Direct observation of creep strengthening nanoprecipitate formation in ausformed ferritic/martensitic steels

It is well known the effectiveness of ausforming on increasing the dislocation density of fresh martensite. Here, this work demonstrates, using atom probe tomography, that this increase in the dislocation density has a strong influence on the nucleation of nanoprecipitates during tempering. Therefore, ausforming might be a powerful processing route for the two-fold improvement of ferritic/martensitic steels where creep resistance is of paramount importance. Firstly, ausforming refines the martensitic microstructure (high strength and toughness), and secondly, it increases the number density of thermally stable nanoprecipitates (creep resistance).

36 MATERIALS SCIENCE↗

Equal channel angular extrusion for bulk processing of Fe–Co–2V soft magnetic alloys, part II: Texture analysis and magnetic properties

In Part I, equal channel angular extrusion (ECAE) was demonstrated as a novel, simple-shear deformation process for producing bulk forms of the low ductility Fe–Co–2V (Hiperco 50A®) soft ferromagnetic alloy with refined grain sizes. Microstructures and mechanical properties were discussed. In this Part II contribution, the crystallographic textures and quasi-static magnetic properties of ECAE-processed Hiperco were characterized. The textures were of a simple-shear character defined by partial {110} and <111> fibers inclined relative to the extrusion direction, in agreement with the expectations for simple-shear deformation textures of BCC metals. These textures were observed throughout all processing conditions and only slightly reduced in intensity by subsequent recrystallization heat treatments. Characterization of the magnetic properties revealed a lower coercivity and higher permeability for ECAE-processed Hiperco specimens relative to the conventionally processed and annealed Hiperco bar. In conclusion, the effects of the resultant microstructure and texture on the coercivity and permeability magnetic properties are discussed.

36 MATERIALS SCIENCE↗

Physical forces influencing Skylab experiments M551, M552, and M553

The forces concerned with metals melting, exothermic brazing, and sphere forming experiments on Skylab 1 mission are reported. The conclusions reached are that no significant practical differences exist between terrestrial and microgravity electron beam melting, and braze gap clearances are far less critical to joining operations in space than on earth. Altered microstructures, increased grain refinement, and the appearance of a single, large interior shrinkage pore were found in the Skylab specimens.

Bourgeois, S. V.↗

Improved ultrasonic standard reference blocks

A program to improve the quality, reproducibility and reliability of nondestructive testing through the development of improved ASTM-type ultrasonic reference standards is described. Reference blocks of aluminum, steel, and titanium alloys were considered. Equipment representing the state-of-the-art in laboratory and field ultrasonic equipment was obtained and evaluated. Some RF and spectral data on ten sets of ultrasonic reference blocks were taken as part of a task to quantify the variability in response from nominally identical blocks. Techniques for residual stress, preferred orientation, and microstructural measurements were refined and are applied to a reference block rejected by the manufacturer during fabrication in order to evaluate the effect of metallurgical condition on block response.

Eitzen, D. G.↗

Effect of temperature on the formation of creep substructure in sodium chloride single crystals

The effect of temperature on the substructure morphology and the cell and subgrain size was investigated experimentally in NaCl single crystals under creep in the temperature range 573-873 K. It is found that the effect of temperature on the cell and subgrain sizes is weak in comparison with the effect of stress. However, there was a qualitative change in the substructure morphology with temperature, with the cells and subgrains better defined at higher temperatures. The volume fraction of the cell boundaries decreased with increasing temperature, thereby indicating a refinement of the microstructure at higher temperatures.

Raj, Sai V.↗

A laboratory means to produce tough aluminum sheet from powder

The rapid solidification of aluminum alloys as powder and the subsequent fabrication processes can be used to develop and tailor alloys to satisfy specific aerospace design requirements, including high strength and toughness. Laboratory procedures to produce aluminum powder-metallurgy (PM) materials are efficient but require evidence that the laboratory methods used can produce a product with superior properties. This paper describes laboratory equipment and procedures which can be used to produce tough aluminum PM sheet. The processing of a 2124 + 0.9 percent Zr aluminum alloy powder is used as an example. The fully hardened sheet product is evaluated in terms of properties and microstructure. The key features of the vacuum hot press pressing operation used to consolidate the powder are described. The 2124 + 0.9 percent Zr - T8 temper aluminum sheet produced was both strong (460-490 MPa yield strength) and tough (Kahn Tear unit-propagation- energy values over three times those typical for ingot metallurgy 2024-T81). Both the longitudinal and longitudinal-transverse directions of the sheet were tested. The microstructure was well refined with subgrains of one or two micrometers. Fine dispersoids of Al3Zr in the precipitate free regions adjacent to boundaries are believed to contribute to the improved toughness.

