Search NASA⌕ Search

SEARCH · Search NASA

Results for “GAS WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Stainless Steel 18-10 CO2 Laser Welding And Plasma Diagnostics

The welding of materials by CO2 laser took significant considerations in industry, for the reason of the quality of the carried out weldings, and for other many advantages, but the automation of the welding operation requires a control system in real time. The operation of welding is an operation of interaction between the radiation (laser), and the matter (welded part), which is characterized by the vaporization of the matter, formation of the keyhole in material, and appearance of plasma over the material. This study relates to the relation between the welding (molten material) and the plasma which is formed on material. The light emitted by plasma during laser welding was recorded by an OMA detector (Optical Multichannel Analyzer) over a wavelength width of 450 A ring . The analysis of this light allows to determine the composition of this plasma, its dimensions, and the state of its energy according to the laser parameters. The welded material is the stainless steel 18-10, it was found that the intensity of the light emitted by plasma depends on laser power, the welding speed, the flow rate of assist gas. The relation between the plasma and the state of the bead were analyzed for on-line monitoring welding.

36 MATERIALS SCIENCE↗

Progress in developing laser based post irradiation examination infrastructure

To be able to understand the performance of reactor fuels and materials, irradiated materials must be characterized effectively and efficiently in high rad environments. This characterization work is performed remotely and in environments generally hostile to instrumentation. Laser based characterization techniques provide the ability to operate remotely and robustly in a hot-cell environment. Laser based instrumentation also can provide high spatial resolution suitable for scanning and imaging large areas. The INL is currently developing three laser based Post Irradiation Examination (PIE) stations for the Hot Fuel Examination Facility (HFEF) at the INL. These laser based systems will characterize irradiated materials and fuels. The characterization systems are the following: -) laser shock, -) laser based ultrasonic C-scan system and -) gas assay, sample and recharge system (GASR, up-grade to an existing system). The laser shock technique will characterize material properties and failure loads/mechanisms in various materials such as Light Water Reactor (LWR) fuel, plate fuel, and next generation fuel forms in high radiation areas. The laser shock-technique induces large amplitude shock waves to mechanically characterize interfaces such as the fuel-clad bond. As part of the laser shock system, a laser-based ultrasonic C-scan system will be used to detect and characterize de bonding caused by the application of the laser shock as well as performing classical non-destructive evaluation testing and imaging functions such as microstructure characterization, flaw detection and dimensional metrology. A spectroscopy capability can be added later as the salient components to perform Light Induced Breakdown Spectroscopy will be in place. Additional fiber ports in the feed-through will also enable future spectroscopic techniques to be efficiently installed and operated. The purpose of the GASR is to measure the pressure/volume of the plenum of an irradiated fuel element/capsule and obtain fission gas samples for analysis. The study of pressure and volume in the plenum of an irradiated fuel element/capsule and the analysis of fission gases released is important to understanding the performance of reactor fuels and materials. The main function of the laser in this application is to puncture the fuel rod or plate to allow the fission gas to escape and if necessary to weld the hole close. This system may also be used to measure the pressure/volume of other components (such as control blades) and obtain gas samples from these components for analysis. The GASR upgrade will match the functionality of the current system and provide these important functions on fuels made from current and future engineered materials. The GASR station will also have the inherent capability to perform cutting welding and joining functions within a hot-cell. The extra fiber ports built into the hot cell feed-through will also enable the efficient installation of future laser processing work benches. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Modular In-Chamber Electron Beam Welding – Process Planning: Welding, Cladding, Inspection, and Manufacturing

Electron beam welding (EBW) is commonly employed by industry today to join relatively thin section components. Industrial sectors which utilize the technology include; automotive, aircraft, aerospace, defense, medical, oil & gas, etc. The ability to produce single pass, thick section (up to 6 inches, 150mm) welds has also been available for more than 40 years; however, the technology has not been deployed for civil nuclear manufacturing and fabrication such as reactor pressure vessels, steam generators, or pressurizers. Instead, thick section joining is performed much in the same manner it has been for decades using submerged arc or gas tungsten arc welding processes. Recent research performed under U.S. Department of Energy (DOE) project DE-NE0008629 has demonstrated that the overall welding time to produce one major reactor pressure vessel (RPV) girth weld can be reduced from weeks to less than 90 minutes, while maintaining exceptional quality and inspection characteristics. The subject project (DE-NE0008846) investigates a modular in-chamber (MIC) EBW approach which allows various RPV sections to be joined within a “modular” chamber. The MIC-EBW approach utilizes individual modules that can be stacked and de-stacked to various heights to enable production girth welds to be performed at a given elevation. This report describes the various processing methodology necessary to complete major girth weldments for the NuScale Power small modular reactor including welding development, manufacturing, production sequence, inspection, and cladding.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Hydrogen accelerated fatigue crack growth of friction stir welded X52 steel pipe

