Search NASA⌕ Search

SEARCH · Search NASA

Results for “SiC Ceramic Fiber”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Constituent-Based Life Models Being Developed for SiC/SiC Composites

For the successful utilization of ceramic matrix composites (CMC) as hot-section components in advanced aeropropulsion engines, the CMC constituents will need to be tailored and optimized to meet all the critical property demands of each component. Under the High-Speed Research (HSR) and Advanced High-Temperature Engine Materials Technology (HITEMP) Programs, the NASA Glenn Research Center at Lewis Field initiated research to develop mechanistic models for key CMC thermostructural properties. These models would describe the effects of different constituent factors (composition, geometry, and volume fraction) and of potential application conditions (stress, time, temperature, and environment) on these properties. Particular focus was placed on both analytical and numerical modeling of state-of-the-art SiC/SiC composites where the primary load-bearing constituents are stoichiometric SiC fibers in a complex multiphase SiC matrix produced by chemical vapor infiltration and melt infiltration. Recent studies have resulted in computer-based numerical models for the elastic modulus, thermal expansion, and thermal conductivity properties of the SiC/SiC system. Additional studies have generated analytical and empirical models for the time dependence of composite rupture strength at temperatures above 2200 F (1200 C), where CMC's have an important thermostructural advantage over current nickel-based superalloys. These life models utilize thermal activation theory and fiber stress-rupture results measured at Glenn to generate Larson-Miller (L M) plots of fiber rupture strength versus q, a single time- and temperature-dependent parameter. Assuming a worse case in which the SiC matrix is cracked, rupture is then controlled by the time-dependent fracture characteristics of the fiber bundles bridging the matrix cracks. With this as the controlling mechanism, one can then use simple composite theory and the fiber L M plots to predict CMC rupture strength versus the q parameter. The dashed line shows the predicted rupture strength of a SiC/SiC composite that is reinforced by a state-of-the-art stoichiometric SiC fiber. For the q parameter, time is in hours and temperature in degrees kelvin. To generate these predictions, a two-dimensional 0 /90 composite with approximately 16 percent fiber in the applied stress direction and an air test environment were assumed. As such, it is possible to compare the model predictions against limited stress-rupture data for this CMC as shown by the data points. The good agreement confirms the rupture model at least for the selected CMC and test conditions. Thus for this particular SiC/SiC composite, one can estimate a 1000-hr rupture strength of approximately 12 ksi at 2400 F (T = 1588 K and q = 39 700 K). At lower CMC application stresses, the SiC matrix is typically uncracked, so both the fiber and matrix constituents share the composite load. In this case, CMC rupture is controlled by the constituent with the longest rupture time based on the creep rate of the composite. Measured Monkman-Grant plots of rupture time versus creep rate for the two SiC constituents have been used to develop CMC life models for this important application condition. NASA and DOD are currently using this information to establish application and material goals for more advanced CMC's that can be used at even higher temperatures.

DiCarlo, James A.↗

Joining and Attachment Technologies for Ceramic Matrix Composites: Current Status and Future Prospects

Fiber reinforced ceramic composites are either currently being used, or are under active consideration for use in a wide variety of high temperature applications. The engineering designs require fabrication and manufacturing of complex shaped parts. In many instances, it is more economical to build up complex shapes by joining simple geometrical shapes. Thus, joining and attachment have been recognized as enabling technologies for successful utilization of ceramic components in various aerospace and ground based applications. In this presentation, various challenges and opportunities in design, fabrication, and testing of high temperature joints in composites will be presented. Various joint design philosophies and design issues in joining of composites will be discussed along with an affordable, robust ceramic joining technology (ARCJoinT). A wide variety of ceramic composites (C/C, C/SiC, and SiC), in different shapes and sizes, have been joined using this technology. Microstructure and mechanical properties of joints will be reported. Current status of various ceramic joining technologies and future prospects for their applications will also be discussed.

