At least 235 records · Page 13

Microstructure Stability During Creep of Friction Stir Welded AA2024-T3 Alloy

The poor weldability of the AA2024 aluminum alloy limits its use in industrial applications. Because friction stir welding (FSW) is a non-fusion welding process, it seems to be a promising solution for welding this alloy. In the current study, FSW was applied to butt weld AA2024-T3 aluminum alloy plates. Creep tests were conducted at 250 and at 315 °C on both the parent material and the friction stir welded specimens. The microstructures of the welded and non-welded AA2024-T3 specimens before and after the creep tests were studied and compared. A comprehensive transmission electron microscopy study together with a high-resolution scanning electron microscopy study and energy-dispersive x-ray spectroscopy analysis was conducted to investigate the microstructure stability. The parent material seems to contain two kinds of Cu-rich precipitates—coarse precipitates of a few microns each and uniformly dispersed fine nanosized precipitates. Unlike the parent material, the crept specimens were found to contain the two kinds of precipitates mentioned above together with platelet-like precipitates. In addition, extensive decoration of the grain boundaries with precipitates was clearly observed in the crept specimens. Controlled aging experiments for up to 280 h at the relevant temperatures were conducted on both the parent material and the welded specimens in order to isolate the contribution of exposure to high temperatures to the microstructure changes. TEM study showed the development of dislocation networks into a cellular dislocation structure in the case of the parent metal. Changes in the dislocation structure as a function of the creep strain and the FSW process were recorded. A detailed creep data analysis was conducted, taking into account the instability of the microstructure.

36 MATERIALS SCIENCE↗

Friction Stir Welding of Al-B{sub 4}C Composite Fabricated by Accumulative Roll Bonding: Evaluation of Microstructure and Mechanical Behavior

In this investigation, friction stir welding (FSW) of Al-B{sub 4}C composite fabricated by 10 cycles accumulative roll bonding was conducted. In order to investigate the influences of pin geometry on microstructure and mechanical properties, four different pin geometries (cylindrical, square, triangular and hexagonal) were selected. It was found that FSW parameters had a major effect on the fragmentation and distribution of reinforcement particles in stir zone. When the tool travel speed was increased, the distribution of B{sub 4}C particles was become gradually uniform in the aluminum matrix. The effect of tool rotational speed on the peak temperature was determined to be greater than the tool travel speed. The attained data of tensile properties and microhardness tests showed that the tool travel speed had bilateral effect on the tensile strength. The maximum tensile joint efficiency was obtained as 238% for FSWed of Al-2%B{sub 4}C composite to annealed base Al sheet.

36 MATERIALS SCIENCE↗

Improving Joint Formation and Tensile Properties of Dissimilar Friction Stir Welding of Aluminum and Magnesium Alloys by Solving the Pin Adhesion Problem

Friction stir welding (FSW), as a solid-state welding technology invented by TWI in 1991, has potential to join dissimilar Al/Mg alloys. In this study, the pin adhesion phenomenon affecting joint quality during FSW of 6061-T6 aluminum and AZ31B magnesium alloys was investigated. The adhesion phenomenon induced by higher heat input easily transformed the tapered-and-screwed pin into a tapered pin, which greatly reduced the tool’s ability to drive the plasticized materials and further deteriorated joint formation. Under the condition without the pin adhesion, the complex intercalated interlayer at the bottom of stir zone was beneficial to mechanical interlocking of Al/Mg alloys, improving tensile properties. However, the formation of intermetallic compounds was still the main reason of the joint fracture, significantly deteriorating tensile properties. Under the welding speed of 60 mm/min without the pin adhesion phenomenon, the maximum tensile strength of 107 MPa and elongation of 1.2% were achieved.

