Search NASA⌕ Search

SEARCH · Search NASA

Results for “CORROSION TEST”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

YF-12 Lockalloy ventral fin program, volume 1

Results are presented of the YF-12 Lockalloy Ventral Fin Program which was carried out by Lockheed Aircraft Corporation - Advanced Development Projects for the joint NASA/USAF YF-12 Project. The primary purpose of the program was to redesign and fabricate the ventral fin of the YF-12 research airplane (to reduce flutter) using Lockalloy, and alloy of beryllium and aluminum, as a major structural material. A secondary purpose, was to make a material characterization study (thermodynamic properties, corrosion; fatigue tests, mechanical properties) of Lockalloy to validate the design of the ventral fin and expand the existing data base on this material. All significant information pertinent to the design and fabrication of the ventral fin is covered. Emphasis throughout is given to Lockalloy fabrication and machining techniques and attendant personnel safety precautions. Costs are also examined. Photographs of tested alloy specimens are shown along with the test equipment used.

Duba, R. J.↗

Investigation of test methods, material properties, and processes for solar cell encapsulants

A study of potentially useful low cost encapsulation materials for the Flat-Plate Solar Array project is discussed. The goal is to identify, evaluate, test and recommend encapsulant materials and processes for the production of cost-effective, long life solar cell modules. Technical investigations included studies of aging and degradation of candidate encapsulation materials, continued identification of primers for durable bonding of module interfaces, continued evaluation of soil resistant treatments for the sunlit surface of the module and testing of corrosion protective coatings for use low cost mild steel substrates.

Willis, P. B.↗

Comparison of compliance results for the wedge-loaded compact specimen

Results of the ratio of stress intensity factor to crack-mouth displacement as a function of crack length are presented for the wedge-loaded compact specimen. Comparisons are made between experimental compliance results, numerical results from collocation methods, and deep-crack limit-solution results. Applications are for crack-arrest and stress-corrosion-cracking tests for metals and other materials under predominantly linear elastic conditions.

Underwood, J. H.↗

Calcification prevention tablets

Citric acid tablets, which slowly release citric acid when flushed with water, are under development by the Navy for calcification prevention. The citric acid dissolves calcium carbonate deposits and chelates the calcium. For use in urinals, a dispenser is not required because the tablets are non-toxic and safe to handle. The tablets are placed in the bottom of the urinal, and are consumed in several hundred flushes (the release rate can be tailored by adjusting the formulation). All of the ingredients are environmentally biodegradable. Mass production of the tablets on commercial tableting machines was demonstrated. The tablets are inexpensive (about 75 cents apiece). Incidences of clogged pipes and urinals were greatly decreased in long term shipboard tests. The corrosion rate of sewage collection pipe (90/10 Cu/Ni) in citric acid solution in the laboratory is several mils per year at conditions typically found in traps under the urinals. The only shipboard corrosion seen to date is of the yellow brass urinal tail pieces. While this is acceptable, the search for a nontoxic corrosion inhibitor is underway. The shelf life of the tablets is at least one year if stored at 50 percent relative humidity, and longer if stored in sealed plastic buckets.

Lindsay, Geoffrey A.↗

FAA/NASA International Symposium on Advanced Structural Integrity Methods for Airframe Durability and Damage Tolerance, part 2

The international technical experts in the areas of durability and damage tolerance of metallic airframe structures were assembled to present and discuss recent research findings and the development of advanced design and analysis methods, structural concepts, and advanced materials. The principal focus of the symposium was on the dissemination of new knowledge and the peer-review of progress on the development of advanced methodologies. Papers were presented on the following topics: structural concepts for enhanced durability, damage tolerance, and maintainability; new metallic alloys and processing technology; fatigue crack initiation and small crack effects; fatigue crack growth models; fracture mechanics failure criteria for ductile materials; structural mechanics methodology for residual strength and life prediction; development of flight load spectra for design and testing; and corrosion resistance.