Singh, M.↗

Brazing SiC/SiC Composites to Metals

Experiments have shown that active brazing alloys (ABAs) can be used to join SiC/SiC composite materials to metals, with bond strengths sufficient for some structural applications. The SiC/SiC composite coupons used in the experiments were made from polymerbased SiC fiber preforms that were chemical-vapor-infiltrated with SiC to form SiC matrices. Some of the metal coupons used in the experiments were made from 304 stainless steel; others were made from oxygen-free, high-conductivity copper. Three ABAs were chosen for the experiments: two were chosen randomly from among a number of ABAs that were on hand at the time; the third ABA was chosen because its titanium content (1.25 percent) is less than those of the other two ABAs (1.75 and 4.5 percent, respectively) and it was desired to evaluate the effect of reducing the titanium content, as described below. The characteristics of ABAs that are considered to be beneficial for the purpose of joining SiC/SiC to metal include wettability, reactivity, and adhesion to SiC-based ceramics. Prior to further development, it was verified that the three chosen ABAs have these characteristics. For each ABA, suitable vacuum brazing process conditions were established empirically by producing a series of (SiC/SiC)/ABA wetting samples. These samples were then sectioned and subjected to scanning electron microscopy (SEM) and energy-dispersive x-ray spectrometry (EDS) for analysis of their microstructures and compositions. Specimens for destructive mechanical tests were fabricated by brazing of lap joints between SiC/SiC coupons 1/8-in. (.3.2- mm) thick and, variously, stainless steel or copper tabs. The results of destructive mechanical tests and the SEM/EDS analysis were used to guide the development of a viable method of brazing the affected materials.

Steffier, Wayne S.↗

Influence of Constituents on Creep Properties of SiC/SiC Composites

SiC-SiC composites are being considered as potential candidate materials for next generation turbine components such as combustor liners, nozzle vanes and blades because of their low density, high temperature capability, and tailorable mechanical properties. These composites are essentially fabricated by infiltrating matrix into a stacked array of fibers or fiber preform by one or a combination of manufacturing methods such as, Melt Infiltration (MI) of molten silicon metal, Chemical Vapor Infiltration (CVI), Polymer Infiltration and Pyrolysis (PIP). To understand the influence of constituents, the SiC-SiC composites fabricated by MI, CVI, and PIP methods were creep tested in air between 12000 and 14500 degrees Centigrade for up to 500 hours. The failed specimens were analyzed under a scanning electron microscope to assess damage mechanisms. Also, knowing the creep deformation parameters of the fiber and the matrix under the testing conditions, the creep behavior of the composites was modeled and compared with the measured data. The implications of the results on the long term durability of these composites will be discussed.

modeling↗

Computational Modeling in Structural Materials Processing

High temperature materials such as silicon carbide, a variety of nitrides, and ceramic matrix composites find use in aerospace, automotive, machine tool industries and in high speed civil transport applications. Chemical vapor deposition (CVD) is widely used in processing such structural materials. Variations of CVD include deposition on substrates, coating of fibers, inside cavities and on complex objects, and infiltration within preforms called chemical vapor infiltration (CVI). Our current knowledge of the process mechanisms, ability to optimize processes, and scale-up for large scale manufacturing is limited. In this regard, computational modeling of the processes is valuable since a validated model can be used as a design tool. The effort is similar to traditional chemically reacting flow modeling with emphasis on multicomponent diffusion, thermal diffusion, large sets of homogeneous reactions, and surface chemistry. In the case of CVI, models for pore infiltration are needed. In the present talk, examples of SiC nitride, and Boron deposition from the author's past work will be used to illustrate the utility of computational process modeling.