36 MATERIALS SCIENCE↗

Nugget Structure Evolution with Rotation Speed for High-Rotation-Speed Friction-Stir-Welded 6061 Aluminum Alloy

High-rotation-speed friction stir welding (HRS-FSW) is a promising technique to reduce the welding loads during FSW and thus facilitates the application of FSW for in situ fabrication and repair. In this study, 6061 aluminum alloy was friction stir welded at high-rotation speeds ranging from 3000 to 7000 rpm at a fixed welding speed of 50 mm/min, and the effects of rotation speed on the nugget zone macro- and microstructures were investigated in detail in order to illuminate the process features. Temperature measurements during HRS-FSW indicated that the peak temperature did not increase consistently with rotation speed; instead, it dropped remarkably at 5000 rpm because of the lowering of material shear stress. The nugget size first increased with rotation speed until 5000 rpm and then decreased due to the change of the dominant tool/workpiece contact condition from sticking to sliding. At the rotation speed of 5000 rpm, where the weld material experienced weaker thermal effect and higher-strain-rate plastic deformation, the nugget exhibited relatively small grain size, large textural intensity, and high dislocation density. Consequently, the joint showed superior nugget hardness and simultaneously a slightly low tensile ductility.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Rapidly Cooled Friction Stir Welded Ti-6Al-4V Alloys

Two mm-thick Ti-6Al-4V alloy plates were friction stir butt welded under natural- and rapid-cooling conditions. The microstructures and mechanical properties of joints were investigated and compared. The rapid cooling via spraying cooling liquid nitrogen on the plate top surface was beneficial to obtaining a narrower cross section and finer and more uniform grains in the stir zone than those obtained by natural cooling. Joint tensile strength of 1021 MPa and elongation of 1.88% under the rapid-cooling condition respectively reached 102.7 and 150.4% of those under the natural-cooling condition, respectively. The uniform-and-compact equiaxed grains led to equiaxed dimples on the fracture surface, which demonstrated a ductile fracture of the welding joints.

36 MATERIALS SCIENCE↗

Microstructure Evolution and Mechanical Properties of Keyhole Repair Welds in AA 2219-T851 Using Refill Friction Stir Spot Welding

The search for a suitable friction-based keyhole repair technique that fulfills the requirements for high-quality repair welds has become an important research topic, especially for aerospace applications. In order to provide and analyze an universal keyhole repair method for lightweight metals, refill friction stir spot welding is applied to through-hole repairs in 3- and 6-mm-thick sheets of precipitate hardening AA 2219-T851. Keyholes with a diameter of 7.5 mm were repair welded achieving a defect-free microstructure. The correlation between the microstructural evolution imposed by the repair process and the resulting mechanical properties is shown. A comprehensive analysis of the precipitate evolution in peak-aged AA 2219 during RFSSW is presented. Thermal cycle measurements revealed high heating rates and peak temperatures of up to 520 °C in the weld center. The thermal cycle caused mainly dissolution and minor equilibrium phase formation in the stirred zone. In the HAZ, overaging of the strengthening precipitates dominates with minor dissolution and equilibrium phase formation only in the direct proximity of the SZ. Microstructural analysis revealed typical weld zone formation with inhomogeneous grain size distribution in the SZ. The resulting mechanical properties are dominated by an inhomogeneous hardness distribution with lowest hardness in the TMAZ at 5 mm from the center of the weld. During tensile loading main yielding and the final fracture occur in the area of lowest strength. Tensile testing showed yield strength of 40 to 46% and UTS of 28 to 25% below BM values in 3- and 6-mm-thick sheets, respectively. The sheet thickness and post-weld natural aging were found to influence the mechanical properties of the weld significantly.

36 MATERIALS SCIENCE↗

Influence of Cu/Li Ratio on the Welding Forces and Mechanical Properties of Two Bobbin Tool Friction Stir Welded Al-Cu-Li Alloys

Increasing space activities produce a high number of space objects and lead to increasing collision risks which urges leading industries to look for future removal strategies. Material substitution in order to raise demisability during atmospheric reentry is a possible solution. Modern aluminum lithium alloys are under consideration to replace high-temperature melting materials like titanium. Further, friction stir welding was proposed as suitable joining technology in order to avoid high heat inputs during manufacturing. In this work, two modern Al-Li-Cu alloys, AA 2060 and AA 2196, in peak-aged temper were welded using the stationary shoulder variant of bobbin tool friction stir welding. Identical process parameters led to defect-free welds in both alloys. The macrostructural and microstructural features are shown and analyzed. The welds were mechanically tested to an efficiency of 78 and 70% of the base metal ultimate tensile strength for AA 2060 T8 and AA 2196 T8, respectively. The process forces as well as the thermal cycle experienced by the workpiece material were used to explain the mechanical performance. The difference in composition regarding the Cu/Li ratio of the alloys was taken into account when the mechanical properties were correlated with the thermally affected microstructure of the weldments.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded 316L Austenitic Stainless Steels

