Search NASA⌕ Search

SEARCH · Search NASA

Results for “ALS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Al partitioning during phase separation in Fe-20%Cr-6%Al ODS alloy

Phase separation in a commercial Fe-20 wt.%Cr-6%Al oxide dispersion-strengthened PM 2000 steel has been characterized with a local-electrode atom probe after isothermal aging at 708 K and 748 K for times up to 3,600 h. A progressing decrease in the Al content of the Cr-rich {alpha}{prime} phase was observed with time at both aging temperatures. The Al partitioning trend was consistent with theoretical calculations. However, the experimentally observed Al partitioning factor was significantly lower than the predicted equilibrium value. A {approx}10 nm diameter, roughly spherical, Al- and Ti-enriched {beta}{prime} Fe(AlTi) phase was also observed.

Capdevila, C.↗

Influence of Al{sub 2}O{sub 3} Level in CaO-SiO{sub 2}-MgO-Al{sub 2}O{sub 3} Refining Slags on Slag/Magnesia-Doloma Refractory Interactions

The influence of the Al{sub 2}O{sub 3} level in CaO-SiO{sub 2}-MgO-Al{sub 2}O{sub 3} (CSMA) stainless steel refining slags on the degradation of magnesia-doloma refractories was investigated through static refractory finger corrosion tests. The tests were performed at 1620 °C under Ar atmosphere, using slags with Al{sub 2}O{sub 3} contents of 5, 10, and 20 wt pct, respectively. The results indicate that the formation of 2CaO·SiO{sub 2} at the slag/refractory interface was suppressed by increasing the Al{sub 2}O{sub 3} content to 20 wt pct, thereby changing the corrosion mechanism from an indirect dissolution to a direct dissolution of CaO and MgO from the refractories. The increased solubility limit of MgO by the Al{sub 2}O{sub 3}-rich CSMA slags results in an overall higher corrosion rate of the MgO-doloma refractory.

36 MATERIALS SCIENCE↗

Reduction in the Number of Mg Acceptors with Al Concentration in Al x Ga 1-x N

High hole concentrations in Al x Ga 1-x N become increasingly difficult to obtain as the Al mole fraction increases. The problem is believed to be related to compensation, extended defects, and the band gap of the alloy. Whereas electrical measurements are commonly used to measure hole density, we used electron paramagnetic resonance (EPR) spectroscopy to investigate a defect related to the neutral Mg acceptor. The amount and symmetry of neutral Mg in MOCVD-grown Al x Ga 1-x N with x = 0 to 0.28 was monitored for films with different dislocation densities and surface conditions. EPR measurements indicated that the amount of neutral Mg decreased by 60% in 900°C-annealed Al x Ga 1-x N films for x = 0.18 and 0.28 as compared with x = 0.00 and 0.08. A decrease in the angular dependence of the EPR signal accompanied the increased x, suggesting a change in the local environment of the Mg. Neither dislocation density nor annealing conditions contribute to the reduced amount of neutral Mg in samples with the higher Al concentration. Rather, compensation is the simplest explanation of the observations, because a donor could both reduce the number of neutral acceptors and cause the variation in the angular dependence.

36 MATERIALS SCIENCE↗

Spatially-correlated Site Occupancy in the Nonstoichiometric Meta-stable ε -Al 60 Sm 11 Phase during Devitrification of Al-10.2 at.% Sm Glasses

A metastable ε-Al 60 Sm 11 phase appears during the initial devitrification of as-quenched Al-10.2 at.% Sm glasses. The ε phase is nonstoichiometric in nature since Al occupation is observed on the 16 f Sm lattice sites. Scanning transmission electron microscopic images reveal profound spatial correlation of Sm content on these sites, which cannot be explained by the “average crystal” description from Rietveld analysis of diffraction data. Thermodynamically favorable configurations, established by Monte Carlo (MC) simulations based on a cluster-expansion model, also give qualitatively different correlation functions from experimental observations. On the other hand, molecular dynamics simulations of the growth of ε-Al 60 Sm 11 in undercooled liquid show that when the diffusion range of Sm is limited to ~4 Å, the correlation function of the as-grown crystal structure agrees well with that of the scanning transmission electronic microscopy (STEM) images. Furthermore, our results show that kinetic effects, especially the limited diffusivity of Sm atoms plays the fundamental role in determining the nonstoichiometric site occupancies of the ε-Al 60 Sm 11 phase during the crystallization process.

