Search NASA⌕ Search

SEARCH · Search NASA

Results for “Atomic Oxygen”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Atomic oxygen interactions with protected organic materials on the Long Duration Exposure Facility (LDEF)

The Long Duration Exposure Facility (LDEF) has provided an excellent opportunity to understand the nature of directed atomic oxygen interactions with protected polymers and composites. Although there were relatively few samples of materials with protective coatings on their external surfaces on LDEF which were exposed to a high atomic oxygen fluence, analysis of such samples has enabled an examination of the shape of atomic oxygen undercut cavities at defect sites in the protective coatings. Samples of front-surface aluminized (Kapton) polyimide were inspected by scanning electron microscopy to identify and measure crack defects in the aluminum protective coatings. After chemical removal of the aluminum coating, measurements were also made of the width of the oxidized undercut cavities below the crack defects. The LDEF flight undercut cavity geometries were then compared with Monte Carlo computational model undercut cavity predictions. The comparison of the LDEF results and computational modeling indicates agreement in specific undercut cavity geometries for atomic oxygen reaction probabilities dependent upon the 0.68 to 3.0 power of the energy. However, no single energy dependency was adequate to replicate flight results over a variety of aluminum crack widths.

Banks, Bruce A.↗

Analyses of atomic oxygen, the green line, and Herzberg bands in the lower thermosphere

Measured altitude profiles of atomic oxygen, 557.7-nm emissions, and Herzberg I emission between 80 and 120 km were used to test the proposed mechanisms leading to these emissions. As generally assumed, the O2(A 3 Sigma u +) that emits the Herzberg I bands is excited by three-body recombination of atomic oxygen. The quenching of this state is by N2 or O2; for N2 the lifetime times the rate is 2.75 x 10 to the -13th per cu cm; other quenchers are insignificant. It is found that the atomic oxygen O(1S) emitting the green line is excited by the Barth mechanism.

Thomas, R. J.↗

Simulation of the synergistic low Earth orbit effects of vacuum thermal cycling, vacuum UV radiation, and atomic oxygen

In order to assess the low Earth orbit (LEO) durability of candidate space materials, it is necessary to use ground laboratory facilities which provide LEO environmental effects. A facility combining vacuum thermal cycling and vacuum ultraviolet (VUV) radiation has been designed and constructed at NASA Lewis Research Center for this purpose. This facility can also be operated without the VUV lamps. An additional facility can be used to provide VUV exposure only. By utilizing these facilities, followed by atomic oxygen exposure in an RF plasma asher, the effects of the individual vacuum thermal cycling and VUV environments can be compared to the effect of the combined vacuum thermal cycling/VUV environment on the atomic oxygen durability of materials. The synergistic effects of simulated LEO environmental conditions on materials were evaluated by first exposing materials to vacuum thermal cycling, VUV, and vacuum thermal cycling/VUV environments followed by exposure to atomic oxygen in an RP plasma asher. Candidate space power materials such as atomic oxygen protected polyimides and solar concentrator mirrors were evaluated using these facilities. Characteristics of the Vacuum Thermal Cycling/VUV Exposure Facility which simulates the temperature sequences and solar ultraviolet radiation exposure that would be experienced by a spacecraft surface in LEO are discussed. Results of durability evaluations of some candidate space power materials to the simulated LEO environmental conditions will also be discussed. Such results have indicated that for some materials, atomic oxygen durability is affected by previous exposure to thermal cycling and/or VUV exposure.

Dever, Joyce A.↗

Sounding rocket observation of a hot atomic oxygen geocorona

A sounding rocket measurement of the ultraviolet, atomic oxygen dayglow reveals an excess of emission compared to standard thermospheric model calculations at exospheric altitudes. We explore two explanations for this discrepancy: a breakdown of the radiative transfer model due to nonlocal thermal equilibrium (non-LTE) conditions above the exobase and a hot atomic oxygen geocorona. In particular, the effects of non-LTE on the 3P2, 1, 0 sublevel populations are modeled, and a hot O component in the upper thermosphere and lower exosphere is added to investigate the effects on the modeled emissions. For both cases, the data are reanalyzed and compared with the results using a standard LTE model. A hot O geocorona having a peak density of 10(exp 6)/cc at 550 km and a temperature of 4000 K is consistent with the data and appears to be the most reasonable explanation of the high-altitude enhanced emissions observed in the data.