Fusion welding of austenitic stainless steels (ASSs) causes undesirable metallographic changes. An attempt has been made to join 3-mm-thick 316L ASS plates using friction stir welding and correlate the microstructural evolution and the mechanical properties under various welding conditions. Tungsten alloy (W-Re) tool was employed for welding. Successful joints were obtained within a range of traverse speeds (45-85 mm/min) used in this work. Various zones were observed across the joint line. The stir zone exhibited considerable grain refinement and traces of delta ferrite phase. EBSD images showed a decreasing grain size with increased traverse speed. XRD patterns and TEM images confirmed the existence of delta ferrite. The mechanical properties of the joints including microhardness, tensile strength, impact toughness and bending were further reported.

36 MATERIALS SCIENCE↗

Statistical Strength Analysis of Dissimilar AA2024-T6 and AA6061-T6 Friction Stir Welded Joints

Friction stir welding has been emerged as one of the most reliable processes for joining aerospace-grade aluminum alloys. However, limited studies have been focused so far on the reliability of these joint types. In this study, the effect of welding parameters (traverse and rotation speeds) on the fracture strength of dissimilar AA2024-T6 and AA6061-T6 friction stir welded joints was statistically analyzed by the Weibull approach. Based on the results, the Weibull approach was found to be much more accurate than widely used standard deviation for evaluating the scatter of the fracture strength data. The improper selection of the process parameters not only decreased the average fracture strengths of the joints, but also scattered them around the mean value, and increased the failure probability under the same applied tension. According to the microscopic and macroscopic examinations and microhardness measurements, although the microstructural inhomogeneities caused by the improper setting of the welding parameters negatively affected the joints hardness and fracture strength, the welding defects were likely to be the most responsible factor affecting the fracture strength and its reliability.

36 MATERIALS SCIENCE↗

Fabrication and Characterization of A5083-WC-Al{sub 2}O{sub 3} Surface Composite by Friction Stir Processing

In this study, WC-Al{sub 2}O{sub 3} ceramic composite was incorporated into Al5083 to produce a surface composite by friction stir processing (FSP), and the microstructure, hardness and wear properties of Al5083-WC-Al{sub 2}O{sub 3} surface composite were evaluated. Optical microscopy of FSPed samples showed grain refinement in the stir zone. The addition of WC-Al{sub 2}O{sub 3} particles as well as increase in FSP pass number had a considerable effect on grain refinement, and the grain size of Al5083 base metal of 36 µm reduced to 11 µm for Al5083-WC-Al{sub 2}O{sub 3} surface composite after four passes. The SEM observation of the surface composite revealed that the WC-Al{sub 2}O{sub 3} particles distributed homogenously in the matrix and by increasing the FSP passes, the initial agglomerates of mechanochemically synthesized WC-Al{sub 2}O{sub 3} powders could be fractured. Microhardness evaluation showed a substantial improvement by adding WC-Al{sub 2}O{sub 3} particles and increase in FSP pass number. The maximum microhardness value of 101 HV belonged to surface composite after four passes, while the microhardness of the base metal was 65 HV. Wear test results revealed enhanced tribological behavior with a similar trend of microhardness values. Scanning electron microscopy tests revealed both adhesive and abrasive wear mechanisms on the surface of the wear test specimens.

