Search NASA⌕ Search

SEARCH · Search NASA

Results for “Tensile strength”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Large-diameter carbon-composite monofilaments

Large-diameter carbon composite monofilaments with high strength and high modulus were produced by pregging multifiber carbon bundles with suitable organic resins and pyrolysing them together. Two approaches were developed to increase the utilization of fiber tensile strength by minimizing stress concentration defects induced by dissimilar shrinkage during pyrolysis. These were matrix modification to improve char yield and strain-to-failure and fiber-matrix copyrolysis to alleviate matrix cracking. Highest tensile strength and modulus were obtained by heat treatments to 2873 K to match fiber and matrix strain-to-failure and develop maximum monofilament tensile-strength and elastic modulus.

Bradshaw, W. G.↗

Characterization of Mechanical Performance of Composites Fabricated Using Innovative Carbon Fiber Wet Laid Process

Recent innovation in production of optimized nonwoven wet laid (WL) carbon fiber (CF) mats raised the question of optimal translation of the performance and isotropy into composites formed through these dry preforms. This work explores the mechanical behavior of composites produced from WL-CF mats in conjunction with the microstructure predicted through Object Oriented Finite Element Analysis (OOF). The mats used for the composites were prepared in two dispersion regimes using 25.4 mm long CF. The mixing regimes discussed in the author’s previous work, are identified as Method 1 for the traditional processing regime and Method 2 for the innovative regime that provided optimal nonwoven WL-CF mats. Composite panels from Method 2 mats showed a normalized tensile strength increase of 52% over those from Method 1 panels. Reproducibility analysis of composites made from Method 2 mats demonstrated a standard deviation of 2% in fiber weight content, 2% in tensile modulus and 9% in tensile strength, while composites made from Method 1 mats demonstrated a standard deviation of 5% in fiber weight content, 5% in tensile modulus and 17% in tensile strength. Systematic study of the microstructure and its analysis through OOF confirmed the isotropy translation of mats produced through method 2 to the composites. This study validated the hypothesis that optimal nonwoven mats lead to a well-balanced composite with optimal performance and that non-optimal nonwoven mats do not pack into a well-balanced composite.

36 MATERIALS SCIENCE↗

Pressure effects on the thermal stability of SiC fibers

Commercially available polymer derived SiC fibers were treated at temperatures from 1000 to 2200 C in vacuum and argon gas pressure of 1 and 1360 atm. Effects of gas pressure on the thermal stability of the fibers were determined through property comparison between the pressure treated fibers and vacuum treated fibers. Investigation of the thermal stability included studies of the fiber microstructure, weight loss, grain growth, and tensile strength. The 1360 atm argon gas treatment was found to shift the onset of fiber weight loss from 1200 to above 1500 C. Grain growth and tensile strength degradation were correlated with weight loss and were thus also inhibited by high pressure treatments. Additional heat treatment in 1 atm argon of the fibers initially treated at 1360 atm argon caused further weight loss and tensile strength degradation, thus indicating that high pressure inert gas conditions would be effective only in delaying fiber strength degradation. However, if the high gas pressure could be maintained throughout composite fabrication, then the composites could be processed at higher temperatures.

Jaskowiak, Martha H.↗

Pressure effects on the thermal stability of silicon carbide fibers

Commercially available polymer derived SiC fibers were treated at temperatures from 1000 to 2200 C in vacuum and argon gas pressure of 1 and 1360 atm. Effects of gas pressure on the thermal stability of the fibers were determined through property comparison between the pressure treated fibers and vacuum treated fibers. Investigation of the thermal stability included studies of the fiber microstructure, weight loss, grain growth, and tensile strength. The 1360 atm argon gas treatment was found to shift the onset of fiber weight loss from 1200 to above 1500 C. Grain growth and tensile strength degradation were correlated with weight loss and were thus also inhibited by high pressure treatments. Additional heat treatment in 1 atm argon of the fibers initially treated at 1360 atm argon caused further weight loss and tensile strength degradation, thus indicating that high pressure inert gas conditions would be effective only in delaying fiber strength degradation. However, if the high gas pressure could be maintained throughout composite fabrication, then the composites could be processed at higher temperatures.

