Search NASA⌕ Search

SEARCH · Search NASA

Results for “catalyst layer”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Oxygen Reduction on Platinum-Nickel and Platinum-Cobalt Alloy Based Catalysts for High Temperature Proton Exchange Membrane Fuel Cells

Catalyst layers, with commercial PtNi/TKK (TECNiE52; platinum 46.5 wt%), PtCo/TKK (TEC36E52; platinum 45.8 wt%) catalysts, and an in-house catalyst PtNi-NC (platinum 38.4 wt%), synthesised using acoustic mixer and a tube furnace, are prepared using three different ionomers: 20 wt% Nafion®, 60 wt% polytetrafluoroethylene (PTFE), and an in-house 5 wt% ionomer (‘Ionomer X’). These inks are bar-coated onto carbon paper gas diffusion layers (GDLs), which are cut into 3 cm × 5 cm pieces. The coated layers are tested for oxygen reduction in a commercial gas diffusion electrode (GDE) test cell, FlexCell® (Gaskatel GmbH, Germany), using 85 wt% phosphoric acid at both room temperature and at 155°C. This study evaluates the polynorbornene (PNB)-based in-house ionomer performance as binder and in-house catalyst oxygen reduction reaction (ORR) activity in comparison to commercial products. The catalyst layers are characterised using X-ray diffraction (XRD) analysis, X-ray photoelectron spectroscopy (XPS), and high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM). Among the catalyst layers prepared with PTFE ionomer and tested at 155°C, the in-house catalyst demonstrates the highest ORR activity. Ionomer X proves to be a good candidate to be used as a per- and polyfluoroalkyl-free binder for high-temperature (HT) proton exchange membrane fuel cell (PEMFC) applications.

85 wt% phosphoric acid↗

Application of a temporal multiscale method for efficient simulation of degradation in PEM Water Electrolysis under dynamic operating conditions

Hydrogen is emerging as a vital energy carrier, driven by the need to reduce carbon emissions. Proton Electrolyte Membrane Water Electrolysis (PEMWE) enables hydrogen production under fluctuating renewable power conditions but requires improved understanding and stability of the anode catalyst layer under dynamic operating conditions, especially with low noble metal loadings. Long-term degradation experiments are both time-consuming and costly; therefore, a systematic, model-aided approach is essential. In the present work, a temporal multiscale method is applied to reduce the computational effort of simulating long-term degradation processes in PEMWE, with an exemplary focus on catalyst dissolution. A mechanistic model incorporating the oxygen evolution reaction, catalyst dissolution, and hydrogen permeation from the cathode to the anode was hypothesized and implemented. In this way, the local periodicity of transport and reaction processes in dynamic PEMWE operation, which influence the gradual degradation of the catalyst layer, is captured. The temporal multiscale method significantly reduces the computational effort of simulation, decreasing processing time from hours to mere minutes. This efficiency gain is attributed to the limited evolution of Slow-Scale variables during each period of time P of the Fast-Scale variables. Consequently, simulation is required only until local periodicity is achieved within each Slow-Scale time step. Hence, the fully resolved dynamic problem is decoupled into these two scales, employing a heterogeneous multiscale technique. The developed approach effectively accelerates parameter estimation and predictive simulations, supporting systematic modeling of PEMWE degradation under dynamic conditions.

08 HYDROGEN↗

Molybdenum Disulfide as a Protection Layer and Catalyst for Gallium Indium Phosphide Solar Water Splitting Photocathodes

Gallium indium phosphide (GaInP2) is a semiconductor with promising optical and electronic properties for solar water splitting, but its surface stability is problematic as it undergoes significant chemical and electrochemical corrosion in aqueous electrolytes. Molybdenum disulfide (MoS2) nanomaterials are promising to both protect GaInP2 and to improve catalysis since MoS2 is resistant to corrosion and also possesses high activity for the hydrogen evolution reaction (HER). In this work, we demonstrate that GaInP2 photocathodes coated with thin MoS2 surface protecting layers exhibit excellent activity and stability for solar hydrogen production, with no loss in performance (photocurrent onset potential, fill factor, and light limited current density) after 60 hours of operation. This represents a five-hundred fold increase in stability compared to bare p-GaInP2 samples tested in identical conditions.