36 MATERIALS SCIENCE↗

Evaluating the accuracy of common γ-Al 2 O 3 structure models by selected area electron diffraction from high-quality crystalline γ-Al 2 O 3

Single crystal and textured polycrystalline γ-Al 2 O 3 thin films were synthesized by oxidation of NiAl(110) in air at 850 °C for 1 and 2 hours, respectively, and used to evaluate the accuracy of two spinel-based and two nonspinel models by comparison of selected-area electron diffraction (SAED). The lattice interplanar distances derived from the polycrystalline SAED pattern most closely matched the cubic spinel γ-Al 2 O 3 model. The single-crystal SAED spot pattern reflected symmetry consistent with both the cubic spinel and tetragonal nonspinel models, yet, the Al cation distribution better matched the cubic spinel model based on the relative intensities of diffraction spots. Our work indicates that the traditional cubic spinel model is a more accurate model of γ-Al 2 O 3 than the other models considered. Furthermore, the spinel-based monoclinic model is more accurate than the monoclinic nonspinel model. The understanding of the relative accuracy of the different models is key for simulating γ-Al 2 O 3 containing systems and is of general interest for the metal oxide and ceramic communities.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

The microstructure and mechanical properties of Al-containing 9Cr ODS ferritic alloy

In this study, a 9Cr oxide-dispersion strengthened (ODS) alloy with additional corrosion resistant element Al was fabricated by mechanical alloying (MA) and hot pressing (HP) to explore the impact of Al on the microstructure and mechanical property of a 9Cr ODS alloy. It is found that the Al completely dissolved into the FeeCr matrix after milling for 30 h. The minor phases in the Al-containing 9Cr ODS ferritic alloy were investigated by a high-energy X-ray, and were identified to be orthorhombic-YAlO3 (YAP), bcc-Y3Al5O12 (YAG), monoclinic-Al2Y4O9 (YAM), and hexagonal-YAlO3 (YAH). These phases were further confirmed by selected area diffraction pattern (SADP), energy dispersive spectroscopy (EDS), and high resolution transmission electron microscopy (HRTEM). In addition, their volume fractions were also calculated from the integrated intensities. According to the analysis of the particles and their formation sequences, the larger particles (greater than 100 nm) are identified as mainly YAG and Al2O3 particles, while the particles with small size (less than 30 nm) are likely primarily YAM, YAH, and YAP particles. The yielding strength (YS) and ultimate tensile strength (UTS) at RT are 563 MPa and 744 MPa, respectively, while the YS and UTS at 700 C are 245 MPa and 276 MPa, respectively. Although the addition Al in ODS alloys decreases the strength at RT, the values at high temperature are similar to those obtained for 9Cr ODS alloys strengthened by fine YeTieO particles.

Microstructure↗

Crystal structure of Ca{sub 12}Al{sub 14}O{sub 32}Cl{sub 2} and luminescence properties of Ca{sub 12}Al{sub 14}O{sub 32}Cl{sub 2}:Eu{sup 2+}

