick yttria stabilized zirconia (YSZ) coating was applied to a Ti2AlC MAX phase bar sample by plasma spray physical vapor deposition (PS-PVD) and tested face-on in an atmospheric Mach 0.3 jet fuel burner, using 5-h thermal cycles. No thermal barrier coating (TBC) spallation or recession was observed, only a 2.4 mg/cm2 mass gain. The modest weight gain precluded severe volatility losses under high velocity burner conditions. The coating surface exhibited colonies of (111)flourite fiber-textured columns separated by craze patterns, with no visible moisture attack. The metastable tetragonal t' YSZ phase was obtained initially, transitioning to equilibrium teq and cubic YSZ, but with little detrimental monoclinic. The thickness of the alumina TGO was ~21 to 23 μm under the heated YSZ face and ~13 to 15 μm on the uncoated, cooler backside. The backside exhibited removal of initial transient TiO2 nodules and partial etching of the underlying Al2O3 scale by volatile hydroxides formed in high temperature, high velocity water vapor. Aerodynamic forces produced some bending of the cantilevered sample via creep. The test indicated exceptional stability of YSZ coatings on Ti2AlC under turbine conditions, with thermal expansion matching playing a key role. The purpose of this study was to demonstrate long term durability of YSZ/MAX phase system in aggressive high temperature burner rig testing. MAX phases have been keenly studied because of their unique crystal structure and intriguing properties (Refs. 1 and 2). Having Mn+1(Al,Si)(C,N)n general composition, they are defined as ceramics, but possess unusual desirable attributes such as high conductivity, thermal shock resistance, easy machinability, and deformation tolerance. The mechanical properties derive from weak M-(Al,Si) bonding in the basal plane that leads to sliding and kinking in preference to catastrophic crack growth. Like most ceramics they are phase stable at high temperatures, generally up to 1500 °C. High temperature oxidation resistance is excellent for alumina-forming Ti3AlC2, Ti2AlC, and Cr2AlC, as reviewed by Tallman, et al. (Ref. 3). Compatibility with α-Al2O3 scales is further enhanced in cyclic exposures by a close matching of thermal expansion coefficients, (Ref. 4) i.e., (~9.3, 10.2, 11.3×10–6/K for Al2O3, Ti2AlC, and YSZ, to be discussed). Turbine environments generally contain 10 percent water vapor in the combustion gases, therefore moisture effects can be a concern for some materials (Ref. 5). Furnace tests of MAX phases in high temperature steam generally showed little effect on Al2O3 scale growth (Ref. 6). However, high velocity and high pressure gas can influence scale losses by the formation of volatile reaction products, such as TiO(OH)2 and Al(OH)3 (Refs. 7 to 10). This phenomenon had been discussed for 1100 to 1300 °C high pressure burner rig tests of Ti2AlC (Ref. 11). A single cubic growth rate parameter kcubic was measurably lower than comparable furnace TGA data, but it could be matched reasonably well if corrected for a slight volatility term. In general, a two-parameter cubic-linear growth-volatility law was believed to apply. Corresponding scale volatility loss rates, directly measured at 1300 °C on a pre-oxidized sample, were moderate (0.012 mg/cm2/h) and largely attributed to removal of the initial TiO2 transient scale. A related CH4 burner study of high purity Cr2AlC MAX phase demonstrated 1200 °C durability after 500 rapid (5 min. heat and 2 min. cool) thermal shock cycling (29 h hot time) (Ref. 12). Heating and cooling rates were ~1000 and 500 °C per minute, with a gas velocity of 5 m/s, producing a 75 °C/mm gradient. A 7 μm Al2O3 surface scale and a 13 μm Cr7C3 depletion zone formed with no signs of failure. No evidence of scale volatility was evident, although weight change was not provided, the velocity was moderate, and the total hot time was not extensive. The same high gradient BRT was used to produce 1400 °C surface temperatures for a YSZ/Cr2AlC/IN738 system in the first study of MAX phases used as bond coats for thermal barrier coatings (TBC) (Ref. 25). Here TBC failure was reported after 745 cycles, with only a 1.5 μm Al2O3 scale entrained within a porous, Cr7C3 bondcoat depletion phase. YSZ thermal barrier coatings have been considered to be a compatible complement to Al-MAX phases because of thermal expansion matching and extremely low volatility in water vapor. Initial studies showed superior oxidative stability up to 1300 °C, for long times (at least 500 h) for Ti2AlC substrates and less (268 h) for Cr2AlC, while withstanding large alumina TGO scale thickness (~35 to 40 μm) (Refs. 13 and 14). By comparison, typical superalloy systems can only survive 1150 °C maximum interface temperatures for extended periods, with a maximum sustained TGO below 10 μm (Ref. 15). High temperature SiC based systems are known to form slow-growing SiO2 scales. But these are subject to rate enhancement and volatile Si(OH)4 products in the presence of water vapor, as described comprehensively by Opila, et al. (Refs. 5, 16 to 19). Net weight losses are generally observed in high velocity, high pressure burner rig studies (e.g., 0.084 mg/cm2/h at 1300 °C) (Ref. 20). Furthermore, the loss rates have been shown from chemical physics to scale with v1/2 and pH2O 2 (Ref. 16). Low activity, moisture-resistant environmental barrier coatings (EBC), such as rare earth silicates, are needed to prevent substrate recession under turbine conditions (Refs. 21 to 23).

Smialek, James L.↗