Jaskowiak, Martha H.↗

Additional development of large diameter carbon monofilament

The chemical vapor process for preparing a large diameter carbon-base monofilament from a BCl3, Ch4 and H2 gas mixture with a carbon substrate fiber was studied. The effect of reactor geometry, total gas flows and deposition temperature on the tensile strength of the monofilament were investigated. It was noted that consistent results could only be obtained when the carbon substrate fiber was cleaned. The strength of the monofilament was found to depend on the highest temperature and the temperature profile of the monofilament in the reactor. The strength of monofilament produced in the dc and RF reactors were found to be similar and similar alloy compositions in the monofilament were attained when the same gas ratios were used. The tensile strength of the monofilament at 500 C was found to be 60 to 70% of the room temperature tensile strength. No degradation was noted after exposure to molten aluminum.

Jacob, B. A.↗

The effect of ultrasonics on the strength properties of carbon steel processed by cold plastic deformation

A study was made of the influence of ultrasounds on the mechanical properties of OLT 35 carbon steel tubes cold-drawn on a plug ultrasonically activated by longitudinal waves. Experimental results indicate that: 1. The reduction in the values of the flow limit and tensile strength is proportional to the increase in acoustic energy introduced into the material subjected to deformation. 2. The diminution in influence of ultrasounds on tensile strength and flow rate that is due to an increased degree of deformation is explained by a reduction in specific density of the acoustic energy at the focus of deformation. 3. The relations calculated on the basis of the variation in the flow limit and tensile strength as a function of acoustic energy intensity was verified experimentally.

Atanasiu, N.↗

Structure-performance relationships in lignin-based transesterification vitrimers: The role of lignin structural features

Lignin has been hailed as an ideal renewable alternative for petrochemical-based prepolymers in material synthesis for a sustainable and circular economy, due to its abundant aromatic network and high carbon content. However, the properties and performance of lignin-derived macromolecules are strongly influenced by the lignin itself. While numerous studies have explored the impact of lignin content on the thermomechanical performance of lignin-based vitrimers, literature on how the inherent structural features of lignin affect these properties is scanty. In this study, hardwood organosolv lignin was fractionated in ethyl acetate, ethanol, and acetone to obtain lignin fractions with varying structural characteristics. These fractions were then modified through carboxylation and crosslinked with epoxidized soybean oil (ESO) at a hydroxyl to epoxy group ratio of 1:1 to produce lignin-based transesterification vitrimers (LVs). The thermal properties (i.e. glass transition temperature and thermal stability), tensile strength, storage modulus, and stress relaxation behavior of the LVs were studied and carefully related to the structural features of lignin. The results revealed a positive relationship between strong hydroxyl content in modified lignin and the tensile strength (5.10–9.71 MPa), storage modulus (1099.4 – 1372.8 MPa), crosslinking density, and stress relaxation of the LVs. Additionally, both the storage modulus and tensile strength exhibited a positive relationship with the ratio of rigid linkages in modified lignin, while lignin molecular weight was found to significantly impact the thermal properties of LVs (i.e Tg and thermal stability). This study not only highlights the valorization of lignin in vitrimer synthesis but also provide insights for designing lignin-based materials with tailored properties for specific applications.

Bio-based polymer↗

Application of an Elongated Kelvin Model to Space Shuttle Foams

The space shuttle foams are rigid closed-cell polyurethane foams. The two foams used most-extensively oil space shuttle external tank are BX-265 and NCFL4-124. Because of the foaming and rising process, the foam microstructures are elongated in the rise direction. As a result, these two foams exhibit a nonisotropic mechanical behavior. A detailed microstructural characterization of the two foams is presented. Key features of the foam cells are described and the average cell dimensions in the two foams are summarized. Experimental studies are also conducted to measure the room temperature mechanical response of the two foams in the two principal material directions (parallel to the rise and perpendicular to the rise). The measured elastic modulus, proportional limit stress, ultimate tensile strength, and Poisson's ratios are reported. The generalized elongated Kelvin foam model previously developed by the authors is reviewed and the equations which result from this model are summarized. Using the measured microstructural dimensions and the measured stiffness ratio, the foam tensile strength ratio and Poisson's ratios are predicted for both foams and are compared with the experimental data. The predicted tensile strength ratio is in close agreement with the measured strength ratio for both BX-265 and NCFI24-124. The comparison between the predicted Poisson's ratios and the measured values is not as favorable.