The crystal structure of Ca{sub 12}Al{sub 14}O{sub 32}Cl{sub 2} was determined from laboratory X-ray powder diffraction data (CuK{alpha}{sub 1}) using the Rietveld method, with the anisotropic displacement parameters being assigned for all atoms. The crystal structure is cubic (space group I4-bar 3d, Z=2) with lattice dimensions a=1.200950(5) nm and V=1.73211(1) nm{sup 3}. The reliability indices calculated from the Rietveld method were R{sub wp}=8.48% (S=1.21), R{sub p}=6.05%, R{sub B}=1.27% and R{sub F}=1.01%. The validity of the structural model was verified by the three-dimensional electron density distribution, the structural bias of which was reduced as much as possible using the maximum-entropy methods-based pattern fitting (MPF). The reliability indices calculated from the MPF were R{sub B}=0.75% and R{sub F}=0.56%. In the structural model there are one Ca site, two Al sites, two O sites and one Cl site. This compound is isomorphous with Ca{sub 12}Al{sub 10.6}Si{sub 3.4}O{sub 32}Cl{sub 5.4}. Europium-doped sample Ca{sub 12}Al{sub 14}O{sub 32}Cl{sub 2}:Eu{sup 2+} was prepared and the photoluminescence properties were presented. The excitation spectrum consisted of two wide bands, which were located at about 268 and 324 nm. The emission spectrum, when excited at 324 nm, resulted in indigo light with a peak at about 442 nm. - Graphical abstract: A portion of the crystal structure of Ca{sub 12}Al{sub 14}O{sub 32}Cl{sub 2} showing eight-membered AlO{sub 4} rings and Ca-Cl-Ca unit.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ion-beam irradiation of lanthanum compounds in the systems La{sub 2}O{sub 3}-Al{sub 2}O{sub 3} and La{sub 2}O{sub 3}-TiO{sub 2}

Thin crystals of La{sub 2}O{sub 3}, LaAlO{sub 3}, La{sub 2/3}TiO{sub 3}, La{sub 2}TiO{sub 5}, and La{sub 2}Ti{sub 2}O{sub 7} have been irradiated in situ using 1 MeV Kr{sup 2+} ions at the Intermediate Voltage Electron Microscope-Tandem User Facility (IVEM-Tandem), Argonne National Laboratory (ANL). We observed that La{sub 2}O{sub 3} remained crystalline to a fluence greater than 3.1x10{sup 16} ions cm{sup -2} at a temperature of 50 K. The four binary oxide compounds in the two systems were observed through the crystalline-amorphous transition as a function of ion fluence and temperature. Results from the ion irradiations give critical temperatures for amorphisation (T{sub c}) of 647 K for LaAlO{sub 3}, 840 K for La{sub 2}Ti{sub 2}O{sub 7}, 865 K for La{sub 2/3}TiO{sub 3}, and 1027 K for La{sub 2}TiO{sub 5}. The T{sub c} values observed in this study, together with previous data for Al{sub 2}O{sub 3} and TiO{sub 2}, are discussed with reference to the melting points for the La{sub 2}O{sub 3}-Al{sub 2}O{sub 3} and La{sub 2}O{sub 3}-TiO{sub 2} systems and the different local environments within the four crystal structures. Results suggest that there is an observable inverse correlation between T{sub c} and melting temperature (T{sub m}) in the two systems. More complex relationships exist between T{sub c} and crystal structure, with the stoichiometric perovskite LaAlO{sub 3} being the most resistant to amorphisation. - Graphical abstract: La{sub 2}TiO{sub 5} with atypical co-ordination for Ti, TiO{sub 5} is found to be different in radiation resistance to La{sub 2}Ti{sub 2}O{sub 7} and La{sub 2/3}TiO{sub 3}. Irradiation of La-Ti-O, and La-Al-O based systems has found that radiation damage resistance is related to the ability of the system to disorder.

36 MATERIALS SCIENCE↗

Al flux synthesis of the oxidation-resistant quaternary phase REFe{sub 4}Al{sub 9}Si{sub 6} (RE = Tb, Er).