14 SOLAR ENERGY↗

Ice formation in PEM fuel cells operated isothermally at sub-freezing temperatures

The effect of MEA and GDL structure and composition on the performance of single-PEM fuel cells operated isothermally at subfreezing temperatures is presented. The cell performance and durability are not only dependent on the MEA/GDL materials used but also on their interfaces. When a cell is operated isothermally at sub-freezing temperatures in constant current mode, the water formation due to the current density initially hydrates the membrane/ionomer and then forms ice in the catalyst layer/GDL. An increase in high frequency resistance was also observed in certain MEAs where there is a possibility of ice formation between the catalyst layer and GDL leading to a loss in contact area. The total water/ice holding capacity for any MEA was lower at lower temperatures and higher current densities. The durability of MEAs subjected to multiple isothermal starts was better for LANL prepared MEAs as compared to commercial MEAs, and cloth GDLs when compared to paper GDLs. The ice formation was monitored using high-resolution neutron radiography and was found to be concentrated near the cathode catalyst layer. However, there was significant ice formation in the GDLs especially at the higher temperature ({approx} -10 C) and lower current density (0.02 A/cm{sup 2}) operations. These results are consistent with the longer-term durability observations that show more severe degradation at the lower temperatures.

36 MATERIALS SCIENCE↗

High resolution neutron imaging of water in the polymer electrolyte membrane

To achieve a deeper understanding of water transport and performance issues associated with water management, we have conducted in situ water examinations to help understand the effects of components and operation. High Frequency Resistance (HFR), AC Impedance and neutron radiography were used to measure water content in operating fuel cells under various operating conditions. Variables examined include: sub-freezing conditions, inlet relative humidities, cell temperature, current density and response transients, different flow field orientations and different component materials (membranes, GDLs and MEAs). Quantification of the water within the membrane was made by neutron radiography after equilibration to different humidified gases, during fuel cell operation and in hydrogen pump mode. The water content was evaluated in bare Nafion{reg_sign} membranes as well as in MEAs operated in both fuel cell and H{sub 2} pump mode. These in situ imaging results allow measurement of the water content and gradients in the PEFC membrane and relate the membrane water transport characteristics to the fuel cell operation and performance under disparate materials and operational combinations. Flow geometry makes a large impact on MEA water content. Higher membrane water with counter flow was measured compared with co-flow for sub-saturated inlet RH's. This correlates to lower HFR and higher performance compared with co-flow. Higher anode stoichiometry helps remove water which accumulates in the anode channels and GDL material. Cell orientation was measured to affect both the water content and cell performance. While membrane water content was measured to be similar regardless of orientation, cells with the cathode on top show flooding and loss of performance compared with similarly operated cells with the anode on top. Transient fuel cell current measurements show a large degree of hysteresis in terms of membrane hydration as measured by HFR. Current step transients from 0.01 A cm{sup -2} to 0.68 A cm{sup -2} consistently show PEM wetting occurring within 5 to 20 sec. Whereas the PEM drying response to the reverse step transient of 0.68 A cm{sup -2} to 0.01 A cm{sup -2}, takes several minutes. The observed faster wetting response is due to reaction water being produced in the cathode and back diffusing into the membrane. The slower PEM drying is due to the water slowly being removed out of the wetted GDLs. This rate of removal of water and hence the PEM hydration level was found to be influenced strongly by the PTFE loadings in the GDL substrate and Microporous layer (MPL). The drying of the membrane is influenced by both the anode and cathode GDL PTFE loadings. Lower PTFE loading in the anode GDL leads to better membrane hydration probably due to the easier incorporation of water from the anode GDL into the membrane. Similarly a lower PTFE loading in the cathode GDL also results in better membrane hydration probably due to the better water retention properties (less hydrophobic) of this GDL. Fuel cells operated isothermal at sub-freezing temperatures show gradual cell performance decay over time and eventually drops to zero. AC impedance analysis indicates that losses are initially due to increasing charge transfer resistance. After time, the rate of decay accelerates rapidly due to mass transport limitations. High frequency resistance also increases over time and is a function of the initial membrane water content. These results indicate that catalyst layer ice formation is influenced strongly by the MEA and is responsible for the long-term degradation of fuel cells operated at sub-freezing temperatures. Water distribution measurements indicate that ice may be fonning mainly in the GDLs at -10 C but are concentrated in the catalyst layer at -20 C.

