At least 217 records · Page 12

Modeling synergistic fuel cell membrane degradation with mitigating effects of cerium

During operation, polymer-electrolyte fuel cells undergo mechanical and chemical degradation, which behave synergistically and lead to accelerated membrane deterioration over time. This study builds upon previous modeling work on mechanical degradation, as described by a pinhole in the membrane, and chemical degradation mitigation by using cerium. By combining these two models, analysis can be carried out on the coupled degradation methods and how the mitigation effects of cerium disrupt the degradation cycle. The model results show how the presence of a pinhole in the membrane changes the distribution of cerium in the cell and modifies chemical degradation rates. In addition, the model shows how cerium affects the rate of pinhole growth by slowing down the rate of change in mechanical properties due to chemical degradation. Finally, the model shows how cerium modifies the mechanical and chemical degradation rates of the membrane under humidity- and voltage-cycling conditions.

Ehlinger, VM↗

Independence of Environmental and Mechanical Damages on Silicone Adhesive Stored in a Thermo-Oxidative Environment

Abstract Elastomeric polymer materials hold a special place in today’s industrial sectors with respect to structural application needs. Low quality materials are detrimental to industries like aerospace, and automotive engineering. Assessment of the durability of elastomers for structural applications has been of much interest among the literary circles for decades and new materials keep outperforming the existing ones. Polymeric adhesives are one of the most abundantly used materials in these industries. All polymeric materials get damaged when in contact with aggressive environments in presence of high temperature and oxygen. Commonly referred to as thermo-oxidation, this environment exposes the material to heat and oxidation reactions in presence of oxygen. Resultantly, during service life, the damage to the polymer matrix is primarily caused by two factors: mechanical damage and environmental aging. Environmental aging is an irreversible phenomenon caused by changes in the molecular structure while mechanical damage maintains the shape of the polymer matrix, and the deterioration is mostly due to polymer chain mobility. Environmental aging can be caused by a single environmental agent or by a synergized impact of several environmental elements. Increasing temperature is found to be proportional to decreasing tensile strength and toughness of material. The rate and extent of degradation can be accessed by scrutinizing the changes in constitutive behavior of material through mechanical and chemical properties. Accelerated thermal aging is among the most common modes of process related degradation, leading generally to chain scission, and crosslinking phenomena and reduced resistance to fracture stress, and strain. In this experimental study, our goal is to separate the environmental degradation from mechanical damage. A silicone-based adhesive was aged in thermo-oxidative at (0%RH) aging environment. The damage and decay mechanisms have been used to draw a distinction between environmental degradation and mechanical damage. Material characterization included uniaxial tensile test (failure and cyclic) and scanning electron microscopy (SEM) tests on as-received and aged samples. Aging was conducted at three different temperatures (60°C, 80°C and 95°C) and six different exposure durations (1, 3, 10, 30, 90 and 200 days). This work confirms that environmental damage is superposed on top of the mechanical damage, and thus, they are separable. The total mechanical and environmental damage is a synergized effect of all exposure conditions and parameters involved i.e., aging time, temperature, and oxygen. The chemistry and mechanics of the polymer degradation were found to be in good agreement with each other.

Alazhary, Sharif↗

Degradation of Spacecraft Materials in the Space Environment

When we think of space, we typically think of a vacuum containing very little matter that lies between the Earth and other planetary and stellar bodies. However, the space above Earth's breathable atmosphere and beyond contains many things that make designing durable spacecraft a challenge. Depending on where the spacecraft is flyng, it may encounter atomic oxygen, ultraviolet and other forms of radiation, charged particles, micrormeteoroids and debris, and temperature extremes. These environments on their own and in combination can cause degradation and failure of polymers, composites, paints and other materials used on the exterior of spacecraft for thermal control, structure, and power generation. This article briefly discusses and gives examples of some of the degradation experienced on spacecraft and night experiments as a result of the space environment and the use of ground and space data to predict durability.