Sullivan, Roy M.↗

Process Variability Effects on Tensile Response in Injection Molded, Fluorinated Thermoplastics

The mechanical properties of fluorinated thermoplastics (i.e., tensile strength and elongation) can vary with changes in injection molding processing parameters. Four fluoropolymers are examined: poly(vinylidene fluoride) (PVDF) and random poly(vinylidene fluoride-co-chlorotrifluoroethylene) (PVDF-CTFE) with three CTFE concentrations. Dog bones were manufactured with various cylinder dwell times and mold cooling times to assess the manufacturing sensitivity to the tensile response. Dwell and cooling times increasingly impact mechanical performance as CTFE concentration increases. Specimens exhibit higher tensile strength as a function of injection order. The first injected specimen exhibits the lowest tensile strength and highest elongation in all copolymers. This trend becomes more pronounced among fluoropolymers with higher CTFE concentration and lower weight-averaged molecular weight. Parallel plate rheology was used to obtain the zero-shear viscosity as a function of material type, process, and injection order. We found that in the copolymers, the first injected sample exhibited a lower zero-shear viscosity than the next, which indicates a lower molecular weight in the first injected specimen. This phenomenon was not presented for the PVDF homopolymer. Copolymer mechanical uncertainties are hypothesized to result from the shorter molecular weight chains extruding out of the specimens' sides as a flash due to higher mobility with CTFE segments.

36 MATERIALS SCIENCE↗

Process Variability Effects on Tensile Response in Injection Molded, Fluorinated Thermoplastics

The mechanical properties of fluorinated thermoplastics (i.e., tensile strength and elongation) can vary with changes in injection molding processing parameters. Four fluoropolymers are examined: poly(vinylidene fluoride) (PVDF) and random poly(vinylidene fluoride-co-chlorotrifluoroethylene) (PVDF-CTFE) with three CTFE concentrations. Dog bones were manufactured with various cylinder dwell times and mold cooling times to assess the manufacturing sensitivity to the tensile response. Dwell and cooling times increasingly impact mechanical performance as CTFE concentration increases. Specimens exhibit higher tensile strength as a function of injection order. The first injected specimen exhibits the lowest tensile strength and highest elongation in all copolymers. This trend becomes more pronounced among fluoropolymers with higher CTFE concentration and lower weight-averaged molecular weight. Parallel plate rheology was used to obtain the zero-shear viscosity as a function of material type, process, and injection order. We found that in the copolymers, the first injected sample exhibited a lower zero-shear viscosity than the next, which indicates a lower molecular weight in the first injected specimen. This phenomenon was not present for the PVDF homopolymer. Copolymer mechanical uncertainties are hypothesized to result from the shorter molecular weight chains extruding out of the specimens’ sides as a flash due to higher mobility with CTFE segments.

36 MATERIALS SCIENCE↗

Mechanical behavior of carbonated MgO-based Engineered Cementitious Composite (ECC) after high temperatures exposure

Carbonated MgO-based Engineered Cementitious Composite (ECC) has ultrahigh tensile ductility and tight crack width control behavior. However, the expectation of improved fire-resistant has not been confirmed. This study explored the alterations to mechanical and microstructure characteristics of this material after exposure to temperatures up to 500 °C. Material mass loss, compressive strength, tensile strength, strain capacity, and matrix fracture toughness were measured. Scanning electron microscopy, mercury intrusion porosimetry, thermogravimetric analysis, and X-ray diffraction were used to probe the degradation of the cement matrix and fibers. The effect of elevated temperature on carbonated MgO-based ECC was further assessed via examination of the micromechanical behavior of the fiber-matrix. The objective of this research was to assess the performance of carbonated MgO-based ECC exposed to fire hazards. The tensile ductility of carbonated MgO-based ECC was found to be enhanced when exposed to ~100 °C as compared with those at room temperature ~20 °C. Further increase in exposure temperature, however, posed a negative impact on the composite compressive strength, ultimate tensile strength, and ability to control crack width. Here the results provide a useful database for further investigations into carbonated MgO-based ECC for fire safety enhancement.