Meyyappan, Meyya↗

High Temperature Mechanical Characterization of Ceramic Matrix Composites

A high temperature mechanical characterization laboratory has been assembled at NASA Lewis Research Center. One contribution of this work is to test ceramic matrix composite specimens in tension in environmental extremes. Two high temperature tensile testing systems were assembled. The systems were assembled based on the performance and experience of other laboratories and meeting projected service conditions for the materials in question. The systems use frames with an electric actuator and a center screw. A PC based data acquisition and analysis system is used to collect and analyze the data. Mechanical extensometers are used to measure specimen strain. Thermocouples, placed near the specimen, are used to measure the specimen gage section temperature. The system for testing in air has a resistance element furnace with molybdenum disilicide elements and pneumatic grips with water cooling attached to hydraulic alignment devices. The system for testing in an inert gas has a graphite resistance element furnace in a chamber with rigidly mounted, water cooled, hydraulically actuated grips. Unidirectional SiC fiber reinforced reaction bonded Si3N4 and triaxially woven, two dimensional, SiC fiber reinforced enhanced SiC composites were tested in unidirectional tension. Theories for predicting the Young's modulus, modulus near the ultimate strength, first matrix cracking stress, and ultimate strength were applied and evaluated for suitability in predicting the mechanical behavior of SiC/RBSN and enhanced SiC/SiC composites. The SiC/RBSN composite exhibited pseudo tough behavior (increased area under the stress/strain curve) from 22 C to 1500 C. The rule of mixtures provides a good estimate of the Young's modulus of the SiC/RBSN composite using the constituent properties from room temperature to 1440 C for short term static tensile tests in air or nitrogen. The rule of mixtures significantly overestimates the secondary modulus near the ultimate strength. The ACK theory provides the best approximation of the first matrix cracking stress when residual stresses are ignored. The theory of Cao and Thouless, based on Weibull statistics, gave the best prediction for the composite ultimate strength. The enhanced SiC/SiC composite exhibited nonlinear stress/strain behavior from 24 C to 1370 C in air with increased ultimate strain when compared to monolithic SiC. The theory of Yang and Chou with the assumption of a frictional fiber/matrix interface provided the best estimate of the Young's modulus. The theory of Cao and Thouless gave the best estimate for the ultimate strength.

Gyekenyesi, John Z.↗

Phase Equilibria and Thermochemistry of Advanced Fuels: Modeling Burnup Behavior (Final Report)

Achieving the goal of developing advanced fuel concepts that meet the DOE objectives of being robust, demonstrating high performance, and are more tolerant of accident conditions than current fuel systems will require a thorough understanding of the thermophysical and thermochemical properties of the constituent materials. Non-oxide fuel systems are being explored under the Advanced Fuels Program that hold significant promise for improved performance and accident tolerance, including the uranium silicide-based system considered in the current work. Prospective cladding materials currently considered that contribute to improved accident tolerance include silicon carbide composites and ferritic alloys (Fe-Cr-Al base compositions). Thus, the effort developed thermochemical models and values, supported with targeted experiments, to evaluate the ferritic alloy and silicon carbide composite cladding systems in contrast to current zirconium alloy cladding. The developed detailed understanding will serve to aid in relatively early screening of candidate systems to avoid wasted effort, guide development of new fuel forms, and to provide a basis for predicting and modeling fuel performance. Major deliverables for the project included: Thermochemical assessment and models of phases in the U-Si and U-Si-N systems; thermochemical evaluation supported by experimental measurements of fuel-cladding interactions of silicide fuel with baseline zirconium, ceramic composite, and ferritic alloy cladding; thermochemical assessment and models of phases supported by experimental measurements for silicide fuel with key fission products provided in a dataset and reported in refereed publications. Within the project a significantly refined U-Si phase diagram was developed and reported that now includes homogeneity ranges for key phases, such at the U 3 Si 2 proposed fuel phase, and settles issues with regard to uncertainty in the stability of some phases. Computational efforts together with key experiments has determined phase formation in interactions between U 3 Si 2 and Zircaloy-4 cladding material, a ferritic FeCrAlY alloy of interest as an advanced cladding material, and silicon carbide, also of interest as a fiber-reinforced composite cladding. As expected, very significant reactions occur between U3Si2 and Zircaloy-4, with much less interaction at higher temperatures for the ferritic alloy, and finally interactions with SiC only in the region of contact. A potentially major issue is the stability of U 3 Si 2 fuel that has undergone significant burnup. The result is the loss of the uranium metal, liberating silicon, and the formation of concomitant fission product elements that either dissolve in the U 3 Si 2 phase or form independent, and possibly silicide phases. A combination of experimental determinations of phase formation of U 3 Si 2 reacted with representative fission products yttrium, gadolinium, cerium, zirconium, and molybdenum and first principles calculations has helped understand the fuel chemistry. The behavior of the U 3 Si 2 phase and the partitioning of silicon to possible fission product phases with burnup was thus determined, with significant dissolution in U 3 Si 2 of cerium, gadolinium, zirconium, and plutonium predicted along with independent phase formation of a U-Mo-Si ternary phase, yttrium silicide, and elemental selenium. It can be concluded that at significant burnup there will be a very minor amount of the U 3 Si 2 fuel phase that will decompose to a lower silicide or a uranium alloy as silicon preferentially forms a secondary phase.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Statistical Analysis of CMC Constituent and Processing Data