Miller, Sharon K. R.↗

Multifunctional Composites for Improved Polyimide Thermal Stability

The layered morphology of silicate clay provides an effective barrier to oxidative degradation of the matrix resin. However, as resin thermal stability continues to reach higher limits, development of an organic modification with comparable temperature capabilities becomes a challenge. Typically, phyllosilicates used in polymer nanocomposites are modified with an alkyl ammonium ion. Such organic modifiers are not suited for incorporation into high temperature polymers as they commonly degrade below 200oC. Therefore, the development of nanoparticle specifically suited for high temperature applications is necessary. Several nanoparticles were investigated in this study, including pre-exfoliated synthetic clay, an organically modified clay, and carbon nanofiber. Dispersion of the layered silicate increases the onset temperature of matrix degradation as well as slows oxidative degradation. The thermally stable carbon nanofibers are also observed to significantly increase the resin thermal stability.

Miller, Sandi G.↗

Thermal stability of filler‐based ethylene/vinyl acetate/vinyl alcohol terpolymer in nitroplasticizer oxidative environment

Abstract To study the thermal stability of ethylene/vinyl acetate/vinyl alcohol (EVA‐OH) composite with filler particles, systematic thermogravimetric analysis (TGA) investigation was conducted in both nonisothermal and isothermal modes. The effect of polymer concentration on the aging behavior of EVA‐OH was investigated in the nitroplasticizer (NP) environment. Fourier transform infrared spectroscopy was used to probe chemical structural changes in the EVA‐OH polymer before and after thermal aging. The results suggest that filler addition accelerates the rate of NP exudation out of the EVA‐OH composites and deteriorates the thermal stability of NP at moderate temperatures (up to 70°C). The degradation of NP, in turn, accelerates the degradation of EVA‐OH polymer in its composite form through oxidation and hydrolysis indicating the importance of antioxidants in such phase blends.

36 MATERIALS SCIENCE↗

Probing Heterogeneous Degradation of Catalyst in PEM Fuel Cells under Realistic Automotive Conditions with Multi-Modal Techniques

The heterogeneity of polymer electrolyte fuel cell catalyst degradation is studied under varied relative humidity and types of feed gas. Accelerated stress tests (ASTs) are performed on four membrane electrode assemblies (MEAs) under wet and dry conditions in an air or nitrogen environment for 30 000 square voltage cycles. The largest electrochemically active area loss is observed for MEA under wet conditions in a nitrogen gas environment AST due to constant upper potential limit of 0.95 V and significant water content. The mean Pt particle size is larger for the ASTs under wet conditions compared to dry conditions, and the Pt particle size under land is generally larger than under the channel. Observations from ASTs in both conditions and gas environments indicate that water content promotes Pt particle size growth. ASTs under wet conditions and an air environment show the largest difference in Pt particle size growth for inlet versus outlet and channel versus land, which can be attributed to larger water content at outlet and under land compared to inlet and under channel. From X-ray fluorescence experiments Pt particle size increase is a local phenomenon as Pt loading remains relatively uniform across the MEA.

25 ENERGY STORAGE↗

Impact of Irradiation on Corrosion Performance of Hybrid Organic/Inorganic Coatings on Austenitic Stainless Steel

The effects of gamma radiation on the performance of two corrosion-resistant coatings applied to stainless-steel 304L (SS304L) surfaces are presented. Specifically, the ability of the coatings to mitigate corrosion of SS304L surfaces as a function of the dose received (0–1300 Mrad) and dose rate (176 compared to 1054 rad/s) is evaluated using electrochemical methods, spectroscopy, and microscopy. Coating A, an organic/inorganic hybrid coating consisting of a two-part silica ceramic component and a polymer linker was evaluated in comparison to Coating B, which utilized Coating A as a topcoat for a commercial, off-the-shelf, Zn-rich primer. Post irradiation, Coating A demonstrated some corrosion protection following exposure to low levels of gamma radiation, but coating degradation occurred with an increased exposure dose and resulted in isolated regions of corrosion initiation. For Coating B, greater corrosion resistance was observed compared to Coating A due to the sacrificial nature of the Zn at elevated doses of gamma radiation. No effect of the dose rate (for the single dose examined) was observed for either coating. It is proposed for Coating B that as the polymer coating thermally degrades above 250 °C (bond scission of the polymer occurs), the remaining Zinc layer adhered to the SS304L post-irradiation enables enhanced corrosion resistance as compared to Coating A, which displays solely polymer degradation. The results presented herein establish an understanding of coating behavior with radiation exposure, specifically the relationship between corrosion coating performance and radiation dose, and can inform ageing and lifetime management for various applications.

degradation↗

Insights into the Enhanced Oxidative Thermal Stability of Nanoparticle Organic Hybrid Materials Developed for Carbon Capture and Energy Storage