36 MATERIALS SCIENCE↗

Cooling Environment Effect on the Microstructure and Mechanical Properties of Friction Stir-Welded Joints

The heat input in friction stir welding (FSW) influences the localized properties in welded joint. The external cooling during FSW reduces the localized heating and post-weld cooling time by extracting heat comparatively at a faster rate. In the present study, we have investigated the effect of different cooling environments on the performance of friction stir-welded (FSWed) AA5052 strain-hardenable aluminum alloy. Welding was performed under three different cooling environments such as natural air, water and liquid nitrogen in order to understand their effects on grain structure, metallurgical changes and mechanical properties of the joints. It has been noted that the width of weld nugget zone, thermo-mechanically affected zone and heat-affected zone has been decreased with the respective change in cooling environments. Welding speed could also influence the width of different zones in weldment alike the cooling environments. Finer grain size has been noticed with water cooling against the liquid nitrogen cooling. Comparatively, water was observed to be more favorable cooling environment against liquid nitrogen because of its better weld quality (97%) compared with base metal. The favorable mechanical properties resulting from the different weldment regions for different cooling environments have been elaborated in the present study.

36 MATERIALS SCIENCE↗

Microstructure Evolution of Ultra-Fine-Grained AZ31 B Magnesium Alloy Produced by Submerged Friction Stir Processing

Ten-millimeter-thick strain-hardened AZ31B-H24 magnesium sheets were subjected to friction stir processing (FSP) in air and submerged friction stir processing (SFSP) under water to investigate their microstructures and microhardness properties. Different rotational speeds of 500, 630, 800, and 1000 rpm and traverse speeds of 50, 100, 200, and 350 mm/min were employed for processing the materials. For SFSPed samples, the rotational speed of 500 rpm and 200 mm/min of traverse speed resulted in an ultra-fine-grained structure with a minimum grain size of about 400-500 nm, which is half compared to that of FSPed. It was found that both processes led to variation of crystallographic orientation, and enhancing the rotational speed and lowering the traverse speed promoted the development of a {0002} basal texture. The microhardness of SFSPed material increased significantly up to 110% (~ 95 Hv), while the microhardness was 45% (~ 65 Hv) higher than the base metal (~ 45 Hv) for FSPed material.

36 MATERIALS SCIENCE↗

Effect of Rotational Speed on Microstructure and Mechanical Properties in Submerged Friction Stir Welding of ME20M Magnesium Alloy

Submerged friction stir welding of magnesium alloys has not been well investigated to date. ME20M is an important lightweight magnesium (Mg) alloy with enhanced yield strength and heat resistance that merits further research. In this paper, submerged friction stir welding of the ME20M Mg alloy was carried out using different parameters for the underwater cooling. Defect-free weld joints were produced, and the macrostructure, microstructure, tensile properties, and hardness were investigated. The results show that by increasing the rotational speed, the grain size of the weld nugget increased, the tensile strength of the joint decreased, and the microhardness of the different weld zones decreased. The finest obtained grain size was about 3.5 µm in the weld nugget at a rotational speed of 1100 rpm. The highest tensile strength achieved was 183.2 MPa, which was ~ 76.32% of the base metal. The highest and lowest hardness values of the weld joint were obtained at rotational speeds of 1100 and 1600 rpm, respectively, in the weld nugget and heat-affected zones.

36 MATERIALS SCIENCE↗

Effect of Welding Parameters on Junction Structure and Fracture Behavior of Friction-Stir-Welded Joints of 2024 Aluminum Alloys

In this paper, the effect of welding speed and tool rotation speed on the junction structure and fracture behavior of friction-stir-welded joints was investigated with use of 2024 aluminum alloys of 3.2 mm thick. Results show that the formation of junction structure is more affected by tool rotation speed than by welding speed due to the differences of heat input levels. When welding speed is at 100 mm/min and tool rotation speed is in the range of 400-600 r/min, the joint junction structure causes complete bonding with no welding defects. While under improper welding parameters, the junction structure causes the precipitate aggregation on the bonding line and the partial bonding with the appearance of both tunnel defects and kissing bond defects. Meanwhile, the results of tensile tests show that the tensile fracture of all FSW joints occur at the weld center. The failure mode of joints with defects-free junction structure characterized by shear fracture is ductile. While the failure mode of joints with defects-existent junction structure characterized by layered fracture surface is brittle. Furthermore, that heterogeneous microstructure, precipitate aggregation and welding defects converge inside the junction structure is the main factor affecting the tensile properties and fracture behavior of the friction-stir-welded joint.