Cotton, Daniel M.↗

Velocity distributions of oxygen atoms incident on spacecraft surfaces

The angular distributions of oxygen atoms incident on surfaces in low earth orbit have been calculated for a number of ambient gas temperatures. Atom fluxes to surfaces were modeled by integrals over all permitted angles of incidence. Angles of incidence are limited by masking structures, and a number of types of mask were considered. Combustible surfaces exposed to the orbital atmosphere are heavily etched, creating profiles in mask shadows that are sensitive to ambient temperatures. The influence of the angular distributions on the characteristics of etched surfaces is discussed. Profiles measured for a September, 1983 flight were fitted to this model profile with a temperature of 750 + or - 50 K, which agrees with estimates based on solar activity at that time. Applications to sensing ambient temperatures and oxygen atom densities are discussed.

Peters, P. N.↗

Atomic Oxygen Erosion Yield Prediction for Spacecraft Polymers in Low Earth Orbit

The ability to predict the atomic oxygen erosion yield of polymers based on their chemistry and physical properties has been only partially successful because of a lack of reliable low Earth orbit (LEO) erosion yield data. Unfortunately, many of the early experiments did not utilize dehydrated mass loss measurements for erosion yield determination, and the resulting mass loss due to atomic oxygen exposure may have been compromised because samples were often not in consistent states of dehydration during the pre-flight and post-flight mass measurements. This is a particular problem for short duration mission exposures or low erosion yield materials. However, as a result of the retrieval of the Polymer Erosion and Contamination Experiment (PEACE) flown as part of the Materials International Space Station Experiment 2 (MISSE 2), the erosion yields of 38 polymers and pyrolytic graphite were accurately measured. The experiment was exposed to the LEO environment for 3.95 years from August 16, 2001 to July 30, 2005 and was successfully retrieved during a space walk on July 30, 2005 during Discovery s STS-114 Return to Flight mission. The 40 different materials tested (including Kapton H fluence witness samples) were selected specifically to represent a variety of polymers used in space as well as a wide variety of polymer chemical structures. The MISSE 2 PEACE Polymers experiment used carefully dehydrated mass measurements, as well as accurate density measurements to obtain accurate erosion yield data for high-fluence (8.43 1021 atoms/sq cm). The resulting data was used to develop an erosion yield predictive tool with a correlation coefficient of 0.895 and uncertainty of +/-6.3 10(exp -25)cu cm/atom. The predictive tool utilizes the chemical structures and physical properties of polymers to predict in-space atomic oxygen erosion yields. A predictive tool concept (September 2009 version) is presented which represents an improvement over an earlier (December 2008) version.

Banks, Bruce A.↗

Development of a high flow source of energetic oxygen atoms for material degradation studies

A technique for the generation, in the laboratory, of thermally 'cold', high flux of energetic oxygen atoms is presented. The flux of nearly mono-energetic oxygen atoms is obtained after a laser-induced breakdown of oxygen molecules followed by a rapid expansion of the recombining plasma. The experimental apparatus, the optical and spectral measurements, the O-atom source characterization, and the material degradation studies are discussed. Average oxygen atom velocities of about 5 to 13 km/s are measured with an estimated flux of 10 to the 18th per pulse, over pulse durations of several microseconds. The flow of the O2 gas for about 200 microseconds before applying the laser pulse is found to give best results. It is also found that the energetic O-atom irradiation of sample targets such as Al, Fe, and polyethylene, induces mass removal. In addition, spectral scans of the radiation reveals the existence of two main spectral subsets.

Caledonia, G. E.↗

Low Earth orbital atomic oxygen micrometeoroid, and debris interactions with photovoltaic arrays

Polyimide Kapton solar array blankets can be protected from atomic oxygen in low earth orbit if SiO sub x thin film coatings are applied to their surfaces. The useful lifetime of a blanket protected in this manner strongly depends on the number and size of defects in the protective coatings. Atomic oxygen degradation is dominated by undercutting at defects in protective coatings caused by substrate roughness and processing rather than micrometeoroid or debris impacts. Recent findings from the Long Duration Exposure Facility (LDEF) and ground based studies show that interactions between atomic oxygen and silicones may cause grazing and contamination problems which may lead to solar array degradation.

