Search NASA⌕ Search

SEARCH · Search NASA

Results for “thermal aging”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

Fracture surface analysis in composite and titanium bonding: Part 1: Titanium bonding

Fractured lap shear Ti 6-4 adherends bonded with polyphenyquinoxaline (PPQ) and polysulfone were analyzed. The effects of adherend pretreatment, stress level, thermal aging, anodizing voltage, and modified adhesive of Ti 6-4 adherend bonded with PPQ on lap shear strength were studied. The effect of adherend pretreatment on lap shear strength was investigated for PS samples. Results of scanning electron microscopy (SEM) and X-ray photoelectron spectroscopy (XPS) used to study the surface topography and surface composition are also discussed.

Sanderson, K. A.↗

A thermoplastic polyimidesulfone

A polymer system has been prepared which has the excellent thermoplastic properties generally associated with polysulfones, and the solvent resistance and thermal stability of aromatic polyimides. This material, with improved processability over the base polyimide, can be processed in the 260-325 C range in such a manner as to yield high quality, tough unfilled moldings; strong, high-temperature-resistant adhesive bonds; and well consolidated, graphite-fiber-reinforced moldings (composites). The unfilled moldings have physical properties that are similar to aromatic polysulfones which demonstrates the potential as an engineering thermoplastic. The adhesive bonds exhibit excellent retention of initial strength levels even after thermal aging for 5000 hours at 232 C. The graphite-fiber-reinforced moldings have mechanical properties which makes this polymer attractive for the fabrication of structural composites.

St. Clair, T. L.↗

Evaluation of high temperature structural adhesives for extended service

High temperature stable adhesive systems were evaluated for potential Supersonic Cruise Research (SCR) vehicle applications. The program was divided into two major phases: Phase I 'Adhesive Screening' evaluated eleven selected polyimide (PI) and polyphenylquinoxaline (PPQ) adhesive resins using eight different titanium (6Al-4V) adherend surface preparations; Phase II 'Adhesive Optimization and Characterization' extensively evaluated two adhesive systems, selected from Phase I studies, for chemical characterization and environmental durability. The adhesive systems which exhibited superior thermal and environmental bond properties were LARC-TPI polyimide and polyphenylquinoxaline both developed at NASA Langley. The latter adhesive system did develop bond failures at extended thermal aging due primarily to incompatibility between the surface preparation and the polymer. However, this study did demonstrate that suitable adhesive systems are available for extended supersonic cruise vehicle design applications.

Hendricks, C. L.↗

Time-temperature-stress capabilities of composite materials for advanced supersonic technology application

Advanced composites will play a key role in the development of the technology for the design and fabrication of future supersonic vehicles. However, incorporating the material into vehicle usage is contingent on accelerating the demonstration of service capacity and design technology. Because of the added material complexity and lack of extensive data, laboratory replication of the flight service will provide the most rapid method to document the airworthiness of advanced composite systems. Consequently, a laboratory program was conducted to determine the time-temperature-stress capabilities of several high temperature composites. Tests included were thermal aging, environmental aging, fatigue, creep, fracture, tensile, and real-time flight simulation exposure. The program had two phases. The first included all the material property determinations and aging and simulation exposures up through 10,000 hours. The second continued these tests up to 50,000 cumulative hours. This report presents the results of the Phase 1 baseline and 10,000-hr aging and flight simulation studies, the Phase 2 50,000-hr aging studies, and the Phase 2 flight simulation tests, some of which extended to almost 40,000 hours.

Kerr, James R.↗

SEM/XPS analysis of fractured adhesively bonded graphite fibre surface resin-rich/graphite fibre composites

Samples of graphite fiber-reinforced polyimide were fabricated allowing the resin to accumulate at the composite surface. These surface resin-rich composites were then bonded together and tested for lap shear strength both before and after thermal aging. Lap shear strength did not appear to show a significant improvement over that previously recorded for resin-poor samples and was shown to decrease with increasing aging time and temperature.

Devilbiss, T. A.↗

Light weight polymer matrix composite material

A graphite fiber reinforced polymer matrix is layed up, cured, and thermally aged at about 750 F in the presence of an inert gas. The heat treatment improves the structural integrity and alters the electrical conductivity of the materials. In the preferred embodiment PMR-15 polyimides and Celion-6000 graphite fibers are used.