36 MATERIALS SCIENCE↗

Forced Cooling Friction Stir Welding of 2060-T8 Al-Li Alloy

Friction stir welding of 2060-T8 Al-Li alloy was experimentally investigated. Forced cooling process was realized by placing two copper pressure plates with a waterway on both sides of weld top surface. The relations between joint formation, microstructures and mechanical properties were mainly discussed. Compared with conventional joint by natural cooling, the welding joint with smaller flashes by forced cooling has the smaller well-distributed grains and higher microhardness in the stir zone (SZ). The tensile strength and elongation of forced cooling joint, respectively, reach 445.7 MPa and 6.7%, which are obviously higher than those of the conventional joint. The fracture locations of the conventional and forced cooling joints are located in the SZ, and the fracture surface morphologies show a typical ductile fracture mode.

36 MATERIALS SCIENCE↗

Effect of Tool Offset and Rotational Speed in Dissimilar Friction Stir Welding of AISI 304 Stainless Steel and Mild Steel

In the present study, dissimilar friction stir welding was carried out between stainless steel (UNS S30400) and mild steel (UNS G10080) plates of 4 mm thickness using a tungsten carbide tool. The influence of tool rotational speeds (600, 875 rpm) and tool offsets (0.6, 1.2 mm) on mechanical properties, i.e., hardness, tensile strength, and impact toughness of welded joints was investigated. Maximum tensile strength of the joint was about 107.6% of the mild steel under rotational speed of 875 rpm and tool offset of 1.2 mm. The maximum hardness reached in the stir zone was about 281 HV{sub 0.5} due to the phase transformations and grain refinement. Charpy’s notch toughness of the welded joints was observed lower than the base materials. The microstructural characterizations were carried by using an optical microscope, and FESEM–EDS analysis which revealed the complex material mixing and material movement during the welding. Tungsten-rich bands were observed in the weld micrograph especially toward the advancing side. During this study, various wear mechanisms like oxidation wear, abrasive wear, and adhesion wear were responsible for the degradation of tungsten carbide tool.

36 MATERIALS SCIENCE↗

Neutron Diffraction Residual Stress Study of a AA2219-T87 Self-Reacting Friction Stir Weld

2219-T87 is a precipitation hardenable aluminum-copper alloy which sees wide use in structural aerospace components. Thick panels of this alloy are joined via self-reacting friction welding (SRFSW); however, this thermomechanical process can result in significant loss of the alloy’s strengthening precipitates and large residual stresses which are detrimental to mechanical behavior and performance. High-resolution maps of the residual strain and stress states along the normal, transverse, and longitudinal directions of 2219-T87 SRFSW were obtained using neutron diffraction measurements. Residual stress had the highest tensile value in the heat-affected zone (HAZ) and the largest compressive stress in the base metal region of the normal and transverse directions. Line profile residual stress distributions displayed an “M”-shaped distribution in each direction with the longitudinal direction being the most pronounced while 2D residual stresses displayed an hourglass-shaped pattern. Further, average maximal longitudinal residual stress values ranged from 60.6 to 85.6% of yield. Microhardness testing across the transverse weld section produced a “V”-shaped curve with slight hardness recovery in the stir zone. Maximal and minimal microhardness values were observed in the base metal (154 HV) and thermomechanically affected zone (82 HV), respectively. Microstructural evolution was recorded using optical microscopy and showed decreasing grain size from the HAZ to the stir zone.

36 MATERIALS SCIENCE↗

Microstructure, texture, and residual stress in a friction stir processed AZ31B magnesium alloy

Spatial variations of microstructure, hardness, chemical composition, tensile behavior, texture and residual stresses were investigated in a friction-stir-processed (FSP) AZ31B magnesium alloy. The residual stresses were measured using two different methods: neutron diffraction and the contour method. No significant variations in the hardness and chemical compositions were found in the FSP zones, including the severely deformed stir zone (SZ), which showed a finer grain size compared to the heat-affected zone and base material. On the other hand, significant changes in the tensile yield strength, texture, and residual stresses were observed in the FSP zones. The relationship between the texture variations and yield strength reduction; and its influence on the decrease in the residual stress near the SZ is discussed. Finally, the residual stresses measured by neutron diffraction and the contour method are compared and the effect of the texture on neutron diffraction residual stress measurements is discussed.

36 MATERIALS SCIENCE↗