36 MATERIALS SCIENCE↗

Development of a process for producing ribbon shaped filaments

Silicon carbide (SiC) ribbon filaments were produced on a carbon ribbon substrate, about 1500 microns (60 mils) wide and 100 microns (4 mils) thick in lengths up to 2 meters (6 ft), and with tensile strengths up to 142 KN/cm sq (206 Ksi). During the course of the study, ribbon filaments of boron were also produced on the carbon ribbon substrate; the boron ribbon produced was extremely fragile. The tensile strength of the SiC ribbon was limited by large growths or flaws caused by anomalies at the substrate surface; these anomalies were either foreign dirt or substrate imperfections or both. Related work carried out on round 100 micron (4 mils) diameter SiC filaments on a 33 micron (1.3 mil) diameter, very smooth carbon monofilament substrate has shown that tensile strengths as high as 551 KN/cm sq (800 Ksi) are obtainable with the SiC-carbon round substrate combination, and indicates that if the ribbon substrate surface and ribbon deposition process can be improved similar strengths can be realizable. Cost analysis shows that 100 micron x 5-10 micron SiC ribbon can be very low cost reinforcement material.

Debolt, H. E.↗

Reinforced Thermoplastic Polyimide with Dispersed Functionalized Single Wall Carbon Nanotubes

Molecular pi-complexes were formed from pristine HiPCO single-wall carbon nanotubes (SWCNTs) and 1-pyrene- N-(4- N'-(5-norbornene-2,3-dicarboxyimido)phenyl butanamide, 1. Polyimide films were prepared with these complexes as well as uncomplexed SWCNTs and the effects of nanoadditive addition on mechanical, thermal, and electrical properties of these films were evaluated. Although these properties were enhanced by both nanoadditives, larger increases in tensile strength and thermal and electrical conductivities were obtained when the SWCNT/1 complexes were used. At a loading level of 5.5 wt %, the Tg of the polyimide increased from 169 to 197 C and the storage modulus increased 20-fold (from 142 to 3045 MPa). The addition of 3.5 wt % SWCNT/1 complexes increased the tensile strength of the polyimide from 61.4 to 129 MPa; higher loading levels led to embrittlement and lower tensile strengths. The electrical conductivities (DC surface) of the polyimides increased to 1 x 10(exp -4) Scm(exp -1) (SWCNT/1 complexes loading level of 9 wt %). Details of the preparation of these complexes and their effects on polyimide film properties are discussed.

Lebron-Colon, Marisabel↗

Effect of dropped plies on the strength of graphite-epoxy laminates

The reduction in the compressive and tensile strengths of graphite-epoxy laminates with thickness discontinuities due to dropped plies was studied by experiment and analysis. The specimens were fabricated with all the dropped plies lumped together in the center of a sixteen-ply quasi-isotropic layup, such that one surface was flat and the slope of the opposite surface changed abruptly at the dropped ply location to accommodate the thickness change. Even though the thick and thin sections are symmetrically laminated, there exists bending-extension coupling due to the geometric eccentricity of the middle planes of the thick and thin sections. Experiments were conducted on fifty-four specimens that differed in the configuration of the dropped plies only. The strength of a laminate with dropped plies is less than the strength of its thin section, and the compressive strength of a laminate with dropped plies is less than its tensile strength. The reduction in strength is directly related to the axial stiffness change between the thick and thin sections. To examine the mechanism of failure, the three-dimensional state of stress in the dropped ply region was evaluated by the finite element method. A tensile interlaminar criterion predicted the correct location of failure, but underestimated the failure load.