Bowles, Kenneth J.↗

Creep strength of niobium alloys, Nb-1%Zr and PWC-11

A study is being conducted at NASA Lewis Research Center to determine the feasibility of using a carbide particle strengthened Nb-1 percent Zr base alloy to meet the anticipated temperature and creep resistance requirements of proposed near term space power systems. In order to provide information to aid in the determination of the suitability of the PWC-11 alloy as an alternative to Nb-1 percent Zr in space power systems this study investigated: (1) the long-time high-vacuum creep behavior of the PWC-11 material and the Nb-1 percent Zr alloy, (2) the effect of prior stress-free thermal aging on this creep behavior, (3) the effect of electron beam (EB) welding on this creep behavior, and (4) the stability of creep strengthening carbide particles.

Titran, Robert H.↗

Polycrystalline SiC fibers from organosilicon polymers

Various organosilicon polymers have been converted into small diameter, fine-grained silicon carbide fibers by melt spinning, crosslinking, and pyrolyzing to greater than 1600 C. The high pyrolysis temperature densifies the fiber and causes CO evolution which removes nearly all oxygen. An additive prevents the loss of strength normally associated with such treatments. Silicon carbide fibres with up to 2.6 GPa (380 ksi) tensile strength, greater than 420 GPa (greater than 60 Msi) elastic modulus, and 3.1-3.2 mg/cu m density have been prepared via this process. Their microstructure consists of greater than 95 wt pct B-SiC crystallites averaging 30-40 nm diameter, with varying amounts of graphitic carbon between the SiC grains. Under inert conditions, the fibers can be thermally aged at least 12 h/1800 C with minimal change in properties.

Lipowitz, Jonathan↗

Investigation of long term stability in metal hydrides

It is apparent from the literature and the results of this study that cyclic degradation of AB(5) type metal hydrides varies widely according to the details of how the specimens are cycled. The Rapid Cycle Apparatus (RCA) used produced less degradation in 5000 to 10000 cycles than earlier work with a Slow Cycle Apparatus (SCA) produced in 1500 cycles. Evidence is presented that the 453 K (356 F) Thermal Aging (TA) time spent in the saturated condition causes hydride degradation. But increasing the cooling (saturation) period in the RCA did not greatly increase the rate of degradation. It appears that TA type degradation is secondary at low temperatures to another degradation mechanism. If rapid cycles are less damaging than slow cycles when the saturation time is equal, the rate of hydriding/dehydriding may be an important factor. The peak temperatures in the RCA were about 30 C lower than the SCA. The difference in peak cycle temperatures (125 C in the SCA, 95 C in RCA) cannot explain the differences in degradation. TA type degradation is similar to cyclic degradation in that nickel peaks and line broadening are observed in X ray diffraction patterns after either form of degradation.

Marmaro, Roger W.↗

High temperature dielectric properties of Apical, Kapton, Peek, Teflon AF, and Upilex polymers

Reliable lightweight systems capable of providing electrical power at the magawatt level are a requirement for future manned space exploration missions. This can be achieved by the development of high temperature insulating materials which are not only capable of surviving the hostile space environment but can contribute to reducing the mass and weight of the heat rejection system. In this work, Apical, Upilex, Kapton, Teflon AF, and Peek polymers are characterized for AC and DC dielectric breakdown in air and in silicone oil at temperatures up to 250 C. The materials are also tested in terms of their dielectric constant and dissipation factor at high temperatures with an electrical stress of 60 Hz, 200 V/mil present. The effects of thermal aging on the properties of the films are determined after 15 hours of exposure to 200 and 250 C, each. The results obtained are discussed and conclusions are made concerning the suitability of these dielectrics for use in capacitors and cable insulations in high temperature environments.

Hammoud, A. N.↗

Development of LaRC (TM): IA thermoplastic polyimide coated aerospace wiring

NASA Langley has invented LaRC(exp TM) IA and IAX which are thermoplastic polyimides with good melting, thermal and chemical resistance properties. It was the objective of this contract to prepare and extrude LaRC (exp TM) polyimide onto aircraft wire and evaluate the polymers performance in this critical application. Based on rheology and chemical resistance studies at Imitec, LaRC (exp TM) IAX melts readily in an extruder, facilitating the manufacture of thin wall coatings. The polyimide does not corode the extruder, develop gel particles nor advance in viscosity. The insulated wire was tested according to MiL-W-22759E test specifications. The resulting wire coated with LaRC (exp TM) IAX displayed exceptional properties: surface resistance, non blocking, non burning, hot fluid resistance, impulse dielectric, insulation resistance, low temperature flexibility, thermal aging, wire weight, dimensions, negligible high temperature shrinkage and stripability. The light weight and other properties merit its application in satellites, missiles and aircraft applications. The extruded IAX results in a polyimide aircraft insulation without seams, outstanding moisture resistance, continuous lengths and abrasion resistance.