Due to the growing need for Direct Air Capture (DAC) and integrated carbon capture and conversion technologies, CO 2 capture materials that can withstand a wide range of environmental conditions, including fluctuating ambient temperatures and high concentrations of oxidizing agents (i.e., oxygen and moisture), are critically needed. Liquid-like Nanoparticle Organic Hybrid Materials (NOHMs) have been proposed as candidates for DAC and electrolyte additives enabling sustainable energy storage (i.e., integrated CO 2 capture and conversion and flow batteries). Liquid-like NOHMs functionalized with an ionic bond have been shown to display greatly enhanced oxidative thermal stability compared to the untethered polymer. However, these studies were limited in terms of reaction conditions and the detailed mechanisms of the oxidative thermal degradation were not reported. In this work, a kinetic thermal degradation analysis was performed on NOHM-I-HPE and the neat polymer, Jeffamine M2070 (HPE), in both non-oxidative and oxidative conditions. NOHM-I-HPE displayed similar thermal stability to the untethered polymer in a nitrogen environment, but interestingly, the thermal stability of the ionically tethered polymer was significantly enhanced in the presence of air. This observed enhancement of oxidative thermal stability is attributed to the orders of magnitude larger viscosity of the liquid-like NOHMs compared to untethered polymer and the bond stabilization of the ionically tethered polymer in the NOHMs canopy. Further, spectroscopic analyses of the liquid residue revealed that in the presence of oxygen, the degradation of HPE and NOHM-I-HPE occurs through the formation of trace amounts of carbonyls. This study illustrated that NOHMs can serve as functional materials for sustainable energy storage applications because of their excellent oxidative thermal stability.

25 ENERGY STORAGE↗

Composite Materials

Langley Research Center researchers invented an advanced polymer, a chemical compound formed by uniting many small molecules to create a complex molecule with different chemical properties. The material is a thermoplastic polyimide that resists solvents. Other polymers of this generic type are soluble in solvents, thus cannot be used where solvents are present. High Technology Services (HTS), Inc. licensed technology and is engaged in development and manufacture of high performance plastics, resins and composite materials. Techimer Materials Division is using technology for composite matrix resins that offer heat resistance and protection from radiation, electrical and chemical degradation. Applications of new polymer include molding resins, adhesives and matrix resins for fiber reinforced composites.

Source record↗

Monitoring of Photovoltaic (PV) Performance and Degradation: Integrated Renewable Energy Systems (IRES) - PV Monitoring Task

The Integrated Renewable Energy System (IRES) testbed demonstration at the Pacific Northwest National Laboratory (PNNL) Sequim campus includes development of a suite of capabilities for tracking the performance of photovoltaic (PV) renewable energy components located on a floating platform (floating PV) and on a shoreline building rooftop. The marine environment represents potentially harsh and corrosive conditions for PV modules. Compared to terrestrial PV, potential concerns for offshore PV arising from high humidity and occasional contact with saltwater, marine wildlife, and aquaculture. These environmental factors can reduce electricity generation efficiency and increase the risk of electrical faults, polymer insulation or jacketing degradation and hydrolysis of the PV cell encapsulant materials. Offshore PV modules may also be exposed to lower temperatures and buoyant and vibrating motions with a floating platform. It is not clear how the long-term performance of floating PV will be affected by these factors. To understand expected energy generation through solar cells on a floating platform, monitoring of the performance of PV modules in the marine environment is needed. This report outlines a plan for long-term testing of IRES PV components utilizing resources of the PNNL Material Aging and Detection (MAaD) Science team and the Marine and Coastal Research Laboratory (MCRL). Equipment applicable for onsite testing and real-time monitoring of the PV performance associated with environmental conditions including temperature, solar irradiance, shading and soiling is included. In case of performance loss, equipment for fault detection, failure analysis, material testing, and further troubleshooting are also available. Through establishment of this capabilities, the enabling IRES project sets the stage for future research to advance off-shore and near-shore energy options for businesses and communities.