Friction stir welded steel pipelines were tested in high pressure hydrogen gas to examine the effects of hydrogen accelerated fatigue crack growth. Fatigue crack growth rate (da/dN) vs. stress-intensity factor range (ΔK) relationships were measured for an X52 friction stir welded pipe tested in 21 MPa hydrogen gas at a frequency of 1 Hz and R = 0.5. Tests were performed on three regions: base metal (BM), center of friction stir weld (FSW), and 15 mm off-center of the weld. For all three material regions, tests in hydrogen exhibited accelerated fatigue crack growth rates that exceeded an order of magnitude compared to companion tests in air. Among tests in hydrogen, fatigue crack growth rates were modestly higher in the FSW than the BM and 15 mm off-center tests. Select regions of the fracture surfaces associated with specified ΔK levels were examined which revealed intergranular fracture in the BM and 15 mm off-center specimens but an absence of intergranular features in the FSW specimens. In conclusion, the X52 friction stir weld and base metal tested in hydrogen exhibited fatigue crack growth rate relationships that are comparable to those for conventional arc welded steel pipeline of similar strength found in the literature.

08 HYDROGEN↗

Effect of Ni content on the microstructure and mechanical properties of weld metal with both-side submerged arc welding technique

Highlights: • This manuscript primarily studied the effects of Ni content on the K65 weld metals; • Increase Ni content could significantly improve the strength and low temperature impact toughness of the weld metal. • The beneficial effect of Ni is attributed to its positive effect on phase transformation. • GBF keeps K-S or N-W relations only with one austenite and the variants belong to the same bain group are two reasons. • The M/A islands are considered to be another reason for the reduced toughness. - Abstract: The effects of nickel (Ni) content on the mechanical properties and microstructure evolution in the weld metals of commercial K65 oil and gas pipeline steel were studied. Increase Ni content could significantly improve the strength and low temperature impact toughness (−40 °C and −60 °C) of the weld metal. The above influences of Ni were attributed to the formation of predominant acicular ferrite (AF), at the expense of grain boundary ferrite (GBF), ferrite side plates (FSP) and martensite/austenite (M/A) constituent in weld metal. EBSD results indicated that GBF keeps K-S or N-W relations only with the prior austensite grain that belongs to one side of the grain boundary and the variants belong to the same bain group which always forms low angle boundary. Moreover, the retained austenite as one part of M/A constituent was mainly found in the weld metal with lower Ni content. It indicated that the transformation process could be promoted more completely by the increase of Ni content. The mechanism of the toughness improvement brought by Ni increasing was ascribed to the relatively uniform transformation to final microstructure, which reduces the appearance of GBF and M/A constituents.

