Search NASA⌕ Search

SEARCH · Search NASA

Results for “STRESS MEASUREMENT, X-RAY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

227 records · Page 13

The ultrahigh pressure stability of silver: An experimental and theoretical study

We measured the atomic volume of Ag in a toroidal diamond anvil cell to a maximum pressure of 416 GPa and calculated the atomic volume and elastic constants of Ag up to 750 and 460 GPa, respectively. Our density functional theory calculations at 0 K utilize an all-electron fully relativistic method and agree well with our volume measurements, particularly at pressures above ~75 GPa. In this work, we corrected our experimental results for non-hydrostaticity using a line shift analysis, and the resulting Vinet equation of state (EOS) parameters are reported. We find that the uniaxial stress sustained by Ag increases linearly up to 4.5 GPa at a pressure of 416 GPa. Our experimental results indicate that the fcc structure of Ag remains stable to at least 416 GPa at room temperature. Our theoretical results show that C44 increases as pressure increases and reaches a maximum at ~100 GPa above which it begins to decrease, a sign that the fcc structure of Ag is becoming unstable, and at V/V 0 = 0.30, the bcc structure is lower in energy than fcc.

36 MATERIALS SCIENCE↗

Applied in-plane strain effects on the polarization response of ferroelectric hafnium zirconium oxide thin films

The influence of biaxial stress on the maximum and remanent polarizations of 10 nm thick hafnium zirconium oxide thin films in metal–ferroelectric–metal capacitor structures has been quantified. In the as-prepared state with a nominal biaxial tensile strain of 0.20% and no applied extrinsic stress, remanent and maximum polarizations of 7.6 and 13.1 μC/cm 2 , respectively, were measured using a 2 MV/cm applied electric field. Reducing the intrinsic strain by 0.111% through the application of a compressive uniaxial stress results in a decrease in the remanent and maximum polarizations to 6.8 and 12.2 μC/cm 2 , respectively. Here, the polarization dependence on strain is nearly linear between these values. The observed variation in polarization with strain is consistent with strain impacting ferroelastic switching whereby in-plane tension increases the fraction of the short polar axis orienting out-of-plane, hence increasing out-of-plane polarization. In contrast, reducing the in-plane strain through compression results in an increase in the fraction of the long non-polar axis orienting out-of-plane, thereby decreasing out-of-plane polarization.

36 MATERIALS SCIENCE↗

Multiscale operando X-ray investigations provide insights into electro-chemo-mechanical behavior of lithium intercalation cathodes

The electrochemical performance and cycle life of lithium-ion batteries (LIBs) depend on the electrochemical, chemical, and mechanical behavior of electrodes and electrolytes. Despite extensive studies conducted previously, challenges exist to decouple these behaviors, capture the evolution of electro-chemo-mechanical behavior in realistic conditions, and correlate atomic-scale stress evolution to micro-scale bulk mechanical degradation. Here, we report multiscale operando techniques to investigate polydisperse battery electrodes by integrating volume-averaged quantitative synchrotron X-ray scattering with high-resolution transmission X-ray microscopy (TXM). The former provides us information spanning a wide spatial range, from Angstrom-level atomic structures to micrometer-level particle scales, while the latter provides time-resolved 2D images of the particles during cycling. The complementarity of the two operando techniques is demonstrated by an over-lithiation test of LiCoO 2 electrodes, where particles crack and eventually pulverize. Additionally, the techniques are applied to study LiCoO 2 cycling stability from 3.0 V to 4.5 V. Operando X-ray scattering result shows nanometer-scale features keep forming in LiCoO 2 electrodes during cycling, resulting in an increased projected area observed by the TXM experiment. The formation of such features is inhibited by a polymer coating on the electrode, leading to vastly improved cycling stability. The polymer coating alleviates LiCoO 2 surface deterioration, reduces side product generation, and inhibits LiCoO 2 particles volume expansion during the cycling test. These operando multimodal X-ray techniques presented herein thus offer a novel, multiscale diagnostic modality for studying existing and emerging battery materials, aiding the development of next-generation LIBs.