Singleton, O. R.↗

Multi-Pass Hybrid Laser Arc Welding of Alloy 740H

The presentation reviews the progress made toward reducing the joining time of an advanced nickel-based alloy, Alloy 740H by a factor of two using a novel two step fusion welding approach. In the first step, a high powered laser is used to rapidly join thick weld groove lands (~10-12 mm thick) during a single pass. Hybrid laser arc welding (HLAW) is then used to fill the remaining weld groove and complete the joint. This sequential process also utilizes laser wobble in both steps to reduce welding defects and refine the weld microstructure to obtain improved properties compared to conventional gas tungsten or gas metal arc welds, GTAW and GMAW, respectively. The creep behavior of laser-only thick weld groove land welds and HLAW welds were found to be the same or slightly improved compared to conventional GMAW or GTAW welds in this alloy. Creep tests have been started to verify the long-term creep behavior (~10,000 hrs) of these welds. Modeling results on deep penetration laser welding are presented and the initial simulations of laser welding with laser wobble are shown. The next phase of the project will combine the two processes to make complete welds - deep penetration laser welds of thick weld groove lands followed by rapid filling of the remaining weld groove by HLAW - in thick plates (32 mm thick) Alloy 740H plate and entails development of narrow weld groove welding to further decrease the joining time of this alloy.

36 MATERIALS SCIENCE↗

Microstructure Evolution and Microhardness Distribution of Copper Processed Using Multiple Passes of Elliptical Cross-Sectional Spiral Equal-Channel Extrusion

The aim of this work is to study the effect of six-pass elliptical cross-sectional spiral equal-channel extrusion (ECSEE) on the microstructure and performance of ultrafine-grained (UFG) copper. Equiaxed grains of average grain size of less than 1 μm are formed into shear bands in the low strain region of ECSEE deformed specimen. More homogeneous and equiaxed microstructure with high misorientation angles is obtained in the high strain. Moreover, the microstructure evolution of ECSEE-induced copper is a dynamic equilibrium process of shear deformation accompanying the interactions of high dislocation density, cellular structure and high-angle grain boundaries. The grain ECSEE refinement mechanism is described as the formation process of dislocations, cells, local grain sub-boundaries rotation and large angle grain restructure. The significantly non-uniform hardness distribution is consistent with the deformation behavior and microstructure refinement in the ECSEE-induced specimen. The homogeneity of microstructure and hardness improves as the ECSEE pass increases.

36 MATERIALS SCIENCE↗

Grain Refinement of a gamma-TiAl Alloy Through Isothermal Forging and Heat Treatment

Effect of initial massive type structure of a gamma-TiAl based alloy on its hot deformed and stabilized microstructure was investigated. A gamma alloy with composition of Ti-47Al-12Nb-0.5Si was subjected to rapid quenching from alpha phase field. The quenched sample was deformed at high temperature. Further post deformation heat treatment was conducted to stabilize the as-deformed structure. It was shown that Nb and Si have important roles in grain refinement of the final product. Presence of niobium in the alloy made the diffusion controlled eutectoid reaction sluggish and assisted the formation of massive type gamma phase (gamma{sub m}) by rapid cooling from alpha phase field. Silicon addition assisted the microstructural refinement by forming hard and finely dispersed titanium silicide particles. These particles act as preferred sites for dynamic recrystallization during hot deformation. Massive gamma phase tends to deform uniformly and decompose to equilibrium phases after final heat treatment and results in a very fine grained microstructure.

36 MATERIALS SCIENCE↗

Microstructural Evolution and Mechanical Properties of Ti-22Al-25Nb (At.%) Orthorhombic Alloy with Three Typical Microstructures

Microstructural evolution, tensile and creep behavior of Ti-22Al-25Nb (at.%) orthorhombic alloy with three typical microstructures were investigated. The three typical microstructures were obtained by different solution and age treatment temperatures and analyzed by the BSE technique. The tensile strengths of the alloy at room temperature and 650 °C were investigated. The creep behaviors of the three typical microstructures were also studied at 650 °C/150 MPa for 100 h in air. The phase transformation mechanisms in creep deformation were also found. The experimental results showed that the formations of the three typical microstructures were decided by the isothermal forging and heat treatment. It was supposed that the high-temperature solution treatment might be dominant for the volume fraction and diameter of the equiaxed particles. While the double age treatment would lead to lamellar O phases. Due to grain refinement strengthening, the equiaxed microstructure presented the best tensile strength and ductility. The fully lamellar microstructure had the best creep resistance than that of other microstructures. In this paper, the phenomenon of creep-induced α{sub 2} phase decomposition was occurred during creep deformation of the equiaxed microstructure.