08 HYDROGEN↗

Intermediate Sr 2 Co 1.5 Fe 0.5 O 6-δ Tetragonal Structure between Perovskite and Brownmillerite as a Model Catalyst with Layered Oxygen Deficiency for Enhanced Electrochemical Water Oxidation

The generation of hydrogen in an environmentally benign way is highly essential to meet future energy demands. However, in the process of splitting water electrochemically, sluggish kinetics of the oxygen evolution reaction (OER) curtails its applicability, as it drags energy input. Herein, we synthesized SrCo-Fe-O oxides to optimize their OER activity by varying the Co/Fe ratio. Among them, Sr 2 Co 1.5 Fe 0.5 O 6-δ exhibited the best OER catalytic activity in the series, with an overpotential of 318 mV at 10 mA cm -2 and Tafel slope of 44.8 mV dec -1 . High-resolution neutron powder diffraction analysis identified an intermediate structure between the perovskite and brownmillerite, with alternating layers of disorderly orientated oxygen-deficient tetrahedra and fully stoichiometric octahedra. The unique stacking of tetrahedral and octahedral units facilitates desired interactions between the electrode surface and electrolyte. Theoretical calculations revealed that increased covalency of Co 3d and O 2p in Sr 2 Co 1.5 Fe 0.5 O 6-δ oxide is another primary contributor to its augmented water oxidation ability. As a model for developing catalysts with such an intermediate structure, the synergetic effect of oxygen vacancy and hybridization between Co 3d and O 2p assured the Sr 2 Co 1.5 Fe 0.5 O 6-δ oxide as a better catalyst for its enhanced OER activity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Revealing in-plane movement of platinum in polymer electrolyte fuel cells after heavy-duty vehicle lifetime

Fuel cell heavy-duty vehicles (HDVs) require increased durability of oxygen-reduction-reaction electrocatalysts, making knowledge of realistic degradation mechanisms critical. Here identical-location micro-X-ray fluorescence spectroscopy was performed on membrane electrode assemblies. The results exposed heavy in-plane movement of electrocatalyst after HDV lifetime, suggesting that electrochemical Ostwald ripening may not be a local effect. Development of local loading hotspots and preferential movement of electrocatalyst away from cathode catalyst layer cracks was observed. The heterogeneous degradation exhibited by a modified cathode gas diffusion layer membrane electrode assembly after HDV lifetime was successfully quantified by the identical-location approach. Further synchrotron micro-X-ray diffraction and micro-X-ray fluorescence experiments were performed to obtain the currently unknown correlation between electrocatalyst nanoparticle size increase and loading change. A direct correlation was discovered which developed only after HDV lifetime. Finally, the work provides a route to engineer immediate system-level mitigation strategies and to develop structured cathode catalyst layers with durable electrocatalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Performance and durability of PEM fuel cells operated at sub-freezing temperatures

The durability of polymer electrolyte membrane (PEM) fuel cells operated at sub-freezing temperatures has received increasing attention in recent years. The Department of Energy's PEM fuel cell stack technical targets for the year 2010 include unassisted start-up from -40 {sup o}C and startup from -20 {sup o}C ambient in as low as 30 seconds with < 5 MJ energy consumption. Moreover, the sub-freezing operations should not have any impact on acieving other technical targets including 5000 hours durability. The effect of MEA preparation on the performance of single-PEM fuel cells operated at sub-freezing temperatures is presented. The cell performance and durability are dependent on the MEA and are probably influenced by the porosity of the catalyst layers. When a cell is operated isothermally at -10 {sup o}C in constant current mode, the voltage gradually decreases over time and eventually drops to zero. AC impedance analysis indicated that the rate of voltage loss is initially due to an increase in the charge transfer resistance and is gradual. After a period, the rate of decay accelerates rapidly due to mass transport limitations at the catalyst and/or gas diffusion layers. The high frequency resistance also increases over time during the isothermal operation at sub-freezing temperatures and was a function of the initial membrane water content. LANL prepared MEAs showed very little loss in the catalyst surface area with multiple sub-freezing operations, whereas the commercial MEAs exhibited significant loss in cathode surface area with the anode being unaffected. These results indicate that catalyst layer ice formation is influenced strongly by the MEA and is responsible for the long-term degradation of fuel cells operated at sub-freezing temperatures. This ice formation was monitored using neutron radiography and was found to be concentrated near cell edges at the flow field turns. The water distribution also indicated that ice may be forming mainly in the GDLs at -10 {sup o}C and could be concentrated in the catalyst layer at -20 {sup o}C.