Keating, Jack↗

Technology Development for a Stirling Radioisotope Power System

NASA Glenn Research Center and the Department of Energy are developing a Stirling convertor for an advanced radioisotope power system to provide spacecraft on-board electric power for NASA deep space missions. NASA Glenn is addressing key technology issues through the use of two NASA Phase II SBIRs with Stirling Technology Company (STC) of Kennewick, WA. Under the first SBIR, STC demonstrated a synchronous connection of two thermodynamically independent free-piston Stirling convertors and a 40 to 50 fold reduction in vibrations compared to an unbalanced convertor. The second SBIR is for the development of an Adaptive Vibration Reduction System (AVRS) that will essentially eliminate vibrations over the mission lifetime, even in the unlikely event of a failed convertor. This paper presents the status and results for these two SBIR projects and also discusses a new NASA Glenn in-house project to provide supporting technology for the overall Stirling radioisotope power system development. Tasks for this new effort include convertor performance verification, controls development, heater head structural life assessment, magnet characterization and thermal aging tests, FEA analysis for a lightweight alternator concept, and demonstration of convertor operation under launch and orbit transfer load conditions.

Thieme, Lanny G.↗

Development and Application of Tools to Characterize the Oxidative Degradation of AP/HTPB/Al Propellants in a Propellant Reliability Study

The oxidative thermal aging of a crosslinked hydroxyl-terminated polybutadiene (HTPB)/isophorone diisocyanate (IPDI) polyurethane rubber was studied at temperatures between 25 C and 125 C. Changes in tensile elongation, mechanical hardening, polymer network properties, density, O2 permeation, and molecular chain dynamics were investigated as a function of age. The techniques used include solvent swelling, detailed modulus profiling, and NMR relaxation measurements. The Arrhenius methodology, which normally assumes a linear extrapolation of high temperature aging data, is critically evaluated by using extensive data superposition and highly sensitive oxygen consumption measurements. Significant curvature in the Arrhenius diagram of these oxidation rates is observed to be similar to previous results found for other rubber materials that have been evaluated by this technique. Preliminary gel/network properties suggest that crosslinking is the dominant process at higher temperatures. The effect on the oxidation rate of the binder when other constituents found in propellants are present, such as ammonium perchlorate, plasticizer and aluminum powder, is presented.

Celina, Mathew↗

Acousto-ultrasonics to Assess Material and Structural Properties

This report was created to serve as a manual for applying the Acousto-Ultrasonic NDE method, as practiced at NASA Glenn, to the study of materials and structures for a wide range of applications. Three state of the art acousto-ultrasonic (A-U) analysis parameters, ultrasonic decay (UD) rate, mean time (or skewing factor, "s"), and the centroid of the power spectrum, "f(sub c)," have been studied and applied at GRC for NDE interrogation of various materials and structures of aerospace interest. In addition to this, a unique application of Lamb wave analysis is shown. An appendix gives a brief overview of Lamb Wave analysis. This paper presents the analysis employed to calculate these parameters and the development and reasoning behind their use. It also discusses the planning of A-U measurements for materials and structures to be studied. Types of transducer coupling are discussed including contact and non-contact via laser and air. Experimental planning includes matching transducer frequency range to material and geometry of the specimen to be studied. The effect on results of initially zeroing the DC component of the ultrasonic waveform is compared with not doing so. A wide range of interrogation problems are addressed via the application of these analysis parameters to real specimens is shown for five cases: Case 1: Differences in density in [0] SiC/RBSN ceramic matrix composite. Case 2: Effect of tensile fatigue cycling in [+/-45] SiC/SiC ceramic matrix composite. Case 3: Detecting creep life, and failure, in Udimet 520 Nickel-Based Super Alloy. Case 4: Detecting Surface Layer Formation in T-650-35/PMR-15 Polymer Matrix Composites Panels due to Thermal Aging. Case 5: Detecting Spin Test Degradation in PMC Flywheels. Among these cases a wide range of materials and geometries are studied.