14 SOLAR ENERGY↗

Useful Life of Tantalum Capacitors

Currently, the major reliability characteristic of tantalum capacitors is the failure rate, which is a constant used to characterize random failures of electronic components. However, contemporary MnO2 and polymer tantalum capacitors have both infant mortality (IM) and wear-out (WO) failures. This requires assessments of the useful life of the parts that is limited by the time of inception of WO failures that can be determined using an adequate reliability model and results of highly accelerated life testing (HALT). In this presentation, a modified time dependent dielectric breakdown (TDDB) model is used to describe both IM and WO failures during HALT. Specifics of physical processes resulting in degradation and failures in polymer and MnO2 tantalum capacitors are discussed, and the increase of IM failures with the level of stress is explained. The model justifies exponential dependence of the acceleration factors on voltage and predicts higher values of the voltage acceleration constant for IM compared to WO failures.

tantalum capacitors↗

Solid polymer membrane program

The results are presented for a solid polymer electrolyte fuel cell development program. Failure mechanism was identified and resolution of the mechanism experienced in small stack testing was demonstrated. The effect included laboratory analysis and evaluation of a matrix of configurations and operational variables for effects on the degree of hydrogen fluoride released from the cell and on the degree of blistering/delamination occurring in the reactant inlet areas of the cell and to correlate these conditions with cell life capabilities. The laboratory evaluation tests were run at conditions intended to accelerate the degradation of the solid polymer electrolyte in order to obtain relative evaluations as quick as possible. Evaluation of the resolutions for the identified failure mechanism in space shuttle configuration cell assemblies was achieved with the fabrication and life testing of two small stack buildups of four cell assemblies and eight cells each.

Source record↗

Polysulfamates as “Macroisosteres” of Polyurethanes with Improved Degradability

Abstract Addressing the environmental persistence of plastics requires the development of next‐generation polymers that combine high performance with enhanced degradability. Progress toward this grand challenge has been impeded, in part, by the absence of a general blueprint for the macromolecular design of such materials. Herein, we introduce a “macroisostere” design strategy, where the carbonyl group (–CO–) in polyurethanes (PUs) is replaced with a sulfonyl group (–SO 2 –), resulting in a virtually unknown family of polymers called polysulfamates. This approach, inspired by the use of bioisosteres in drug discovery, aims to preserve key interchain interactions that contribute to thermomechanical performance while enhancing the hydrolytic lability of the polymer backbone. The optimization of a Sulfur(VI) Fluoride Exchange (SuFEx) polymerization allowed the synthesis of ten polysulfamates structurally analogous to common PUs. Comparative analysis of one PU and its polysulfamate analog showed that this isosteric substitution increases thermal stability, slightly lowers the glass transition temperature, and retains similar hardness and reduced Young's modulus. Notably, the S(VI)‐based polysulfamate demonstrated significantly enhanced hydrolytic degradability. These results highlight the potential of the “macroisostere” approach as a generalizable strategy for designing high‐performance, degradable alternatives to traditional plastics.

Chemistry↗

Three-dimensional hierarchical nanoporous copper via direct ink writing and dealloying

Three-dimensional (3D) hierarchical nanoporous Cu (3DHNP-Cu) is synthesized using a combination of direct ink writing (DIW) based 3D printing, thermal sintering, and chemical dealloying of Mn–Cu alloys. Through tuning processing conditions such as ink composition and cooling rate (after sintering), with consideration of Mn loss during sintering, 3DHNP-Cu with fully bicontinuous nanostructures and negligible residual Mn can be produced after dealloying. The 3DHNP-Cu is comprised of structural features that span seven orders of magnitude, where DIW digitally controls macroscale porous features, thermal sintering and degradation of the binding polymer determines microscale porous features, and dealloying gives rise to nanoscale pores.

36 MATERIALS SCIENCE↗

Relief Zones Enhance the Durability of Ultrathin Membranes in Electrochemical Conversion Devices

Premature failures in electrochemical conversion systems often result when membrane electrode assemblies (MEAs) use ultrathin (≤15 μm-thick) polymer electrolyte membranes, susceptible to mechanical degradation from stress concentrations arising from device-level integration. Herein, relief zones were developed to mitigate mechanical degradation by alleviating excess and nonuniform compression across active areas. Relief zones, created through ablation of carbonaceous diffusion media, enable seamless adaptation across MEA dimensions without need for hardware modifications. Demonstrated using fuel cells as a case study, accelerated stress tests revealed a 6-fold lifetime improvement (∼1500 h) compared to conventional edge-protected MEAs, decoupling device-level engineering effects from material limitations.

accelerated stress test↗