36 MATERIALS SCIENCE↗

PDC IC Weld Failure Evaluation and Resolution

During final preparations for start of the PDCF Inner Can (IC) qualification effort, welding was performed on an automated weld system known as the PICN. During the initial weld, using a pedigree canister and plug, a weld defect was observed. The defect resulted in a hole in the sidewall of the canister, and it was observed that the plug sidewall had not been consumed. This was a new type of failure not seen during development and production of legacy Bagless Transfer Cans (FB-Line/Hanford). Therefore, a team was assembled to determine the root cause and to determine if the process could be improved. After several brain storming sessions (MS and T, R and D Engineering, PDC Project), an evaluation matrix was established to direct this effort. The matrix identified numerous activities that could be taken and then prioritized those activities. This effort was limited by both time and resources (the number of canisters and plugs available for testing was limited). A discovery process was initiated to evaluate the Vendor's IC fabrication process relative to legacy processes. There were no significant findings, however, some information regarding forging/anneal processes could not be obtained. Evaluations were conducted to compare mechanical properties of the PDC canisters relative to the legacy canisters. Some differences were identified, but mechanical properties were determined to be consistent with legacy materials. A number of process changes were also evaluated. A heat treatment procedure was established that could reduce the magnetic characteristics to levels similar to the legacy materials. An in-situ arc annealing process was developed that resulted in improved weld characteristics for test articles. Also several tack welds configurations were addressed, it was found that increasing the number of tack welds (and changing the sequence) resulted in decreased can to plug gaps and a more stable weld for test articles. Incorporating all of the process improvements for the actual can welding process, however, did not result in an improved weld geometry. Several possibilities for the lack of positive response exist, some of which are that (1) an insufficient number of test articles were welded under prototypic conditions, (2) the process was not optimized so that significant improvements were observable over the "noise", and (3) the in-situ arc anneal closed the gap down too much so the can was unable to exhaust pressure ahead of the weld. Several operational and mechanical improvements were identified. The weld clamps were changed to a design consistent with those used in the legacy operations. A helium puff operation was eliminated; it is believed that this operation was the cause of the original weld defect. Also, timing of plug mast movement was found to correspond with weld irregularities. The timing of the movement was changed to occur during weld head travel between tacks. In the end a three sequential tack weld process followed by a pulse weld at the same current and travel speed as was used for the legacy processes was suggested for use during the IC qualification effort. Relative to legacy welds, the PDC IC weld demonstrates greater fluctuation in the region of the weld located between tack welds. However, canister weld response (canister to canister) is consistent and with the aid of the optical mapping system (for targeting the cut position) is considered adequate. DR measurements and METs show the PDC IC welds to have sufficient ligament length to ensure adequate canister pressure/impact capacity and to ensure adequate stub function. The PDC welding process has not been optimized as a result of this effort. Differences remain between the legacy BTC welds and the PDC IC weld, but these differences are not sufficient to prevent resumption of the current PDC IC qualification effort. During the PDC IC qualification effort, a total of 17 cans will be welded and a variety of tests/inspections will be performed. The extensive data collected during that qualification effort should be of a sufficient population to determine if additional weld process optimization is necessary prior to production release.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Friction surfaced Stellite6 coatings

Solid state Stellite6 coatings were deposited on steel substrate by friction surfacing and compared with Stellite6 cast rod and coatings deposited by gas tungsten arc and plasma transferred arc welding processes. Friction surfaced coatings exhibited finer and uniformly distributed carbides and were characterized by the absence of solidification structure and compositional homogeneity compared to cast rod, gas tungsten arc and plasma transferred coatings. Friction surfaced coating showed relatively higher hardness. X-ray diffraction of samples showed only face centered cubic Co peaks while cold worked coating showed hexagonally close packed Co also. - Highlights: Black-Right-Pointing-Pointer Stellite6 used as coating material for friction surfacing. Black-Right-Pointing-Pointer Friction surfaced (FS) coatings compared with casting, GTA and PTA processes. Black-Right-Pointing-Pointer Finer and uniformly distributed carbides in friction surfaced coatings. Black-Right-Pointing-Pointer Absence of melting results compositional homogeneity in FS Stellite6 coatings.

