Synthesis, sintering, and grain growth kinetics of Hf 6 Ta 2 O 17
Here Aasystematic study of the solid-state synthesis, pressureless sintering, and grain growth kinetics of Hf 6 Ta 2 O 17 is presented. The ideal conditions for solids-state synthesis of Hf 6 Ta 2 O 17 powder with minimal particle necking was 1250 °C for 2 h in air. The resultant powder has an average particle size of 210 ± 70 nm. The combined synthesis and ball-milling procedure produces highly sinterable Hf 6 Ta 2 O 17 powder, achieving > 97 % of theoretical density after pressureless sintering at 1600 °C for 2 h in air. The grain growth mechanism was sensitive to processing conditions, appearing to be primarily driven by surface diffusion below 1600 °C and grain boundary diffusion above 1650 °C. The respective activation energies for grain growth were found to be Q S = 659 ± 79 kJ mol -1 and Q GB = 478 ± 63 kJ mol -1 .