Search NASA⌕ Search

SEARCH · Search NASA

Results for “CHROMIUM OXIDES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Factors Affecting Al Depletion During Cyclic Oxidation of Fe-Base Alumina-Forming Alloys

In order to develop an improved oxidation-limited lifetime model, experiments are being conducted to assess the critical factors that affect the rate of Al loss from Fe-base alumina-forming alloys during cyclic oxidation. Both wrought and dispersion strengthened ferritic and intermetallic Fe-Al {+-} Cr alloys are being investigated at exposure temperatures from 1100-1300 C. Higher temperatures, thinner specimens and cycle frequency are used to accelerate degradation during oxidation. However, the effects of these experimental choices often have not been critically assessed in prior work. Electron probe microanalysis has been used to measure the residual Al content under various conditions and at various stages of life. For 0.5-2 mm thick specimens, lifetime repeatedly showed a linear relationship to thickness. Increasing the oxidation temperature appears to be the most viable strategy to accelerate the evaluation of oxidation resistance for comparing and developing alloys.

36 MATERIALS SCIENCE↗

Iron-based alloy and nitridation treatment for PEM fuel cell bipolar plates

A corrosion resistant electrically conductive component that can be used as a bipolar plate in a PEM fuel cell application is composed of an alloy substrate which has 10-30 wt. % Cr, 0.5 to 7 wt. % V, and base metal being Fe, and a continuous surface layer of chromium nitride and vanadium nitride essentially free of base metal. A oxide layer of chromium vanadium oxide can be disposed between the alloy substrate and the continuous surface nitride layer. A method to prepare the corrosion resistant electrically conductive component involves a two-step nitridization sequence by exposing the alloy to a oxygen containing gas at an elevated temperature, and subsequently exposing the alloy to an oxygen free nitrogen containing gas at an elevated temperature to yield a component where a continuous chromium nitride layer free of iron has formed at the surface.

Brady, Michael P↗

Oxidation Behavior of Binary Niobium Alloys

This investigation concludes a study to determine the effects of up to 25 atomic percent of 55 alloying additions on the oxidation characteristics of niobium. The alloys were evaluated by oxidizing in an air atmosphere for 4 hours at 1000 C and 2 hours at 1200 C. Titanium and chromium improved oxidation resistance at both evaluation conditions. Vanadium and aluminum improved oxidation resistance at 1000 C, even though the V scale tended to liquefy and the Al specimens became brittle and the scale powdery. Copper, cobalt, iron, and iridium improved oxidation resistance at 1200 C. Other investigations report tungsten and molybdenum are protective up to about 1000 C, and tantalum at 1100 C. The most important factor influencing the rate of oxidation was the ion size of the alloy additions. Ions slightly smaller than the Nb(5+) ion are soluble in the oxide lattice and tend to lower the compressive stresses in the bulk scale that lead to cracking. The solubility of the alloying addition also depends on the valence to some extent. All of the elements mentioned that improve the oxidation resistance of Nb fit this size criterion with the possible exception of Al, whose extremely small size in large concentrations would probably lead to the formation of a powdery scale. Maintenance of a crack-free bulk scale for as long as possible may contribute to the formation of a dark subscale that ultimately is rate- controlling in the oxidation process. The platinum-group metals, especially Ir, appear to protect by entrapment of the finely dispersed alloying element by the incoming Nb2O5 metal-oxide interface. This inert metallic Ir when alloyed in a sufficient amount with Yb appears to give a ductile phase dispersed in the brittle oxide. This scale would then flow more easily to relieve the large compressive stresses to delay cracking. Complex oxide formation (which both Ti and Zr tend to initiate) and valence effects, which probably change the vacancy concentration in the scale, are masked by the overriding tendency for a porous scale.