36 MATERIALS SCIENCE↗

Catalyst containing oxygen transport membrane

A composite oxygen transport membrane having a dense layer, a porous support layer and an intermediate porous layer located between the dense layer and the porous support layer. Both the dense layer and the intermediate porous layer are formed from an ionic conductive material to conduct oxygen ions and an electrically conductive material to conduct electrons. The porous support layer has a high permeability, high porosity, and a high average pore diameter and the intermediate porous layer has a lower permeability and lower pore diameter than the porous support layer. Catalyst particles selected to promote oxidation of a combustible substance are located in the intermediate porous layer and in the porous support adjacent to the intermediate porous layer. The catalyst particles can be formed by wicking a solution of catalyst precursors through the porous support toward the intermediate porous layer.

36 MATERIALS SCIENCE↗

Editors’ Choice—Ionomer Side Chain Length and Equivalent Weight Impact on High Current Density Transport Resistances in PEMFC Cathodes

Cell voltage at high current densities (HCD) of an operating proton-exchange membrane fuel cell (PEMFC) suffers from losses due to the local-O 2 and bulk-H + transport resistances in the cathode catalyst layer (CCL). Particularly, the interaction of perfluorosulfonic acid (PFSA) ionomer with the carbon supported platinum catalyst plays a critical role in controlling reactant transport to the active site. In this study, we perform a systematic analysis of the side chain length and equivalent weight (EW) of PFSA ionomers on the CCL transport resistances. Ex situ measurements were carried out to quantify the ionomer characteristics such as the molecular weight, proton conductivity and water uptake. Nanomorphology of ionomers cast as 60–120 nm thin-films is characterized using grazing-incidence X-ray scattering. In situ fuel cell electrochemical diagnostic measurements were carried out to quantify the reactant (H + /O 2 ) transport properties of the CCL. Ionomer EW was found to play a major role with decreasing EW yielding higher proton conductivity and water uptake that led to lower bulk-H + and local-O 2 transport resistances in the CCL. Finally, a 1D-semi-empirical performance model has been developed to quantify the impact of ionomer EW on cell voltage loss factors.

08 HYDROGEN↗

Understanding Platinum Ionomer Interface Properties of Polymer Electrolyte Fuel Cells

A well-designed cathode catalyst layer with optimal ionomer distribution is critical to minimizing amount of Platinum (Pt) content in polymer electrolyte fuel cells (PEFCs). The impact of Pt loading, ionomer content and carbon support types on the catalyst/ionomer interface were also investigated at dry and wet conditions. Higher Pt loadings resulted in higher double layer capacity (C dl ) and similar electrochemical surface area (ECSA) due to well dispersed ionic phase material. Higher ionomer content resulted in higher ionic conductivity but also showed similar SO 3 − group coverage. High surface area (HSA) carbon support had larger ECSA and C dl at both dry and wet conditions, as less agglomerated Pt was well dispersed in the meso-pores of the support. Lower SO 3 − group coverages were observed for HSA carbon than for Vulcan carbon due to Pt particles being buried within the porous HSA carbon support. The effect of cell conditioning and voltage recovery on the PEFC cathode catalyst layer was shown to have minimal impact on SO 3 − group coverage despite a decrease in C dl and ECSA due to the size increase of Pt particles. At dry condition, a significant increases in SO 3 − group coverage were observed for all MEAs due to higher adsorptivity of ionomer in dry conditions.