Banks, Bruce A.↗

Changes in Polymeric Tether Properties Due to Atomic Oxygen

The Propulsive Small Expendable Deployer System (ProSEDS) mission is designed to provide an on-orbit demonstration of the electrodynamic propulsion capabilities of tethers in space. The ProSEDS experiment will be a secondary payload on a Delta II unmanned expendable booster. A 5-km conductive tether is attached to the Delta II second stage and collects current fiom the low Earth orbit (LEO) plasma to facilitate de-orbit of the spent stage. The conductive tether is attached to a 10-km non-conductive tether, which is then attached to an endmass containing several scientific instruments. Atomic oxygen (AO) erodes most organic materials. As the orbit of the Delta II second stage decas, the AO flux (atoms/sq cm sec) increases. A nominal AO fluence of 1 x l0(exp 21) atoms/sq cm was agreed upon by the investigators as an adequate level for evaluating the performance of the tether materials. A test series was performed to determine the effect of atomic oxygen (AO) on the mechanical integrity and possible strength loss of ProSEDS tether materials. The tether materials in this study were Dyneema, an ultra-high molecular weight polyethylene material used as the non-conducting portion of the ProSEDS tether, and the Kevlar core strength fiber used in the conductive tether. Samples of Dyneema and Kevlar were exposed to various levels of atomic oxygen up to 1.07 x 10(exp 21) atoms/sq cm in the Marshall Space Flight Center Atomic Oxygen Beam Facility (AOBF). Changes in mass were noted after AO exposure. The tethers were then tensile-tested until failure. AO affected both the Dyneema and Kevlar tether material strength. Dyneema exposed to 1.07 x 10(exp 21) atoms/sq cm of atomic oxygen failed due to normal handling when removed fiom the AOBF and was not tensile-tested. Another test series was performed to determine the effect of AO on the electrical properties of the ProSEDS conductive tether. The conductive tether consists of seven individually coated strands of 28 AWG 1350-0 aluminum wire. The conductive coating, developed by Triton Systems, Inc., is a mix of polyanaline and COR, a clear AO-resistant polymer.

Finckenor, Miria M.↗

Performance and properties of atomic oxygen protective coatings for polymeric materials

Such large LEO spacecraft as the Space Station Freedom will encounter high atomic oxygen fluences which entail the use of protective coatings for their polymeric structural materials. Such coatings have demonstrated polymer mass losses due to oxidation that are much smaller than those of unprotected materials. Attention is here given to protective and/or electrically conductive coatings of SiO(x), Ge, and indium-tin oxide which have been exposed to atomic oxygen in order to ascertain mass loss, electrical conductivity, and optical property dependence on atomic oxygen exposure.

Banks, Bruce A.↗

Experimental results on atomic oxygen corrosion of silver

The results of an experimental study of the reaction kinetics of silver with atomic oxygen in 10 degree increments over the temperature range of 0 to 70 C is reported. The silver specimens, of the order of 10,000 A in thickness, were prepared by thermal evaporation onto 3 inch diameter polished silicon wafers. There were later sliced into pieces having surface areas of the order of 1/4 to 1/2 square inch. Atomic oxygen was generated by a gas discharge in a commercial plasmod asher operating in the megahertz frequency range. The sample temperature within the chamber was controlled by means of a thermoelectric unit. Exposure of the silver specimens to atomic oxygen was incremental, with oxide film thickness measurements being carried out between exposures by means of an automated ellipsometer. For the early growth phase, the data can be described satisfactorily by a logarithmic growth law: the oxide film thickness increases as the logarithm of the exposure time. Furthermore, the oxidation process is thermally activated, the rate increasing with increasing temperature. However, the empirical activation energy parameter deduced from Arrhenius plots is quite low, being of the order of 0.1 eV.