Ceramic Matrix Composites (CMCs) are the next "big thing" in high-temperature structural materials. In the case of jet engines, it is widely believed that the metallic superalloys currently being utilized for hot structures (combustors, shrouds, turbine vanes and blades) are nearing their potential limits of improvement. In order to allow for increased turbine temperatures to increase engine efficiency, material scientists have begun looking toward advanced CMCs and SiC/SiC composites in particular. Ceramic composites provide greater strength-to-weight ratios at higher temperatures than metallic alloys, but at the same time require greater challenges in micro-structural optimization that in turn increases the cost of the material as well as increases the risk of variability in the material s thermo-structural behavior. to model various potential CMC engine materials and examines the current variability in these properties due to variability in component processing conditions and constituent materials; then, to see how processing and constituent variations effect key strength, stiffness, and thermal properties of the finished components. Basically, this means trying to model variations in the component s behavior by knowing what went into creating it. inter-phase and manufactured by chemical vapor infiltration (CVI) and melt infiltration (MI) were considered. Examinations of: (1) the percent constituents by volume, (2) the inter-phase thickness, (3) variations in the total porosity, and (4) variations in the chemical composition of the Sic fiber are carried out and modeled using various codes used here at NASA-Glenn (PCGina, NASALife, CEMCAN, etc...). The effects of these variations and the ranking of their respective influences on the various thermo-mechanical material properties are studied and compared to available test data. The properties of the materials as well as minor changes to geometry are then made to the computer model and the detrimental effects observed using statistical analysis software. The ultimate purpose of this study is to determine what variations in material processing can lead to the most critical changes in the materials property. The work I have taken part in this summer explores, in general, the key properties needed In this study SiC/SiC composites of varying architectures, utilizing a boron-nitride (BN)

Fornuff, Jonathan↗

Joining and Assembly of Silicon Carbide-based Advanced Ceramics and Composites for High Temperature Applications

Silicon carbide based advanced ceramics and fiber reinforced composites are under active consideration for use in wide variety of high temperature applications within the aeronautics, space transportation, energy, and nuclear industries. The engineering designs of ceramic and composite component require fabrication and manufacturing of large and complex shaped parts of various thicknesses. In many instances, it is more economical to build up complex shapes by joining simple geometrical shapes. In addition these components have to be joined or assembled with metallic sub-components. Thus, joining and attachment have been recognized as enabling technologies for successful utilization of ceramic components in various demanding applications. In this presentation, various challenges and opportunities in design, fabrication, and testing o high temperature joints in ceramic matrix composites will be presented. Silicon carbide based advanced ceramics (CVD and hot pressed), and C/SiC and SiC/SiC composites, in different shapes and sizes, have been joined using an affordable, robust ceramic joining technology (ARCJoinT). Microstructure and high temperature mechanical properties of joints in silicon carbide ceramics and CVI and melt infiltrated SiC matrix composites will,be reported. Various joint design philosophies and design issues in joining of ceramics and composites well be discussed.