Two rare earth iron aluminum silicides, REFe{sub 4}Al{sub 9}Si{sub 6} (RE = Tb, Er), were synthesized in liquid Al at temperatures below 850 C. They crystallize in the tetragonal space group P4{sub 2}/nmc (no. 137) with cell dimensions of a = 8.718(1) {angstrom} and c = 15.171(3) {angstrom} for the Tb analogue. The structure, which is highly intricate and represents a rare structural arrangement, is based on that of NdRh{sub 4}Al{sub 15.4}. It can be understood in terms of highly corrugated layers of merged Al{sub 6} rings stacking to form a three-dimensional framework. The Fe and Si atoms are situated in various sites in the framework. The RE atoms have a very high coordination number (20) and sit in remaining pockets formed by the bonding arrangements in the structure. Magnetic measurements show that the rare earth ions are in a 3+ state, whereas Moessbauer measurements show that the Fe atoms do not exhibit a magnetic moment and are more reduced than in elemental Fe. The possible insights gained from these results into the metallurgical processing of advanced aluminum matrix alloys are discussed. Thermal gravimetric analysis experiments in air show that REFe{sub 4}Al{sub 9}Si{sub 6} is resistant to oxidation up to 900 C, which is attributable to an alumina/silica surface scale.

36 MATERIALS SCIENCE↗

Influence of the surface potential on electrical properties of Al{sub x}Ga{sub 1-x}N/GaN heterostructures with different Al-content: Effect of growth method

The influence of the growth method on the surface potential and thus on the sheet carrier concentration of GaN capped Al{sub x}Ga{sub 1-x}N/GaN heterostructures was evaluated. Nominally undoped low pressure metal-organic vapor-phase (MOVPE) and plasma-assisted molecular beam epitaxial (PA-MBE) grown structures with an Al-content between 12% and 30% yield carrier concentrations from 3.6x10{sup 12} to 1.2x10{sup 13} cm{sup -2}. A difference of the concentrations for a fixed Al-content was found between the different epitaxial techniques. This result indicates unambiguously different surface potentials determined quantitatively from the carrier concentration, and is verified in addition by the results of photoreflectance spectroscopy. The GaN surface potentials of MOVPE and PA-MBE grown samples amounts to (0.26{+-}0.04) and (0.61{+-}0.10) eV irrespective of the Al-content of the barrier layer. After device fabrication, we find that due to the identical surface potential defined by the Ni Schottky gate, the threshold voltage for a given Al-content is the same for samples grown with different techniques. Thus, the interplay between epitaxy and process technology defines the threshold voltage.

36 MATERIALS SCIENCE↗

In situ microscopy of rapidly heated nano-Al and nano-Al/WO{sub 3} thermites

The initiation and reaction mechanism of nano-Al and nano-Al thermites in rapid heating environments is investigated in this work. A semiconductor-based grid/stage was used, capable of in situ heating of a sample from room temperature to 1473 K, and at a rate of 10{sup 6} K/s, inside an electron microscope. Nano-Al was rapidly heated in a transmission electron microscope, and before and after images indicate that the aluminum migrates through the shell, consistent with a diffusion-based mechanism. A nano-Al/WO{sub 3} composite was then heated in a scanning electron microscope. The results indicate that a reactive sintering mechanism is occurring for the nano-Al/WO{sub 3} thermite, as the products are found to be in surface contact and significantly deformed after the heating pulse.

36 MATERIALS SCIENCE↗

Ionic versus metallic bonding in Al n Na m and Al n Mg m (m ≤ 3, n + m ≤ 15) clusters

First principles electronic structure studies on the ground state geometries, stability, and the electronic structure of Al n Na m and Al n Mg m (m ≤ 3, n + m ≤ 15) clusters have been carried out to examine the nature of bonding between Na or Mg and Al. Identifying whether the bonding is ionic or metallic in bulk materials is typically straightforward; however, in small clusters where quantum confinement is important, the nature of bonding may become unclear. Here, we have performed a critical analysis of the bonding in these bimetallic clusters using charge analysis, electrical dipole moments, hybridization of the atomic orbitals, the Laplacian of the charge density at the bond critical points, and the change in the bonding energy between neutral and anionic forms of the cluster. For Na n Al m clusters, we find that the Na binding is primarily ionic, while the bonding in Al n Mg m is primarily metallic. We find that the Mulliken population of the 3 p orbital of Na and Mg can provide a rapid assessment of the nature of bonding. We also find that the Hirshfeld charge and dipole moments are effective indicators, when placed in context. We found that the Laplacian of the charge density at the bond critical points can be misleading in identifying whether the bonding is ionic or metallic in small clusters.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Alloying of U-Al-SS as a Simulant for Pu-Al-SS Alloying