25 ENERGY STORAGE↗

Effect of thermal aging on microstructure and crack growth response of Alloy 152 weld

Nickel-based Alloy 690 and the associated weld Alloys 52 and 152 are typically used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels, because of their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate for 40-80 years. Likewise, advanced water-cooled small modular reactors (SMRs) will use Ni-Cr alloys and are expected to receive initial operating licenses for 60 years. Hence, the thermal stability of Ni-Cr alloys is a potential concern for the long-term performance of both existing and advanced nuclear power plants, and possibly spent fuel storage containers. The objective of this research is to understand the microstructural changes occurring in high-Cr, Ni-based Alloy 152 weldments during long time exposure to the reactor operating temperatures, and the effect of these changes on the service performance. One area of particular concern is the potential for long range ordering (LRO), i.e. formation of the intermetallic Ni2Cr phase under prolonged exposure to reactor temperatures and/or irradiation, which can increase strength, decrease ductility, and cause dimensional changes or lead to in-service embrittlement of components made with these alloys. Hence, this research focused on the microstructural evolution and the SCC response of Alloy 152 under accelerated thermal aging. The materials studied involved three heats of Alloy 152 used to produce a dissimilar metal weld (DMW) joining an Alloy 690 plate to an Alloy 533 low alloy steel (LAS) plate, thermally aged at three different temperatures (370°C, 400°C and 450°C) for up to 75,000h (equivalent to 60 years of service). The microstructural characterization by means of synchrotron X-ray did not find evidence of LRO in any of the three heats aged to an equivalent of 60 years of service. Testing in a primary water environment of a heat of Alloy 152 aged at 370°C to a 60-year service equivalent revealed a fatigue and corrosion fatigue crack growth responses similar to those measured on the un-aged alloy. However, the SCC CGR response of the aged sample appears to show a deterioration in performance.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Strain-induced topological transitions in epitaxial films of cadmium arsenide

Strain in epitaxial thin films can have a profound influence on their electronic bands. Here, we investigate the influence of epitaxial strains on the electronic states of (001)-oriented cadmium arsenide (Cd 3 As 2 ) thin films, which are two-dimensional topological insulators. Cd 3 As 2 films were grown coherently on Al 1−x In x Sb buffer layers with varying degrees of lattice mismatch to Cd 3 As 2 , producing in-plane stresses that ranged from compressive to tensile. Using magneto-transport measurements of the Landau levels of the lowest subbands, we show that films under compression remain in the two-dimensional topological insulator state, while a sufficiently large tensile stress induces a transition to a topologically trivial phase. These results qualitatively agree with expectations from theoretical models for these films. At the topological transition, the gap avoids completely closing, and we discuss possible origins.

36 MATERIALS SCIENCE↗

Development of a Comprehensive Two-Phase Flow Database for the Validation of NEK-2P