Barrett, Charles A.↗

Process Development for Permanganate Addition During Oxidative Leaching of Hanford Tanks Sludges

Previous Bechtel National, Incorporated (BNI)-sponsored studies have targeted optimizing sodium permanganate for the selective oxidation of chromium from washed Hanford tank sludges (Rapko et al. 2004; Rapko et al. 2005). The recommendation from previous work was that contact with sodium permanganate in a minimally caustic solution, i.e., 0.1 to 0.25 M [OH-] initially, provided maximum Cr dissolution while minimizing concomitant Pu dissolution. At the request of BNI, further work on oxidative alkaline leaching was performed.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effects of chromium and aluminum on mechanical and oxidation properties of iron-nickel-base superalloys based on CG-27

The effects of chromium and aluminum on the mechanical and oxidation properties of a series of gamma-prime-strengthened alloys based on CG-27 were studied. Gamma-prime dispersion and solid-solution strengthening were the principal modes of alloy strengthening. The oxidation attack parameter K sub a decreased with increasing Cr and Al contents for each alloy group based on Al content. As a group, alloys with 3 wt % Al had the lowest attack parameters. Therefore, 3 wt % is the optimum level of Al for parabolic oxidation behavior. Spalling, due to diffusion-induced grain growth, was controlled by the overall Cr and Al levels. The alloy with 4 wt % Cr and 3 wt % Al had stress-rupture properties superior to those of the base alloy, CG-27, and maintained parabolic oxidation behavior while the Cr content was reduced by two-thirds of its value in cast CG-27.

Schuon, S. R.↗

Influences of doping Cr/Fe/Ta on the performance of Ni/CeO{sub 2} catalyst under microwave irradiation in dry reforming of CH{sub 4}

The structure of Ni/CeO{sub 2} catalyst with doping of Cr, Fe and Ta was investigated with XRD, N{sub 2} physisorption, XPS and HRTEM and the catalytic activity of the catalysts under microwave irradiation in dry reforming of methane was tested in a microwave reactor. The results show that the introduction of Cr and Ta to Ni/CeO{sub 2} can enhance the interaction between Ni and the support/promoter and inhibit the enlargement of NiO particles during the synthesis. The CH{sub 4} conversions in dry reforming on the catalysts follow the order: Ni/CeO{sub 2}<2Fe–Ni<2Ta–Ni<2Cr–Ni. The superior performance of 2Ta–Ni and 2Cr–Ni may be attributed to the locally-heated Ni particles caused by the strong microwave absorption of the in-situ grown graphene attached on them under microwave irradiation. - Highlights: • The influences of doping Cr, Fe and Ta on Ni/CeO{sub 2} were investigated. • The catalytic performances before and after doping were investigated. • The in-situ grown graphene can promote the conversion of reactants.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-Temperature Oxidation of Stellite 12 Hardfacings: Effect of Mo on Characteristics of Oxide Scale

This study aims to understand the oxide scale formation on the surfaces of commercial and Mo (10 wt.%)-modified Stellite 12 hardfacings deposited on 4140 steel. For this purpose, samples of the hardfacings were isothermally oxidized in air at various temperatures in between 500 and 900 °C for 30 h. As a result of changes in the microstructure upon Mo addition, about 50% higher mass gain at all oxidation temperatures was observed. The characteristics of the developed oxide scales were examined by utilizing Raman spectroscopy, scanning electron microscopy and x-ray diffraction analysis. The oxide scale formed over Stellite 12 consisted of CoO-, Co{sub 3}O{sub 4-} and Cr{sub 2}O{sub 3}-type oxides, while additionally CoMoO{sub 4}-type complex oxide was detected on Mo-modified hardfacing, more likely at the alloy–scale interface. On the basis of findings of isothermal oxidation tests, the formation mechanisms of this complex oxide imposing better wear resistance as reported in our previous studies were explained during high-temperature wear testing, i.e., dynamic oxidation conditions.

36 MATERIALS SCIENCE↗

Effects of Composition and Oxidation States on the Structures of Chromium-Containing Sodium Silicate Glasses: Molecular Dynamics Simulations using Machine Learning Interatomic Potentials