Harris, Charles E.↗

Testing

Testing is conducted to verify that the connectors will properly perform over time (reliability) per the application requirements. Testing by the manufacturer usually involves performance testing per the datasheet requirements. However, the customer may have applications that require performance under unique operational and environmental conditions. In general, electrical tests for connectors include dielectric withstanding voltage, low-signal-level contact resistance, insulation resistance, contact resistance, and standing wave ratio. Environmental tests include humidity, temperature, and contaminating conditions, as well as mechanical stress environments including vibration, mechanical shock, and durability cycling exposures.

Connectors, testing, Dielectric Withstanding Volta↗

Refinement of Promising Coating Compositions for Directionally Cast Eutectics

The successful application of high creep strength, directionally solidified gamma/gamma prime-delta (Ni-19.7Cb-6Cr-2.5Al) eutectic superalloy turbine blades requires the development of suitable coatings for airfoil, root and internal blade surfaces. In order to improve coatings for the gamma/gamma prime-delta alloy, the current investigation had the goals of (1) refining promising coating compositions for directionally solidified eutectics, (2) evaluating the effects of coating/ substrate interactions on the mechanical properties of the alloy, and (3) evaluating diffusion aluminide coatings for internal surfaces. Burner rig cyclic oxidation, furnace cyclic hot corrosion, ductility, and thermal fatigue tests indicated that NiCrAlY+Pt(63 to 127 micron Ni-18Cr-12Al-0.3Y + 6 micron Pt) and NiCrAlY(63 to 127 micron Ni-18Cr-12Al-0.3Y) coatings are capable of protecting high temperature gas path surfaces of eutectic alloy airfoils. Burner rig (Mach 0.37) testing indicated that the useful coating life of the 127 micron thick coatings exceeded 1000 hours at 1366 K (2000 deg F). Isothermal fatigue and furnance hot corrosion tests indicated that 63 micron NiCrAlY, NiCrAlY + Pt and platinum modified diffusion aluminide (Pt + Al) coating systems are capable of protecting the relatively cooler surfaces of the blade root. Finally, a gas phase coating process was evaluated for diffusion aluminizing internal surfaces and cooling holes of air-cooled gamma/gamma prime-delta turbine blades.

Strangman, T. E.↗

ZM-21 magnesium alloy corrosion properties and cryogenic to elevated temperature mechanical properties

The mechanical properties of bare ZM-21 magnesium alloy flat tensile specimens were determined for test temperatures of +400 F, +300 F, +200 F, +80 F, 0 F, -100 F, -200 F, and -320 F. The ultimate tensile and yield strengths of the material increased with decreasing temperature with a corresponding reduction in elongation values. Stress corrosion tests performed under: (1) MSFC atmospheric conditions; (2) 95% relative humidity; and (3) submerged in 100 ppm chloride solution for 8 weeks indicated that the alloy is not susceptible to stress corrosion. The corrosion tests indicated that the material is susceptible to attack by crevice corrosion in high humidity and chemical type attack by chloride solution. Atmospheric conditions at MSFC did not produce any adverse effects on the material, probably due to the rapid formation of a protective oxide coating. In both the mechanical properties and the stress corrosion evaluations the test specimens which were cut transverse to the rolling direction had superior properties when compared to the longitudinal properties.

Montana, J. W.↗

Study of development and utilization of a multipurpose atmospheric corrosion sensor

There has been a critical need for analyzing various aspects of atmospheric corrosion and for the development of atmospheric corrosion microsensors. The project work has involved the following activities: (1) making of multielectrode corrosion monitors on dielectric substrates; (2) testing them in the laboratory for functional characteristics; (3) preparing a report on the state of the art of atmospheric corrosion sensor development around the world; and (4) corrosion testing of electrochemical changes of sensor specimens and related fog testing. The study included work on the subject of development and utilization of a multipurpose atmospheric corrosion sensor and this report is the annual report on work carried out on this research project. This has included studies on the development of sensors of two designs, stage 1 and stage 2, and with glass and alumina substrate, experimentation and development and characterization of the coating uniformity, aspects of corrosion monitoring, literature search on the corrosion sensors and their development. A state of the art report on atmospheric corrosion sensor development was prepared and submitted.

Diwan, Ravinder M.↗