36 MATERIALS SCIENCE↗

Creep Rupture Testing of Alloy 617 and A508/533 Base Metals and Weldments

The NGNP, which is an advanced HTGR concept with emphasis on both electricity and hydrogen production, involves helium as the coolant and a closed-cycle gas turbine for power generation with a core outlet/gas turbine inlet temperature of 750-1000°C. Alloy 617 is a prime candidate for VHTR structural components such as reactor internals, piping, and heat exchangers in view of its resistance to oxidation and elevated temperature strength. However, lack of adequate data on the performance of the alloy in welded condition prompted to initiate a creep test program at Argonne National Laboratory. In addition, Testing has been initiated to evaluate the creep rupture properties of the pressure vessel steel A508/533 in air and in helium environments. The program, which began in December 2009, was certified for quality assurance NQA-1 requirements during January and February 2010. Specimens were designed and fabricated during March and the tests were initiated in April 2010. During the past year, several creep tests were conducted in air on Alloy 617 base metal and weldment specimens at temperatures of 750, 850, and 950°C. Idaho National Laboratory, using gas tungsten arc welding method with Alloy 617 weld wire, fabricated the weldment specimens. Eight tests were conducted on Alloy 617 base metal specimens and nine were on Alloy 617 weldments. The creep rupture times for the base alloy and weldment tests were up to ~3900 and ~4500 h, respectively. The results showed that the creep rupture lives of weld specimens are much longer than those for the base alloy, when tested under identical test conditions. The test results also showed that the creep strain at fracture is in the range of 7-18% for weldment samples and were much lower than those for the base alloy, under similar test conditions. In general, the weldment specimens showed more of a flat or constant creep rate region than the base metal specimens. The base alloy and the weldment exhibited tertiary creep after 50-60% of the rupture life, irrespective of test temperature in the range of 750-950°C. The results showed that the stress dependence of the creep rate followed a power law for both base alloy and weldments. The data also showed that the stress exponent for creep is the same and one can infer that the same mechanism is operative in both base metal and weldments in the temperature range of the current study. SEM fractography analysis indicated that both base metal and weldment showed combined fracture modes consisting of dimple rupture and intergranular cracking. Intergranular cracking was more evident in the weldment specimens, which is consistent with the observation of lower creep ductility in the weldment than in the base metal.

08 HYDROGEN↗

Experimental Study of High-Velocity Projectile Impact Welding

The purpose of this study is to investigate the effect of various parameters on the welding process with high-velocity projectiles. For carrying out Impact Spot Welding tests, a single stage compressed gas gun impact test facility was used to launch flat- and conical-nosed projectiles within the velocity range from 100 to 150 m/s and performed. Different types of materials such as steel, copper, brass, and aluminum alloy were used. In the present experimental study, the steel plate with a thickness of 4 mm was considered as a back layer and the other plates made of copper, brass, and aluminum alloy were considered as front layers. Different gaps of 0.1, 0.2, and 0.5 mm were considered between the layers. The shape of the welded interface was studied by Scanning Electron Microscopy (SEM). The depth of penetration in the specimen and the kinetic energy of the projectiles were calculated. The experimental results showed that a complete bonding has occurred in the collision zone, especially in the central areas.

36 MATERIALS SCIENCE↗

Oxidation Behavior of Welded Fe-Based and Ni-Based Alloys in Supercritical CO 2

Next-generation supercritical CO 2 (sCO 2 ) power cycles will require different classes of alloy throughout the operational temperatures to optimize tradeoff of creep strength, oxidation performance and cost. This will necessitate joining methods such as welding, which might pose compatibility concerns at the joined interfaces. In this study, similar and dissimilar metal welds were generated from a variety of candidate alloys for sCO 2 systems including ferritic/martensitic steels, austenitic steels, and Ni-based superalloys. Samples were extracted from different regions of the welds and exposed to sCO 2 at 550 °C and 20 MPa for 2500 h, then characterized to understand their behavior in this environment. Unsurprisingly, the local oxidation behavior was largely dictated by the Cr content in the underlying metal. High-Cr austenitic steels and Ni alloys formed slow-growing Cr-rich oxide scales with minimal carburization of the underlying metal, while low-Cr ferritic/martensitic steels formed fast-growing Fe-rich oxide scales with significant carburization. Most welds did not show any unusual oxidation behavior at the interfaces, considering the local Cr content. The one exception was the 347H similar metal weld, where a larger grain size and complex grain structure in the fusion zone led to a significantly higher rate of Fe-rich oxide nodule formation compared to the base metal. This suggests that microstructural changes at joined interfaces can play an important role on the oxidation-limited lifetimes in future sCO 2 systems. The composition changes across the interfaces enabled study of the effect of Fe on the growth rate of Cr-rich oxides and of the origins of the sub-surface recrystallization zone that forms beneath them.