Singh, M.↗

Effects of Control Mode and R-Ratio on the Fatigue Behavior of a Metal Matrix Composite

Composite Because of their high specific stiffness and strength at elevated temperatures, continuously reinforced metal matrix composites (MMC's) are under consideration for a future generation of aeropropulsion systems. Since components in aeropropulsion systems experience substantial cyclic thermal and mechanical loads, the fatigue behavior of MMC's is of great interest. Almost without exception, previous investigations of the fatigue behavior of MMC's have been conducted in a tension-tension, load-controlled mode. This has been due to the fact that available material is typically less than 2.5-mm thick and, therefore, unable to withstand high compressive loads without buckling. Since one possible use of MMC's is in aircraft skins, this type of testing mode may be appropriate. However, unlike aircraft skins, most engine components are thick. In addition, the transient thermal gradients experienced in an aircraft engine will impose tension-compression loading on engine components, requiring designers to understand how the MMC will behave under fully reversed loading conditions. The increased thickness of the MMC may also affect the fatigue life. Traditionally, low-cycle fatigue (LCF) tests on MMC's have been performed in load control. For monolithic alloys, low-cycle fatigue tests are more typically performed in strain control. Two reasons justify this choice: (1) the critical volume from which cracks initiate and grow is generally small and elastically constrained by the larger surrounding volume of material, and (2) load-controlled, low-cycle fatigue tests of monolithics invariably lead to unconstrained ratcheting and localized necking--an undesired material response because the failure mechanism is far more severe than, and unrelated to, the fatigue mechanism being studied. It is unknown if this is the proper approach to composite testing. However, there is a lack of strain-controlled data on which to base any decisions. Consequently, this study addresses the isothermal, LCF behavior of a [0]_32 MMC tested under strain- and load-controlled conditions for both zero-tension and tension-compression loading conditions. These tests were run at 427 C on thick specimens of SiC-reinforced Ti-15-3. For the fully-reversed tests, no difference was observed in the lives between the load- and strain-controlled tests. However, for the zero-tension tests, the strain-controlled tests had longer lives by a factor of 3 in comparison to the load-controlled tests. This was due to the fact that under strain-control the specimens cyclically softened, reducing the cracking potential. In contrast, the load-controlled tests ratcheted toward larger tensile strains leading to an eventual overload of the fibers. Fatigue tests revealed that specimens tested under fully-reversed conditions had lives approximately an order of magnitude longer than for those specimens tested under zero tension. When examined on a strain-range basis, the fully reversed specimens had similar, but still shorter lives than those of the unreinforced matrix material. However, the composite had a strain limitation at short lives because of the limited strain capacity of the brittle ceramic fiber. The composite also suffered at very high lives because of the lack of an apparent fatigue limit in comparison to the unreinforced matrix. The value of adding fibers to the matrix is apparent when the fatigue lives are plotted as a function of stress range. Here, the composite is far superior to the unreinforced matrix because of the additional load-carrying capacity of the fibers.

Source record↗

Ceramic Composite Intermediate Temperature Stress-Rupture Properties Improved Significantly

Silicon carbide (SiC) composites are considered to be potential materials for future aircraft engine parts such as combustor liners. It is envisioned that on the hot side (inner surface) of the combustor liner, composites will have to withstand temperatures in excess of 1200 C for thousands of hours in oxidizing environments. This is a severe condition; however, an equally severe, if not more detrimental, condition exists on the cold side (outer surface) of the combustor liner. Here, the temperatures are expected to be on the order of 800 to 1000 C under high tensile stress because of thermal gradients and attachment of the combustor liner to the engine frame (the hot side will be under compressive stress, a less severe stress-state for ceramics). Since these composites are not oxides, they oxidize. The worst form of oxidation for strength reduction occurs at these intermediate temperatures, where the boron nitride (BN) interphase oxidizes first, which causes the formation of a glass layer that strongly bonds the fibers to the matrix. When the fibers strongly bond to the matrix or to one another, the composite loses toughness and strength and becomes brittle. To increase the intermediate temperature stress-rupture properties, researchers must modify the BN interphase. With the support of the Ultra-Efficient Engine Technology (UEET) Program, significant improvements were made as state-of-the-art SiC/SiC composites were developed during the Enabling Propulsion Materials (EPM) program. Three approaches were found to improve the intermediate-temperature stress-rupture properties: fiber-spreading, high-temperature silicon- (Si) doped boron nitride (BN), and outside-debonding BN.