Fromhold, Albert T.↗

The Materials Chemistry of Atomic Oxygen with Applications to Anisotropic Etching of Submicron Structures in Microelectronics and the Surface Chemistry Engineering of Porous Solids

Neutral atomic oxygen is the most abundant component of the ionospheric plasma in the low Earth orbit environment (LEO; 200 to 700 kilometers altitude) and can produce significant degradation of some spacecraft materials. In order to produce a more complete understanding of the materials chemistry of atomic oxygen, the chemistry and physics of O-atom interactions with materials were determined in three radically different environments: (1) The Space Shuttle cargo bay in low Earth orbit (the EOIM-3 space flight experiment), (2) a high-velocity neutral atom beam system (HVAB) at Los Alamos National Laboratory (LANL), and (3) a microwave-plasma flowing-discharge system at JSC. The Space Shuttle and the high velocity atom beam systems produce atom-surface collision energies ranging from 0.1 to 7 eV (hyperthermal atoms) under high-vacuum conditions, while the flowing discharge system produces a 0.065 eV surface collision energy at a total pressure of 2 Torr. Data obtained in the three different O-atom environments referred to above show that the rate of O-atom reaction with polymeric materials is strongly dependent on atom kinetic energy, obeying a reactive scattering law which suggests that atom kinetic energy is directly available for overcoming activation barriers in the reaction. General relationships between polymer reactivity with O atoms and polymer composition and molecular structure have been determined. In addition, vacuum ultraviolet photochemical effects have been shown to dominate the reaction of O atoms with fluorocarbon polymers. Finally, studies of the materials chemistry of O atoms have produced results which may be of interest to technologists outside the aerospace industry. Atomic oxygen 'spin-off' or 'dual use' technologies in the areas of anisotropic etching in microelectronic materials and device processing, as well as surface chemistry engineering of porous solid materials are described.

Koontz, Steve L.↗

Kinetics of oxygen atom formation during the oxidation of methane behind shock waves

An experimental and analytical study of the formation of oxygen atoms during the oxidation of methane and methane-hydrogen mixtures behind incident shock waves was carried out over the temperature range 1790-2584 K at reaction pressures between 1.2 and 1.7 atm. Oxygen atom levels were determined indirectly by measurement of emission from reaction of O with CO. On the basis of these data and ignition-delay data reported in the literature, a kinetic scheme for methane oxidation was assembled. The proposed kinetic mechanism, in general, predicts higher peak oxygen atom levels than the current oxidation mechanisms proposed by Bowman and Seery and by Skinner and his co-workers.

Jachimowski, C. J.↗

Atomic Oxygen Durability Evaluation of Protected Polymers Using Thermal Energy Plasma Systems

The durability evaluation of protected polymers intended for use in low Earth orbit (LEO) has necessitated the use of large-area, high-fluence, atomic oxygen exposure systems. Two thermal energy atomic oxygen exposure systems which are frequently used for such evaluations are radio frequency (RF) plasma ashers and electron cyclotron resonance plasma sources. Plasma source testing practices such as ample preparation, effective fluence prediction, atomic oxygen flux determination, erosion measurement, operational considerations, and erosion yield measurements are presented. Issues which influence the prediction of in-space durability based on ground laboratory thermal energy plasma system testing are also addressed.

Banks, Bruce A.↗

Mars Upper Atmospheric Temperature and Atomic Oxygen Density Derived from the O i 130.4 nm Emission Observed by NASA’s MAVEN Mission

The abundance of atomic oxygen is a major unknown for the Mars upper atmosphere, and systematic measurements of this key species is a primary objective of NASA’s Mars Atmosphere and Volatile Evolution (MAVEN) mission. Moreover, the Martian dayside temperature structure and its variability has been a subject of considerable debate in the past. In this study, an inversion analysis of the periapsis limb scans of the O i 130.4 nm emission observed by MAVEN is performed to quantify the neutral temperature and atomic oxygen abundance in the Mars upper atmosphere. Our analysis yields unprecedented resolution of the spatial variation of Mars atomic oxygen, showing that its exobase density decreases with the solar zenith angle (SZA) from ∼0° to 60° by about an order of magnitude, from ∼10{sup 8} to ∼10{sup 7} cm{sup −3} near perihelion (2015 April) and from ∼10{sup 7} to ∼10{sup 6} cm{sup −3} near aphelion (2017 November). For a given SZA the exobase densities near perihelion are about an order of magnitude higher than those near aphelion. The [O]/[CO{sub 2}] mixing ratio at 130 km altitude can vary from ∼0.1% to 4.6%, which also decreases with increasing SZA. Moreover, it is shown that the Mars exobase temperature does not vary significantly with SZA from ∼0° to ∼60°, which is estimated to be ∼239.2 ± 27.6 K near perihelion and ∼162.4 ± 19.9 K near aphelion, with a difference of 76.8 K between these two seasonal extremes.

79 ASTRONOMY AND ASTROPHYSICS↗