36 MATERIALS SCIENCE↗

Progress In Developing Laser Based Post Irradiation Examination Infrastructure

To be able to understand the performance of reactor fuels and materials, irradiated materials must be characterized effectively and efficiently in a high rad environment. The characterization work must be performed remotely and in an environment hostile to instrumentation. Laser based characterization techniques provide the ability to be remote and robust in a hot-cell environment. Laser based instrumentation also can provide high spatial resolution suitable for scanning and imaging large areas. The INL is currently developing three laser based Post Irradiation Examination (PIE) stations for the Hot Fuel Examination Facility at the INL. These laser based systems will characterize irradiated materials and fuels. The characterization systems are the following: Laser Shock Laser based ultrasonic C-scan system Gas Assay, Sample, and Recharge system (GASR, up-grade to an existing system). The laser shock technique will characterize material properties and failure loads/mechanisms in various materials such as LWR fuel, plate fuel, and next generation fuel forms, for PIE in high radiation areas. The laser shock-technique induces large amplitude shock waves to mechanically characterize interfaces such as the fuel-clad bond. The shock wave travels as a compression wave through the material to the free (unconfined) back surface and reflects back through the material under test as a rarefaction (tensile) wave. This rarefaction wave is the physical mechanism that produces internal de-lamination failure. As part of the laser shock system, a laser-based ultrasonic C-scan system will be used to detect and characterize debonding caused by the laser shock technique. The laser ultrasonic system will be fully capable of performing classical non-destructive evaluation testing and imaging functions such as microstructure characterization, flaw detection and dimensional metrology in complex components. The purpose of the GASR is to measure the pressure/volume of the plenum of an irradiated fuel element and obtain fission gas samples for analysis. The study of pressure and volume in the plenum of an irradiated fuel element and the analysis of fission gases released from the fuel is important to understanding the performance of reactor fuels and materials. This system may also be used to measure the pressure/volume of other components (such as control blades) and obtain gas samples from these components for analysis. The main function of the laser in this application is to puncture the fuel element to allow the fission gas to escape and if necessary to weld the spot close. The GASR station will have the inherent capability to perform cutting welding and joining functions within a hot-cell.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Innovative compact braze-free accelerating cavity

We report that high energy physics experiments using particle accelerators as well as industrial and medical applications are continuously seeking more compact, robust and cheaper accelerating structures. As of today, stable operating gradients, exceeding 100 MV/m, have been demonstrated by the SLAC group in the X-Band (11.424 GHz). These experiments show that hard structures, fabricated without high-temperature processes, achieve a better high gradient performance in terms of accelerating gradients. Therefore, we present an innovative and compact type of accelerating cavity that avoids any high-temperature processes like brazing or diffusion bonding. All cells are joined together by means of specifically designed and proprietary screws which ensure good vacuum and RF contacts. Two three-cell standing-wave accelerating structures, designed to operate in the pi-mode at 11.424 GHz, have been successfully built and cold tested. In order to guarantee a vacuum envelope and mechanically robust assembly, we used the Electron Beam Welding (EBW) and the Tungsten Inert Gas (TIG) processes. Lastly, this work has been carried out in the framework of a funded project by the Vth Committee of the INFN for the Laboratori Nazionali di Frascati (LNF), within a large international collaboration between LNF, SLAC and KEK for the development of X-Band accelerating cavities using "hard structure" technology.

43 PARTICLE ACCELERATORS↗

Challenges and successes in establishing a multipurpose fuels and materials irradiation capsule [Slides]

This presentation discusses the challenges and success related to designing and fabricating multipurpose capsules for irradiation experiments for irradiation within the Advanced Test Reactor (ATR) to be presented at tje DEVICE-MTR irradiation experiment design working group meeting hosted by the Japanese Atomic Energy Agency (JAEA). The information herein is limited to the design of the capsules only and no programmatic information from any project supporting the design of the multipurpose capsule is discussed. The intent of the design team was establish a capsule design that could accommodate multiple different irradiation project needs for the irradiation of nuclear fuel and materials of interest in the nuclear field. The main points of the presentation are as follows: use of tin as a molten thermal bond material was selected for the fueled capsule design and was found to be inadequate as it would corrode the stainless steel at high temperatures, this capsule design has high sensitivity to manufacturing of the gas gap and control of the gas mixture, and the fueled capsule has experienced welding challenges with the inner capsule material 800H Incoloy.