Morscher, Gregory N.↗

Creep/Rupture Behavior of Melt-Infiltrated SiC/SiC Composites Being Investigated

The failure behavior of melt-infiltrated SiC/SiC ceramic matrix composites is under investigation at the NASA Glenn Research Center as part of NASA's Ultra-Efficient Engine Technology Program. This material was originally developed under the High Speed Research Office's Enabling Propulsion Materials Program. Creep and rupture data provide accelerated testing information to predict material behavior under engine use situations (1500 to 2400 F). This information gives insights into various material development paths to improve composites as well as improve understanding of failure mechanisms. The left figure shows the fracture surface of a CMC material following over 200 hr of testing at 2400 F. This surface demonstrates the kind of fibrous pullout desirable for maximum crack deflection, hence non-brittle failure. Microscopy suggests that creep and rupture of these materials can best be considered as a probabilistic property, rather than a material property. Fiber failure occurs first in isolated regions, while stronger adjacent fibers remain intact. The right figure shows a region where oxide deposits blur and round the fiber images. Because the oxidation kinetics of SiC are well understood, this oxide scale can be used as a measure of the length of time various regions of the composites have been exposed to the environment, hence providing vital information regarding the sequence of failure. The oxide scale in the right figure indicates an early failure of this tow of fibers, whereas adjacent tows remain oxide free, suggesting failure much later in time. The path of various cracks can be followed throughout the composite in this manner, suggesting failure mechanisms.

Hurst, Janet B.↗

Development and Characterization of SiC)/ MoSi2-Si3N4(p) Hybrid Composites

Intermetallic compound MoSi2 has long been known as a high temperature material that has excellent oxidation resistance and electrical/thermal conductivity. Also its low cost, high melting point (2023 C), relatively low density (6.2 g/cu cm versus 9 g/cu cm for current engine materials), and ease of machining, make it an attractive structural material. However, the use of MoSi2 has been hindered due to its poor toughness at low temperatures, poor creep resistance at high temperatures, and accelerated oxidation (also known as 'pest' oxidation) at temperatures between approximately 450 and 550 C. Continuous fiber reinforcing is very effective means of improving both toughness and strength. Unfortunately, MoSi2 has a relatively high coefficient of thermal expansion (CTE) compared to potential reinforcing fibers such as SiC. The large CTE mismatch between the fiber and the matrix resulted in severe matrix cracking during thermal cycling. Addition of about 30 to 50 vol % of Si3N4 particulate to MoSi2 improved resistance to low temperature accelerated oxidation by forming a Si2ON2 protective scale and thereby eliminating catastrophic 'pest failure'. The Si3N4 addition also improved the high temperature creep strength by nearly five orders of magnitude, doubled the room temperature toughness and significantly lowered the CTE of the MoSi2 and eliminated matrix cracking in SCS-6 reinforced composites even after thermal cycling. The SCS-6 fiber reinforcement improved the room temperature fracture toughness by seven times and impact resistance by five times. The composite exhibited excellent strength and toughness improvement up to 1400 C. More recently, tape casting was adopted as the preferred processing of MoSi2-base composites for improved fiber spacing, ability to use small diameter fibers, and for lower cost. Good strength and toughness values were also obtained with fine diameter Hi-Nicalon tow fibers. This hybrid composite remains competitive with ceramic matrix composites as a replacement for Ni-base superalloys in aircraft engine applications.