25 ENERGY STORAGE↗

High Performance non-PGM Transition Metal Oxide ORR Catalysts of PEMFCs

This project was designed to develop acid-stable PGM-free transition metal oxide oxygen reduction reaction (ORR) electrocatalysts to meet or exceed the performance and durability of the DOE 2020 Technical Targets for platinum-group metal (PGM) free electrocatalysts from first-principles to incorporation into membrane-electrode assemblies (MEAs) for polymer electrolyte membrane (PEM) fuel cells. The planned project was to accomplish this goal with a multi-step approach: 1) materials modeling and experimental screening to identify acid-stable oxides with high ORR activity, 2) optimization of catalyst particle size and catalyst/carbon/ionomer catalyst layer composition, 3) fabrication of MEAs for performance and durability testing. During the course of this project: 1) acid-stability descriptors were developed for manganese oxides; 2) a family of acid-stable multicomponent oxides based on antimony were developed; 3) a flexible synthesis for the formation of nanocrystalline nonstoichiometric oxides was developed; 4) limited ORR activity but modest and improving oxygen evolution reaction (OER) activity was measured for multicomponent antimony oxides. The project was programmed into five technical tasks: The development of acid-stable ORR electrocatalytic oxides through 1) identification and optimization of acid-stable oxide compositions, and 2) electrochemical characterization; 3) optimization of catalyst layer composition for MEAs using identified ORR electrocatalysts; 4) MEA fabrication and performance testing to result in performance of 44 mA-cm-2 at 0.9 V vs. RHE; and 5) accelerated-stress testing of optimized MEAs. Because no acid-stable oxide was identified with the requisite activity for ORR (4.4 µA-cm-2oxide intrinsic activity at 0.9 V vs. RHE) within the time and budget allotted in Tasks 1 and 2, the project was halted at the end of phase 1, with no activity in Tasks 3-5. The research output, while not succeeding in developing ORR electrocatalysts, advanced the development of acid-stable oxide materials, showing potential for further improvement as OER electrocatalysts.

08 HYDROGEN↗

Membrane Degradation in PEM Fuel Cells: Part I. Modeling Gas Crossover and the Pt Band

Understanding chemical degradation of the proton-exchange membrane in fuel cells is crucial for extending their lifetimes. Herein, various degradation reactions reported in literature are organized and analyzed, including direct radical generation and an indirect (Fenton) pathway. To understand the transport of dissolved H 2 and O 2 crossover gases as they relate to membrane degradation, an agglomerate-scale model is introduced, treating gas, ionomer, and catalyst as discrete phases. The model reveals a key phenomenon: at working potentials, dissolved gases are mostly consumed at the interface between the catalyst layer and the membrane, leaving little gas to cross the membrane. Under open-circuit conditions, dissolved gases are not consumed and can then cross the membrane. This explains high H 2 O 2 concentrations and degradation rates seen in experiments but not captured in previous models. Following mixed-potential theory, crossover gases supply the hydrogen-oxidation and oxygen-reduction reactions, which occur simultaneously on individual Pt particles comprising the Pt band in the membrane, forming reactive species (H 2 O 2 , OH·). Results show crossover gas almost entirely reacts on the Pt band, allowing little to reach the opposite electrode. Furthermore, the micro-scale geometry of the catalyst-layer/membrane interface impacts the gas crossover at working potentials, indicating that cell construction affects membrane durability.

Johnson, Evan F. [Lawrence Berkeley National Labor↗

Fabrication and operational considerations of hydrogen permeable Mo 2 C/V metal membranes and improvement with application of Pd

Mo 2 C has previously been demonstrated as an effective catalyst layer to enable stable H 2 permeation through vanadium foils at high temperatures. Here, in this paper, this approach was extended to several group V metal foils (V, Nb, and Ta) as well as mixed gas testing. The best permeability was achieved with V, and an activation process was developed to recover the performance of V foils displaying evidence of oxidation. Nb foils yielded ~20% the permeability of V, while Ta was too brittle to operate effectively. Mo 2 C/V membranes were operated at feed conditions well above the ductile-to-brittle transition pressure without embrittlement; however, the H 2 permeability of Mo 2 C/V membranes was significantly attenuated at lower temperatures (< 600 °C). H 2 permeation was also severely inhibited by the presence of N 2 or CO 2 in mixed gas environments due to strong competitive adsorption. The addition of a Pd catalyst layer on top of Mo 2 C improved mixed gas stability and increased H 2 permeability to 2 × 10 -8 mol·m -1 ·s -1 ·Pa -0.5 at 500 °C for V based membranes. Lastly, as an interlayer, Mo 2 C was demonstrated to be a stable barrier preventing Pd-V interdiffusion at 500 °C while simultaneously allowing significant H 2 permeation.