36 MATERIALS SCIENCE↗

Influence of rolling reduction and annealing on recrystallization and grain structure in Ta-2.5W alloys

The microstructural evolution of wrought Tantalum - 2.5 wt% Tungsten (Ta-2.5W) alloys during thermomechanical processing is critical for optimizing their mechanical reliability in demanding applications such as aerospace, chemical processing, and nuclear technology. Despite the widespread use of Ta-W alloys, a comprehensive understanding of how rolling reduction, annealing temperature, and elemental inhomogeneity interact to determine recrystallization behavior and grain refinement remains incomplete. Here, in this study, we systematically investigate the effects of cold rolling and subsequent annealing on the microstructure of Ta-2.5W, with particular attention to grain orientation, stored energy, and elemental banding. Our results demonstrate that higher rolling reduction rates lower the onset and completion temperatures for recrystallization, resulting in finer and more homogeneous grain structures. Electron backscatter diffraction (EBSD) analysis reveals that grains with a 〈111〉 parallel to the plate normal possess higher stored energy and nucleate recrystallization more readily than grains with a 〈001〉 parallel to the plate normal. Elemental mapping shows that tungsten inhomogeneity leads to localized bands of accelerated recrystallization and hardness variation. These findings provide new insights into the mechanisms of microstructure refinement in Ta-2.5W alloys, offering guidance for tailoring processing routes to achieve superior performance in demanding engineering environments.

Annealing↗

Grain Refinement of Freeform Fabricated Ti-6Al-4V Alloy Using Beam/Arc Modulation

Grain refinement can significantly improve the mechanical properties of freeform-fabricated Ti-6Al-4V alloy, promoting increased strength and enhanced isotropy compared with coarser grained material. Large beta-grains can lead to a segregated microstructure, in regard to both alpha-phase morphology and alpha-lath orientation. Beam modulation, which has been used in conventional fusion welding to promote grain refinement, is explored in this study for use in additive manufacturing processes including electron beam freeform fabrication (EBF(sup 3)) and gas-tungsten arc (GTA) deposition to alter solidification behavior and produce a refined microstructure. The dynamic molten pool size induced by beam modulation causes rapid heat flow variance and results in a more competitive grain growth environment, reducing grain size. Consequently, improved isotropy and strength can be achieved with relatively small adjustments to deposition parameters.

Mitzner, Scott↗

Dynamic Recrystallization and Grain Refinement of Fe-P-C-Si and Fe-P-C-Si-N Steels

Grain refinement is an effective technique to improve the mechanical properties of steels. In the present work, single-pass hot compression experiments have been conducted on two different compositions of high phosphorous steels to study the microstructural evolution and ferrite grain refinement at various strain rates and deformation temperatures, i.e., 0.01-10 s{sup −1} and 750-1050 °C, respectively. Optical metallography has been employed to understand the physical processes that take place during hot deformation process. The results indicate that when these compositions of high phosphorous steels are worked at relatively low temperatures in the intercritical regions, a ferrite grain size of 5-7 µm is obtained. It is observed that the grain size decreases with an increase in strain rate and with the decrease in deformation temperature. Based on the values of stress exponent (n) obtained in the present work, dislocation creep is identified as the deformation mechanism. The activation energies for deformation of these two types of high phosphorous steels have been calculated. The effect of the alloying elements on the stress–strain curve, microstructure, and grain refinement has been discussed.

36 MATERIALS SCIENCE↗

Achieving Grain Refinement and Related Mechanical Property Improvement of an Al-Zn-Mg-Cu Alloy Through Severe Plastic Deformation

Microstructural features and mechanical properties of an Al-Zn-Mg-Cu alloy processed by equal-channel angular pressing (ECAP) have been investigated. The equivalent plastic strain obtained from the simulation agrees well with that from the analytical calculation in a way that both increase with an increase in deformation, but the strain distribution is non-uniform, appearing as a strain gradient along the norm direction. Microstructure investigation shows that grain refinement is achieved in frequency of low-angle grain boundaries fabricated by ECAP. The pole density is reduced by ECAP, during which the Brass and Goss type textures are introduced. TEM results show chain-like recrystallized grains formed at the grain boundaries and broken second-phase particles come into being due to the heavy shear force. After ECAP, the hardness and strength increase significantly while the elongation is reduced. Besides, an extreme strengthening is confirmed because of the balance between dynamic hardening and softening. The microstructure evolution mechanism is revealed in terms of grain refinement, precipitate phase breakage and texture evolution.

36 MATERIALS SCIENCE↗

Rapidly solidifying Pb-free Sn-Ag-Cu-Al or Sn-Cu-Al solder

A solder alloy includes Sn, optional Ag, Cu, and Al wherein the solder alloy composition together with the solder alloy superheat temperature and rapid cooling rate from the superheat temperature are controlled to provide a dispersion of fine hard Cu—Al intermetallic particles in an as-solidified solder alloy microstructure wherein the particles are retained even after multiple solder reflow cycles often used in modern electronic assembly procedures to provide a particle strengthening to the solder joint microstructure as well as exert a grain refining effect on the solder joint microstructure, providing a strong, impact- and thermal aging-resistant solder joint that has beneficial microstructural features and is substantially devoid of Ag3Sn blades.