Hebsur, Mohan G.↗

The high temperature creep behavior of oxides and oxide fibers

A thorough review of the literature was conducted on the high-temperature creep behavior of single and polycrystalline oxides which potentially could serve as fiber reinforcements in ceramics or metal matrix applications. Sapphire when oriented with the basal plane perpendicular to the fiber axis (c-axis oriented) is highly creep resistant at temperatures in excess of 1600 C and applied loads of 100 MPa and higher. Pyramidal slip is preferentially activated in sapphire under these conditions and steady-state creep rates in the range of 10(exp -7) to 10 (exp -8)/s were reported. Data on the creep resistance of polycrystalline beryllia suggest that C-axiz oriented single crystal beryllia may be a viable candidate as a fiber reinforcement material; however, the issure of fabricability and moisture sensitivity must be addressed for this material. Yttrium aluminum garnet (YAG) also appears to be a fiber candidate material having a high resistance to creep which is due to it's complex crystal structure and high Peierl resistance. The high creep resistance of garnet suggests that there may be other complex ternary oxides such as single crystal mullite which may also be candidate materials for fiber reinforcements. Finally, CVD and single crystal SiC, although not oxides, do possess a high resistance to creep in the temperature range between 1550 and 1850 C and under stresses of 110 to 220 MPa. From a review of the literature, it appears that for high creep resistant applications sapphire, silicon carbide, yttrium aluminum garnet, mullite, and beryllia are desirable candidate materials which require further investigation.

Jones, Linda E.↗

MoSi2-Base Hybrid Composite Passed Engine Test

The intermetallics compound molybdenum disilicide (MoSi2) is an attractive high-temperature structural material for advanced engine applications. It has excellent oxidation resistance, a high melting point, relatively low density, and high thermal conductivity, and it is easily machined. Past research'at the NASA Lewis Research Center has resulted in the development of a hybrid composite consisting of a MoSi2 matrix reinforced with silicon nitride (Si3N4) Particulate and silicon carbide (SiC) fibers. This composite has demonstrated attractive strength, toughness, thermal fatigue, and oxidation resistance, including resistance to "pest" oxidation. These properties attracted the interest of the Office of Naval Research and Pratt & Whitney, and a joint NASA/Navy/Pratt & Whitney effort was developed to continue to mature the MoSi2 Composite technology. A turbine blade outer air seal, which was part of the Integrated High Performance Turbine Engine Technology (IHPTET) program, was chosen as a first component on which to focus. The first tasks of the materials development effort were to develop improved processing methods to reduce costs and to use fine-diameter fibers that enable the manufacturing of complex shapes. Tape-casting methods were developed to fully infiltrate the fine SiC fibers with matrix powders. The resulting composites were hot pressed to 100-percent density. Composites with cross-plied fiber architectures with 30 vol. % hi-nicalon SiC fibers and 30 vol. % nitride particles are now made routinely and demonstrate a good balance of properties. The next task entailed the measurement of a wide variety of mechanical properties to confirm the suitability of this composite in engines. In particular, participants in this effort demonstrated that composites made with Hi-Nicalon fibers had strength and toughness properties equal to or better than those of the composites made with the large-diameter fibers that had been used previously. Another critically important property measured was impact resistance. Aircraft engine components require sufficient toughness to resist manufacturing defects, assembly damage, stress concentrations at notches, and foreign object damage. Engine company designers indicated that impact resistance would have to be measured before they would seriously consider these types of composites. The Charpy V-notch test was chosen to assess impact resistance, and both monolithic and composite versions Of MOSi2 were tested from -300 to 1400 C. The results (see the following graphs) show that nitride-particulate-reinforced MoSi2 exhibited impact resistance higher than that of many monolithic ceramics and intermetallics, and that the fiber-reinforced composites had even higher values, approaching that of cast superalloys.