Curry, James M.↗

Mechanical evaluation of WC-Co materials with varying microstructures

Tungsten carbide–cobalt materials are useful in a variety of extreme applications due to a desirable blend of properties, yet the technology has not significantly changed since their initial development in the 1920s. The mechanical properties of this class of materials is highly dependent on two variables, the size of the tungsten carbide grains, and the amount of binder phase present in the final body. In this study, the amount of binder phase is isolated across three commercial materials from the same manufacturer with three different grain sizes to investigate the effect on mechanical properties. The mechanical properties investigated are indentation hardness, flexure and tensile strength, as well as fracture toughness. In general, an increase in hardness and tensile strength with decreasing grain size was observed, while the fracture toughness showed the opposite trend with toughness increasing with increasing grain size. The flexure strength results did not show a correlation to grain size. Fractographic analysis identified the dominant strength-limiting flaw for each sample, which largely were in the form of porosity. Other flaws types, such as inclusions from the milling process, clusters of large grains, and machining cracks from the surface finishing process, were also identified. Finally, Weibull analysis was performed and deemed appropriate for analysis of these materials, but strength-size scaling was not conducted due to the variability in the strength-limiting feature between the different specimen geometries.

36 MATERIALS SCIENCE↗

Tensile test of pressureless-sintered silicon nitride at elevated temperature

Uniaxial tensile strength tests of pressureless sintered silicon nitride were carried out in air at temperatures ranging from room temperature up to 1600 C. Silicon nitrides containing Y2O3, Al2O3, Al2O3-MgO, or MgO-CeO2 additives were tested. The results show that the composition of the additive used influences the strength characteristics of the silicon nitride. The tensile strength rapidly decreased at temperatures above 1000 C for the materials containing MgO as the additive and above 1000 C for the material with Y2O3. When the temperature increased to as high as 1300 C, the strength decreased to about 10 percent of the room temperature strength in each case. Observations of the fracture origin and of the crack propagation on the fracture surfaces are discussed.

Matsusue, K.↗

Dependency of Shear Strength on Test Rate in SiC/BSAS Ceramic Matrix Composite at Elevated Temperature

Both interlaminar and in-plane shear strengths of a unidirectional Hi-Nicalon(TM) fiber-reinforced barium strontium aluminosilicate (SiC/BSAS) composite were determined at 1100 C in air as a function of test rate using double notch shear test specimens. The composite exhibited a significant effect of test rate on shear strength, regardless of orientation which was either in interlaminar or in in-plane direction, resulting in an appreciable shear-strength degradation of about 50 percent as test rate decreased from 3.3 10(exp -1) mm/s to 3.3 10(exp -5) mm/s. The rate dependency of composite's shear strength was very similar to that of ultimate tensile strength at 1100 C observed in a similar composite (2-D SiC/BSAS) in which tensile strength decreased by about 60 percent when test rate varied from the highest (5 MPa/s) to the lowest (0.005 MPa/s). A phenomenological, power-law slow crack growth formulation was proposed and formulated to account for the rate dependency of shear strength of the composite.

Choi, Sung R.↗

The effect of thermal exposure on the mechanical properties of aluminum-graphite composites

The mechanical properties of aluminum-graphite composites were measured at room temperature in the as-received condition, after elevated temperature exposure and after thermal cycling. The composites were fabricated by solid-state diffusion bonding of liquid-phase Al-infiltrated Thornel 50 fibers. The results showed that the maximum longitudinal tensile strength of the as-received material was 80,000 psi, which corresponds well with the rule of mixture value. The composite strength was observed to vary widely, depending on the extent of wetting of the fibers by the aluminum. The strength of the composites in the transverse direction was generally very low, due to poor interfacial bonding. Aluminum carbide (Al4C3) formed at the surface of the fibers at temperatures greater than 500 C. Development of the carbide was shown to be diffusion-controlled and was dependent on the time and temperature used. It was shown that the tensile strength was virtually unaffected by heat-treatment up to 500 C; beyond that temperature a drastic degradation of tensile strength occurred. Thermal cycling of the composites below 500 C resulted in an observable degradation of the composite strength.

Khan, I. H.↗