36 MATERIALS SCIENCE↗

Microstructural evolution and phase stability in Nb-containing interstitial Fe-Mn-Co-Cr-C high-entropy alloys: An in-situ synchrotron X-ray diffraction study during laser melting

The influence of Nb on phase stability and microstructural evolution in an interstitial Fe-Mn-Co-Cr-C high-entropy alloy was investigated using in-situ synchrotron X-ray diffraction (SXRD) during laser melting. Scheil-Gulliver simulations predict the formation of σ and γ-f.c.c. phases in all three alloys, along with NbC in Nb-containing compositions. SXRD confirmed the presence of most predicted phases, but the σ phase was absent. Nb promotes crystallite refinement and increases dislocation density, though excessive additions reduce refinement efficiency due to solubility limits and secondary phase formation. Furthermore, Nb addition also enhances ε-h.c.p. phase formation by reducing stacking fault energy through NbC-induced carbon depletion. Analysis of intensity peak evolution reveals that Nb alters preferred grain orientations, reducing {111} γ intensity while enhancing {220} γ , leading to a more isotropic grain distribution. Overall, Nb plays a key role in phase selection, microstructure refinement, and preferred orientation evolution, allowing the tailored microstructure of high-entropy alloys via rapid solidification.

Interstitial high entropy alloys↗

On the Hot Deformation Behavior of a Ni-Free Austenitic Stainless Steel Interstitially Alloyed with Low Nitrogen Content

Hot deformation behavior of a Ni-free, Fe-17Cr-12Mn-0.28N-0.06C (wt.%) austenitic stainless steel, hereinafter coded as FeCrMnN, was investigated using hot compression tests conducted under different deformation conditions comprising temperature and strain rate ranges of 800-1200 °C and 0.01-10 s{sup −1}, respectively. While the hot deformation at high strain rate and low temperatures (e.g., 10 s{sup −1} and 800 or 900 °C) showed essentially dynamic recovery, resulting in a pancake-shaped microstructure, most of the other conditions exhibited occurrence of dynamic recrystallization (DRX). Increasing deformation temperature and decreasing strain rate showed a decrease in the critical stress and strain for initiating DRX. In general, DRX resulted in extensive microstructural reconstitution and grain refinement. For instance, hot deformation at 1000 °C/0.01 s{sup −1} resulted in a fully recrystallized fine-grained microstructure with an average grain size of about 15 μm in comparison with the initial grain size of 60 µm. Increasing the temperature enhanced grain growth, but an increase in strain rate resulted in a finer grain structure. The amount of delta ferrite in the present steel varied under different conditions of deformation such that the lowest amount of delta ferrite (about 4.5%) was observed at 1000 °C. The activation energy of deformation (Q{sub def}) for the present FeCrMnN steel with the initial grain size of 60 µm was estimated to be about 502 kJ/mol, which is higher than that of the conventional austenitic stainless steels.

36 MATERIALS SCIENCE↗

Effect of Y{sub 2}O{sub 3} Addition on the Microstructure, Wear Resistance, and Corrosion Behavior of W-4.9Ni-2.1Fe Heavy Alloy

Binding and particle phases are the two important parameters influencing materials properties. In this study, a series of novel W-4.9Ni-2.1Fe-xY{sub 2}O{sub 3} (in weight%) alloys with different Y{sub 2}O{sub 3} contents are prepared by secondary ball milling and spark plasma sintering (SPS) techniques to obtain uniformly distributed γ-(Ni, Fe) binding phases and finer grains. The microstructure, mechanical, wear resistance, and corrosion behavior of the sintered bodies with different Y{sub 2}O{sub 3} were obtained by x-ray diffraction, scanning electron microscopy, Rockwell hardness tester, friction wear tester, and three-dimensional profile instruments. The results showed that a certain addition of Y{sub 2}O{sub 3} led to refined grains and uniformed microstructures; but, if excessive, a weak grain refinement would be appeared. Moreover, the grain size tends to be stable with enhancing of the Y{sub 2}O{sub 3} content. Considering properties such as density, hardness, compression yield strength, grain size, and uniform distribution of tungsten hard phase and γ-(Ni, Fe) binding phase, the comprehensive optimal amount of 0.7 wt.% of Y{sub 2}O{sub 3} was attained for the alloy. Meanwhile, the SPS sintered body also exhibited the best friction, wear behavior, and corrosion resistance in 3.5% of NaCl solution.