Keith, Theo G., Jr.↗

An Improved Fracture Mechanics-Informed Multiscale Thermomechanical Damage Model for Ceramic Matrix Composites

This paper extends recent work done by the authors in modeling length scale-dependent damage behavior of ceramic matrix composites (CMCs) to include effects of local anisotropy introduced by matrix cracking. This model captures scale-dependent damage initiation and propagation behavior of the brittle matrix by employing internal state variable (ISV) theory within a multiscale modeling framework to obtain damaged matrix stress/strain constitutive relationships at each length scale. The damage ISV captures the effects of matrix cracking and growth by using fracture mechanics and the self-consistent scheme to determine the reduced stiffness of the cracked matrix. Matrix cracks, which activate when stress intensity factors near manufacturing induced cavities exceed the fracture toughness of the material, are assumed to be transversely isotropic in the plane of the crack, and matrix anisotropy occurs when the damaged stiffness tensor is rotated from the crack plane to the global axes. The crack progression and temporal evolution of the damage ISV are governed by fracture mechanics and crack growth kinetics. The model effectively captures first matrix cracking, which is the first significant deviation from linear elasticity. The nonlinear predictive capabilities of the material model are demonstrated for monolithic silicon carbide (SiC) and a 2D woven five-harness satin (5HS) carbon fiber SiC matrix (C/SiC) CMC.

Skinner, Travis↗

Performance of Embedded Sensors in 3D Printed SiC

This report summarizes recent advances in embedding sensors in 3D printed silicon carbide (SiC) ceramic components under the Transformational Challenge Reactor (TCR) program. The additive manufacturing technologies developed under this program will enable fabrication of complex structures with embedded fuels and sensors. The sensors will be capable of characterizing fuel performance using spatially distributed measurements at the most strategic locations that would be otherwise inaccessible using conventional manufacturing techniques. While previous programmatic updates describe initial concepts for embedding sensors, materials selection, and initial characterization of the embedded sensors, the technology requires further demonstration, and quality-significant procedures must be established before the embedding technology is ready for adoption by industry. To this end, this report describes the most effective techniques that have been used to embed functional sensors in 3D printed components using a combination of binder-jet additive manufacturing and chemical vapor infiltration (CVI). A detailed procedure describes each step in the process and is available upon request. Molybdenum (Mo)-sheathed thermocouples have been successfully embedded in complex SiC components, and temperatures were monitored in situ during the embedding process. Post-embedding measurements showed no significant hysteresis, and characterization of the interface revealed qualitatively strong bonding around the entire perimeter of the sensor sheath. Distributed fiber-optic temperature sensors were able to briefly measure temperature profiles during CVI, but they ultimately failed prior to completion of the CVI run. The failure appears to be related to the fiber coating at temperatures close to 1,000°C. Future work will focus on irradiation testing of embedded thermocouples and other sheathed electrical sensors, as well as the identification of fiber-optic sensor coatings that can survive CVI.

42 ENGINEERING↗

Effects of high-dose neutron irradiation at light-water reactor relevant temperature on the mechanical properties of SiC/SiC composites

For this study, the neutron dose-dependent evolutions and the underlying mechanisms of properties of SiC fiber-reinforced SiC matrix (SiC/SiC) composites at a temperature relevant to light-water reactors (∼600 K) were investigated and analyzed. Chemical vapor infiltrated (CVI) SiC/SiC composites reinforced with Hi-Nicalon Type S or Tyranno SA3 fiber were neutron-irradiated to doses up to 30 dpa. The irradiated composites retained their flexural strengths. The thermal diffusivity and dimensional changes were mostly retained from 2.0 to 30.2 dpa. Discrepancies in irradiation responses among CVI SiC/SiC composites from different sources were found. Additional microstructural analysis using Raman spectroscopy and numerical analysis on irradiation effect on residual stress were used to explain how the microstructural variables, especially of carbon interphases, affect the mechanical properties in the 30–40 dpa dose range.

Continuous fiber-reinforced ceramic matrix composi↗