Chromium represents a significant challenge for the vitrification of high-level nuclear waste into silicate and borosilicate glasses due to its low solubility and variable oxidation states, which can limit the waste loading due to promotion of crystallization or phase separation during processing. In this study, we modeled chromium containing silicate glasses using molecular dynamics simulations with three machine learning interatomic potentials (MLIPs), MACE, CHGNet, and PFP were employed, to gain insights on glass composition and oxidation states on the structures of these glasses. One of the goals is to evaluate their ability of these MLIPs to accurately represent the general structure of silicate glasses and chromium local environments as a function of chromium oxidation states. Density Functional Theory (DFT) based calculations and experimental data such as neutron structure factors were used to validate the structural models. It was found that the foundation models of all three MLIPs are able to reproduce general structural features of the sodium silicate glass structure consistent with experimental and DFT data, but only CHGNet and PFP can accurately capture the oxidation states and local environment of chromium: tetrahedral for Cr6+ and octahedral for Cr3+. Furthermore, we studied the effect of varying Cr3+/ Cr6+ (Cr3+/Crtotal) ratio and total chromium content using PFP. Our results show that Cr6+ enhances network polymerization by reducing non-bridging oxygens through Na? charge compensation required due to the formation of chromate (CrO42-) species, while Cr³? acts as a network modifier that disrupts connectivity. System size effects on the structural characteristics and chromium environments were also tested using the PFP potential. This work highlights the importance of careful validation on the precision, transferability, and potential of MLIPs for modeling glasses containing transition metal elements that can exist in multiple oxidation states. It is also encouraging to see the foundational models are all three MLFFs are able to reproduce the basic sodium silicate glass structures, while suggesting additional training or refining is needed to improve the description of more complex systems containing transition metals.

Puga, Christina L.↗

Investigation of the oxide film on 308L weld surface produced during welding process

Highlights: • Double layer film formed under welding of no shielding was first deeply studied. • Micro-cracks and nano-scale gaps were found in outer and inner layer. • Outer layer was composed of Fe{sub 2}O{sub 3}, inner layer included Fe{sub 3}O{sub 4} and FeCr{sub 2}O{sub 4.} • Cr deficiency of film related to the volatilization of CrO{sub 3} over 1000 °C. • Oxidation rule of 308L weld during GTAW was found based on thermodynamics. The oxide film formed during welding on the inner surface of 308L weld was investigated. The morphology, composition and structure of the oxide film were characterized by optical microscopy, scanning electron microscopy, laser Raman spectroscopy, X-ray diffraction, Auger electron spectroscopy and transmission electron microscopy. The results indicated that the oxidation degree of the weld metal was generally uniform from the weld center to the fusion line. Micro-scale cracks were found on the outer surface of the oxide film and nano-scale gaps scattered on the inner oxide film-weld interface. The oxide film exhibited a duplex structure including outer and inner layers. The outer layer, made of tightly bound particles, was mainly composed of Fe{sub 2}O{sub 3} oxide particles with a diameter of 50–150 nm. And the inner layer, made of relative loosely bound particles, was mainly composed of Fe{sub 3}O{sub 4} and FeCr{sub 2}O{sub 4} oxide particles with a diameter of 10–50 nm. The corresponding oxidation behavior and mechanism of the oxide film were also discussed.

36 MATERIALS SCIENCE↗

Oxygen Plasma Activation of Cr(CO)(6) on α-Fe2O3(0001)

The chemistry of Cr(CO)6 on the Fe3O4(111) surface termination of α-Fe2O3(0001) was explored using temperature programmed desorption (TPD), Auger electron spectroscopy (AES), static secondary ion mass spectrometry (SSIMS) and low energy electron diffraction (LEED) both with and without activation from an oxygen plasma source. No thermal decomposition of Cr(CO)6 was detected on the surface in the absence of O2 plasma treatment, with first layer molecules desorbing in TPD at 215 K from a close-packed overlayer. The interaction of first layer Cr(CO)6 with the Fe3O4(111)-termination was weak, desorbing only ~30 K above the leading edge of the multilayer state. Activation of multilayer coverages of Cr(CO)6 with the O2 plasma source at 100K resulted in complete conversion of the outer Cr(CO)6 layers, presumably to a disordered Cr oxide film, with Cr(CO)6 molecules near the surface left unaffected. Absence of CO or CO2 desorption states suggests that all carbonyl ligands are liberated for each Cr(CO)6 molecule activated by the plasma. AES and SSIMS both show that O2 plasma activation of Cr(CO)6 results in a carbon-free surface (after desorption of unreacted Cr(CO)6). LEED, however, shows that the Cr oxide film is disordered at 600 K and likely O-terminated based on subsequent water TPD. Attempts to order the film at temperatures above 650 K results in dissolution of Cr into the α-Fe2O3(0001) crystal based on SSIMS, an observation that is linked to the Fe3O4(111) termination of the surface and not to the properties of α-Cr2O3/α-Fe2O3 corundum interfaces. Nevertheless, this study shows that O2 plasma activation of Cr(CO)6 is an effect means of depositing Cr oxide films on surface without accompanying carbon contamination.