Kautz, Harold E.↗

Thermomechanical Properties of Interface Modified M40J Carbon/PMR-II-50 Composites

To increase performance and durability of high-temperature composites for potential rocket engine components, it is necessary to optimize wetting and interfacial bonding between high modulus carbon fibers and high-temperature polyimide resins. It has been previously demonstrated that the electro-oxidative shear treatments used by fiber manufacturers are not effective on higher modulus fibers that have fewer edge and defect sites in the surface crystallites. In addition, sizings commercially supplied on most carbon fibers are not compatible with polyimides. In this study, the surface chemistry and energy of high modulus carbon fibers (M40J and M60J, Torray) and typical fluorinated polyimide resins, such as PMR-11-50 were characterized. A continuous desizing system that uses an environmentally friendly chemical- mechanical process was developed for tow level fiber. Composites were fabricated with fibers containing the manufacturer's sizing, desized, and further treated with a reactive finish. Results of room temperature tests show that desizing reduces interface sensitive properties compared to the manufacturer's sizing and that subsequent surface re-treatment with reactive finish increases interface sensitive properties. Properties of thermally aged composites and composites with varying finish concentrations will also be discussed.

Allred, Ronald E.↗

Thermomechanical Properties of M40J Carbon/PMR-II-50 Composites

To increase performance and durability of high-temperature composites for potential rocket engine components, it is necessary to optimize wetting and interfacial bonding between high modulus carbon fibers and high-temperature polyimide resins. It has been previously demonstrated that the electro-oxidative shear treatments used by fiber manufacturers are not effective on higher modulus fibers that have fewer edge and defect sites in the surface crystallites. In addition, sizings commercially supplies on most carbon fibers are not compatible with polyimides. In this study, the surface chemistry and energy of high modulus carbon fibers (M40J and M60J, Torray) and typical fluorinated polyimide resins, such as PMR-II-50 were characterized. A continuous desizing system that uses an environmentally friendly chemical-mechanical process was developed for tow level fiber. Composites were fabricated with fibers containing the manufacturer's sizing, desized, and further treated with a reactive finish. Results of room temperature tests show that desizing reduces interface sensitive properties compared to the manufacturer's sizing and that subsequent surface re-treatment with reactive finish increases interface sensitive properties. Properties of thermally aged composites and composites with varying finish concentrations are also discussed.

Ronald E. Allred↗

The Influence of Sizings on the Durability of High-Temperature Polymer Composites

To increase performance and durability of high-temperature composites for potential rocket engine components, it is necessary to optimize wetting and interfacial bonding between high modulus carbon fibers and high-temperature polyimide resins. Sizings commercially supplied on most carbon fibers are not compatible with polyimides. In this study, the chemistry of sizings on two high-modulus carbon fibers (M40J and M60J, Toray) was characterized as was the chemistry of PMR-II-50 fluorinated polyimide resin. The carbon fibers were characterized using single filament wetting, scanning electron microscopy, fourier transform infrared spectroscopy, and x-ray photoelectron spectroscopic measurements. The polyimide matrix resins were coated onto glass filaments for characterization by wetting measurements. Surface energy components were obtained by wetting with nondispersive (methylene iodide), acidic (ethylene glycol), and basic (formamide) probes. A continuous desizing system that uses an environmentally friendly chemical-mechanical process was developed for tow level fiber. Composites were fabricated with fibers containing the manufacturer's sizing, desized, and further treated with a reactive finish. Results of room-temperature tests after thermal aging show that the reactive finish produces a higher strength and more durable interface compared to the manufacturer's sizing. When exposed to moisture blistering tests, however, the better bonded composite displayed a tendency to delaminate, presumably due to trapping of volatiles.

Allred, Ronald E.↗

Effect of Sizings on the Durability of High Temperature Polymer Composites

To increase performance and durability of high-temperature composite for potential rocket engine components, it is necessary to optimize wetting and interfacial bonding between high modulus carbon fibers and high-temperature polyimide resins. Sizing commercially supplied on most carbon fiber are not compatible with polyimides. In this study, the chemistry of sizing on two high modulus carbon fiber (M40J and M60J, Tiray) was characterized. A continuous desizling system that uses an environmentally friendly chemical-mechanical process was developed for tow level fiber. Composites were fabricated with fibers containing the manufacturer's sizing, desized, and further treated with a reactive finish. Results of room-temperature tests after thermal aging show that the reactive finish produces a higher strength and more durable interface compared to the manufacturer's sizing. When exposed to moisture blistering tests, however, the butter bonded composite displayed a tendency to delaminate, presumably due to trapping of volatiles.

Allred, Ronald E.↗