Three-dimensional (3-D) two-phase Computational Fluid Dynamics (CFD) codes are emerging as a powerful and potentially practical tool for applications in which detailed local flow information is needed. However, two-phase flow models and associated closure relations are not well established for CFD applications, which is partly due to the lack of high-quality validation data. The main objective of this work is to develop a comprehensive database of two-phase flows that can be used to validate two-phase CFD codes such as NEK-2P. In this project, four advanced local measurement systems, including Particle Image Velocimetry and Planar Laser-Induced Fluorescence (PIV-PLIF), high-speed imaging, x-ray densitometry, and multi-sensor conductivity probe are employed to measure the local two-phase flow parameters of both gas and liquid phases. By combining these techniques, the local void fraction, bubble velocity, interfacial area concentration, bubble frequency, liquid velocity, turbulence intensity, etc., in various two-phase flow regimes can be obtained. These local measurement techniques are first used in a 25.4 mm circular pipe test section. Seven air-water two-phase flow conditions spanning the bubbly, slug, churn-turbulent, and annular flow regimes are measured in this facility. The obtained database contains the radial profiles of both gas- and liquid-phase parameters at three axial locations along the test section. The second facility used in this work contains a 30 mm × 10 mm rectangular test section, in which three two-phase flow and two single-phase flow conditions are measured. Two-dimensional distributions of local two-phase flow parameters in the cross-sectional plane are measured in this facility at three axial locations as well. A facility featuring a 3×3 electrically heated rod bundle is also designed and being constructed in this project. This facility is specially designed for optical measurements and is expected to provide high-quality boiling data in the future. Preliminary analyses have been performed for the data taken in the 25.4 mm circular pipe. Both center-peaked and wall-peaked void fraction profiles have been observed in the data depending on the two-phase flow conditions and/or developing lengths. The 1-D drift-flux model was evaluated with the newly obtained datasets, in which both gas- and liquid-phases data were directly measured. The distribution parameter model has been optimized based on a new void-profile classification method proposed in this study. The optimized drift-flux model shows a significant improvement in predicting both gas velocity and void fraction. The measured liquid-phase turbulence was used to benchmark Sato’s turbulence model considering the bubble-induced shear stress for the three tested bubbly flows. The benchmark results showed good agreement between the PIV measurements and model predictions. In the bubbly flows tested that have low void fractions less than 3%, the effect of the bubble-induced turbulence was found not significant. However, the bubble-induced shear stress becomes important with the increase of the void fraction. The Conjugate Heat Transfer (CHT) model was developed and implemented in NEK-2P. This model allows the coupled simulation of the solid domain and two-phase fluid domain, allowing the specification of realistic boundary conditions. The CHT implementation was verified first with non-boiling simulations. The predicted temperatures in the fluid domain were shown to be identical in simulations with or without the CHT model. The CHT model was then validated through simulations of three Becker benchmark CHF tests performed under both Dryout (DO) and Departure from Nucleate Boiling (DNB) conditions. Reasonably good agreement was obtained between calculated wall temperatures and corresponding experimental data.

42 ENGINEERING↗

Effect of thermal aging on microstructure and stress corrosion cracking behavior of Alloy 152 weldment

Nickel-based Alloy 690 and the associated weld Alloys 52 and 152 are typically used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels, because of their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate for 40-80 years. Likewise, water-cooled small modular reactors (SMRs) will use Ni-Cr alloys and are expected to receive initial operating licenses for 60 years. Hence, the thermal stability of Ni-Cr alloys is a potential concern for the long-term performance of both existing and advanced nuclear power plants, and possibly spent fuel storage containers. The objective of this research is to understand the microstructural changes occurring in high-Cr, Ni-based Alloy 152 weldments during long time exposure to the reactor operating temperatures, and the effect of these changes on the service performance. One area of particular concern is the potential for long range ordering (LRO), i.e. formation of the intermetallic Ni2Cr phase under prolonged exposure to reactor temperatures and/or irradiation, which can increase strength, decrease ductility, and cause dimensional changes or lead to in-service embrittlement of components made with these alloys. Hence, this research focused on the microstructural evolution and the SCC response of Alloy 152 under accelerated thermal aging. The materials studied involved three heats of Alloy 152 used to produce a dissimilar metal weld (DMW) joining an Alloy 690 plate to an Alloy 533 low alloy steel (LAS) plate, thermally aged at three different temperatures (370°C, 400°C and 450°C) for up to 75,000h (equivalent to 60 years of service). The microstructural characterization by means of synchrotron X-ray conducted in small, 0.2 mm - step line scans in the high-deformation regions of the weld root – covering areas spanning from the weld heat affected zone (HAZ) in Alloy 690 to the weld and weld butter on LAS - did not show evidence of LRO in any of the three Alloy 152 heats aged to an equivalent of 60 years of service. Testing in a primary water environment of two heats of Alloy 152 aged at 370°C to a 60-year service equivalent revealed a fatigue and corrosion fatigue crack growth responses similar to those measured on the un-aged alloys. However, the SCC CGR response of the aged samples appears to show a deterioration in performance, confirming our previous observation.