08 HYDROGEN↗

Aging gracefully? Investigating iridium oxide ink's impact on microstructure, catalyst/ionomer interface, and PEMWE performance

Here, in this study, we conducted a thorough investigation of the impact of aging iridium oxide (IrO 2 ) perfluorosulfonic acid ionomer ink for up to 14 days on the properties of the ink and the resulting catalyst layers. We examined ink properties, such as zeta potential, dynamic light scattering (DLS), density, surface tension, and rheology, as functions of ink aging time. To evaluate the microstructure and catalyst/ionomer interface, we employed transmission electron microscopy (TEM), X-ray scattering, and X-ray photoelectron spectroscopy (XPS) techniques. Furthermore, we assessed the effect of ink aging on the performance of proton exchange membrane water electrolyzers (PEMWEs). Our findings reveal that most ink properties remain stable for 14 days. The variations in PEMWE cell performance are minimal, and no clear trend is observed in relation to ink aging time. This study demonstrates that the effects of aging the inks for 14 days on ink properties, catalyst layer structure, catalyst/ionomer interface, and PEMWE performance are negligible, indicating a substantial time window after ink preparation without any significant changes in its properties. These insights provide crucial guidance for the commercial production and coating processes of ink, which is necessary for scaling up PEM technologies to meet future demand.

30 DIRECT ENERGY CONVERSION↗

Optimization of electrode characteristics for the Br-2/H-2 redox flow cell

The Br-2/H-2 redox flow cell shows promise as a high-power, low-cost energy storage device. The effect of various aspects of material selection, processing, and assembly of electrodes on the operation, performance, and efficiency of the system is determined. In particular, (+) electrode thickness, cell compression, hydrogen pressure, and (-) electrode architecture are investigated. Increasing hydrogen pressure and depositing the (-) catalyst layer on the membrane instead of on the carbon paper backing layers have a large positive impact on performance, enabling a limiting current density above 2 A cm(-2) and a peak power density of 1.4 W cm(-2). Maximum energy efficiency of 79 % is achieved. In addition, the root cause of limiting-current behavior in this system is elucidated, where it is found that Br- reversibly adsorbs at the Pt (-) electrode for potentials exceeding a critical value, and the extent of Br- coverage is potential-dependent. This phenomenon limits maximum cell current density and must be addressed in system modeling and design. These findings are expected to lower system cost and enable higher efficiency.

Tucker, MC↗

A Direct Ammonia Fuel Cell with a KOH-Free Anode Feed Generating 180 mW cm −2 at 120 °C

The motivations to operate the direct ammonia fuel cell (DAFC) with no addition of aqueous base, include facilitated fuel management and prevention of corrosion and shunt currents in the DAFC stack. We describe here a polymer electrolyte DAFC, operating at a cell temperature (T cell ) of 120 °C on ammonia and water alone as anode feed, that demonstrated peak power of 180 mW cm −2 —a record for this type of fuel cell. We offer a detailed analysis of polarization curves recorded for PE-DAFCs in the T cell range of 60 °C–120 °C, allowing to estimate the effects of KOH-free operation on the ionic and faradaic resistances, R i and R F , that determine together the value of R app , CL – an , the apparent resistance of the anode catalyst layer. The latter resistance drops ten times between 60 °C and 120 °C as result mainly of the drop in R F . Consequently, DAFC performance at T cell > 100 °C improves substantially, including the cell performance on a KOH-free anode feed. The demsontrated performance levels reported here for KOH-free DAFCs support further development of this type of ammonia/air fuel cells.

Achrai, Ben↗