36 MATERIALS SCIENCE↗

Activation of Tungsten Oxide for Propane Dehydrogenation and Its High Catalytic Activity and Selectivity

Dehydrogenation of propane to propene is one of the important reactions for the production of higher-value chemical intermediates. In the commercial processes, platinum- or chromium oxide-based catalysts have been used for catalytic propane dehydrogenation. Herein, we first report that bulk tungsten oxide can serve as the catalyst for propane dehydrogenation. Tungsten oxide is activated by hydrogen pretreatment and/or co-feeding of hydrogen. Its catalytic activity strongly depends on hydrogen pretreatment time and partial pressure of hydrogen in the feed gas. The activation of tungsten oxide by hydrogen is attributed to reduction of the metal oxide and presence of multivalent oxidation states. Comparison of the catalytic performance of partially reduced WO 3-x to other highly active metal oxides shows that WO 3-x exhibits superior catalytic activity and selectivity than Cr2O 3 and Ga 2 O 3 . The findings of this work provide the possibility for activation of metal oxides for catalytic reactions and the opportunity for the development of new type of catalytic systems utilizing partially reduced metal oxides.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-velocity-oxidation performance of metal-chromium-aluminum (MCrAl), cermet, and modified aluminide coatings on IN-100 and type VIA alloys at 1093 C

Cermet, MCrAl, and modified aluminide types of coatings applied to IN-100 and NASA-TRW-VIA alloy specimens were cyclically oxidation tested in a high velocity (Mach 1) gas flame at 1093 C. Several coating compositions of each type were evaluated for oxidation resistance. The modified aluminide coating, Pt-Al, applied to alloy 6A proved to be the best, providing oxidation protection to approximately 750 hours based on weight change measurements. The second best, a CoCrAlY coating applied to 6A, provided protection to 450 hours. The third best was a cermet + aluminide coating on 6A with a protection time to 385 hours.

Deadmore, D. L.↗

High temperature oxidation and microstructural evolution of cold spray chromium coatings on Zircaloy-4 in steam environments

Oxidation kinetics and microstructural evolution of cold sprayed Cr coatings on Zircaloy-4 at 1130–1310 °C in flowing steam at atmospheric pressure have been studied. The study is aimed at understanding of the response of Cr coated Zr-alloy under a steam environment and high temperatures pertinent to design basis accidents (DBAs) and beyond design basis accidents (BDBAs) in light water reactors (LWRs). Surface morphology, microstructure, and phases of post-oxidation test samples were characterized using Scanning Electron Microscopy (SEM), x-ray diffraction (XRD), and Scanning Transmission Electron Microscopy (STEM). Growth kinetics of the Cr-oxide scale and interdiffusion layers between the Cr coating and the Zr-alloy substrate were quantified from cross-sectional SEM images. Cross-sectional analysis showed that the Cr coatings offered a 50 times reduction in oxidation rate over bare Zircaloy-4 in a 1310 °C steam environment. Oxidation kinetics at 1130 °C followed parabolic law (i.e., n ~ 0.5 in power law kinetics) but at 1230 °C and 1310 °C the value of n was suppressed to below 0.5 possibly due to the volatilization of Cr species at the two highest temperatures. Interdiffusion at coating/substrate interface resulted in formation of a brittle Cr 2 Zr or Zr(Fe, Cr) 2 intermetallic compound layer on the order of micrometer in thickness and scattered Cr-rich precipitates were observed well below the interface within the Zr-alloy substrate after cooling. These experimental results could provide data to LWR system simulation codes for better estimation of coping time in the event of accidents.