36 MATERIALS SCIENCE↗

Molecular Origin of Strain-Induced Chain Alignment in PDPP-Based Semiconducting Polymeric Thin Films

Donor–acceptor (D–A) type semiconducting polymers have shown great potential for the application of deformable and stretchable electronics in recent decades. However, due to their heterogeneous structure with rigid backbones and long solubilizing side chains, the fundamental understanding of their molecular picture upon mechanical deformation still lacks investigation. Here, the molecular orientation of diketopyrrolopyrrole (DPP)-based D–A polymer thin films is probed under tensile deformation via both experimental measurements and molecular modeling. The detailed morphological analysis demonstrates highly aligned polymer crystallites upon deformation, while the degree of backbone alignment is limited within the crystalline domain. Besides, the aromatic ring on polymer backbones rotates parallel to the strain direction despite the relatively low overall chain anisotropy. Additionally, the effect of side-chain length on the DPP chain alignment is observed to be less noticeable. These observations are distinct from traditional linear-chain semicrystalline polymers like polyethylene due to distinct characteristics of backbone/side-chain combination and the crystallographic characteristics in DPP polymers. Furthermore, a stable and isotropic charge carrier mobility is obtained from fabricated organic field-effect transistors. This study deconvolutes the alignment of different components within the thin-film microstructure and highlights that crystallite rotation and chain slippage are the primary deformation mechanisms for semiconducting polymers.

36 MATERIALS SCIENCE↗

Effect of Thermal Aging on Microstructure and Stress Corrosion Cracking Behavior of an Alloy 152 1st Layer Butter Weldment

Nickel-based Alloy 690 and the associated weld Alloys 52 and 152 are typically used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels, because of their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate for 40- 80 years. Likewise, water-cooled small modular reactors (SMRs) will use Ni-Cr alloys and are expected to receive initial operating licenses for 60 years. Hence, the thermal stability of Ni-Cr alloys is critical for the long-term performance of both existing and advanced nuclear power plants, and possibly spent fuel storage containers. The objective of this research is to understand the microstructural changes occurring in high-Cr, Ni-based Alloy 152 weldments during long time exposure to the reactor operating temperatures, and the effect of these changes on the service performance. One area of particular concern is the potential for long range ordering (LRO), i.e. formation of the intermetallic Ni2Cr phase under prolonged exposure to reactor temperatures and/or irradiation, which can increase strength, decrease ductility, and cause dimensional changes or lead to in-service embrittlement of components made with these alloys. Hence, this research focused on the microstructural evolution and the SCC response of Alloy 152 under accelerated thermal aging. The materials studied involved three heats of Alloy 152 used to produce a dissimilar metal weld (DMW) joining an Alloy 690 plate to an Alloy 533 low alloy steel (LAS) plate, thermally aged at three different temperatures (370°C, 400°C and 450°C) for different durations up to 75,000h (equivalent to 60 years of reactor service). The microstructural characterization by means of synchrotron X-ray conducted in small, 0.2 mm - step line scans in the high-deformation regions of the weld root – covering areas spanning from the weld heat affected zone (HAZ) in Alloy 690 to the weld and weld butter on LAS - did not show evidence of LRO in any of the three Alloy 152 heats aged at 370°C and 450°C to an equivalent of 60 years of service. However, the first weld butter layer has high levels of deformation and is highly susceptible to SCC even in its non-aged condition. Nanohardness testing confirmed the extreme hardening with aging (ΔHV ≅ 100) at two locations within this weldment. In absence of LRO, hardening is suspected to be due to thermally-induced Cr carbide precipitation and coarsening. Testing in a primary water environment of the 1st layer of Alloy 152 weld butter aged at 370°C to a 60-year service equivalent revealed a fatigue and corrosion fatigue crack growth responses similar to those measured on the un-aged alloys. Similarly, the SCC CGR response of the aged weld butter does not appear to show a deterioration in performance, however, the difficult-to-test weldment geometry may affect the test results.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Optimizing ablator thickness for laser shock experiments

In laser shock experiments, a well-defined, flat-top shock wave at the ablator/sample interface is important for accurately probing material response under uniaxial strain compression. However, the relationship between the ablator thickness and the resulting shock wave characteristics is insufficiently understood, limiting the ability to design optimal experiments. To address this need, we conducted a systematic experimental study using a 100 J laser to shock-compress polyimide ablators to peak stresses ranging from 20.4 to 111.6 GPa. Laser interferometry diagnostics measured the transmitted wave profiles at the ablator/sample interface, consistently showing a single jump followed by a constant peak state before the arrival of release waves. Here, by analyzing shock transit time, flat-top duration, and stress, our results establish a framework for selecting ablator thickness to maximize the flat-top duration, improving the precision and reproducibility of laser shock experiments.

design of experiments↗