42 ENGINEERING↗

Tritium Aging Effects on Fracture Toughness of Stainless Steel Weldments

The long-term embrittlement effects of tritium and decay helium on the structural properties of stainless steels have been studied for years at Savannah River to provide required data for establishing safe operating conditions and lifetimes of pressure vessels used to contain tritium gas. In this study, the fracture toughness properties of the longest-aged tritium-precharged stainless-steel base metals and weldments tested at Savannah River were measured and compared to earlier results. The fracture toughness values were the lowest recorded here for tritium-exposed stainless steel. As-forged and as-welded specimens were thermally precharging with tritium gas at 34.5 MPa and 623 K, then aged for up to 17 years to buildin decay helium prior to testing. ASTM J-Integral fracture mechanics analyses, transmission electron microscopy (TEM), and small angle neutron scattering (SANS) examinations were conducted to characterize the effects of tritium and its radioactive decay product, helium-3. Results show that the fracture toughness values were reduced to less than 2-4% of the as-forged values for specimens with more than 1300 appm helium from tritium decay. The trend of decreasing fracture toughness values with increasing helium content was consistent with earlier observations, and the data show that Type 304L stainless steel is more resistant to tritium-induced cracking than Type 21-6-9 stainless at similar decay helium levels. The fracture toughness properties of long-aged weldments were also affected, but the reductions were not as severe over time because weldments did not retain as much tritium as did the base metals. TEM observations were used to characterize the effects of decay helium bubbles on the deformation substructures, but nanometer-sized helium bubbles were not easily resolved because of high dislocation densities within the forged microstructures. SANS results are presented that suggest the technique can provide information on decay helium bubble size, spacing, and distribution in these steels.

36 MATERIALS SCIENCE↗

Continuation of Studies on Development of ODS Heat Exchanger Tubing

The Department of Energy (DOE), National Energy Technology Center (NETL), has initiated a strategic plan for the development of advanced technologies needed to design and build fossil fuel plants with very high efficiency and environmental performance. These plants, referred to as 'Vision 21' and FutureGen programs by DOE, will produce electricity, chemicals, fuels, or a combination of these products, and possibly secondary products such as steam/heat for industrial use. MA956 is a prime candidate material being considered for a high temperature heat exchanger in the 'Vision 21' and FutureGen programs. This material is an oxide dispersion strengthened (ODS) alloy; however, there are some gaps in the data required to commit to the use of these alloys in a full-size plant. To fill the technology gaps for commercial production and use of the material for 'Advanced Power Generation Systems' this project has performed development activity to significant increase in circumferential strength of MA956 as compared to currently available material, investigated bonding technologies for bonding tube-to-tube joints through joining development, and performed tensile, creep and fire-side corrosion tests to validate the use and fabrication processes of MA956 to heat exchanger tubing applications. Development activities within this projected has demonstrated increased circumferential strength of MA956 tubes through flow form processing. Of the six fabrication technologies for bonding tube-to-tube joints, inertia friction welding (IFW) and flash butt welding (FBW) were identified as processes for joining MA956 tubes. Tensile, creep, and fire-side corrosion test data were generated for both base metal and weld joints. The data can be used for design of future systems employing MA956. Based upon the positive development activities, two test probes were designed and fabricated for field exposure testing at 1204 C ({approx}2200 F) flue gas. The probes contained tube portions with FBW and IFW welded MA956. Field testing of the probes and remaining heat exchanger design activity will be performed by Oak Ridge National Laboratory under DOE Contract DE-AC05-00OR22725.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

The effect of atmosphere on the composition of wire arc additive manufactured metal components

The effects of atmospheric contamination on wire arc additively manufactured (WAAM) components were studied by producing AM multilayer parts under controlled conditions. Gas impurity levels were maintained using an argon purge box at levels from atmospheric (210,000 ppm O 2 ) to 1 ppm O 2 , and with corresponding levels of nitrogen. Stainless steel (308L), titanium (Ti–6Al–4V) and pure Ta were studied, each having different affinities for oxygen and nitrogen. Results show that WAAM parts made in air produce unacceptable oxygen and/or nitrogen levels for most applications. However, with moderate purging, all three metals can be deposited by WAAM with compositions similar to the starting wire, and the results are used to provide recommended minimum purge box atmospheres for each metal.

36 MATERIALS SCIENCE↗