36 MATERIALS SCIENCE↗

Investigation of high temperature corrosion behavior on 304L austenite stainless steel in corrosive environments

In this work, 304L stainless steel samples were exposed at 700 °C for 10hrs in different corrosive environments; dry oxygen, molten salt, and molten salt + dry oxygen. The corrosion behavior of samples was analyzed using weight change measurement technique, optical microscope (OM) and Scanning Electron Microscope (SEM) equipped with Energy Dispersive X-ray (EDX). The existence phases of corroded sample were determined using X-ray Diffraction (XRD). The lowest corrosion rate was recorded in dry oxygen while the highest was in molten salt + dry oxygen environments with the value of 0.0062 mg/cm{sup 2} and −13.5225 mg/cm{sup 2} respectively. The surface morphology of sample in presence of salt mixture showed scale spallation. Oxide scales of Fe{sub 3}O{sub 4}, Fe{sub 2}O{sub 3} were the main phases developed and detected by XRD technique. Cr{sub 2}O{sub 3} was not developed in every sample as protective layers but chromate-rich oxide was developed. The cross-section analysis found the oxide scales were in porous, thick and non-adherent that would not an effective barrier to prevent from further degradation of alloy. EDX analysis also showed the Cr-element was low compared to Fe-element at the oxide scale region.

36 MATERIALS SCIENCE↗

High-temperature oxidation and quenching of chromium-coated zirconium alloy ATF cladding tubes with and w/o pre-damage

Chromium-coated zirconium alloys are one of the promising candidates for accident-tolerant fuel cladding (ATF) tubes for light water reactors (LWRs). In this study, the high temperature oxidation and degradation of two types of Cr coatings (cold spray and physical vapor deposition) with and without pre-damage by scratches were investigated on prototype rod segment samples filled with ZrO 2 pellets and tightly sealed with welded end caps. Isothermal tests at 1100 and 1200 °C were terminated by quenching with water; transient tests were performed up to 1500–1600 °C until complete coating failure. The positive effect of both types of Cr coatings was observed in all tests. Pre-damaged specimens showed only locally increased oxidation of the scratched zone, but no negative effects on the adjacent Cr coating. Finally, the behavior of the two types of coatings is compared and the degradation mechanisms are discussed based on hydrogen release data, extensive metallographic post-test examinations, and the current state of global research.

36 MATERIALS SCIENCE↗

Capabilities to improve corrosion resistance of fuel claddings by using powerful laser and plasma sources

The treatment conditions of fuel claddings of the E110 alloy by using powerful UV or IR laser radiation, which lead to the increase in the corrosion resistance at the high-temperature (T = 1100°C) oxidation simulating a loss-of-coolant accident, are determined. The possibility of the complete suppression of corrosion under these conditions by using pulsed laser deposition of a Cr layer is demonstrated. The behavior of protective coatings of Al, Al{sub 2}O{sub 3}, and Cr planted on steel EP823 by pulsed laser deposition, which is planned to be used in the BREST-OD-300, is studied. The methods of the almost complete suppression of corrosion in liquid lead to the temperature of 720°C are shown.

36 MATERIALS SCIENCE↗

Pore Scale Modeling of the Reactive Transport of Chromium in the Cathode of a Solid Oxide Fuel Cell

We present a pore scale model of a solid oxide fuel cell (SOFC) cathode. Volatile chromium species are known to migrate from the current collector of the SOFC into the cathode where over time they decrease the voltage output of the fuel cell. A pore scale model is used to investigate the reactive transport of chromium species in the cathode and to study the driving forces of chromium poisoning. A multi-scale modeling approach is proposed which uses a cell level model of the cathode, air channel and current collector to determine the boundary conditions for a pore scale model of a section of the cathode. The pore scale model uses a discrete representation of the cathode to explicitly model the surface reactions of oxygen and chromium with a cathode material. The pore scale model is used to study the reaction mechanisms of chromium by considering the effects of reaction rates, diffusion coefficients, chromium vaporization, and oxygen consumption on chromium’s deposition in the cathode. The study shows that chromium poisoning is most significantly affected by the chromium reaction rates in the cathode and that the reaction rates are a function of the local current density in the cathode.

30 DIRECT ENERGY CONVERSION↗