The Savannah River National Laboratory evaluated several options for disposition of stainless steel (SS)–clad plutonium metal, particularly Pu-10.6 at. % Al (Pu- 1.3 wt% Al) alloy fuel. One technology considered was alloying fuel with SS. The goal of the alloying would be to make a SS-Pu alloy that was a nonproliferable waste form with secondary Pu-rich microencapsulated regions distributed throughout the refractory SS. The microencapsulation of the Pu regions should therefore allow the waste form to meet the requirements for a low attractiveness waste as defined by the U.S. Department of Energy. Plutonium-bearing alloys at these levels could potentially be suitable for disposal at a waste isolation pilot plant. Four metal ingots were successfully fabricated using U and Al as a surrogate for Pu-Al. The U was distributed and microencapsulated by the alloy matrix, thereby setting the stage for subsequent tests using SS-clad fuel elements containing Pu-10.6Al.

36 MATERIALS SCIENCE↗

Thermonuclear {sup 25}Al(p,{gamma}){sup 26}Si reaction rate in classical novae and Galactic {sup 26}Al

The nuclear physics uncertainty associated with the production of the Galactic {beta}-delayed {gamma}-ray emitter {sup 26}Al in classical novae is currently dominated by the uncertainty in the thermonuclear {sup 25}Al(p,{gamma}){sup 26}Si reaction rate. By combining the results of recent experiments with past work, the center-of-mass energy of the key J{sup {pi}}=3{sup +}, {sup 25}Al(p,{gamma}){sup 26}Si resonance is determined to be 412(2) keV, and a lower limit of {gamma}{sub p}/{gamma}{sub {gamma}}>5.6 is set for this resonance. The resulting large reduction in the {sup 25}Al(p,{gamma}){sup 26}Si rate uncertainty is expected to constrain uncertainties in the nova contribution to Galactic {sup 26}Al.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Unveiling the mechanism of phase and morphology selections during the devitrification of Al-Sm amorphous ribbon

The complex interplay between energetic and kinetic factors that governs the phase and morphology selections can originate at the earliest stage of crystallization in the amorphous parent phases. Because of the extreme difficulties in capturing the microscopic nucleation process, a detailed picture of how initial disordered structures affect the transformation pathway remains unclear. Here, we report the experimental observation of widely varying phase selection and grain size evolution during the devitrification of a homogeneous melt-spun glassy ribbon. Two different crystalline phases, θ-Al 5 Sm and ε-Al 60 Sm 11 , are found to form in the different regions of the same metallic glass ribbon during the devitrification. The grain size of ε-Al 60 Sm 11 phase shows a strong spatial heterogeneity. Coarse-grained ε-Al 60 Sm 11 phase coupled with the small volume fraction of θ-Al 5 Sm phase is preferably formed close to wheel side of the melt-spun ribbon. Combining experimental characterization and computational simulations, we show that phase selection and microstructure evolution can be traced back to different types and populations of atomic clusters that serve as precursors for the nucleation of different crystalline phases. Inhomogeneous cooling rates cause different structure orders across the glass sample during the quenching process. Our findings provide direct insight into the effect of structural order on the crystallization pathways during the devitrification of metallic glass. It also opens an avenue to study the detailed nucleation process at the atomic level using the metallic glass as a platform and suggests the opportunity of microstructure and property design via controlling the cooling process.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